Degradability of linear polyolefins under natural weathering

Open access
Ojeda, Telmo, Freitas, Ana, Birck, Kátia, Dalmolin, Emilene, Jacques, Rodrigo, Bento, Fátima, Camargo, Flávio·2011·Polymer Degradation and Stability

Abstract

High density polyethylene (HDPE), linear low density polyethylene (LLDPE), and isotactic polypropylene (PP) containing antioxidant additives at low or zero levels were extruded and blown moulded as films. An HDPE/LLDPE commercial blend containing a pro-oxidant additive (i.e., an oxo-biodegradable blend) was taken from the market as supermarket bag. These four polyolefin samples were exposed to natural weathering for one year during which their structure and thermal and mechanical properties were monitored. This study shows that the real durability of olefin polymers may be much shorter than centuries, as in less than one year the mechanical properties of all samples decreased virtually to zero, as a consequence of severe oxidative degradation, that resulted in substantial reduction in molar mass accompanied by a significant increase in content of carbonyl groups. PP and the oxo-bio HDPE/LLDPE blend degraded very rapidly, whereas HDPE and LLDPE degraded more slowly, but significantly in a few months. The main factors influencing the degradability were the frequency of tertiary carbon atoms in the chain and the presence of a pro-oxidant additive. The primary (sterically hindered phenol) and secondary (phosphite) antioxidant additives added to PP slowed but did not prevent rapid photo-oxidative degradation, and in HDPE and LLDPE the secondary antioxidant additive had little influence on the rate of abiotic degradation at the concentrations used here.

Overview

The claims and statistics of this paper haven’t been checked yet.

Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1016/j.polymdegradstab.2010.12.004

Cites

2 of 2 references verified0 citation errors · 0 not checkable

Statistics

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.

A few free checks a day · papers already verified open instantly · results are public

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Show all 2 references

Research works printed but not linked: 15

  1. Corrales, 2002, Photooxidative and thermal degradation of polyethylenes: interrelationship by chemiluminescence, thermal gravimetric analysis and FTIR data, J Photochem Photobiol A, 147, 213, 10.1016/S1010-6030(01)00629-3 · DOI
  2. Guadagno, 2001, Chemical and morphological modifications of irradiated linear low density polyethylene (LLDPE), Polym Degrad Stab, 72, 175, 10.1016/S0141-3910(01)00024-6 · DOI
  3. Sudhakar, 2008, Marine microbe-mediated biodegradation of low- and high-density polyethylenes, Int Biodeterior Biodegrad, 61, 203, 10.1016/j.ibiod.2007.07.011 · DOI · Paper page
  4. Alexander, 1965, Biodegradation: problems of molecular recalcitrance and microbial fallibility, Adv Appl Microbiol, 7, 35, 10.1016/S0065-2164(08)70383-6 · DOI · Paper page
  5. Arkatkar, 2009, Degradation of unpretreated and thermally pretreated polypropylene by soil consortia, Int Biodeterior Biodegrad, 63, 106, 10.1016/j.ibiod.2008.06.005 · DOI · Paper page
  6. Corti, 2010, Oxidation and biodegradation of polyethylene films containing pro-oxidant additives: synergistic effects of sunlight exposure, thermal aging and fungal biodegradation, Polym Degrad Stab, 95, 1106, 10.1016/j.polymdegradstab.2010.02.018 · DOI · Paper page
  7. Naddeo, 2004, Photooxidation of spherilene linear low-density polyethylene films subjected to environmental weathering. 1. Changes in mechanical properties, Polym Degrad Stab, 85, 1009, 10.1016/j.polymdegradstab.2003.04.005 · DOI
  8. Craig, 2005, Photo-induced scission and crosslinking in LDPE, LLDPE and HDPE, Polym Eng Sci, 45, 579, 10.1002/pen.20313 · DOI
  9. Chiellini, 2003, Biodegradation of thermally-oxidized, fragmented low-density polyethylenes, Polym Degrad Stab, 81, 341, 10.1016/S0141-3910(03)00105-8 · DOI · Paper page
  10. Chiellini, 2006, Oxo-biodegradable carbon backbone polymers - oxidative degradation of polyethylene under accelerated test conditions, Polym Degrad Stab, 91, 2739, 10.1016/j.polymdegradstab.2006.03.022 · DOI · Paper page
  11. Takeuchi, 1969, Near-infrared spectrophotometric analysis of ethylene-propylene copolymers, Anal Chem, 41, 184, 10.1021/ac60270a029 · doi:10.1021/ac60270a029
  12. Gulmine, 2003, Degradation profile of polyethylene after artificial accelerated weathering, Polym Degrad Stab, 79, 385, 10.1016/S0141-3910(02)00338-5 · DOI · Paper page
  13. Winslow, 1977, Photooxidation of high polymers, Pure Appl Chem, 49, 495, 10.1351/pac197749040495 · DOI
  14. Iring, 1986, Thermal oxidation of linear low density polyethylene, Polym Degrad Stab, 14, 319, 10.1016/0141-3910(86)90036-4 · doi:10.1016/0141-3910(86)90036-4
  15. Rabello, 1997, Crystallization and melting behavior of photodegraded polypropylene. 2. Recrystallization of degraded molecules, Polymer, 38, 6389, 10.1016/S0032-3861(97)00214-0 · doi:10.1016/s0032-3861(97)00214-0

Cited by

See all 284

Metadata

Authors
Ojeda, T., Freitas, A., Birck, K., Dalmolin, E., Jacques, R., Bento, F., & Camargo, F.
Venue
Polymer Degradation and Stability
Publisher
Elsevier BV
Published
2011-04
Volume
96
Issue
4
Pages
703-707
ISSN
0141-3910 (ISSN-L)
OpenAlex
W2073176776
Cited by
284
References
2
FWCI
3.66
Type
journal article
Language
en
Open access
bronze
Licence
Funders
  • National Council for Scientific and Technological Development
  • Coordination for the Improvement of Higher Education Personnel

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

How to cite

Cite CoChat for the checks on this page, and the paper for its own findings.

This page
CoChat. (2026). Citation check: Degradability of linear polyolefins under natural weathering. https://app.cochat.ai/papers/10.1016/j.polymdegradstab.2010.12.004
The paper
Ojeda, T., Freitas, A., Birck, K., Dalmolin, E., Jacques, R., Bento, F., & Camargo, F. (2011). Degradability of linear polyolefins under natural weathering. Polymer Degradation and Stability. https://doi.org/10.1016/j.polymdegradstab.2010.12.004

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.