Pyrolysis kinetics of poly(l-lactide) with carboxyl and calcium salt end structures
Open accessThe DOI matches its Crossref record; 11 of the 11 references it cites were found in a registry or an index.
Abstract
Abstract To clarify the pyrolysis mechanism of poly( l -lactide), which has been reported as complex, the thermal decomposition of carboxyl type and calcium ion end capped PLLA (PLLA-H and PLLA-Ca, respectively) was investigated by means of thermogravimetric analysis (TG), and pyrolysis–gas chromatography–mass spectrometry (Py–GC–MS). The TG data revealed that PLLA-Ca has a lower pyrolysis temperature (220–360 °C) than that of carboxyl type PLLA-H (280–370 °C). The apparent activation energy of the decomposition reaction was estimated from TG curves at different heating rates by plural methods to be 176 and 98 kJ mol −1 for PLLA-H and PLLA-Ca, respectively. Further kinetic studies indicated that PLLA-H degraded mainly through a random reaction with a pre-exponential factor A =2.0×10 12 s −1 , whereas PLLA-Ca degraded by way of a 1st-order reaction with A =8.4×10 5 s −1 . Pyrolysis products of PLLA-H were composed of lactides and other cyclic oligomers, while the degradation products of PLLA-Ca were principally lactides. The main reaction pathway for PLLA-H pyrolysis was regarded as the random transesterification, whereas for PLLA-Ca pyrolysis the unzipping depolymerization process was dominant.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Biodegradation and biocompatibility of PLA and PLGA microspheres
Anderson, J. M., & Shive, M. S. (1997) · Advanced Drug Delivery Reviews · doi:10.1016/s0169-409x(97)00048-3 · Cited by 2,617
Large-scale production, properties and commercial applications of polylactic acid polymers
Lunt, J. (1998) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(97)00148-1 · Cited by 1,366 · cited 1×
“Thus, recently, PLLA and related copolymers have attracted industrial attention for use as commodity resins [7].”
BackgroundThermal characterization of polylactides
Jamshidi, K., Hyon, S.-H., & Ikada, Y. (1988) · Polymer · doi:10.1016/0032-3861(88)90116-4 · Cited by 692 · cited 1×
“Studies on PLLA pyrolysis have been reported by several groups [12-21].”
BackgroundThermal decomposition of biodegradable polyesters—II. Poly(lactic acid)
Kopinke, F.-D., Remmler, M., Mackenzie, K., Möder, M., & Wachsen, O. (1996) · Polymer Degradation and Stability · doi:10.1016/0141-3910(96)00102-4 · Cited by 614
Thermal degradation of poly[(R)-3-hydroxybutyrate], poly[ε-caprolactone], and poly[(S)-lactide]
Aoyagi, Y., Yamashita, K., & Doi, Y. (2002) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(01)00265-8 · Cited by 456
Polylactones: 31. Sn(II)octoate-initiated polymerization of L-lactide: a mechanistic study
Kricheldorf, H. R., Kreiser-Saunders, I., & Boettcher, C. (1995) · Polymer · doi:10.1016/0032-3861(95)93928-f · Cited by 411 · cited 2×
“59 ppm for -CH(CH3)-OCO- and -CH(CH3)-OCO- in the main chain, respectively [25].”
BackgroundLewis acid catalyzed polymerization of L-lactide. Kinetics and mechanism of the bulk polymerization
Nijenhuis, A. J., Grijpma, D. W., & Pennings, A. J. (1992) · Macromolecules · doi:10.1021/ma00050a006 · Cited by 407
McNeill, I. C., & Leiper, H. A. (1985) · Polymer Degradation and Stability · doi:10.1016/0141-3910(85)90035-7 · Cited by 404 · cited 3×
“Other reactions, such as cis-elimination and non-selective radical reactions, can also occur competitively [12-14].”
BackgroundRadano, C. P., Baker, G. L., & Smith, M. R. (2000) · Journal of the American Chemical Society · doi:10.1021/ja9930519 · Cited by 403 · cited 1×
“Commonly, PLLA is prepared by the ring-opening polymerization of L-lactide, a cyclic dimmer of L-lactic acid [8-10].”
BackgroundAjioka, M., Enomoto, K., Suzuki, K., & Yamaguchi, A. (1995) · Journal of Environmental Polymer Degradation · doi:10.1007/bf02068677 · Cited by 322 · cited 1×
“PLLA has many good properties such as mechanical strength, transparency, and compostability [4-6].”
Background
Cited by
Chemically recyclable polymers: a circular economy approach to sustainability
Hong, M., & Chen, E. Y.-X. (2017) · Green Chemistry · doi:10.1039/c7gc01496a · Cited by 876
Payne, J., & Jones, M. D. (2021) · ChemSusChem · doi:10.1002/cssc.202100400 · Cited by 426
Toward Infinitely Recyclable Plastics Derived from Renewable Cyclic Esters
Tang, X., & Chen, E. Y.-X. (2019) · Chem · doi:10.1016/j.chempr.2018.10.011 · Cited by 389
Control of thermal degradation of polylactide (PLA)-clay nanocomposites using chain extenders
Najafi, N., Heuzey, M. C., Carreau, P. J., & Wood-Adams, P. M. (2012) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2012.01.016 · Cited by 315
The Chemical Recycling of PLA: A Review
McKeown, P., & Jones, M. D. (2020) · Sustainable Chemistry · doi:10.3390/suschem1010001 · Cited by 294
Zou, H., Yi, C., Wang, L., Liu, H., & Xu, W. (2009) · Journal of Thermal Analysis and Calorimetry · doi:10.1007/s10973-009-0121-5 · Cited by 255
Chrissafis, K., Paraskevopoulos, K. M., & Bikiaris, D. N. (2005) · Thermochimica Acta · doi:10.1016/j.tca.2005.05.011 · Cited by 232
Thermal degradation behaviour of poly(lactic acid) stereocomplex
Fan, Y., Nishida, H., Shirai, Y., Tokiwa, Y., & Endo, T. (2004) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2004.03.001 · Cited by 199
Self-citationDe Clercq, R., Dusselier, M., & Sels, B. F. (2017) · Green Chem. · doi:10.1039/c7gc02040f · Cited by 194
Biodegradation of poly(l-lactide)
Tokiwa, Y., & Jarerat, A. (2004) · Biotechnology Letters · doi:10.1023/b:bile.0000025927.31028.e3 · Cited by 191
“pyrolysis (Fan et al. 2003) and chemical hydrolysis (Tsuji & Nakahara 2002), have been reported.”
MethodSelf-citationEffect of tin on poly(l-lactic acid) pyrolysis
Nishida, H., Mori, T., Hoshihara, S., Fan, Y., Shirai, Y., & Endo, T. (2003) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(03)00152-6 · Cited by 176
Self-citationBourissou, D., Moebs-Sanchez, S., & Martín-Vaca, B. (2007) · Comptes Rendus. Chimie · doi:10.1016/j.crci.2007.05.004 · Cited by 169
Thermal stability of poly (l-lactide): influence of end protection by acetyl group
Fan, Y., Nishida, H., Shirai, Y., & Endo, T. (2004) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2003.10.004 · Cited by 104
“According to our previous studies [20,25,32], it is considered that the thermal degradation of metal free PLLA-H proceeds mainly through the random scission, evolving many kinds of pyrolyzates.”
BackgroundMethodResultSelf-citationJarerat, A., Tokiwa, Y., & Tanaka, H. (2006) · Applied Microbiology and Biotechnology · doi:10.1007/s00253-006-0343-4 · Cited by 96
“Methods for PLA recycling at a temperature higher than 200°C, e.g., by pyrolysis ( Fan et al. 2003 ) and hydrolysis in water (Tsuji et al. 2003) have been studied.”
MethodSelf-citationAriffin, H., Nishida, H., Shirai, Y., & Hassan, M. A. (2010) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2010.01.018 · Cited by 85
“[Figure 1] Apparent activation energy values, Ea, for PHB-H and PHB-H/MCs degradation were estimated by using the method previously proposed by our research group [22], which is an improved method from the Doyle’s [23,24] and Reich’s [25] methods and plotted against residual weight, w, in Figure 2.”
MethodSelf-citationEffects of chain end structures on pyrolysis of poly(-lactic acid) containing tin atoms
MORI, T. (2004) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2003.11.008 · Cited by 76
“The Ea value of PLLA-H, which started from about 135 kJ mol -1 and rose to 176 kJ mol as degradation progressed, agrees with the previously reported values for purified PLLA [23,30].”
BackgroundMethodResultChemical Recycling Technology of Polylactic Acid/talc—Application into Agricultural Materials—
TSUKEGI, T., NAGASAWA, N., HORII, T., & NISHIDA, H. (2015) · KOBUNSHI RONBUNSHU · doi:10.1295/koron.2015-0008 · Cited by 4
Self-citation
Metadata
- Authors
- Fan, Y., Nishida, H., Hoshihara, S., Shirai, Y., Tokiwa, Y., & Endo, T.
- Venue
- Polymer Degradation and Stability
- Publisher
- Elsevier BV
- Published
- 2003-03
- Volume
- 79
- Issue
- 3
- Pages
- 547-562
- ISSN
- 0141-3910 (ISSN-L)
- OpenAlex
- W2018834497
- Cited by
- 124
- References
- 11
- FWCI
- 4.45
- Type
- journal article
- Language
- en
- Open access
- green
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.