Pore solution in alkali-activated slag cement pastes. Relation to the composition and structure of calcium silicate hydrate
The DOI matches its Crossref record; 28 of the 29 references it cites were found in a registry or an index.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“The composition of the gel, secondary phases, and pore solution in AAS are affected by both initial slag composition14–16 and choice of alkaline activator17–19.”
From Spatially resolved nanostructural analysis of disordered phases in carbonated alkali-activated slag (2025) · cites this paper as [16]
In the citing paper
“The weak resistance of alkali-activated slag against carbonation can be attributed to the absence of portlandite in contrast to hydrated Portland cement 27,28 .”
From Thermodynamic Modeling and Experimental Study of Carbonation of Alkali-Activated Slag Cements (2023) · cites this paper as [27]
Citations
Cites
High-resolution solid-state NMR of silicates and zeolites
Boddenberg, B. (1988) · Applied Catalysis · doi:10.1016/s0166-9834(00)80098-6 · Cited by 1,819
High-resolution solid-state NMR of silicates and zeolites
Engelhardt, G., & Michel, D. (1987) · Medical Entomology and Zoology · Cited by 1,592
Hydration products of alkali activated slag cement
Wang, S.-D., & Scrivener, K. L. (1995) · Cement and Concrete Research · doi:10.1016/0008-8846(95)00045-e · Cited by 997
PHREEQE : a computer program for geochemical calculations
(1980) · doi:10.3133/wri8096 · Cited by 842
Sodium silicate-based, alkali-activated slag mortars
Brough, A. R., & Atkinson, A. (2002) · Cement and Concrete Research · doi:10.1016/s0008-8846(02)00717-2 · Cited by 694
Expression and analysis of pore fluids from hardened cement pastes and mortars
Barneyback, R. S., & Diamond, S. (1981) · Cement and Concrete Research · doi:10.1016/0008-8846(81)90069-7 · Cited by 604
Fernández-Jiménez, A., Palomo, J. G., & Puertas, F. (1999) · Cement and Concrete Research · doi:10.1016/s0008-8846(99)00154-4 · Cited by 598
Self-citationFernández‐Jiménez, A., Puertas, F., Sobrados, I., & Sanz, J. (2003) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2003.tb03481.x · Cited by 481
Self-citationAlkali-activated slag cement and concrete: a review of properties and problems
Wang, S.-D., Pu, X.-C., Scrivener, K. L., & Pratt, P. L. (1995) · Advances in Cement Research · doi:10.1680/adcr.1995.7.27.93 · Cited by 474
A calorimetric study of early hydration of alkali-slag cements
Shi, C., & Day, R. L. (1995) · Cement and Concrete Research · doi:10.1016/0008-8846(95)00126-w · Cited by 468
Research works printed but not linked: 5
- Glukhoskij, 1983, Slag-alkaline cements and concretes-structures, properties, technologies and economical aspects of the use, Silic. Ind., 10, 197
- S.A. Stronach, Thermodinamic modeling and phase relations of cementitious systems, Thesis, University of Aberdeen, Scotland, 1996.
- Teoreanu, 1991, The interaction mechanism of blast-furnace slags with water. The role of the activating agents, Il Cemento, 2, 91
- Shi, 1997, Early hydration and microstructure development of alkali-activated slag cement pastes, vol. 3
- Wieker, 1997, Recent results of solid-state NMR investigations and their possibilities of use in cement chemistry, vol. 1
Cited by
Items 101–200 of 418
Zhu, X., Zhang, Z., Yang, K., Magee, B. J., Wang, Y., Yu, L., Nanukuttan, S. V., Li, Q., Mu, S., Yang, C., et al. (2018) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2018.02.016 · Cited by 86
“The sodium silicate solution provides the essential [SiO4] and Na in C-(N)-A-S-H gel [43], then the ion concentration decreases sharply with the hydration of slag [44-45].”
BackgroundMikhailova, O., del Campo, A., Rovnaník, P., Fernández, J. F., & Torres‐Carrasco, M. (2019) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2019.02.004 · Cited by 85
Althoey, F., Zaid, O., de‐Prado‐Gil, J., Palencia, C., Ali, E., Hakeem, I. Y., & Martínez‐García, R. (2022) · Journal of Building Engineering · doi:10.1016/j.jobe.2022.104610 · Cited by 80
RetractedExploring the Potential of Nonclassical Crystallization Pathways to Advance Cementitious Materials
Ruiz‐Agudo, C., & Cölfen, H. (2024) · Chemical Reviews · doi:10.1021/acs.chemrev.3c00259 · Cited by 81
Hydration of mechanically activated granulated blast furnace slag
Kumar, R. R., Kumar, S., Badjena, S., & Mehrotra, S. (2005) · Metallurgical and Materials Transactions B · doi:10.1007/s11663-005-0089-x · Cited by 89
Geopolymerization behavior of Cu–Ni slag mechanically activated in air and in CO2 atmosphere
Kalinkin, A. M., Kumar, S., Израильевна, Г. Б., Alex, T. C., Владимировна, К. Е., Тюкавкина, В. В., Калинников, В. Т., & Kumar, R. R. (2012) · International Journal of Mineral Processing · doi:10.1016/j.minpro.2012.05.001 · Cited by 87
Wang, W., Chen, H., Li, X., & Zhu, Z. (2017) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2017.03.132 · Cited by 78
A Roadmap for Production of Cement and Concrete with Low-CO2 Emissions
van Deventer, J. S. J., White, C. E., & Myers, R. J. (2020) · Waste and Biomass Valorization · doi:10.1007/s12649-020-01180-5 · Cited by 84
Zhang, Z., Chen, R., Hu, J., Wang, Y., Huang, H., Ma, Y., Zhang, Z., Wang, H., Yin, S., Wei, J., et al. (2021) · Composites Part B Engineering · doi:10.1016/j.compositesb.2021.109215 · Cited by 77
Nanoscale Chemical Degradation Mechanisms of Sulfate Attack in Alkali-activated Slag
Gong, K., & White, C. E. (2018) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.7b11270 · Cited by 77
Assessing the chemical involvement of limestone powder in sodium carbonate activated slag
Yuan, B., Yu, Q., & Brouwers, H. J. H. (2017) · Materials and Structures · doi:10.1617/s11527-017-1003-0 · Cited by 77
“The sharp peak at around 946 cm is generally observed for sodium carbonate activated slags of the generated C–(A)–S–H [25, 42], while for the waterglass activated slags the position of this peak shifts to a higher wavenumber between 950 and 1000 cm [52–54], pointing to a different chemical proportion (Si/Ca ratio) [51…”
BackgroundAlkali-activated slag mortars reinforced with ar glassfibre. Performance and properties
Puertas, F., Gil-Maroto, A., Palacios, M., & Amat, T. (2006) · Materiales de Construcción · doi:10.3989/mc.2006.v56.i283.10 · Cited by 72
Self-citationHamdan, A., Song, H., Yao, Z., Alnahhal, M. F., Kim, T., & Hajimohammadi, A. (2023) · Cement and Concrete Research · doi:10.1016/j.cemconres.2023.107311 · Cited by 72
Durability of Alkali-Activated Slag Concretes Prepared Using Waste Glass as Alternative Activator
Torres‐Carrasco, M., Tognonvi, M. T., Tagnit‐Hamou, A., & Puertas, F. (2015) · ACI Materials Journal · doi:10.14359/51687903 · Cited by 71
Self-citationA parametric study of accelerated carbonation in alkali-activated slag
McCaslin, E. R., & White, C. E. (2021) · Cement and Concrete Research · doi:10.1016/j.cemconres.2021.106454 · Cited by 65
Nanoscale Ordering and Depolymerization of Calcium Silicate Hydrates in the Presence of Alkalis
Garg, N., Özçelik, V. O., Skibsted, J., & White, C. E. (2019) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.9b06412 · Cited by 65
Durability performance evaluation of green geopolymer concrete
Luhar, S., Luhar, I., & Gupta, R. (2020) · European Journal of Environmental and Civil engineering · doi:10.1080/19648189.2020.1847691 · Cited by 67
“The existing Naþ ions were found occupying the pores of the material must be present to counteract the Chloride ions which were diffused (applied electrically in the pore network) directing to an enhanced relocate of charge (Gruskovnjak et al., 2006; Puertas et al., 2004).”
BackgroundCriado, M., Walkley, B., Ke, X., Provis, J. L., & Bernal, S. A. (2018) · Sustainability · doi:10.3390/su10124709 · Cited by 63
Slag-Based Cements That Resist Damage Induced by Carbon Dioxide
Ke, X., Criado, M., Provis, J. L., & Bernal, S. A. (2018) · ACS Sustainable Chemistry & Engineering · doi:10.1021/acssuschemeng.7b04730 · Cited by 62
Moon, H., Ramanathan, S., Suraneni, P., Shon, C.-S., Lee, C. J., & Chung, C.-W. (2018) · Materials · doi:10.3390/ma11101847 · Cited by 62
“Its reactivity is, however, increased as pH increases [18,19].”
BackgroundMitigation of efflorescence of alkali-activated slag mortars by incorporating calcium hydroxide
Tang, D., Yang, C., Li, X., Zhu, X., Yang, K., & Yu, L. (2021) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2021.123873 · Cited by 62
Jiang, H., Ren, L., Zhang, Q., Zheng, J., & Cui, L. (2021) · Powder Technology · doi:10.1016/j.powtec.2022.117322 · Cited by 66
New insights into the hydration of slag in alkaline media using a micro-reactor approach
Suraneni, P., Palacios, M., & Flatt, R. J. (2015) · Cement and Concrete Research · doi:10.1016/j.cemconres.2015.09.015 · Cited by 62
A critical review on the interaction between calcium silicate hydrate (C-S-H) and different ions
Liu, X., Feng, P., Chen, J., Liu, Q., Yu, X., Cai, Y., Zhu, H., Qing, L., & Hong, J. (2024) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2024.134931 · Cited by 64
Durability test methods and their application to AAMs: case of sulfuric-acid resistance
Aliques-Granero, J., Tognonvi, M. T., & Tagnit‐Hamou, A. (2016) · Materials and Structures · doi:10.1617/s11527-016-0904-7 · Cited by 60
“0, which is different from that in the OPC mortar and typical for such systems [15, 16, 36].”
BackgroundReddy, K. C., Gudur, C., & Subramaniam, K. V. L. (2020) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2020.119514 · Cited by 62
Cements Made From Blastfurnace Slag
Moranville, M., & Kamali-Bernard, S. (2019) · Elsevier eBooks · doi:10.1016/b978-0-08-100773-0.00010-1 · Cited by 66
Geopolymers and Other Alkali-Activated Materials
Provis, J. L., & van Deventer, J. S. J. (2019) · Elsevier eBooks · doi:10.1016/b978-0-08-100773-0.00016-2 · Cited by 75
Wattez, T., Patapy, C., Frouin, L., Waligora, J., & Cyr, M. (2020) · Transportation Geotechnics · doi:10.1016/j.trgeo.2020.100412 · Cited by 62
Modeling and simulation of alkali-activated materials (AAMs): A critical review
Zuo, Y., Chen, Y., Liu, C., Gan, Y., Göbel, L., Ye, G., & Provis, J. L. (2024) · Cement and Concrete Research · doi:10.1016/j.cemconres.2024.107769 · Cited by 64
Increasing the sustainability of alkali-activated binders: The use of sugar cane straw ash (SCSA)
Moraes, J. C. B., TASHIMA, M. M., Akasaki, J. L., Melges, J. L. P., Monzó, J., Borrachero, M. V., Soriano, L., & Payá, J. (2016) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2016.07.090 · Cited by 57
“Additionally, some crystalline phases were formed: N-100/0 showed peaks of katoite (PDF Card #380368), stratlingite (PDF Card #290285) and hydrotalcite (PDF Card #140191), produced during the activation process [27,28].”
BackgroundMicro- and macro-scale characterization of nano-SiO2 reinforced alkali activated slag composites
Long, W.-J., Xiao, B.-X., Gu, Y.-C., & Xing, F. (2017) · Materials Characterization · doi:10.1016/j.matchar.2017.12.013 · Cited by 58
Omur, T., Kabay, N., Miyan, N., Özkan, H., & Özkan, Ç. (2022) · Journal of Building Engineering · doi:10.1016/j.jobe.2022.104998 · Cited by 67
Hakeem, I. Y., Zaid, O., Arbili, M. M., Alyami, M., Alhamami, A. H., & Alharthai, M. (2024) · Heliyon · doi:10.1016/j.heliyon.2024.e24263 · Cited by 55
RetractedMaldonado-Alameda, À., Giró-Paloma, J., Alfocea-Roig, A., Formosa, J., & Chimenos, J. M. (2020) · Applied Sciences · doi:10.3390/app10124129 · Cited by 56
“The broad band at 984 cm−1 ascribed to T–O stretching vibrations (where T=Si or Al) was displaced towards higher frequencies, indicating the formation of C-(A)-S-H gel [52].”
BackgroundInfluentialModeling of aqueous species interaction energies prior to nucleation in cement-based gel systems
Yang, K., & White, C. E. (2020) · Cement and Concrete Research · doi:10.1016/j.cemconres.2020.106266 · Cited by 56
Martínez-Ramírez, S., Blanco‐Varela, M. T., ERENA, I., & Gener, M. (2006) · Applied Clay Science · doi:10.1016/j.clay.2005.12.001 · Cited by 67
Self-citationAli, B., Gulzar, M. A., & Raza, A. (2021) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2021.122329 · Cited by 55
Interpretation of the early stiffening process in alkali-activated slag pastes
Sun, Y., de Lima, L. M., Rossi, L., Jiao, D., Li, Z., Ye, G., & Schutter, G. D. (2023) · Cement and Concrete Research · doi:10.1016/j.cemconres.2023.107118 · Cited by 56
Mobasher, N., Bernal, S. A., Hussain, O. H., Apperley, D. C., Kinoshita, H., & Provis, J. L. (2014) · Cement and Concrete Research · doi:10.1016/j.cemconres.2014.07.006 · Cited by 52
ASR expansion of alkali-activated cement glass aggregate mortars
He, P., Zhang, B., Lu, J., & Poon, C. S. (2020) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2020.119925 · Cited by 50
Alkali-activated materials without commercial activators: a review
Wu, Y., Jia, Z., Qi, X., Wang, W., & Guo, S. (2024) · Journal of Materials Science · doi:10.1007/s10853-024-09478-8 · Cited by 52
“H gels are produced [135].”
An experimental review of the reaction paths followed by alkali-activated slag pastes
Paillard, C., Paillard, C., Sanson, N., Palacios, M., Berté, A., Boustingorry, P., Jachiet, M., Giraudeau, C., & Kocaba, V. (2024) · Cement and Concrete Research · doi:10.1016/j.cemconres.2024.107765 · Cited by 49
Falah, M., Ohenoja, K., Obenaus-Emler, R., Kinnunen, P., & Illikainen, M. (2020) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2020.118659 · Cited by 51
Effect of hydrophobicity on autogenous shrinkage and carbonation of alkali activated slag
Qu, Z., Gauvin, F., Wang, F. Z., Liu, G., & Brouwers, H. J. H. (2020) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2020.120665 · Cited by 49
Wang, Y., Chen, R., Hu, J., Zhang, Z., Huang, H., Ma, Y., Wei, J., Zhang, Z., Yin, S., Wang, H., et al. (2021) · Corrosion Science · doi:10.1016/j.corsci.2021.109657 · Cited by 49
El-Didamony, H., Amer, A. A., El-Sokkary, T. M., & Abd-El-Aziz, H. (2012) · Ceramics International · doi:10.1016/j.ceramint.2012.06.007 · Cited by 51
TASHIMA, M. M., Reig, L., Santini, M., Moraes, J. C. B., Akasaki, J. L., Payá, J., Borrachero, M. V., & Soriano, L. (2016) · Waste and Biomass Valorization · doi:10.1007/s12649-016-9659-1 · Cited by 49
Amran, M., Onaizi, A. M., Makul, N., Abdelgader, H. S., Tang, W., Alsulami, B. T., Alluqmani, A. E., & Gamil, Y. (2023) · Results in Engineering · doi:10.1016/j.rineng.2023.101452 · Cited by 53
“This is consistent with research conducted by Bakharev et al. [133], who found that the crack intensity in the matrix phase rises as the ratio of silica to sodium oxide values increases [134].”
ResultGao, H., Al‐Damad, I. M. A., Siddika, A., Kim, T., Foster, S. J., & Hajimohammadi, A. (2025) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2025.105928 · Cited by 49
Nanomaterial and fiber-reinforced sustainable geopolymers: A systematic critical review
Ünal, M. T., Gökçe, H. S., Ayough, P., Alnahhal, A. M., Şimşek, O., & Nehdi, M. L. (2023) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2023.133325 · Cited by 46
Krivenko, P. V., Petropavlovskyi, O., & Kovalchuk, O. Y. (2018) · Eastern-European Journal of Enterprise Technologies · doi:10.15587/1729-4061.2018.119624 · Cited by 50
Yang, T., Zhang, Z., Wang, Q., & Wu, Q. (2020) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2020.119990 · Cited by 47
Effect of activator nature on property development of alkali-activated slag binders
Makhadmeh, W. A., & Soliman, A. (2020) · Journal of Sustainable Cement-Based Materials · doi:10.1080/21650373.2020.1833256 · Cited by 46
“Increasing Na2O% will lead to a high pH which boosts slag dissolutions [8,44].”
BackgroundSun, Y., Ghorbani, S., Dai, X., Ye, G., & Schutter, G. D. (2022) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2022.104415 · Cited by 47
Vance, K., Aguayo, M., Dakhane, A., Ravikumar, D., Jain, J. A., & Neithalath, N. (2014) · International Journal of Concrete Structures and Materials · doi:10.1007/s40069-014-0082-3 · Cited by 46
“…the reaction rate and extent, and the reaction products formed, thereby exerting a significant influence on the earlyand later-age properties of alkali-activated binder systems (Chithiraputhiran and Neithalath 2013; Ravikumar and Neithalath 2012a, b; Puertas et al. 2004; Hajimohammadi et al. 2011).”
BackgroundDecalcification of alkali-activated slag pastes. Effect of the chemical composition of the slag
Varga, C., Alonso, M. M., de Gutiérrez, R. M., Arcila, J. M. M., & Puertas, F. (2014) · Materials and Structures · doi:10.1617/s11527-014-0422-4 · Cited by 47
“H gel, the main reaction product of AAS pastes [11, 29, 30].”
BackgroundSelf-citationZhao, K., Liang, Y., Ji, T., Lu, Y., & Lin, X. (2020) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2020.120044 · Cited by 47
Nguyễn, T. N., Phung, Q. T., Yu, Z., Frederickx, L., Jacques, D., Sakellariou, D., Dauzères, A., Elsen, J., & Pontikes, Y. (2022) · Scientific Reports · doi:10.1038/s41598-022-09491-4 · Cited by 53
A novel high-efficient MOFs-based corrosion inhibitor for the reinforcing steel in cement extract
Wang, Y., Hu, J., Ma, Y., Zhang, Z., Huang, H., Wei, J., Yin, S., & Yu, Q. (2021) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2021.125946 · Cited by 44
Thermodynamic Modeling and Experimental Study of Carbonation of Alkali-Activated Slag Cements
Park, S., Lothenbach, B., Jang, J. G., Kim, H.-K., & Lee, N. (2023) · ACS Sustainable Chemistry & Engineering · doi:10.1021/acssuschemeng.2c05789 · Cited by 43
Part, W. K., Ramli, M. B., & Cheah, C. B. (2016) · Elsevier eBooks · doi:10.1016/b978-0-12-804524-4.00011-7 · Cited by 47
Li, C., Zhang, N., Zhang, J., Song, S., & Zhang, Y. (2021) · Materials · doi:10.3390/ma15010112 · Cited by 45
“[26] states that the peaks at −77 to −82 ppm corresponds to SiQ1 unit, and the peaks near −85 ppm corresponds to SiQ2 unit.”
BackgroundResistance of Alkali-Activated Slag Concrete to Chloride-Induced Corrosion
Park, J. W., Ann, K. Y., & Cho, C. (2015) · Advances in Materials Science and Engineering · doi:10.1155/2015/273101 · Cited by 42
“Despite debates on pozzolanic materials and their environmental impact, the pozzolanic materials have been thoroughly studied as noncarbon emitting materials [3–5].”
BackgroundEngineering and mineralogical characteristics of stabilized unfired montmorillonitic clay bricks
El-Mahllawy, M. S., & Kandeel, A. M. (2013) · HBRC Journal · doi:10.1016/j.hbrcj.2013.08.009 · Cited by 41
Application of Ca-based geopolymer with blast furnace slag, a review
Davidovits, J. (2011) · Cited by 41
Alharbi, N. A., Varela, B., & Hailstone, R. K. (2020) · Materials Characterization · doi:10.1016/j.matchar.2020.110504 · Cited by 41
Early-age strength of CO2 cured alkali-activated blast furnace slag pastes
Jun, Y., Han, S. H., & Kim, J. H. (2021) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2021.123075 · Cited by 41
On the mechanisms of shrinkage reducing admixture in alkali activated slag binders
Makhadmeh, W. A., & Soliman, A. (2022) · Journal of Building Engineering · doi:10.1016/j.jobe.2022.104812 · Cited by 47
Puertas, F., Torres‐Carrasco, M., & Alonso, M. M. (2015) · Elsevier eBooks · doi:10.1533/9781782422884.1.75 · Cited by 46
Self-citationHamdan, A., Hajimohammadi, A., Rawal, A., & Kim, T. (2022) · Cement and Concrete Research · doi:10.1016/j.cemconres.2022.107058 · Cited by 41
Allahverdi, A., Shaverdi, B., & Kani, E. N. (2010) · Cited by 40
Navarro, R., Alcocel, E. G., Sanchez, I., Garcés, P., & Zornoza, E. (2019) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2019.116917 · Cited by 41
Guo, W., Hu, J., Ma, Y., Huang, H., Yin, S., Wei, J., & Yu, Q. (2019) · Corrosion Science · doi:10.1016/j.corsci.2019.108366 · Cited by 40
Zhang, J., Sun, G., Wang, C., Zhang, Y., Wang, P., & Yan, N. J. (2020) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2020.103556 · Cited by 40
Historical Aspects and Overview
Provis, J. L., Duxson, P., Kаvalerova, Е., Krivenko, P. V., Pan, Z., Puertas, F., & van Deventer, J. S. J. (2013) · RILEM state-of-the-art reports · doi:10.1007/978-94-007-7672-2_2 · Cited by 41
Self-citationKaraca, H., Altıntığ, E., Türker, D., & Teker, M. (2018) · Journal of Dispersion Science and Technology · doi:10.1080/01932691.2018.1462191 · Cited by 43
Microstructure of chemically activated gamma-dicalcium silicate paste
Ashraf, W. (2018) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2018.07.030 · Cited by 40
Analysing the relation between pore structure and permeability of alkali-activated concrete binders
Zhang, Z., & Wang, H. (2015) · Elsevier eBooks · doi:10.1533/9781782422884.2.235 · Cited by 39
Influence of ferronickel slag on the reaction kinetics and microstructure of alkali-activated slag
Cao, R., Zhang, S., Jia, Z., Chen, C., Zhang, Z., Banthia, N., Gao, Y., & Zhang, Y. (2023) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2023.105173 · Cited by 39
Development of silica fume-based geopolymer foams
Shakouri, S., Bayer, Ö., & Erdoğan, S. T. (2020) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2020.120442 · Cited by 41
Liang, K., Cui, K., Sabri, M. M. S., & Huang, J. (2022) · Materials · doi:10.3390/ma15186436 · Cited by 38
“[47] found that the Na+ concentration in AAMs pore solutions activated by SS exceeded 1200 mmol/L.”
BackgroundChloride penetration and binding behavior in unsaturated alkali-activated slag mortars
Zhang, Y., Fang, Y., Shen, Y., Yang, Z., & Wu, K. (2023) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2023.105098 · Cited by 38
Tran, T. T., & Kwon, H.-M. (2018) · Materials · doi:10.3390/ma11081296 · Cited by 35
“The reduction of Ca/Si ratio in C‐S‐H structure indicates an enhancement in binding ability of C‐S‐H [49,50].”
BackgroundInfluentialPuligilla, S., Chen, X., & Mondal, P. (2018) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2018.09.184 · Cited by 36
Yang, Z., Shi, P., Zhang, Y., & Li, Z. (2021) · Journal of Building Engineering · doi:10.1016/j.jobe.2021.103934 · Cited by 40
Understanding the strength evolution of alkali-activated slag pastes cured at subzero temperature
Zhang, H., Ai, J., Ren, Q., Zhu, X., He, B., & Jiang, Z. (2023) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2023.104993 · Cited by 37
Application of electrochemical methods for studying steel corrosion in alkali‐activated materials
Mundra, S., Samson, G., Masi, G., Achenbach, R., Bastidas, D. M., Bernal, S. A., Bignozzi, M. C., Criado, M., Cyr, M., Gartner, N., et al. (2023) · Materials and Corrosion · doi:10.1002/maco.202313743 · Cited by 38
Cementitious composites with glass waste from recycling of cathode ray tubes
Moncea, A., Bădănoiu, A. I., Georgescu, M., & Stoleriu, S. P. (2013) · Materials and Structures · doi:10.1617/s11527-013-0041-5 · Cited by 35
Kaya, M., Köksal, F., Nodehi, M., Bayram, M., Gençel, O., & Ozbakkaloglu, T. (2022) · Sustainability · doi:10.3390/su142013496 · Cited by 38
Oinam, Y., Ju, S., Shin, M., & Pyo, S. (2023) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2023.131747 · Cited by 34
Unfired clay bricks: from laboratory to industrial production
Oti, J. E., Kinuthia, J. M., & Bai, J. (2009) · Proceedings of the Institution of Civil Engineers - Engineering Sustainability · doi:10.1680/ensu.2009.162.4.229 · Cited by 40
Kim, H.-J., Tafesse, M., Lee, H. K., & Kim, H.-K. (2019) · Cement and Concrete Research · doi:10.1016/j.cemconres.2019.05.016 · Cited by 34
Zhao, C. B., Li, Z., Peng, S., Liu, J., Wu, Q., & Xu, X. (2024) · Case Studies in Construction Materials · doi:10.1016/j.cscm.2024.e03124 · Cited by 50
Gong, K., Cheng, Y. Q., Daemen, L. L., & White, C. E. (2019) · Physical Chemistry Chemical Physics · doi:10.1039/c9cp00889f · Cited by 38
Impact of activator chemistry on permeability of alkali‐activated slags
Blyth, A. C., Eiben, C. A., Scherer, G. W., & White, C. E. (2017) · Journal of the American Ceramic Society · doi:10.1111/jace.14996 · Cited by 33
Zhang, J., Pan, G., & Yan, Y. (2021) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2021.123517 · Cited by 33
Hydration and Carbonation of Alternative Binders
Kraft, B. I. E., Achenbach, R., Ludwig, H., & Raupach, M. (2022) · Corrosion and Materials Degradation · doi:10.3390/cmd3010003 · Cited by 32
Green binding material using alkali activated blast furnace slag with silica fume
Sayed, M., & Zeedan, S. R. (2012) · HBRC Journal · doi:10.1016/j.hbrcj.2012.10.003 · Cited by 34
Maldonado-Alameda, À., Giró-Paloma, J., Andreola, F., Barbieri, L., Chimenos, J. M., & Lancellotti, I. (2022) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2022.126983 · Cited by 30
Metadata
- Authors
- Puertas, F., Fernández-Jiménez, A., & Blanco-Varela, M. T.
- Affiliations
- Instituto de Ciencias de La Construcción Eduardo Torroja (ES)
- Corresponding author
- Puertas, F
- ORCID
- Puertas, F
- Venue
- Cement and Concrete Research
- Publisher
- Elsevier BV
- Published
- 2004-01
- Volume
- 34
- Issue
- 1
- Pages
- 139-148
- ISSN
- 0008-8846 (ISSN-L)
- OpenAlex
- W2022113185
- Semantic Scholar
- 60664cf125af03ec738838ba6efc80ed97b41611
- Cited by
- 409
- References
- 29
- Citations by year
- 2026: 31 · 2025: 35 · 2024: 34 · 2023: 37 · 2022: 38 · 2021: 24 · 2020: 32 · 2019: 19 · 2018: 20 · 2017: 19 · 2016: 10 · 2015: 16 · 2014: 20 · 2013: 14 · 2012: 17
- FWCI
- 12.27
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.elsevier.com/tdm/userlicense/1.0/ (tdm)
- www.elsevier.com/legal/tdmrep-license (tdm)
- Locations
- Cement and Concrete Research (publishedVersion)
- DIGITAL.CSIC (Spanish National Research Council (CSIC)) (submittedVersion)
- Topics
- Physical Sciences › Engineering › Civil and Structural Engineering › Concrete and Cement Materials Research
- Physical Sciences › Materials Science › Materials Chemistry › Magnesium Oxide Properties and Applications
- Physical Sciences › Engineering › Civil and Structural Engineering › Geotechnical Engineering and Soil Stabilization
- Keywords
- alkali-activated slag cement, pore solution, calcium silicate hydrate, sodium hydroxide activator, Qn units, Ca/Si ratio, structural order, hydration kinetics, ion composition
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.