Thermal runaway mechanism of lithium-ion battery with LiNi0.8Mn0.1Co0.1O2 cathode materials
Open accessThe DOI matches its Crossref record; 31 of the 31 references it cites were found in a registry or an index.
Abstract
Abstract Battery safety is critical to the application of lithium-ion batteries, especially for high energy density battery applied in electric vehicles. In this paper, the thermal runaway mechanism of LiNi0.8Co0.1Mn0.1O2 based lithium-ion battery is illustrated. And the reaction between cathode and flammable electrolyte is proved as the trigger of the thermal runaway accident. In detail, with differential scanning calorimeter tests for battery components, the material combination contributing to thermal runaway was decoupled. Characterization with synchrotron X-ray diffraction and transmission electron microscopy with in-situ heating proved that the vigorous exothermic reaction is initiated by the liberated oxygen species. The pulse of highly active oxygen species reacted quickly with the electrolyte, accompanied with tremendous heat release, which accelerated the phase transformation of charged cathode. Also, the mechanism is verified by a confirmatory experiment when the highly active oxygen species were trapped by anion receptor, the phase transformation of the charged cathode was inhibited. Clarifying the thermal runaway mechanism of LiNi0.8Co0.1Mn0.1 based lithium-ion battery may light the way to battery chemistries of both high energy density and high safety.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
30 Years of Lithium‐Ion Batteries
Li, M., Lu, J., Chen, Z., & Amine, K. (2018) · Advanced Materials · doi:10.1002/adma.201800561 · Cited by 6,039
Self-citationThermal runaway mechanism of lithium ion battery for electric vehicles: A review
Feng, X., Ouyang, M., Liu, X., Lu, L., Xia, Y., & He, X. (2018) · Energy Storage Materials · doi:10.1016/j.ensm.2017.05.013 · Cited by 4,182
Self-citationA review on the key issues of the lithium ion battery degradation among the whole life cycle
Han, X., Lu, L., Zheng, Y., Feng, X., Li, Z., Li, J., & Ouyang, M. (2019) · eTransportation · doi:10.1016/j.etran.2019.100005 · Cited by 1,745
Self-citationAbuse behavior of high-power, lithium-ion cells
Spotnitz, R., & Franklin, J. (2003) · Journal of Power Sources · doi:10.1016/s0378-7753(02)00488-3 · Cited by 1,373
Nanostructured high-energy cathode materials for advanced lithium batteries
Sun, Y.-K., Chen, Z., Noh, H.-J., Lee, D.-J., Jung, H.-G., Ren, Y., Wang, S., Yoon, C. S., Myung, S.-T., & Amine, K. (2012) · Nature Materials · doi:10.1038/nmat3435 · Cited by 1,093
Self-citationBak, S.-M., Hu, E., Zhou, Y., Yu, X., Senanayake, S. D., Cho, S.-J., Kim, K.-B., Chung, K. Y., Yang, X.-Q., & Nam, K.-W. (2014) · ACS Applied Materials & Interfaces · doi:10.1021/am506712c · Cited by 1,010
Feng, X., Fang, M., He, X., Ouyang, M., Lu, L., Wang, H., & Zhang, M. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2014.01.005 · Cited by 918
Self-citationA three-dimensional thermal abuse model for lithium-ion cells
Kim, G.-H., Pesaran, A., & Spotnitz, R. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.04.018 · Cited by 877
Thermal Runaway of Lithium-Ion Batteries without Internal Short Circuit
Liu, X., Ren, D., Hsu, H., Feng, X., Xu, G.-L., Zhuang, M., Gao, H., Lu, L., Han, X., Chu, Z., et al. (2018) · Joule · doi:10.1016/j.joule.2018.06.015 · Cited by 869
Self-citationFeng, X., Zheng, S., Ren, D., He, X., Wang, L., Cui, H., Liu, X., Jin, C., Zhang, F., Xu, C., et al. (2019) · Applied Energy · doi:10.1016/j.apenergy.2019.04.009 · Cited by 771
Self-citation
Cited by
Designing safer lithium-based batteries with nonflammable electrolytes: A review
Zhang, S., Li, S., & Lu, Y. (2021) · eScience · doi:10.1016/j.esci.2021.12.003 · Cited by 337
Challenges and Opportunities to Mitigate the Catastrophic Thermal Runaway of High‐Energy Batteries
Wang, Y., Feng, X., Huang, W., He, X., Wang, L., & Ouyang, M. (2023) · Advanced Energy Materials · doi:10.1002/aenm.202203841 · Cited by 252
Self-citationUnlocking the self-supported thermal runaway of high-energy lithium-ion batteries
Hou, J., Feng, X., Wang, L., Liu, X., Ohma, A., Lu, L., Ren, D., Huang, W., Li, Y., Yi, M., et al. (2021) · Energy Storage Materials · doi:10.1016/j.ensm.2021.04.035 · Cited by 221
“Before the combination, O * could react with EC and the electrolyte 51 .”
Self-citationReductive gas manipulation at early self-heating stage enables controllable battery thermal failure
Wang, Y., Feng, X., Peng, Y., Zhang, F., Ren, D., Liu, X., Lu, L., Nitta, Y., Wang, L., & Ouyang, M. (2022) · Joule · doi:10.1016/j.joule.2022.10.010 · Cited by 213
Self-citationSchomburg, F., Heidrich, B., Wennemar, S., Drees, R., Roth, T., Kurrat, M., Heimes, H., Jossen, A., Winter, M., Cheong, J. Y., et al. (2024) · Energy & Environmental Science · doi:10.1039/d3ee03559j · Cited by 193
Ouyang, D., Chung, Y.-H., Liu, J., Bai, J., Zhou, Y., Chen, S., Wang, Z., & Shu, C.-M. (2025) · Progress in Energy and Combustion Science · doi:10.1016/j.pecs.2025.101209 · Cited by 191
Self-citationMolecular anchoring of free solvents for high-voltage and high-safety lithium metal batteries
Cui, Z., Jia, Z., Ruan, D., Nian, Q., Fan, J., Chen, S., He, Z., Wang, D., Jiang, J., Ma, J., et al. (2024) · Nature Communications · doi:10.1038/s41467-024-46186-y · Cited by 161
Wang, H., Xu, H., Zhao, Z., Wang, Q., Jin, C., Li, Y., Sheng, J., Li, K., Du, Z., Xu, C., et al. (2022) · Applied Thermal Engineering · doi:10.1016/j.applthermaleng.2022.118418 · Cited by 87
Self-citation
Metadata
- Authors
- Li, Y., Liu, X., Wang, L., Feng, X., Ren, D., Wu, Y., Xu, G., Lu, L., Hou, J., Zhang, W., Wang, Y., Xu, W., Ren, Y., Wang, Z., Huang, J., Meng, X., Han, X., Wang, H., He, X., Chen, Z., Amine, K., & Ouyang, M.
- Venue
- Nano Energy
- Publisher
- Elsevier BV
- Published
- 2021-07
- Volume
- 85
- Pages
- 105878
- ISSN
- 2211-2855 (ISSN-L)
- OpenAlex
- W3133457690
- Cited by
- 315
- References
- 31
- FWCI
- 14.59
- Type
- journal article
- Language
- en
- Open access
- bronze
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.