The DOI matches its Crossref record; 5 of the 5 references it cites were found in a registry or an index.
Thermal, thermo-oxidative and thermomechanical degradation of PLA: A comparative study based on rheological, chemical and thermal properties
Open accessAbstract
This research studies the effect of thermal, thermo-oxidative and thermomechanical degradation conditions on the melt rheological, chemical and thermal properties of PLA at temperatures around its normal processing temperature. Thermal and thermo-oxidative degradations were conducted on a rheometer by using nitrogen or air as gas, respectively, and the thermomechanical degradation was performed on a mixer equipped with two counter-rotating rollers. Dynamic oscillatory rheology, TGA, DSC and FTIR were performed on PLA samples subjected to different degradation conditions: temperature (180, 200 or 220 °C), time (15, 30 or 60 min), atmosphere (air or atmosphere) and the application of mechanical stress or not. Thus, rheological results indicate the synergic effect that temperature, mechanical stress and time exerts on the extent of chain scission phenomena, which was also corroborated by FTIR results; however, the individual contribution of mechanical stress diminishes gradually with the degradation time, being more pronounced for higher degradation temperature. In addition, degree of crystallinity (χ c ) turned out not to be a suitable parameter for comparing degraded samples, since all of them became amorphous after degradation. Instead, glass transition (T g ) and cold crystallization (T cc ) temperatures as well as the cold crystallization enthalpy (ΔH cc ) reveal that the chain scission phenomena makes degraded samples easier to crystallize. Finally, TGA results point out a worsening of the PLA thermal stability, with lower values of the characteristic temperatures (T 5% and T max ) for degraded samples.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Al-Itry, R., Lamnawar, K., & Maazouz, A. (2012) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2012.06.028 · Cited by 906
McNeill, I. C., & Leiper, H. A. (1985) · Polymer Degradation and Stability · doi:10.1016/0141-3910(85)90035-7 · Cited by 404
Degradation of polymer blends: A brief review
La Mantia, F. P., Morreale, M., Botta, L., Mistretta, M. C., Ceraulo, M., & Scaffaro, R. (2017) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2017.07.011 · Cited by 268
Oxidative degradation of polylactide (PLA) and its effects on physical and mechanical properties
Rasselet, D., Ruellan, A., Guinault, A., Miquelard-Garnier, G., Sollogoub, C., & Fayolle, B. (2014) · European Polymer Journal · doi:10.1016/j.eurpolymj.2013.10.011 · Cited by 196 · cited 4×
“group and known to be a suitable as internal standa rd for PLA [4,5,10,16].”
BackgroundInfluentialCrystallization kinetics of virgin and processed poly (lactic acid)
Pantani, R., De Santis, F., Sorrentino, A., De Maio, F., & Titomanlio, G. (2010) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2010.04.018 · Cited by 161
Cited by
A review on PLA-based biodegradable materials for biomedical applications
Hussain, M., Khan, S. M., Shafiq, M., & Abbas, N. (2024) · Giant · doi:10.1016/j.giant.2024.100261 · Cited by 326
Review on the Degradation of Poly(lactic acid) during Melt Processing
Velghe, I., Buffel, B., Vandeginste, V., Thielemans, W., & Desplentere, F. (2023) · Polymers · doi:10.3390/polym15092047 · Cited by 146
Influence of Addition of Organic Fillers on the Properties of Mechanically Recycled PLA
Beltrán, F. R., Gaspar, G., Dadras Chomachayi, M., Jalali-Arani, A., Lozano-Pérez, A. A., Cenis, J. L., de la Orden, M. U., Pérez, E., & Martínez Urreaga, J. M. (2021) · Environmental Science and Pollution Research · doi:10.1007/s11356-020-08025-7 · Cited by 54
Metadata
- Authors
- Cuadri, A. A., & Martín-Alfonso, J. E.
- Venue
- Polymer Degradation and Stability
- Publisher
- Elsevier BV
- Published
- 2018-04
- Volume
- 150
- Pages
- 37-45
- ISSN
- 0141-3910 (ISSN-L)
- OpenAlex
- W2790791628
- Cited by
- 175
- References
- 5
- FWCI
- 4.06
- Type
- journal article
- Language
- en
- Open access
- green
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.