Mechanical behaviour of biodegradable agricultural films under real field conditions
Integrity signals
Registry
Cites
Statistics
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
The resistance to tear propagation is expected to be much lower than the resistance of tear initiation.
“The resistance to tear propagation is expected to be much lower than the resistance of tear initiation [33].”
From Uncompatibilized PBAT/PLA Blends: Manufacturability, Miscibility and Properties (2020) · cites this paper as [33]
Cited by
Sorted by citations
Polymer biodegradation: Mechanisms and estimation techniques – A review
Lucas, N., Bienaime, C., Belloy, C., Queneudec, M., Silvestre, F., & Nava-Saucedo, J.-E. (2008) · Chemosphere · doi:10.1016/j.chemosphere.2008.06.064 · Cited by 1,384 · see citing works
Vroman, I., & Tighzert, L. (2009) · Materials · doi:10.3390/ma2020307 · Cited by 1,355 · see citing works
Biodegradable Polymers-A Review on Recent Trends and Emerging Perspectives
Luckachan, G. E., & Pillai, C. K. S. (2011) · Journal of Polymers and the Environment · doi:10.1007/s10924-011-0317-1 · Cited by 767 · see citing works
Rudnik, E., & Briassoulis, D. (2011) · Industrial Crops and Products · doi:10.1016/j.indcrop.2010.12.031 · Cited by 272 · see citing works
Self-citationUncompatibilized PBAT/PLA Blends: Manufacturability, Miscibility and Properties
Su, S., Duhme, M., & Kopitzky, R. (2020) · Materials · doi:10.3390/ma13214897 · Cited by 159 · see citing works
Hayes, D. G., Wadsworth, L. C., Sintim, H. Y., Flury, M., English, M., Schaeffer, S., & Saxton, A. M. (2017) · Polymer Testing · doi:10.1016/j.polymertesting.2017.07.027 · Cited by 136 · see citing works
Cowan, J. S., Saxton, A. M., Liu, H., Leonas, K. K., Inglis, D., & Miles, C. A. (2016) · HortScience · doi:10.21273/hortsci.51.3.245 · Cited by 8 · see citing works
- Authors
- Briassoulis, D.
- Affiliations
- Agricultural University of Athens (GR)
- Corresponding author
- Briassoulis, D.
- ORCID
- Briassoulis, D.
- Venue
- Polymer Degradation and Stability
- Publisher
- Elsevier BV
- Published
- 2006-06
- Volume
- 91
- Issue
- 6
- Pages
- 1256-1272
- ISSN
- 0141-3910 (ISSN-L)
- OpenAlex
- W2143209465
- Cited by
- 211
- References
- 0
- Citations by year
- 2026: 3 · 2025: 9 · 2024: 12 · 2023: 9 · 2022: 20 · 2021: 15 · 2020: 9 · 2019: 22 · 2018: 10 · 2017: 9 · 2016: 10 · 2015: 9 · 2014: 12 · 2013: 13 · 2012: 9
- FWCI
- 2.38
- Type
- journal article
- Language
- en
- Open access
- closed
- Locations
- Polymer Degradation and Stability (publishedVersion)
- Topics
- Physical Sciences › Materials Science › Biomaterials › biodegradable polymer synthesis and properties
- Physical Sciences › Engineering › Biomedical Engineering › Polymer-Based Agricultural Enhancements
- Physical Sciences › Materials Science › Biomaterials › Nanocomposite Films for Food Packaging
- Keywords
- mechanical properties, aging materials, degradation, Mater-Bi, mulching film, field exposure, polyethylene film, additives, film thickness, processing conditions
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review