The DOI matches its Crossref record; 1 of the 1 references it cites were found in a registry or an index.
The oxidation behaviour of metals and alloys at high temperatures in atmospheres containing water vapour: A review
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Citations
Cites
Asteman, H., Svensson, J.-E., Norell, M., & Johansson, L.-G. (2000) · Oxidation of Metals · doi:10.1023/a:1004642310974 · Cited by 325
Research works printed but not linked: 145
- Larring, 2003, HT corrosion of Cr–5wt%Fe–1wt% Y2O3 alloy and conductivity of the oxide scale – effects of water vapor, J Electrochem Soc, 150, B374, 10.1149/1.1587726 · DOI
- Douglass, 1996, International workshop on high temperature oxidation – subject area 1: the role of water vapour in the oxidation of metals and alloys, Oxid Met, 45, 529, 10.1007/BF01046850 · DOI
- Buscail, 1997, Water-vapor-effect on the oxidation of Fe 21.5wt.% Cr, 5.6wt.%Al at 1000°C, Oxid Met, 47, 445, 10.1007/BF02134786 · DOI
- Al-Badairy, 2000, The influence of the moisture content of the atmosphere on alumina scale formation and growth during high temperature oxidation of PM2000, Mater High Temp, 17, 133, 10.1179/mht.2000.020 · DOI
- Boggs, 1977, The oxidation of iron aluminium alloys from 450°C to 900°C, J Electrochem Soc, 118, 906, 10.1149/1.2408222 · DOI
- Onal, 2003, Water vapor effects on the cyclic oxidation resistance of alumina forming alloys, Mater High Temp, 20, 81, 10.1179/mht.2003.039 · DOI
- Janakiraman, 1999, The effect of water vapor on the oxidation of alloys that develop alumina scales for protection, Metall Mater Trans A, 30A, 2905, 10.1007/s11661-999-0128-3 · DOI
- Smialek, 2002, Delayed alumina scale spallation on Rene’N5+Y: moisture effects and acoustic emission, Mater Sci Eng, A332, 11, 10.1016/S0921-5093(01)01712-9 · DOI
- Kvernes, 1977, High temperature oxidation of Fe13CrxAl alloys in Air/H2O vapour mixtures, Corrosion Sci, 17, 237, 10.1016/0010-938X(77)90049-X · DOI
- Regina, 2004, The effect of water vapor on passive-layer stability and corrosion behavior of Fe–Al–Cr base alloys, Oxid Met, 61, 69, 10.1023/B:OXID.0000016277.86061.25 · DOI
- Regina, 2005, Gaseous corrosion resistance of Fe–Al based alloys containing Cr additions. Part II: Scale morphology, Mater Sci Eng A, 405, 102, 10.1016/j.msea.2005.05.085 · DOI
- Zhang, 2004, The effect of water vapor on the oxidation behavior of CVD iron–aluminide coatings, Oxid Met, 62, 103, 10.1023/B:OXID.0000038788.02094.cb · DOI
- Zhou, 2002, Influence of water vapor on the isothermal oxidation behavior of low pressure plasma sprayed NiCrAlY coating at high temperature, Surf Coat Technol, 161, 86, 10.1016/S0257-8972(02)00398-5 · DOI
- Leyens, 1996, Oxide scale formation on an MCrAlY coating in various H2–H2O atmospheres, Surf Coat Technol, 82, 133, 10.1016/0257-8972(95)02665-7 · DOI
- Liu, 2004, Oxidation behavior of TiAl(Cr,Ag) at 900°C in water vapor, Intermetallics, 12, 459, 10.1016/j.intermet.2003.10.008 · DOI
- Å´kermark, 1997, Oxygen exchange in oxidation of an Fe–20Cr–10Al alloy in mbar O2/H2O–gas mixtures at 920°C, Oxid Met, 47, 117, 10.1007/BF01682374 · DOI
- Jacob, 2002, The effect of gas composition on the isothermal oxidation behaviour of PM chromium, Corros Sci, 44, 2027, 10.1016/S0010-938X(02)00022-7 · DOI
- Hultquist, 2000, Hydrogen in chromium: influence on the high-temperature oxidation kinetics in H2O, oxide-growth mechanisms, and scale adherence, Oxid Met, 54, 1, 10.1023/A:1004610626903 · DOI
- Henry, 2000, Characterization of chromia scales grown on pure chromium in different oxidizing atmospheres, Mater High Temp, 17, 231, 10.3184/096034000783640866 · DOI
- Hänsel, 2003, Role of water vapor in chromia-scale growth at low oxygen partial pressure, Oxid Met, 59, 285, 10.1023/A:1023040010859 · DOI
- Schütze, 2005, Chemical–mechanical failure of oxide scales on 9% Cr steels in air with H2O, Mater High Temp, 22, 113, 10.3184/096034005782750536 · DOI
- Galerie, 2005, Mechanisms of chromia scale failure during the course of 15–18Cr ferritic stainless steel oxidation in water vapour, Mater High Temp, 22, 105, 10.3184/096034005782750527 · DOI
- Fujii, 1964, The mechanism of the high temperature oxidation of iron–chromium alloys in water vapour, JECS, 111, 1215
- Źurek, 2005, The effect of water-vapor content and gas flow rate on the oxidation mechanism of a 10%Cr–ferritic steel in Ar–H2O mixtures, Oxid Met, 63, 401, 10.1007/s11085-005-4394-1 · DOI
- Mikkelsen, 2003, High temperature oxidation of Fe–Cr Alloy in O2–H2–H2O atmosphere, microstructure and kinetics, Mater Sci Eng, A361, 198, 10.1016/S0921-5093(03)00527-6 · DOI
- Cheng, 2006, Effect of water vapor on annealing scale formation on 316 SS, Corros Sci, 48, 634, 10.1016/j.corsci.2005.02.014 · DOI
- Yang, 2005, Effects of water vapor on oxidation behavior of ferritic stainless steels under solid oxide fuel cell interconnect exposure conditions, Solid State Ionics, 176, 1495, 10.1016/j.ssi.2005.03.019 · DOI
- Nakagawa, 2003, Corrosion behavior of ferritic steels on the air sides of boiler tubes in a steam/air dual environment. Proceedings of the conference “life cycle issues in advanced energy systems”, Sci Rev, 67
- Peng, 2005, Effect of grain refinement on the resistance of 304 stainless steel to breakaway oxidation in wet air, Acta Mater, 53, 5079, 10.1016/j.actamat.2005.07.019 · DOI
- Jianian, 1997, High-temperature oxidation of Fe–Cr alloys in wet oxygen, Oxid Met, 48, 347, 10.1007/BF01670507 · DOI
- Pieraggi, 2005, Morphological characteristics of oxide scales grown on H11 steel oxidised in dry or wet air, Mater High Temp, 22, 61, 10.3184/096034005782750617 · DOI
- Monteiro Maurı´cio de Jesus, Saunders Stuart, Assunção Fernando Cosme Rizzo. The effect of water vapour on the high-temperature oxidation of a high speed steel. In: Proceedings of ABM 2006; 2006. p. 128–37.
- Zeng, 1994, High-temperature corrosion of Cr2O3-forming alloys in CO–CO2–N2 atmospheres, Oxid Met, 42, 163, 10.1007/BF01052021 · DOI
- Yang, 2004, Oxidation behaviour of ferritic stainless steels under SOFC interconnect exposure conditions, J Electrochem Soc, 151, B669, 10.1149/1.1810393 · DOI
- Ehlers, 2006, Enhanced oxidation of the 9%Cr steel P91 in water vapour containing environments, Corrosion Sci, 48, 3428, 10.1016/j.corsci.2006.02.002 · DOI
- Asteman, 2002, Evidence for chromium evaporation influencing the oxidation of 304L: the effect of temperature and flow rate, Oxid Met, 57, 193, 10.1023/A:1014877600235 · DOI
- Halvarsson, 2006, Microstructural investigation of the breakdown of the protective oxide scale on a 304 steel in the presence of oxygen and water vapour at 600°C, Corrosion Sci, 48, 2014, 10.1016/j.corsci.2005.08.012 · DOI · Paper page
- Asteman, 2002, Oxidation of 310 steel in H2O/O2 mixtures at 600°C: the effect of water-vapour-enhanced chromium evaporation, Corrosion Sci, 44, 2635, 10.1016/S0010-938X(02)00056-2 · DOI · Paper page
- Segerdahl, 2005, Breakdown of the protective oxide on 11% Cr steel at high temperature in the presence of water vapor and oxygen, the influence of chromium vaporization, Mater High Temp, 22, 69, 10.3184/096034005782750572 · DOI
- Yamauchi, 2003, Evaporation of Cr2O3 in atmospheres containing H2O, Oxid Met, 59, 517, 10.1023/A:1023671206976 · DOI
- Opila, 2004, Volatility of common protective oxides in high-temperature water vapor: current understanding and unanswered questions, Mater Sci Forum, 461–464, 765, 10.4028/www.scientific.net/MSF.461-464.765 · DOI
- Holcomb, 2006, The effect of manganese additions on the reactive evaporation of chromium in Ni–Cr alloys, Scripta Mater, 54, 1821, 10.1016/j.scriptamat.2006.01.026 · DOI
- Rahmel, 1965, Einfluss von Wasserdampf und Kohlendioxyd auf die Oxydation von Nickel in Sauerstoff bei Hohen Temperaturen, Corrosion Sci, 5, 815, 10.1016/S0010-938X(65)80011-7 · DOI
- Wood, 1970, A comparison of the oxidation of Fe–Cr, Ni–Cr and Co–Cr alloys in oxygen and water vapour, Werkstoffe und Korrosion, 21, 900, 10.1002/maco.19700211105 · DOI
- England, 2001, Oxidation kinetics of some nickel-based superalloy foils in humidified hydrogen and electronic resistance of the oxide scale formed, Part II, J Electrochem Soc, 148, A330, 10.1149/1.1354611 · DOI
- England, 1999, Oxidation kinetics of some nickel-based superalloy foils and electronic resistance of the oxide scale formed in air, Part I, J Electrochem Soc, 146, 3196, 10.1149/1.1392454 · DOI
- Hussain, 2004, High-temperature oxidation behavior of HASTELLOY C-4 in steam, Oxid Met, 61, 355, 10.1023/B:OXID.0000032328.23022.31 · DOI
- Hussain, 1994, Oxidation of high temperature alloys (superalloys) at elevated temperatures in air: 1, Oxid Met, 41, 251, 10.1007/BF01080783 · DOI
- Deal, 1965, General relationship for the thermal oxidation of silicon, J Phys, 36, 3770
- Irene, 1983, Silicon oxidation studies: a revised model for thermal oxidation, J Appl Phys, 54, 5416, 10.1063/1.332722 · DOI
- Bhat, 2001, Characterization of ultrathin oxides of silicon grown by wet oxidation at 800°C, Solid State Electron, 45, 1127, 10.1016/S0038-1101(01)00136-8 · DOI
- Sofield, 1995, Oxidation of silicon: the VLSI gate dielectric, Semicond Sci Technol, 10, 215, 10.1088/0268-1242/10/3/001 · DOI
- Kovalgin, 2005, Hof A, Schmitz J. An approach to modeling of silicon oxidation in a wet ultra-diluted ambient, Microelectron Eng, 80, 432, 10.1016/j.mee.2005.04.101 · DOI
- Hu, 1983, New oxide growth law and the thermal oxidation of silicon, Appl Phys Lett, 42, 874, 10.1063/1.93797 · DOI
- Opila, 1999, Variation of the oxidation rate of silicon carbide with water vapour pressure, J Am Ceram Soc, 82, 625, 10.1111/j.1151-2916.1999.tb01810.x · DOI
- Opila, 2004, Volatility of common protective oxides in high-temperature water vapor: current understanding and unanswered questions, Mater Sci Forum, 461–464, 65
- Robinson, 1999, SiC recession caused by SiO2 scale volatility under combustion conditions 1: experimental results and empirical model, J Am Ceram Soc, 82, 1817, 10.1111/j.1151-2916.1999.tb02004.x · DOI
- Hansson, 2005, The beneficial effect of water vapour on the oxidation at 600 and 700°C of a MoSi2-based composite, J Eur Ceram Soc, 25, 1, 10.1016/j.jeurceramsoc.2004.01.005 · DOI
- Ishitsuka, 2004, Effect of silicon on the steam oxidation resistance of a 9%Cr heat resistant steel, Oxid Met, 61, 125, 10.1023/B:OXID.0000016280.81734.3f · DOI
- Wouters, 2004, Oxygen and water vapour oxidation of 15Cr ferritic oxygen and water vapour oxidation of 15Cr ferritic stainless steels with different silicon contents, Mater Sci Forum, 461–464, 839, 10.4028/www.scientific.net/MSF.461-464.839 · DOI
- Ueda, 2005, Oxygen potential distribution during disappearance of the internal oxidation zone formed in the steam oxidation of Fe–9Cr–0.26Si ferritic steel at 973K, Mater High Temp, 22, 79, 10.3184/096034005782750545 · DOI
- Ueda, 2003, Formation and disappearance of an internal oxidation zone in the initial stage of the steam oxidation of Fe–9Cr–0.26Si ferritic steel, Mater High Temp, 20, 109, 10.3184/096034003782748964 · DOI
- Wouters, 1997, Thermal oxidation of titanium by water vapour, Solid State Ionics, 104, 89, 10.1016/S0167-2738(97)00400-1 · DOI
- Zeller, 2002, Influence of water vapour on the oxidation behaviour of titanium aluminides, Intermetallics, 10, 59, 10.1016/S0966-9795(01)00104-2 · DOI
- Taniguchi, 2001, Influence of water vapour on the isothermal oxidation behaviour of TiAl at high temperatures, Mater Sci Eng, A307, 107, 10.1016/S0921-5093(00)01967-5 · DOI
- Brady, 1997, The role of Cr in promoting protective alumina scale formation by γ-based Ti–Al–Cr Alloys – II. Oxidation behavior in air, Acta Mater, 45, 2371, 10.1016/S1359-6454(96)00361-8 · DOI
- Rahmel, 1965, Einfluss von Wasserdampf und Kohlendioxyd auf die Oxydation von Eisen in Sauerstoff bei Hohen Temperaturen, Corrosion Sci, 5, 333, 10.1016/S0010-938X(65)90500-7 · DOI
- Mrowec, 1967, On the mechanism of high temperature oxidation of metals and alloys, Corrosion Sci, 7, 563, 10.1016/0010-938X(67)80033-7 · DOI
- Tuck, 1969, The oxidation of iron at 950°C in oxygen/water vapour mixtures, Corrosion Sci, 9, 271, 10.1016/S0010-938X(69)80056-9 · DOI
- Hayashi, 2001, Competitive effect of water vapor and oxygen on the oxidation of Fe–5wt.% Al alloy at 1073K, Oxid Met, 56, 251, 10.1023/A:1010372711563 · DOI
- Fukumoto, 2001, Effect of water vapor on the oxidation behavior of Fe–1.5Si in air at 1073 and 1273K, Oxid Met, 55, 401, 10.1023/A:1010353729663 · DOI
- Hayashi, 2002, Transient oxidation behavior of Fe–5wt.%Al alloy at 1073K in atmospheres containing both oxygen and water vapor, Oxid Met, 58, 319, 10.1023/A:1020106804999 · DOI
- Raynaud, 1984, In situ observation of whiskers, pyramids and pits during high temperature oxidation of metals, Oxid Met, 21, 89, 10.1007/BF00659470 · DOI
- Tallman, 1967, J Electrochem Soc, 114, 1227, 10.1149/1.2426455 · DOI
- Quadakkers, 2005, Steam oxidation of ferritic steels – laboratory test kinetic data, Mater High Temp, 22, 47, 10.3184/096034005782750590 · DOI
- Ikeda, 1984, Mechanism of accelerated oxidation of Fe–Cr alloys in water vapour containing atmosphere, Trans Jpn Inst Met, 26, 52
- Anghel, 2006, Gas-tight oxides – reality or just a hope, Mater Sci Forum, 522–523, 93, 10.4028/www.scientific.net/MSF.522-523.93 · DOI
- Davies, 2005, Theoretical study of steam grown oxides as a function of temperature, pressure and p(O2), Mater High Temp, 22, 15, 10.3184/096034005782750455 · DOI
- Davies, 2002, MTDATA – thermodynamic and phase equilibrium software from the national physical laboratory, CALPHAD, 26, 229, 10.1016/S0364-5916(02)00036-6 · DOI
- Armitt J, Holmes DR, Manning MI, Meadowcroft DB, Metcalfe E. The spalling of steam-grown oxide from superheater and reheater tube steels. EPRI Report FP-686, February 1978. · DOI
- Tedmon, 1966, J Electrochem Soc, 113, 766, 10.1149/1.2424115 · DOI
- Tobias Johnson, 2000, Hydrolysis on transition metal oxide clusters and the stabilities of M–O–M bridges, Inorg Chem, 39, 3192, 10.1021/ic991144l · DOI
- Tobias Johnson, 2000, Water adsorption and hydrolysis on molecular transition metal oxides and oxyhydroxides, Inorg Chem, 39, 3181, 10.1021/ic991150h · DOI
- Milewska, 2004, Coating design using computational codes for steam oxidation conditions, Mater Sci Forum, 461–464, 321, 10.4028/www.scientific.net/MSF.461-464.321 · DOI
- Saunders, 2006, Current understanding of steam oxidation – power plant and laboratory experience, Mater Sci Forum, 522–523, 119, 10.4028/www.scientific.net/MSF.522-523.119 · DOI
- Pinzari, 2000, On the surface acid–base properties of titanium sheets, Appl Surf Sci, 156, 1, 10.1016/S0169-4332(99)00510-3 · DOI
- Sun, 2003, A review of the different techniques for solid surface acid–base characterization, Adv Colloid Interface Sci, 105, 151, 10.1016/S0001-8686(03)00066-6 · DOI
- Kosmulski, 2002, The pH-dependent surface charging and the points of zero charge, J Colloid Interface Sci, 253, 77, 10.1006/jcis.2002.8490 · DOI
- Kosmulski, 2004, pH-dependent surface charging and points of zero charge, II. Update, J Colloid Interface Sci, 275, 214, 10.1016/j.jcis.2004.02.029 · DOI
- Harju, 2004, Surface characterization of plasma sprayed oxide materials: estimation of surface acidity using mass titration, J Colloid Interface Sci, 276, 346, 10.1016/j.jcis.2004.03.058 · DOI
- Anghel, 2004, Gas phase analysis of CO interactions with solid surfaces at high temperatures, Appl Surf Sci, 233, 392, 10.1016/j.apsusc.2004.04.001 · DOI
- Tveten, 2001, Hydrogen and yttria in chromium: influence on the high-temperature oxidation kinetics in O2, oxide-growth mechanisms and scale adherence, Oxid Met, 55, 279, 10.1023/A:1010360111005 · DOI
- Hultquist, 2006, Catalysed self-cleaning of air on the earth’s surface, J Atmosph Chem, 55, 131, 10.1007/s10874-006-9031-0 · DOI
- Å´kermark, 1998, The use of oxygen isotopic labeling to understand oxidation mechanisms, Oxid Met, 50, 167, 10.1023/A:1018832103466 · DOI
- Larsson, 2001, Role of water and oxygen in wet and dry oxidation of diamond, J Appl Phys, 90, 026, 10.1063/1.1376671 · DOI
- Tallman, 1967, Crystal morphology and mechansims of growth of alpha-Fe2O3 whiskers on iron, J Electrochem Soc, 114, 1228
- Kofstad, 1995, Defect and transport properties in metal oxides, Oxid Met, 44, 3, 10.1007/BF01046721 · DOI
- Holt, 1999, Electrical conductivity of Cr2O3 doped with TiO2, Solid State Ionics, 117, 21, 10.1016/S0167-2738(98)00244-6 · DOI
- Holt, 1997, Electrical conductivity and defect structure of Mg-doped Cr2O3, Solid State Ionics, 100, 201, 10.1016/S0167-2738(97)00352-4 · DOI
- Norby, 1993, Protonic defects in oxides and their possible role in high temperature oxidation, J Phys IV C9, 3, 99
- Atkinson, 2003, Accommodation of impurities in α-Al2O3, α-Cr2O3 and α-Fe2O3, J Eur Ceram Soc, 23, 3059, 10.1016/S0955-2219(03)00101-8 · DOI
- Dieckmann, 2005, Solution and transport of water in oxides, Mater High Temp, 22, 93, 10.3184/096034005782750509 · DOI
- Kröger, 1956, Relations between the concentrations of imperfections in crystalline solids, Solid State Phys – Adv Res Appl, 3, 307
- El-Aiat, 1982, Determination of the parameters of native disorder in α-Al2O3, J Am Ceram Soc, 65, 162, 10.1111/j.1151-2916.1982.tb10387.x · DOI
- Pint, 2003, The use of two reactive elements to optimize oxidation performance of alumina-forming alloys, Mater High Temp, 20, 129, 10.1179/mht.2003.044 · DOI
- Kurita, 2003, Hydrogen concentration cell using α-Al2O3 as a solid electrolyte, Solid State Ionics, 162–163, 135, 10.1016/S0167-2738(03)00254-6 · DOI
- Fukatsu, 2003, Incorporation of hydrogen into magnesium-doped α-alumina, Solid State Ionics, 162–163, 147, 10.1016/S0167-2738(03)00218-2 · DOI
- Norby, 1984, High Temp High Pressures, 12, 189
- Caldararu, 2001, Electrical conductivity of γ-Al2O3 at atmospheric pressure under dehydrating/ hydrating conditions, Appl Surf Sci, 181, 255, 10.1016/S0169-4332(01)00393-2 · DOI
- Holt, 1994, Electrical conductivity and defect structure of Cr2O3. I. High temperatures (>1000°C), Solid State Ionics, 69, 127, 10.1016/0167-2738(94)90401-4 · DOI
- Holt, 1994, Electrical conductivity and defect structure of Cr2O3. II. Reduced temperatures (<1000°C), Solid State Ionics, 69, 137, 10.1016/0167-2738(94)90402-2 · DOI
- Atkinson, 2006, Defect properties of Ti-doped Cr2O3, Solid State Ionics, 177, 1767, 10.1016/j.ssi.2005.11.015 · DOI
- Haaß, 2001, High-temperature in situ X-ray absorption studies on the iron valence in iron-doped nickel oxide (Ni1−xFex)1−δO, Solid State Ionics, 141–142, 289, 10.1016/S0167-2738(01)00763-9 · DOI
- Minervini, 1999, Defect clustering in wüstite, J Phys Chem Solids, 60, 235, 10.1016/S0022-3697(98)00273-X · DOI
- Dieckmann, 1998, Point defects and transport in non-stoichiometric oxides: solved and unsolved problems, J Phys Chem Solids, 59, 507, 10.1016/S0022-3697(97)00205-9 · DOI
- Gómes-Garcı´a, 2002, The influence of oxygen partial pressure on creep recovery in magnetite single crystals, J Phys Chem Solids, 63, 185, 10.1016/S0022-3697(01)00083-X · DOI
- Dieckmann, 1993, Point defects and transport in haematite (Fe2O3−ε), Philos Mag A, 68, 725, 10.1080/01418619308213994 · DOI
- Haugsrud, 2003, On the high temperature oxidation of nickel, Corrosion Sci, 45, 211, 10.1016/S0010-938X(02)00085-9 · DOI
- Renusch, 2005, Experience with the use of the acoustic emission techniques for monitoring scale failure in wet and dry environments, Mater High Temp, 22, 34, 10.1179/mht.2005.005 · DOI
- Hughes A, Dooley RB, Paterson S. Oxide exfoliation of 347HFG in high-temperature boilers. In: Paper presented at the 7th international conference and exhibition on operating pressure equipment; 2003.
- Dooley RB. Opening remarks at the EPRI-NPL workshop on scale growth and exfoliation in steam plant. National Physical Laboratory; 2003.
- Evans, 1995, Stress effects in high temperature corrosion, Int Mater Rev, 40, 1, 10.1179/imr.1995.40.1.1 · DOI
- Lipkin, 1997, Stress development in alumina scales formed upon oxidation of (111) NiAl single crystals, Corrosion Sci, 39, 231, 10.1016/S0010-938X(97)83344-6 · DOI
- Tolpygo, 2000, Microstructural study of the theta–alpha transformation in alumina scales, Mater High Temp, 17, 59, 10.1179/mht.2000.011 · DOI
- Nishimura, 2005, Japanese experience with steam oxidation of advanced heat-resistant steel tubes in power boilers, Mater High Temp, 22, 3, 10.3184/096034005782750554 · DOI
- Schütze, 2004, Parameters determining the breakaway oxidation behaviour of ferritic martensitic 9%Cr steels in environments containing H2O, Corrosion Eng, Sci Technol, 39, 157, 10.1179/147842204225016921 · DOI
- Donchev, 2005, The effect of water vapor in increasing growth stresses in the oxide scale on martensitic steam plant alloys, Mater High Temp, 22, 139, 10.3184/096034005782750446 · DOI
- Garcia Vargas, 2004, The effect of water vapour on the oxidation of stainless steels studied in situ by X-ray diffraction, Mater Sci Forum, 461–464, 823, 10.4028/www.scientific.net/MSF.461-464.823 · DOI
- Evans, 2005, Spallation models and their relevance to steam-grown oxides, Mater High Temp, 22, 155, 10.3184/096034005782750608 · DOI
- Osgerby, 2005, Tensile cracking of a chromia layer on a stainless steel during thermal cycling with hold periods, Mater Sci Eng A, 412, 182, 10.1016/j.msea.2005.08.193 · DOI
- Tolpygo, 1999, Tensile cracking during thermal cycling of alumina films formed by high-temperature oxidation, Acta Mater, 47, 3589, 10.1016/S1359-6454(99)00216-5 · DOI
- Freiman, 1976, Effect of environment on fracture of ceramics, Ceramurgia Int, 2, 111, 10.1016/0390-5519(76)90020-X · DOI
- Grosskreutz, 1967, The effect of oxide films on dislocation–surface interactions in aluminium, Surface Sci, 8, 173, 10.1016/0039-6028(67)90080-5 · DOI
- McElhaney, 2004, Investigation of moisture-assisted fracture in SiO2 films using a channel cracking technique, Acta Mater, 52, 3621, 10.1016/j.actamat.2004.04.014 · DOI
- Otsuka, 2005, fracture behavior of steam-grown oxide scales formed on 2–12%Cr steels, Mater High Temp, 22, 131, 10.3184/096034005782750563 · DOI
- Nagl, 1993, The failure of iron oxide scales at growth temperature under tensile stress, J Phys IV, Colloque C9, Supp J Phys III, 3, 933
- Kirchheim, 2003, Metal/oxide interfaces and their reaction with hydrogen, Z Metallkd, 94, 266, 10.3139/146.030266 · DOI
- Huang, 1991, Hydrogen and oxygen at metal/oxide interfaces, Acta Metall Mater, 39, 893, 10.1016/0956-7151(91)90289-D · DOI
- Nagao, 2003, First-principles study of adhesion at Cu/SiO2 interfaces, Phys Rev B, 68, 125403-1, 10.1103/PhysRevB.68.125403 · DOI
- Backhaus-Ricoult, 2002, Changes in Cu–silica interfacial chemistry with oxygen chemical potential, Acta Mater, 50, 4191, 10.1016/S1359-6454(02)00267-7 · DOI
- Hou, 2005, A survey of test methods for scale adhesion measurement, Mater High Temp, 22, 121, 10.3184/096034005782750482 · DOI
- McCartney, 2005, Modelling scale failure in tension (fracture and spallation), Mater High Temp, 22, 167, 10.3184/096034005782750581 · DOI
- Schütze, 2005, Modelling oxide scale fracture, Mater High Temp, 22, 147, 10.3184/096034005782750437 · DOI
- Schütze, 1994, An approach to a global model of the mechanical behaviour of oxide scales, Mater High Temp, 12, 237, 10.1080/09603409.1994.11689491 · DOI
- Wright IG, Schütze M, Paterson SR, Tortorelli PF, Dooley RB. Progress in prediction and control of scale exfoliation on superheater and reheater alloys. In: Proceedings of EPRI international conference on boiler tube and HRSG tube failures and inspections; 2004.
Cited by
Sorted by citations
Oxidation of Fe–10Cr in O2 and in O2+H2O environment at 600°C: A microstructural investigation
Jonsson, T., Pujilaksono, B., Heidari, H., Liu, F., Svensson, J.-E., Halvarsson, M., & Johansson, L.-G. (2013) · Corrosion Science · doi:10.1016/j.corsci.2013.06.016 · Cited by 64
Persdotter, A., Eklund, J., Liske, J., & Jonsson, T. (2020) · Corrosion Science · doi:10.1016/j.corsci.2020.108961 · Cited by 44
Jiang, C., Feng, M., Chen, M., Chen, K., Geng, S., & Wang, F. (2021) · Corrosion Science · doi:10.1016/j.corsci.2021.109484 · Cited by 42
Metadata
- Authors
- Saunders, S. R. J., Monteiro, M., & Rizzo, F.
- Affiliations
- Pontifícia Universidade Católica do Rio de Janeiro (BR)
- Corresponding author
- Rizzo, F.
- ORCID
- Monteiro, M.
- Venue
- Progress in Materials Science
- Publisher
- Elsevier BV
- Published
- 2008-07
- Volume
- 53
- Issue
- 5
- Pages
- 775-837
- ISSN
- 0079-6425 (ISSN-L)
- OpenAlex
- W2082474544
- Cited by
- 675
- References
- 1
- Citations by year
- 2026: 35 · 2025: 55 · 2024: 55 · 2023: 53 · 2022: 41 · 2021: 46 · 2020: 48 · 2019: 41 · 2018: 41 · 2017: 51 · 2016: 23 · 2015: 38 · 2014: 26 · 2013: 33 · 2012: 24
- FWCI
- 24.21
- Type
- journal article
- Language
- en
- Open access
- closed
- Locations
- Progress in Materials Science (publishedVersion)
- Topics
- Physical Sciences › Materials Science › Surfaces, Coatings and Films › High-Temperature Coating Behaviors
- Physical Sciences › Energy › Fuel Technology › Chemical Looping and Thermochemical Processes
- Physical Sciences › Materials Science › Materials Chemistry › Advancements in Solid Oxide Fuel Cells
- Keywords
- high-temperature oxidation, water vapor, oxide scale formation, alumina, chromia, silica, titanium dioxide, iron oxide, nickel oxide, scale morphology, whisker formation, scale porosity, cation diffusion, vacancy condensation, hydroxide formation, oxide stability, water dissociation, proton hopping, oxygen diffusion, inward diffusion
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review