Durability of concrete containing recycled concrete coarse and fine aggregates and milled waste glass in magnesium sulfate environment
The DOI matches its Crossref record; 64 of the 64 references it cites were found in a registry or an index.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Citations
Cites
Etxeberria, M., Vázquez, E., Marí, A., & Barra, M. (2007) · Cement and Concrete Research · doi:10.1016/j.cemconres.2007.02.002 · Cited by 1,774
Mechanical behaviour of concrete made with fine recycled concrete aggregates
Evangelista, L., & de Brito, J. (2007) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2006.12.004 · Cited by 1,059
Performance of concrete made with commercially produced coarse recycled concrete aggregate
Sagoe-Crentsil, K. K., Brown, T., & Taylor, A. H. (2001) · Cement and Concrete Research · doi:10.1016/s0008-8846(00)00476-2 · Cited by 772
Mechanical properties of concrete with recycled coarse aggregate
Rahal, K. (2007) · Building and Environment · doi:10.1016/j.buildenv.2005.07.033 · Cited by 762
Studies on concrete containing ground waste glass
Shao, Y., Lefort, T., Moras, S., & Rodriguez, D. (2000) · Cement and Concrete Research · doi:10.1016/s0008-8846(99)00213-6 · Cited by 742
Influence of parent concrete on the properties of recycled aggregate concrete
Padmini, A. K., Ramamurthy, K., & Mathews, M. S. (2008) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2008.03.006 · Cited by 711
Porosity of recycled concrete with substitution of recycled concrete aggregate
Gómez-Soberón, J. M. (2002) · Cement and Concrete Research · doi:10.1016/s0008-8846(02)00795-0 · Cited by 702
Utilization of waste glass powder in the production of cement and concrete
Aliabdo, A. A., Elmoaty, A. E. M. A., & Aboshama, A. Y. (2016) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2016.08.016 · Cited by 649
Waste glass powder as partial replacement of cement for sustainable concrete practice
Islam, G. M. S., Rahman, M. H., & Kazi, N. (2017) · International Journal of Sustainable Built Environment · doi:10.1016/j.ijsbe.2016.10.005 · Cited by 641
Mechanism of expansion associated with ettringite formation
Mehta, P. K. (1973) · Cement and Concrete Research · doi:10.1016/0008-8846(73)90056-2 · Cited by 601
Research works printed but not linked: 2
- Francis, 2017, Study on the effect of replacement of portland cement by sugar cane bagasse ash ad EGG shell powder on HPC, IJSER, 8, 878
- Singh, 2017, Review on the feasibility of marble dust as replacement of cement in concrete, Int. J. Curr. Eng. Technol., 7, 2119
Cited by
Recycling of waste glass as aggregate in cement-based materials
Harrison, E., Berenjian, A., & Seifan, M. (2020) · Environmental Science and Ecotechnology · doi:10.1016/j.ese.2020.100064 · Cited by 220
“[25] found that 30% replacement of cement for milled waste glass by weight can significantly lower the compressive strengths at 28 and 300 days, having a strength reduction of 40% and 42%, respectively.”
BackgroundMechanical Behavior of Crushed Waste Glass as Replacement of Aggregates
Çelik, A. İ., Özkılıç, Y. O., Zeybek, Ö., Karalar, M., Qaidi, S., Ahmad, J., Burduhos-Nergiș, D. D., & Bejinariu, C. (2022) · Materials · doi:10.3390/ma15228093 · Cited by 202
“, examining 30% of cement by weight for ground CWG, found that the replacement had a strength reduction of 40% and 42%, respectively [34].”
BackgroundCharacteristics of hemp fibre reinforced foam concretes with fly ash and Taguchi optimization
Gençel, O., Bayraktar, O. Y., Kaplan, G., Benli, A., Martínez‐Barrera, G., Brostow, W., Tek, M., & Bodur, B. (2021) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2021.123607 · Cited by 172
Amin, M., Agwa, I. S., Mashaan, N. S., Qaidi, S., & Abd-Elrahman, M. H. (2023) · Sustainability · doi:10.3390/su15043085 · Cited by 166
Waste Glass in Cement and Geopolymer Concretes: A Review on Durability and Challenges
Siddika, A., Hajimohammadi, A., Mamun, M. A. A., Alyousef, R., & Ferdous, W. (2021) · Polymers · doi:10.3390/polym13132071 · Cited by 153
“However, concrete can be vulnerable to sulphate attack, as it degrades the hydration products, decalcifies C–S–H products, and pronounces leaching, which is more vulnerable to magnesium sulfate sulphate attack than sodium [65].”
BackgroundThe Durability of Recycled Fine Aggregate Concrete: A Review
Bu, C., Liu, L., Lu, X., Zhu, D., Sun, Y., Yu, L., OuYang, Y., Cao, X., & Wei, Q. (2022) · Materials · doi:10.3390/ma15031110 · Cited by 123
“exhibits particle stability but will reduce the hydration rate; in contrast, GGBFS has the best impermeability performance with the addition of 5% MgO chloride ions in a 15% FA admixture, and this is because MgO promotes the AAS hydration reaction, which fills the pores of concrete and thus increases the density of th…”
BackgroundSabbrojjaman, M., Liu, Y., & Tafsirojjaman, T. (2024) · Developments in the Built Environment · doi:10.1016/j.dibe.2024.100371 · Cited by 98
Bameri, M., Rashidi, S., Mohammadhasani, M., Maghsoudi, M., Madani, H., & Rahmani, F. (2022) · Advances in Materials Science and Engineering · doi:10.1155/2022/2730391 · Cited by 96
Liu, K., Dai, Z., Zhang, R., Zheng, J., Jiang, Z. J., & Yang, X. (2021) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2021.125917 · Cited by 92
Siddika, A., Hajimohammadi, A., Ferdous, W., & Sahajwalla, V. (2021) · Polymers · doi:10.3390/polym13223935 · Cited by 92
Bayraktar, O. Y., Kaplan, G., & Benli, A. (2021) · Journal of Building Engineering · doi:10.1016/j.jobe.2021.103924 · Cited by 84
Exploring the use of mixed waste materials (MWM) in concrete for sustainable Construction: A review
Jahami, A., & Issa, C. A. (2023) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2023.132476 · Cited by 80
A Systematic Review of the Concrete Durability Incorporating Recycled Glass
Mansour, M. A., Ismail, M. H., Latif, Q. B. A. I., Alshalif, A. F., Milad, A. A., & Bargi, W. A. A. (2023) · Sustainability · doi:10.3390/su15043568 · Cited by 68
Properties of concrete with waste glass after exposure to elevated temperatures
Li, S., Zhang, J., Du, G., Mao, Z., Ma, Q., Luo, Z., Miao, Y. Y., & Duan, Y. (2022) · Journal of Building Engineering · doi:10.1016/j.jobe.2022.104822 · Cited by 67
Ho, L. S., & Huynh, T. (2022) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2022.133144 · Cited by 66
Al-Shwaiter, A., Awang, H., & Khalaf, M. A. (2022) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2022.126482 · Cited by 55
Zhao, H., Li, W., Gan, Y., Wang, K., & Luo, Z. (2023) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2023.131904 · Cited by 51
Thermal and mechanical performance of cool concrete pavements containing waste glass
Balan, L. A., Anupam, B. R., & Sharma, S. K. (2021) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2021.123238 · Cited by 49
Bao, J., Li, S., Yu, Z., Xu, J., Li, Y., Zhang, P., Si, Z., & Gao, S. (2021) · Journal of Building Engineering · doi:10.1016/j.jobe.2021.103373 · Cited by 43
Incorporation of Waste Glass Powder in the Sustainable Development of Concrete
Sivasuriyan, A., & Koda, E. (2025) · Materials · doi:10.3390/ma18143223 · Cited by 42
“Mostofinejad et al. [79] initially analyzed the strength of concrete containing shredded waste glass and coarse and fine recycled aggregates when exposed to magnesium sulfate.”
Properties of sustainable self-compacting concrete made with rice husk ash
Sandhu, R. K., & Siddique, R. (2021) · European Journal of Environmental and Civil engineering · doi:10.1080/19648189.2021.1955747 · Cited by 39
“Magnesium sulphate was selected for this study because it had a more aggressive effect on the concrete when exposed to it as compared to the sodium sulphate solution (Mostofinejad et al., 2020).”
BackgroundInfluentialPerformance evaluation of concrete with waste glass after elevated temperatures
Wu, D., Mao, Z., Zhang, J., Li, S., & Ma, Q. (2023) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2023.130486 · Cited by 39
Jia, Z., Cunha, S., de Aguiar, J. L. B., & Shi, C. (2025) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2025.106135 · Cited by 38
Energy evolution of concrete with cold joint under the action of sulfate dry-wet cycles with loading
Qin, Y., Men, B., Liang, D., Geng, K., Zhang, X., Zhou, H., & Liu, R. (2023) · Journal of Building Engineering · doi:10.1016/j.jobe.2023.106098 · Cited by 37
Deng, C. B., Li, L., Wang, X., Tan, Y., Zhou, Y., Xu, Z., Zhang, D., & Yan, W. (2026) · Waste and Biomass Valorization · doi:10.1007/s12649-026-03501-6 · Cited by 37
Durgun, M. Y., & Sevinç, A. H. (2022) · Journal of Building Engineering · doi:10.1016/j.jobe.2022.104849 · Cited by 34
Elsayed, M., Tayeh, B. A., Taha, Y., & El‐Azim, A. A. (2022) · Structures · doi:10.1016/j.istruc.2022.10.077 · Cited by 33
Semi-flexible pavement with glass for alleviating the heat island effect
Peng, B., Li, J., Ling, T., Li, X., Diao, H., & Huang, X. (2023) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2022.130275 · Cited by 30
Chen, W., Wang, Q., Huang, Z., & Du, H. (2024) · Journal of Sustainable Cement-Based Materials · doi:10.1080/21650373.2023.2295506 · Cited by 29
Que, Y., Chen, X., Zhu, T., Zhang, H., Huang, W., Leung, A. K., Jiang, Z., Xue, B., & Lu, D. (2023) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2023.130305 · Cited by 29
Compatibility of waste glass with other by-products for the production of sustainable concrete
Navaneetha, E. R., Rao, P. N., & Bahurudeen, A. (2023) · Journal of Building Engineering · doi:10.1016/j.jobe.2023.107922 · Cited by 29
Thermal and mechanical performance of cement concrete pavements containing PVC-glass mix
Anupam, B. R., Balan, L. A., & Sharma, S. K. (2021) · Road Materials and Pavement Design · doi:10.1080/14680629.2020.1868328 · Cited by 28
“Researches indicate that the recycled glass wastes can be incorporated in asphalt concrete (Ziari et al., 2020), cement concrete (Mostofinejad et al., 2020), sub-base (Saberian et al., 2020), tiles, masonry blocks, paving blocks (Arulrajah et al., 2018), backfilling, and other decorative purposes…”
BackgroundMen, B., Qin, Y., Zhang, X., Wu, J., Liang, D., Li, M., & Zhou, H. (2023) · Journal of Building Engineering · doi:10.1016/j.jobe.2023.106770 · Cited by 27
Recycled Glass as a Substitute for Quartz Sand in Silicate Products
Borek, K., Czapik, P., & Dachowski, R. (2020) · Materials · doi:10.3390/ma13051030 · Cited by 27
“with Portland cement can, however, cause a decline in concrete strength due to the alkaline reaction, which depends on time [13].”
BackgroundHu, Y., Li, J., Gao, P., Zhan, B., Yu, Y., Yang, Y., Li, H., & Yu, Q. (2024) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2024.134983 · Cited by 19
Liu, K., Fu, K., Bao, J., Chen, C., Zhang, R., & Sang, Y. (2025) · Journal of Building Engineering · doi:10.1016/j.jobe.2024.111664 · Cited by 17
Urrego, Y. F. S., Delvasto, S., Valencia-Saavedra, W. G., & Araya-Letelier, G. (2023) · Journal of Materials in Civil Engineering · doi:10.1061/jmcee7.mteng-15741 · Cited by 17
Deng, Z. (2024) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2024.137134 · Cited by 16
Long-Term Sulfate Resistance of Blended Cement Concrete with Waste Glass Powder
Shalan, A. H., & El-Gohary, M. M. (2022) · Practice Periodical on Structural Design and Construction · doi:10.1061/(asce)sc.1943-5576.0000731 · Cited by 16
Verma, N., Eswari, S., & Mahapatra, C. (2025) · Sustainable materials and technologies · doi:10.1016/j.susmat.2025.e01465 · Cited by 15
Ghazy, A., Emara, M. R., Abdellah, A. M., & Attia, M. I. E.-S. (2024) · Iranian Journal of Science and Technology Transactions of Civil Engineering · doi:10.1007/s40996-024-01426-5 · Cited by 15
“Despite its widespread use, there has been growing concern about the environmental impact of concrete production and its constituents due to the substantial energy requirements and the associated carbon dioxide (CO 2 ) emissions (Mostofinejad et al. 2020).”
Sebsadji, S. K. (2022) · Powder Technology · doi:10.1016/j.powtec.2022.117756 · Cited by 14
Zhao, H., Li, W., Gan, Y., Mahmood, A. H., Zhao, X., & Wang, K. (2024) · Journal of Materials in Civil Engineering · doi:10.1061/jmcee7.mteng-16956 · Cited by 12
Sustainable concrete incorporating waste glass powder and recycled aggregate: performance evaluation
Raman, S., Nateriya, R., & Rathore, Y. (2025) · Procedia Structural Integrity · doi:10.1016/j.prostr.2025.08.055 · Cited by 12
Creating Sustainable Ultra-High-Performance Concrete (UHPC) Utilizing Recycled Glass
Ismaeel, A. M., Usman, F., Hayder, G., & Al-Ani, Y. (2024) · Civil and Environmental Engineering · doi:10.2478/cee-2024-0084 · Cited by 12
Comparison of partially replaced concrete by waste glass with control concrete
Manzoor, A., Kumar, Y., & Sharma, L. (2022) · Materials Today Proceedings · doi:10.1016/j.matpr.2022.09.092 · Cited by 12
Kho, Y. S., Wong, K. S., Pauzi, N. N. M., Joo, M. S., & Hadibarata, T. (2024) · Iranian Journal of Science and Technology Transactions of Civil Engineering · doi:10.1007/s40996-024-01660-x · Cited by 11
“Furthermore, the reconstruction of the old and damaged concrete structures extensively is impractical due to the deficiency of natural resources (Wang et al. 2023; Mostofinejad et al. 2020).”
Sulfate resistance of ultrahigh-performance concrete with recycled fine aggregate
Zhang, B., Ma, Y., Lyu, G., Wu, S., Jiang, H., Hu, Y., & Ji, T. (2022) · Advances in Cement Research · doi:10.1680/jadcr.21.00187 · Cited by 11
Srikanth, K. S., & Lalitha, G. (2021) · Materials Today Proceedings · doi:10.1016/j.matpr.2021.11.594 · Cited by 10
Effectiveness of Bacteria-Based Self-healing Concrete Under Corrosive Environment
Philip, N., R, G. V., & Syriac, T. (2023) · Iranian Journal of Science and Technology Transactions of Civil Engineering · doi:10.1007/s40996-023-01248-x · Cited by 10
Tao, X. (2024) · AIP Advances · doi:10.1063/5.0214890 · Cited by 8
Potentials of upcycling Photovoltaic panels waste in construction: A comparative review
Refaat, O. A., Dai, J., Wang, Y., Dai, J., & Alrefaei, Y. (2026) · Developments in the Built Environment · doi:10.1016/j.dibe.2026.100845 · Cited by 8
Eco-efficient roller-compacted concrete with recycled aggregates and fiber reinforcement
Ahıskalı, M., Bayraktar, O. Y., Ahıskalı, A., Benli, A., & Kaplan, G. (2025) · Sustainable Chemistry and Pharmacy · doi:10.1016/j.scp.2025.102246 · Cited by 8
He, S.-Y., Diao, Y. S., He, H., Wang, J., Yang, Y., & Li, L. (2025) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2025.140083 · Cited by 8
Sustainable recycled aggregate concrete materials and structures
Debbarma, S., Chong, B. W., Shi, X., Singh, S., & Brand, A. S. (2024) · Elsevier eBooks · doi:10.1016/b978-0-443-15672-4.00007-3 · Cited by 7
Alite and Belite obtained from the sludge of a paper recycling process
Pelisser, C., Pelisser, G., Colpani, G. L., Batiston, E. R., Silva, L. L., Fiori, M. A., & de Mello, J. M. M. (2020) · Journal of Material Cycles and Waste Management · doi:10.1007/s10163-020-01016-3 · Cited by 7
Navaneetha, E. R., Rao, P. N., & Bahurudeen, A. (2026) · Progress in Engineering Science · doi:10.1016/j.pes.2026.100223 · Cited by 7
Zhang, S., Chen, S., Min, L., Liu, Y., Rui, H., & Zhang, H. (2024) · Case Studies in Construction Materials · doi:10.1016/j.cscm.2024.e03977 · Cited by 7
Mechanical, durability and solar reflectance properties of colored self‒compacting concrete
Yildizel, S. A. (2023) · Challenge Journal of Concrete Research Letters · doi:10.20528/cjcrl.2023.03.003 · Cited by 6
“These results are also compatible with the literature results (Zhao et al. 2019; Yang et al. 2023; Mostofinejad et al. 2020).”
ResultThe Effect of Sulfate Attack on Physical Properties of Concrete
Kanaujia, P., Banerjee, R., Husain, S. M. A., & Ahmed, S. (2021) · International Journal of Recent Technology and Engineering (IJRTE) · doi:10.35940/ijrte.b6092.0710221 · Cited by 5
Engineering properties of hybrid foam concrete based on waste glass powder and red pine cone powder
Ahıskalı, M., Türkel, İ., Bayrak, B., Ibrahim, S. A., Bayraktar, O. Y., Özel, H. B., Şevik, H., & Kaplan, G. (2025) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2025.144386 · Cited by 5
Xie, S., Chen, Z., Qiu, W., Chen, P., Yuan, C., Wang, C., Ding, S., Zhao, G., Tan, Q., & Wei, F. (2025) · Sustainable materials and technologies · doi:10.1016/j.susmat.2025.e01595 · Cited by 5
State of the Art on Waste Glass Powder as Supplementary Cementitious Material
Ying, J., Yuan, T., Yiting, J., & Fan, L. (2023) · Engineering Science & Technology · doi:10.37256/est.4220232929 · Cited by 4
Singh, N., Choudhury, T., & Roy, A. B. D. (2024) · Iranian Journal of Science and Technology Transactions of Civil Engineering · doi:10.1007/s40996-024-01504-8 · Cited by 4
“Studies have shown optimal performance or turning points at these specific percentages (Habibur Rahman Sobuz et al 2022; Liu et al. 2022; Mostofinejad et al. 2020).”
Zhao, G., Chen, L., Chen, Z., Fang, Y., Zhu, J., Gu, G., Bao, L., Wei, F., & Liu, G. (2026) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2026.145891 · Cited by 3
Zhang, Z., Jiang, Y., Zou, Y., Zhou, H., Yang, J., Li, Y., & Xia, J.-R. (2026) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2026.146998 · Cited by 3
Comprehensive review of LCA studies in Civil Engineering
Thapa, I., Baral, N. P., & Adhikari, K. R. (2023) · BIBECHANA · doi:10.3126/bibechana.v20i3.58552 · Cited by 3
Self-Healing and Sustainable Concrete: A Synergistic Approach with Waste and Microbes
Priyadharsini, P., Anjali, R., Venkatesan, G., & Antonyraj, A. P. M. (2025) · Iranian Journal of Science and Technology Transactions of Civil Engineering · doi:10.1007/s40996-025-01871-w · Cited by 3
“Additionally, replacing fine aggregates with quarry dust up to 50% has been found to improve compressive strength by approximately 5%, attributed to the pozzolanic properties of quarry dust that promote additional calcium silicate hydrate formation (Umar et al. 2025; Mostofinejad et al. 2020).”
Hasan, A. A. A. J., Syamsir, A., Woen, E. L., Najeeb, M. I., & Anggraini, V. (2025) · Revue des composites et des matériaux avancés · doi:10.18280/rcma.350315 · Cited by 3
Baba, S., Dauda, S., & Duah, H. K. (2026) · The Extractive Industries and Society · doi:10.1016/j.exis.2026.101885 · Cited by 3
Gangaraju, H., & Avirneni, D. (2026) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2026.146574 · Cited by 3
Glass as a sustainable supplementary material in cementitious and geopolymer composites: a review
Elyazidi, A., Berroug, F., Cherif, R., & Bouferra, R. (2026) · Journal of Sustainable Cement-Based Materials · doi:10.1080/21650373.2026.2671349 · Cited by 3
“%) along with recycled fine aggregate improved sulfate resistance by reducing expansion and water absorption, the recycled aggregate restricted expansions from sulfate attack, while the pozzolanic action of WGP consumed calcium hydroxide, minimizing the formation of gypsum and ettrin-gite [124].”
ÇINAR, E., DÜNDAR, B., & Uygunoğlu, T. (2021) · Mühendislik Bilimleri ve Tasarım Dergisi · doi:10.21923/jesd.711026 · Cited by 3
Surendran, H., & Akhas, P. K. (2025) · European Journal of Environmental and Civil engineering · doi:10.1080/19648189.2025.2551981 · Cited by 3
Gebremedhin, M. D., & Eryürük, K. (2024) · Iranian Journal of Science and Technology Transactions of Civil Engineering · doi:10.1007/s40996-024-01587-3 · Cited by 2
“The water permeability of concrete specimens decreases with an increase in Mill-Rejected Granular Cement (MRGC) content, both for uncracked specimens and after the crack-healing period (Asrat and Ghebrab 2020; Mostofinejad et al. 2020).”
Davoudi, S. A. M. (2020) · Zenodo (CERN European Organization for Nuclear Research) · doi:10.5281/zenodo.5801589 · Cited by 2
Nano/Microscopic Investigation on the Interfacial Transition Zones in Modelled Aggregate Concrete
Li, W., Zhao, H., & Wang, K. (2025) · Springer eBooks · doi:10.1007/978-981-96-2917-6_8 · Cited by 2
Benarchid, M. Y., Taha, Y., Zidol, A., Tagnit‐Hamou, A., & Benzaazoua, M. (2023) · Elsevier eBooks · doi:10.1016/b978-0-323-91283-9.00001-8 · Cited by 2
Bacterial Solution in GGBS Concrete: A Sustainable Approach to Improving Properties
Gupta, N., Parashar, A. K., Yadav, B., Rusia, S., Saxena, K. K., Rakesh, C., & Srinivas, T. (2025) · Iranian Journal of Science and Technology Transactions of Civil Engineering · doi:10.1007/s40996-025-01859-6 · Cited by 2
“…is substantial, it is necessary to repair the cracks or incorporate additional rein-forcements into the design (Hosseini Balam et al. 2017a; Mostofinejad et al. 2020; Nosouhian et al. 2016; Nosouhian and Mostofinejad 2016) An automated method for crack control in concrete could result in…”
Strength prediction of recycled aggregate concrete under sulfate attack using SVR–NSGA-II
Jin, L., Liu, P., Yang, B., Zhang, Y., Zhou, P., Xue, P., & Liu, X. (2025) · Canadian Journal of Civil Engineering · doi:10.1139/cjce-2024-0487 · Cited by 2
Recycled Glass in Cementitious Composites: A Sustainable Alternative to Natural Aggregates
dos Santos, V. C., Gonçalves, W. R., Rangel, F., de Azevedo, T. M., Renó, M. L. G., & Penha, R. N. (2025) · Environmental Quality Management · doi:10.1002/tqem.70167 · Cited by 2
Alhassan, A., Abdulazeez, A. A., Yusuf, K. O., & Usman, S. (2023) · Zenodo (CERN European Organization for Nuclear Research) · doi:10.5281/zenodo.8227872 · Cited by 1
Enhancing Strength and Durability of Cement Concrete Using Metakaolin, Waste Glass, and Glass Fibres
Yashpal, K., & Bajpai, R. (2025) · Cuestiones de Fisioterapia · doi:10.48047/4sy3h144 · Cited by 1
KAYIHAN, M. R., DÜNDAR, B., & ÇINAR, E. (2025) · Sinop Üniversitesi Fen Bilimleri Dergisi · doi:10.33484/sinopfbd.1602495 · Cited by 1
Que, Y., Huang, H., Liao, J., Lin, Y., & Jiang, Z. (2026) · Journal of Materials in Civil Engineering · doi:10.1061/jmcee7.mteng-19104 · Cited by 1
Chen, A., Xi, Z., Zhan, J., & Han, X. (2026) · International Journal of Concrete Structures and Materials · doi:10.1186/s40069-026-00943-z · Cited by 1
“Nevertheless, RCA’s high water absorption, low strength, and potential durability issues limit its broader application (Mostofinejad et al., 2020; Ortolan et al., 2023; Yu et al., 2020).”
Behaviour Of Concrete by Substituting Recycled Plastic Granules for Coarse Aggregate
Ramesh, S., & Lakshan, S. (2023) · E3S Web of Conferences · doi:10.1051/e3sconf/202339903012 · Cited by 1
Krishna, J., Madhavi, Y., & Chaitanya, B. (2025) · International Journal For Multidisciplinary Research · doi:10.36948/ijfmr.2025.v07i03.49095
Diao, Y. S., He, S., Zou, Y., & Yan, Z. (2025) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2025.142838
Isa, M. N., Awang, H., & Yi, T. Y. (2024) · Research on Engineering Structures and Materials · doi:10.17515/resm2024.451me0920rs
A Critical Review on Utilization of Recycled Fine Aggregates in Concrete
Tyagi, R., & Goyal, P. (2025) · Lecture notes in civil engineering · doi:10.1007/978-981-97-7206-3_2
Alhenawi, E., Al-Hinawi, A. M., Salah, Z., Alidmat, O. K. A., Elsoud, E. A., Alazaidah, R., & Al-Sayyed, R. M. H. (2025) · International Journal of Power Electronics and Drive Systems/International Journal of Electrical and Computer Engineering · doi:10.11591/ijece.v15i5.pp4965-4982
مطالعه ی اثر خواص بتن مادر بر پارامترهای مکانیکی بتن بازیافتی
صالحی, ح., جو, ن. ب., & برخورداری, ه. (2022) · Muhandisī-i ̒umrān-i Sharīf/Muhandisī-i ̒umrān-i Sharīf · doi:10.24200/j30.2021.57419.2909
Study on Mechanical Damage Characteristics of Filling Paste Under Sulfate-Load CouplingPreprint
Du, Y., Du, Y., Wang, C., Min, L., & Chen, S. (2023) · SSRN Electronic Journal · doi:10.2139/ssrn.4481387
Study on Mechanical Damage Characteristics of Filling Pasteunder Sulfate-Load CouplingPreprint
Du, Y., Du, Y., Wang, C., Min, L., & Chen, S. (2023) · SSRN Electronic Journal · doi:10.2139/ssrn.4586526
Wang, Y., Yin, X., Zhao, Y. M., Lin, Q., & Bao, Y. (2025) · Scientific Reports · doi:10.1038/s41598-025-18519-4
Shear Strength of RC Beam with Recycled Glass under Sulfate Attacks
Naser, F. H., Naser, M. H., Hussein, M. J., Almamoori, A. H. N., & Hussein, M. L. (2025) · IOP Conference Series Earth and Environmental Science · doi:10.1088/1755-1315/1545/1/012083
“Mostofinejad et al. [23] proved that using 30% glass powder as a substitute for cement reduces the mass loss in concrete exposed to a 14.7% MgSO 4 solution for 300 days.”
InfluentialExperimental analysis of eco-friendly mortar with industrial waste
da Silva, L. F. B. P. (2024) · LA Referencia (Red Federada de Repositorios Institucionales de Publicaciones Científicas)
Quispe Sandoval, M. T., & Cordova Ymbertis, J. R. (2024) · Repositorio Académico UPC (Universidad Peruana de Ciencias Aplicadas)
Metadata
- Authors
- Mostofinejad, D., Hosseini, S. M., Nosouhian, F., Ozbakkaloglu, T., & Nader Tehrani, B.
- Affiliations
- Isfahan University of Technology (IR)
- Université de Sherbrooke (CA)
- Texas State University (US)
- Corresponding author
- Hosseini, Seyed Mohammad
- Venue
- Journal of Building Engineering
- Publisher
- Elsevier BV
- Published
- 2020-05
- Volume
- 29
- Pages
- 101182
- ISSN
- 2352-7102 (ISSN-L)
- OpenAlex
- W2999069738
- Cited by
- 111
- References
- 64
- Citations by year
- 2026: 17 · 2025: 25 · 2024: 17 · 2023: 20 · 2022: 14 · 2021: 13 · 2020: 5
- FWCI
- 6.43
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.elsevier.com/tdm/userlicense/1.0/ (tdm)
- www.elsevier.com/legal/tdmrep-license (tdm)
- Locations
- Journal of Building Engineering (publishedVersion)
- Topics
- Physical Sciences › Engineering › Building and Construction › Recycled Aggregate Concrete Performance
- Physical Sciences › Engineering › Civil and Structural Engineering › Concrete and Cement Materials Research
- Physical Sciences › Engineering › Building and Construction › Materials Engineering and Processing
- Keywords
- concrete durability, recycled concrete aggregate, recycled fine aggregate, magnesium sulfate attack, sulfate resistance, compressive strength, water absorption, expansion, partial cement replacement, waste recycling in construction
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.