The DOI matches its Crossref record; 48 of the 48 references it cites were found in a registry or an index.
Corrosion behaviour of iron and nickel aluminide coatings under the synergistic effect of NaCl and water vapour
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
Combustion of biomass and waste releases corrosive species such as alkali chlorides and water vapor, which accelerate corrosion of superheaters in boilers.
“However, the combustion of biomass and waste is well-known to result in a corrosive environment within the boiler due to the formation of, e.g., alkali salts and high levels of H2O(g), which accelerate the degradation of various components in the boiler, such as the superheater tubes (SH).1−12”
From High-Temperature Corrosion Behavior of Superheater Materials at 600 °C: Insights from Laboratory and Field Exposures (2025) · cites this paper as [4]
Citations
Cites
Thermochemical data of pure substances
(1993) · Choice Reviews Online · doi:10.5860/choice.31-0632 · Cited by 4,495
Nickel and iron aluminides: an overview on properties, processing, and applications
Deevi, S. C., & Sikka, V. K. (1996) · Intermetallics · doi:10.1016/0966-9795(95)00056-9 · Cited by 772
Diffusion in Solid Metals and Alloys
Mehrer, H. (1990) · Springer eBooks · doi:10.1007/b37801 · Cited by 710
Saunders, S. R. J., Monteiro, M., & Rizzo, F. (2008) · Progress in Materials Science · doi:10.1016/j.pmatsci.2007.11.001 · Cited by 675
Ennis, P. J., Zielinska-Lipiec, A., Wachter, O., & Czyrska‐Filemonowicz, A. (1997) · Acta Materialia · doi:10.1016/s1359-6454(97)00176-6 · Cited by 381
Peng, X., Yan, J., Zhou, Y., & Wang, F. (2005) · Acta Materialia · doi:10.1016/j.actamat.2005.07.019 · Cited by 270
Self-citationOpila, E. J. (2004) · Materials science forum · doi:10.4028/www.scientific.net/msf.461-464.765 · Cited by 251
Yoshizawa, M., Igarashi, M., Moriguchi, K., ISEDA, A., Armaki, H. G., & Maruyama, K. (2008) · Materials Science and Engineering A · doi:10.1016/j.msea.2008.05.055 · Cited by 177
Continuous and cyclic oxidation of T91 ferritic steel under steam
Laverde, D., Gómez-Acebo, T., & Castro, F. (2003) · Corrosion Science · doi:10.1016/s0010-938x(03)00173-2 · Cited by 156
Xiang, Z. D., & Datta, P. K. (2006) · Acta Materialia · doi:10.1016/j.actamat.2006.05.032 · Cited by 154
Yang, L., Chen, M., Wang, J., Qiao, Y., Guo, P., Zhu, S., & Wang, F. (2020) · Journal of Material Science and Technology · doi:10.1016/j.jmst.2019.11.017 · Cited by 131
Self-citationLiao, Y., Zhang, B., Chen, M., Feng, M. H., Wang, J., Zhu, S., & Wang, F. (2020) · Corrosion Science · doi:10.1016/j.corsci.2020.108526 · Cited by 92
Self-citationYang, S., Yang, L., Chen, M., Wang, J., Zhu, S., & Wang, F. (2020) · Acta Materialia · doi:10.1016/j.actamat.2020.116576 · Cited by 90
Self-citationIhara, Y., Ohgame, H., Sakiyama, K., & Hashimoto, K. (1981) · Corrosion Science · doi:10.1016/0010-938x(81)90023-8 · Cited by 79
Prediction of microstructural states in Cr-Mo steels using phase evolution diagrams
Saroja, S., Parameswaran, P., Vijayalakshmi, M., & Raghunathan, V. S. (1995) · Acta Metallurgica et Materialia · doi:10.1016/0956-7151(95)00022-n · Cited by 74
Ihara, Y., Ohgame, H., Sakiyama, K., & Hashimoto, K. (1982) · Corrosion Science · doi:10.1016/0010-938x(82)90060-9 · Cited by 73
The effect of gas composition on the isothermal oxidation behaviour of PM chromium
Jacob, Y. P., Haanappel, V. A. C., frederik, S. M., Buscail, H., Fielitz, P., & Borchardt, G. (2002) · Corrosion Science · doi:10.1016/s0010-938x(02)00022-7 · Cited by 68
In-situ corrosion investigation at Masnedø CHP plant - a straw-fired power plant
Montgomery, M., & Karlsson, A. (1999) · Materials and Corrosion · doi:10.1002/(sici)1521-4176(199910)50:10 · Cited by 67
Basic mechanical properties and lattice defects of intermetallic compounds
Westbrook, J. H., & Fleischer, R. L. (2000) · Wiley eBooks · Cited by 65
Khan, A., Huang, Y., Dong, Z., & Peng, X. (2019) · Corrosion Science · doi:10.1016/j.corsci.2019.01.032 · Cited by 63
Hot corrosion behavior of electrodeposited SiO2 coating on TiAl alloy
Wu, L.-K., Wu, J.-J., Wu, W.-Y., Yan, H.-J., Jiang, M., & Cao, F. (2020) · Corrosion Science · doi:10.1016/j.corsci.2020.108827 · Cited by 59
Cyclic oxidation of an ultrafine-grained and CeO2-dispersed δ-Ni2Al3 coating
Xu, C., Peng, X., & Wang, F. (2009) · Corrosion Science · doi:10.1016/j.corsci.2009.10.034 · Cited by 59
Self-citationXu, J., Kong, X., Chen, M., Wang, Q., & Wang, F. (2021) · Journal of Material Science and Technology · doi:10.1016/j.jmst.2020.12.042 · Cited by 58
Self-citationEinfluß von Natriumchlorid auf die Oxidation von hochlegierten Chrom‐ und Chrom‐Nickel‐Stählen
Reese, E., & Grabke, H. J. (1993) · Materials and Corrosion · doi:10.1002/maco.19930440204 · Cited by 55
Kourtidou, D., Chaliampalias, D., Vogiatzis, C. A., Tarani, E., Kamou, A., Pavlidou, E., Skolianos, S. M., Chrissafis, K., & Vourlias, G. (2018) · Corrosion Science · doi:10.1016/j.corsci.2018.11.003 · Cited by 52
Ihara, Y., Ohgame, H., Sakiyama, K., & Hashimoto, K. (1983) · Corrosion Science · doi:10.1016/0010-938x(83)90114-2 · Cited by 52
Bramhoff, D., Grabke, H. J., & Schmidt, H. (1989) · Materials and Corrosion · doi:10.1002/maco.19890401104 · Cited by 51
Takeda, M., Kushida, H., Onishi, T., Toyama, M., Koizumi, F., & Fujimoto, S. (2009) · Oxidation of Metals · doi:10.1007/s11085-009-9167-9 · Cited by 47
Xiang, Z., Rose, S. R., & Datta, P. K. (2008) · Scripta Materialia · doi:10.1016/j.scriptamat.2008.02.034 · Cited by 45
Lukaszewicz, M., Simms, N. J., Dudziak, T. P., & Nicholls, J. R. (2013) · Oxidation of Metals · doi:10.1007/s11085-013-9358-2 · Cited by 43
Comparison of the dry and wet oxidation at 900°C of η-Fe2Al5 and δ-Ni2Al3 coatings
Zheng, L., Peng, X., & Wang, F. (2010) · Corrosion Science · doi:10.1016/j.corsci.2010.10.003 · Cited by 40
Self-citationSteam oxidation of aluminide coatings under high pressure and for long exposures
Boulesteix, C., Kolarik, V., & Pedraza, F. (2018) · Corrosion Science · doi:10.1016/j.corsci.2018.08.053 · Cited by 37
Development and analyses of self-passivating tungsten alloys for DEMO accidental conditions
Wegener, T., Klein, F., Litnovsky, A. M., Rasinski, M., Brinkmann, J., Koch, F., & Linsmeier, C. (2017) · Fusion Engineering and Design · doi:10.1016/j.fusengdes.2017.03.072 · Cited by 37
Zhou, Y., Wang, L., Wang, G., Jin, D., Wei, H., Zhao, X., Zhang, J., & Xiao, P. (2016) · Corrosion Science · doi:10.1016/j.corsci.2016.04.041 · Cited by 36
Leng, W., Pillai, R., Naumenko, D., Galiullin, T., & Quadakkers, W. J. (2020) · Corrosion Science · doi:10.1016/j.corsci.2020.108494 · Cited by 35
The degradation of metals in a hydrogen chloride-containing gas at high temperature
Prescott, R., Stott, F. H., & Elliott, P. (1989) · Corrosion Science · doi:10.1016/0010-938x(89)90100-5 · Cited by 28
Interdiffusional degradation of oxidation‐resistant aluminide coatings on Fe‐base alloys
Zhang, Y., Liu, A. P., & Pint, B. A. (2007) · Materials and Corrosion · doi:10.1002/maco.200704057 · Cited by 28
Xiang, Z., Rose, S. R., & Datta, P. K. (2006) · Journal of Materials Science · doi:10.1007/s10853-006-0806-0 · Cited by 28
Effect of water vapour on the oxidation of Fe–13Cr–5Ni martensitic alloy at 973K
Liu, L., Yang, Z.-G., Zhang, C., Ueda, M., Kawamura, K., & Maruyama, T. (2012) · Corrosion Science · doi:10.1016/j.corsci.2012.04.008 · Cited by 28
Sui, J., Lehmusto, J., Bergelin, M., & Hupa, L. (2019) · Corrosion Science · doi:10.1016/j.corsci.2019.04.010 · Cited by 26
Wenga, T., Chen, G., Ma, W., & Yan, B. (2019) · Corrosion Science · doi:10.1016/j.corsci.2019.04.013 · Cited by 26
Improved oxidation performance of TiAl alloy by a novel Al–Si composite coating
Wang, Q., Wu, W.-Y., Jiang, M., Cao, F., Wu, H.-X., Sun, D., Yu, H., & Wu, L.-K. (2019) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2019.125126 · Cited by 26
Khan, A., Dong, Z., & Peng, X. (2020) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2020.125861 · Cited by 25
Chemical-mechanical failure of oxide scales on 9% Cr steels in air with H2O
Schütze, M., Renusch, D. P., & Schorr, M. (2005) · Materials at High Temperatures · doi:10.1179/mht.2005.013 · Cited by 21
Sánchez, L., Bolívar, F. J., Hierro, M. P., & Pérez, F. J. (2009) · Thin Solid Films · doi:10.1016/j.tsf.2009.01.031 · Cited by 19
Low-temperature formation and steam oxidation of β-FeAl coating on P92 steel
Zhou, Y., Lu, J., Shen, M., Yuan, Y., Gu, Y., Yang, Z., Huang, J., & Zhao, Q. (2019) · Corrosion Science · doi:10.1016/j.corsci.2019.108227 · Cited by 19
Surface terraces in pure tungsten formed by high temperature oxidation
Yu, H., Das, S., Liu, J., Hess, J., & Hofmann, F. (2019) · Scripta Materialia · doi:10.1016/j.scriptamat.2019.08.007 · Cited by 17
Gorman, D. M., & Fry, A. T. (2016) · Oxidation of Metals · doi:10.1007/s11085-016-9674-4 · Cited by 13
Flagged first, then by citations
Cited by
Sorted by citations
Research progress of marine anti-corrosion and wear-resistant coating
Pei, W., Pei, X., Xie, Z., & Wang, J. (2024) · Tribology International · doi:10.1016/j.triboint.2024.109864 · Cited by 144
Wang, X., Wang, G., Wang, W., Liu, X., Liu, Y., Jin, Y., & Zhang, Y. (2025) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2025.181014 · Cited by 55
Zhang, M., Yu, L., Feng, M. H., Jiang, C., Zhang, Y., Wang, Y., Feng, Y., Ma, L., & Wang, F. (2022) · Corrosion Science · doi:10.1016/j.corsci.2022.110750 · Cited by 39
Self-citationLuo, X., Cao, J., Yu, F., Zhang, Y., Tang, J., Li, X., & Xie, H. (2023) · Heliyon · doi:10.1016/j.heliyon.2023.e13855 · Cited by 33
Controllable preparation of metal-based lubrication coatings in extreme environmental applications
Wu, S., Tang, Y., Gu, J., Li, R., Yu, L., Liu, P., Wang, H., An, C., Deng, Q., Zhao, L., et al. (2024) · Materials & Design · doi:10.1016/j.matdes.2024.112922 · Cited by 29
Li, Y., Zhang, C., Niu, X. Y., Zhang, C. Y., Li, S., Bao, Z., Zhu, S., & Wang, F. H. (2023) · Corrosion Science · doi:10.1016/j.corsci.2023.111493 · Cited by 26
Self-citationImproved high-temperature oxidation resistance of TC4 alloy by electrodeposited SiO2 coating
Yan, H.-J., Tai, Z.-F., Wu, L.-K., & Cao, F. (2021) · Corrosion Communications · doi:10.1016/j.corcom.2021.10.002 · Cited by 24
Li, Y. Y., Huang, D., Zhang, C. Y., Li, S., Bao, Z., Zhu, S. L., & Wang, F. H. (2022) · Corrosion Science · doi:10.1016/j.corsci.2022.110421 · Cited by 24
Self-citationSsenteza, V., Eklund, J., Bigdeli, S., & Jonsson, T. (2024) · Corrosion Science · doi:10.1016/j.corsci.2023.111654 · Cited by 23
Corrosion resistance of cerium-doped Pb-Co alloy coatings in seawater
Jin, X., Wang, J., Wang, S., Wu, S., He, J., Yang, H., Zhou, J., Yang, F., Gong, J., & Dai, Y. (2023) · Corrosion Science · doi:10.1016/j.corsci.2023.111777 · Cited by 19
Xu, J., Geng, S., Wang, J., Chen, G., & Wang, F. (2022) · Corrosion Communications · doi:10.1016/j.corcom.2022.07.004 · Cited by 17
Self-citationHu, Q., Geng, S., Wang, J., Wang, F., Sun, Q., Xia, S., & Wu, Y. H. (2023) · Materials Chemistry and Physics · doi:10.1016/j.matchemphys.2023.128416 · Cited by 17
Self-citationProgress in Novel Electrodeposited Bond Coats for Thermal Barrier Coating Systems
Maniam, K. K., & Paul, S. (2021) · Materials · doi:10.3390/ma14154214 · Cited by 15
Günen, A., Altınay, Y., Sabun, Ş., & Alkan, S. (2024) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2024.130774 · Cited by 13
Yang, H., Wu, Y. H., Sun, Q., Yang, F., Xia, C., Xia, S., & Du, J. (2024) · Coatings · doi:10.3390/coatings14060750 · Cited by 11
Yu, Z., Yang, S., Xie, L., Chen, M., & Wang, F. (2025) · Corrosion Communications · doi:10.1016/j.corcom.2024.04.007 · Cited by 10
Self-citationNon-negligible corrosion from vaporized boric acid on 304 stainless steel
Li, X., Wei, D., Zhang, S., Qi, Y., Sun, W. C., Zhong, J., & Ning, G. (2022) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2022.154188 · Cited by 8
Hu, Q., Geng, S., Niu, X., Wang, J., Huang, Y., & Wang, F. (2025) · Corrosion Science · doi:10.1016/j.corsci.2025.113000 · Cited by 5
Self-citationHu, Q., Geng, S., Wang, J., Wang, F., Sun, Q., Xia, S., & Wu, Y. H. (2025) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2025.132413 · Cited by 5
Self-citationSolid/Molten Na2SO4-Induced Hot Corrosion Behaviors of Mar-M247 Alloy with CVD Aluminide Coatings
Hu, Q., Geng, S., Wang, J., Wang, F., Sun, Q., Xia, S., & Wu, Y. H. (2024) · High Temperature Corrosion of Materials · doi:10.1007/s11085-024-10315-1 · Cited by 4
Self-citationEffect of deposition temperature on corrosion behavior of CVD aluminide coatings on K452 superalloy
Xu, J., Geng, S., Wang, J., Chen, G., Wang, F., Sun, Q., Xia, S., & Wu, Y. H. (2024) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2024.131600 · Cited by 4
Self-citationChen, Z., Du, Y., Lu, Y., Wang, C., Zhu, S., & Wang, F. (2024) · Ceramics International · doi:10.1016/j.ceramint.2024.12.171 · Cited by 3
Self-citationZhang, T., Yu, C., Xiao, B., Liu, J., Zhu, Z., & Zhang, N. (2024) · Acta Metallurgica Sinica (English Letters) · doi:10.1007/s40195-024-01789-8 · Cited by 3
High performance aluminized Monel coatings with prolonged corrosion resistance in saline environment
Aslam, M. S., Ahmed, N., & Khan, Z. S. (2023) · Materials Chemistry and Physics · doi:10.1016/j.matchemphys.2023.128695 · Cited by 3
Electrodeposition of Fe-Zn, Fe-Mn and Fe-Zn-Mn alloys on steel from ionic liquids
Akdogan, C., Bakkaloğlu, Ö. F., Bedır, M., Erdogan, P. Y., & Yavuz, A. (2022) · Digest Journal of Nanomaterials and Biostructures · doi:10.15251/djnb.2022.172.589 · Cited by 3
Feasibility study for the development of Al-Si based coating on Ni-Cu alloy (UNS N04400)
Samvatsar, K., & Rao, V. (2022) · Materials Today Proceedings · doi:10.1016/j.matpr.2022.04.731 · Cited by 3
Wang, M., Zhao, W., Li, X., Li, J., Suo, S., Lv, C., Lin, X., & Sun, J. (2025) · Materials Chemistry and Physics · doi:10.1016/j.matchemphys.2025.131754 · Cited by 2
Chen, Z., Du, Y., Lu, Y., Wang, C., & Zhu, S. (2024) · Ceramics International · doi:10.1016/j.ceramint.2024.07.124 · Cited by 2
Ssenteza, V., Olausson, M. D. P., Eklund, J., Nockert, J., Liske, J., & Jonsson, T. (2025) · Energy & Fuels · doi:10.1021/acs.energyfuels.4c04806 · Cited by 1
Zhang, W., Liu, L., Cui, Y., Wang, W., Chen, W., Li, R., Liu, R., & Wang, F. (2024) · Acta Metallurgica Sinica (English Letters) · doi:10.1007/s40195-024-01699-9 · Cited by 1
Self-citationEffect of CeO2 on the H2O/NaCl-Induced Corrosion Behavior of Ni-Co Coating at 650 °C
Gao, Y., Zhang, P., Ren, P., Yang, Y., Han, G., Du, W., Li, W., & Wang, Q. (2025) · Acta Metallurgica Sinica (English Letters) · doi:10.1007/s40195-025-01818-0 · Cited by 1
Wang, F., Xu, K., Hu, X., Lou, M., Nishimura, K., & Chang, K. (2025) · Corrosion Science · doi:10.1016/j.corsci.2025.113290 · Cited by 1
Self-citationYang, J. Y., Ren, P., Zhang, P., Yang, Y., & Wang, Q. J. (2026) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2026.133562 · Cited by 1
Gao, J., Su, W., Gong, Y., Chen, J., Wang, X., Song, X., Xu, G., & Yu, G. (2025) · Fuel · doi:10.1016/j.fuel.2025.137146 · Cited by 1
Li, Y. Y., Bao, Z., Huang, D., Zhang, C. Y., LI, S., Zhu, S. L., & Wang, F. (2022) · SSRN Electronic Journal · doi:10.2139/ssrn.4071345
Self-citationDudziak, T. P., Rząd, E., Chandran, P., Kateusz, F., Polczyk, T., Boroń, Ł., Wójcicki, M., Tchórz, A., & Krzak, I. (2024) · SSRN Electronic Journal · doi:10.2139/ssrn.4902341
Wang, M., Zhao, W., Li, X. W., Li, J., Suo, S., Lv, C., Lin, X., & Sun, J. (2025) · SSRN Electronic Journal · doi:10.2139/ssrn.5340665
Wu, D., Hu, H., Wu, H., Liu, S., Jiang, Y., Wang, J., Bao, Z., & Zhang, C. (2026) · Corrosion Communications · doi:10.1016/j.corcom.2026.03.015
Hot Corrosion Resistance of a NiCrMoAlSi Cladding Layers Under K2SO4-ZnCl2 Molten Salt Film in Air
Zhang, H., & Wu, J. (2026) · CORROSION · doi:10.5006/4846
Tao, Z., Zhang, H., Yang, N., Xu, Z., Tang, H., Zeng, J., Wei, C., & Wu, B. (2026) · Advanced Engineering Materials · doi:10.1002/adem.70909
Li, X., Chen, L., Wei, B., Ma, R., Li, Y., Guo, F., & Shuang, J. (2026) · Fuel · doi:10.1016/j.fuel.2026.141227
Ma, L., Wang, D., 尚姝雅, Wu, H., Hu, J., & Guo, N. (2026) · Coatings · doi:10.3390/coatings16111274
The chlorine challenges: materials, mechanisms, and mitigation in high-temperature corrosion
Liu, Y., Cao, G., Chen, C., Wang, Y., Zhang, Z., Guo, S., Геннадьевич, Г. Н., Fu, X., & Hu, J. (2026) · Tungsten · doi:10.1007/s42864-026-00410-y
Metadata
- Authors
- Jiang, C., Feng, M., Chen, M., Chen, K., Geng, S., & Wang, F.
- Affiliations
- Shenyang National Laboratory for Materials Science (CN)
- Dongguan University of Technology (CN)
- Corresponding author
- Chen, Minghui
- Venue
- Corrosion Science
- Publisher
- Elsevier BV
- Published
- 2021-07
- Volume
- 187
- Pages
- 109484
- ISSN
- 0010-938X (ISSN-L)
- OpenAlex
- W3154725694
- Cited by
- 42
- References
- 48
- Citations by year
- 2026: 6 · 2025: 9 · 2024: 12 · 2023: 6 · 2022: 7 · 2021: 2
- FWCI
- 3.48
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- Locations
- Corrosion Science (publishedVersion)
- Funders
- National Natural Science Foundation of China
- Ministry of Industry and Information Technology of the People's Republic of China
- Topics
- Physical Sciences › Materials Science › Surfaces, Coatings and Films › High-Temperature Coating Behaviors
- Physical Sciences › Materials Science › Materials Chemistry › Corrosion Behavior and Inhibition
- Physical Sciences › Engineering › Mechanical Engineering › Intermetallics and Advanced Alloy Properties
- Keywords
- aluminide coatings, NiAl coatings, corrosion behavior, sodium chloride, water vapor, marine environment, ferritic-martensitic steel, electroplating, oxychlorination, interdiffusion, breakaway oxidation, high-temperature oxidation
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review