Quantitative measurement of displacement and strain fields from HREM micrographs
The DOI matches its Crossref record; 27 of the 27 references it cites were found in a registry or an index.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Citations
Cites
Physical Properties of Crystals
(2007) · Materials Today · doi:10.1016/s1369-7021(07)70138-4 · Cited by 7,769
Fourier-transform method of fringe-pattern analysis for computer-based topography and interferometry
Takeda, M., Ina, H., & Kobayashi, S. (1982) · Journal of the Optical Society of America · doi:10.1364/josa.72.000156 · Cited by 4,277
The correlation averaging of a regularly arranged bacterial cell envelope protein
Saxton, W. O., & Baumeister, W. (1982) · Journal of Microscopy · doi:10.1111/j.1365-2818.1982.tb00405.x · Cited by 872
Physical properties of crystals, their representation by tensors and matrices
Boas, W. (1958) · Journal of the Mechanics and Physics of Solids · doi:10.1016/0022-5096(58)90012-7 · Cited by 689
Hirsch, P. B., & Whelan, M. J. (1960) · Philosophical Transactions of the Royal Society of London. Series A, Mathematical and Physical Sciences · doi:10.1098/rsta.1960.0013 · Cited by 453
Digital image processing: The semper system
Saxton, W. O., Pitt, T., & Horner, M. (1979) · Ultramicroscopy · doi:10.1016/s0304-3991(79)80044-3 · Cited by 350
A review of phase unwrapping techniques in fringe analysis
Judge, T. R., & Bryanston-Cross, P. J. (1994) · Optics and Lasers in Engineering · doi:10.1016/0143-8166(94)90073-6 · Cited by 286
Direct measurement of local lattice distortions in strained layer structures by HREM
Bierwolf, R., Hohenstein, M., Phillipp, F., Brandt, O., Crook, G. E., & Ploog, K. (1993) · Ultramicroscopy · doi:10.1016/0304-3991(93)90234-o · Cited by 213
Atomistic structure of 90° domain walls in ferroelectric PbTiO3thin films
Stemmer, S., Streiffer, S. K., Ernst, F., & Rüuhle, M. (1995) · Philosophical magazine. A/Philosophical magazine. A. Physics of condensed matter. Structure, defects and mechanical properties · doi:10.1080/01418619508244477 · Cited by 158
Treacy, M. M. J., & Gibson, J. M. (1986) · Journal of Vacuum Science & Technology B Microelectronics Processing and Phenomena · doi:10.1116/1.583473 · Cited by 128
Research works printed but not linked: 8
- Frank, 1982, Optik, 63, 67
- Saxton, 1992, Scanning Microscopy Supplement, 6, 53
- Hetherington, 1992, Scanning Microscopy Supplement, 6, 405
- Amelinckx, 1993, 2, 334
- Gabor, 1946, Proc. Inst. Electr. Eng., 93, 429
- Olmo, 1988, Ferroelectrics, 81, 1257
- F.M. Ross, R. Kilaas, E. Snoeck, M.J. Hÿtch, A. Thorel, L. Normand, Mater. Res. Soc. Proc. (1996), in press.
- Hawkes, 1992, Scanning Microscopy Supplement, 6, 179
Cited by
Items 201–300 of 1,001
Twin Boundary-Assisted Lithium Ion Transport
Nie, A., Gan, L., Cheng, Y., Li, Q., Yuan, Y., Mashayek, F., Wang, H., Klie, R. F., Schwingenschlögl, U., & Shahbazian‐Yassar, R. (2014) · Nano Letters · doi:10.1021/nl504087z · Cited by 100
Structure and Deformations of Pd−Ni Core−Shell Nanoparticles
Joao, S. S., Giorgio, S., Pénisson, J. M., Chapon, C., Bourgeois, S., & Henry, C. R. (2004) · The Journal of Physical Chemistry B · doi:10.1021/jp040473i · Cited by 100
Hruszkewycz, S. O., Holt, M. V., Murray, C. E., Bruley, J., Holt, J. R., Tripathi, A., Shpyrko, O., McNulty, I., Highland, M. J., & Fuoss, P. H. (2012) · Nano Letters · doi:10.1021/nl303201w · Cited by 99
Jiao, W., Chen, C., You, W., Chen, G., Xue, S., Zhang, J., Liu, J., Feng, Y., Wang, P., Wang, Y., et al. (2019) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2019.118298 · Cited by 100
Ultrafast Room Temperature Single-Photon Source from Nanowire-Quantum Dots
Bounouar, S., Elouneg-Jamroz, M., den Hertog, M., Morchutt, C., Bellet-Amalric, E., André, R., Bougerol, C., Genuist, Y., Poizat, J.-P., Tatarenko, S., et al. (2012) · Nano Letters · doi:10.1021/nl300733f · Cited by 110
Direct observation of dual-step twinning nucleation in hexagonal close-packed crystals
He, Y., Li, B., Wang, C., & Mao, S. X. (2020) · Nature Communications · doi:10.1038/s41467-020-16351-0 · Cited by 98
Xu, Z., Guo, X., Song, W., Wang, J., Qin, T., Yuan, Y., & Lu, J. B. (2023) · Advanced Materials · doi:10.1002/adma.202303612 · Cited by 110
Lattice and strain analysis of atomic resolution Z-contrast images based on template matching
Zuo, J., Shah, A. B., Kim, H., Meng, Y., Gao, W., & Rouvière, J. (2013) · Ultramicroscopy · doi:10.1016/j.ultramic.2013.07.018 · Cited by 98
“This avoids the so-called edge effect, which could be an issue in the Fourier transform based analysis [9].”
BackgroundHuang, X. B., Qi, X., Huang, Y., Li, S., Xue, C., Gan, C. L., Boey, F., & Zhang, H. (2010) · ACS Nano · doi:10.1021/nn101803m · Cited by 99
“This technique enables one to measure lattice deformations based on a given HRTEM image.(39) 41”
MethodZhang, J., Huang, L., Zhu, C., Zhou, C., Jabar, B., Li, J., Zhu, X., Wang, L., Song, C., Xin, H., et al. (2019) · Advanced Materials · doi:10.1002/adma.201905210 · Cited by 97
Yang, M., Lei, L., Jiang, Y., Xu, F., & Yin, C. (2023) · Corrosion Science · doi:10.1016/j.corsci.2023.111211 · Cited by 97
Lessons from hafnium dioxide-based ferroelectrics
Noheda, B., Nukala, P., & Acuautla, M. (2023) · Nature Materials · doi:10.1038/s41563-023-01507-2 · Cited by 99
Zhou, Y., Hu, H., Peng, C., Liu, J., Zhao, Y., Shang, X., Guo, C., Shen, Z., Song, M., Zhang, L., et al. (2025) · Corrosion Science · doi:10.1016/j.corsci.2025.113352 · Cited by 97
Afonso, C. R. M., Ferrandini, P. L., Ramirez, A. J., & Caram, R. (2009) · Acta Biomaterialia · doi:10.1016/j.actbio.2009.11.010 · Cited by 97
“4a presents the GPA ð10 1Þb interplanar spacing strain map combined with the original HR-TEM image shown in Fig.”
BackgroundMethodInfluentialEffects of postmetallization annealing on interface properties of Al 2 O 3 /GaN structures
Hashizume, T., Kaneki, S., Oyobiki, T., Ando, Y., Sasaki, S., & Nishiguchi, K. (2018) · Applied Physics Express · doi:10.7567/apex.11.124102 · Cited by 97
Dislocation-strained MoS2 nanosheets for high-efficiency hydrogen evolution reaction
Wang, S., Wang, L., Xie, L., Zhao, W., Liu, X., Zhuang, Z., Zhuang, Y., Chen, J., Liu, S., & Zhao, Q. (2022) · Nano Research · doi:10.1007/s12274-022-4158-0 · Cited by 94
Entropy‐Change Driven Highly Reversible Sodium Storage for Conversion‐Type Sulfide
Zhao, J., Zhang, Y., Chen, X., Sun, G., Yang, X., Zeng, Y., Tian, R., & Du, F. (2022) · Advanced Functional Materials · doi:10.1002/adfm.202206531 · Cited by 99
Nasr, B., Wang, D., Kruk, R., Rösner, H., Hahn, H., & Dasgupta, S. (2012) · Advanced Functional Materials · doi:10.1002/adfm.201202500 · Cited by 108
Observing and measuring strain in nanostructures and devices with transmission electron microscopy
Hÿtch, M. J., & Minor, A. M. (2014) · MRS Bulletin · doi:10.1557/mrs.2014.4 · Cited by 94
Self-citationSeeing Is Believing: Weak Phonon Scattering from Nanostructures in Alkali Metal-Doped Lead Telluride
He, J., Androulakis, J., Kanatzidis, M. G., & Dravid, V. P. (2011) · Nano Letters · doi:10.1021/nl203626n · Cited by 94
Quantitative Structural Analysis of Binary Nanocrystal Superlattices by Electron Tomography
Friedrich, H., Gommes, C., Overgaag, K., Meeldijk, J. D., Evers, W. H., de Nijs, B., Boneschanscher, M. P., de Jongh, P. E., Verkleij, A. J., de Jong, K. P., et al. (2009) · Nano Letters · doi:10.1021/nl901212m · Cited by 94
Effect of lattice mismatch and shell thickness on strain in core@shell nanocrystals
Gamler, J. T. L., Leonardi, A., Sang, X., Koczkur, K. M., Unocic, R. R., Engel, M., & Skrabalak, S. E. (2020) · Nanoscale Advances · doi:10.1039/d0na00061b · Cited by 100
Shen, Q., Xue, J., Li, Y., Gao, G., Li, Q., Liu, X., Jia, H., Xu, B., Wu, Y., & Dillon, S. J. (2020) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2020.119552 · Cited by 94
Controlled stripes of ultrafine ferroelectric domains
Feigl, L., Yudin, P. V., Stolichnov, I., Sluka, T., Shapovalov, K., Mtebwa, M. H., Sandu, C. S., Wei, X., Tagantsev, A. K., & Setter, N. (2014) · Nature Communications · doi:10.1038/ncomms5677 · Cited by 94
Plasticity and Grain Boundary Diffusion at Small Grain Sizes
Wilde, G., Ribbe, J., Reglitz, G., Wegner, M., Rösner, H., Estrin, Y., Zehetbauer, M., Setman, D., & Divinski, S. V. (2010) · Advanced Engineering Materials · doi:10.1002/adem.200900333 · Cited by 95
Artefacts in geometric phase analysis of compound materials
Peters, J. J. P., Beanland, R., Alexe, M., Cockburn, J. W., Revin, D. G., Zhang, S. Y., & Sánchez, A. M. (2015) · Ultramicroscopy · doi:10.1016/j.ultramic.2015.05.020 · Cited by 93
“By repeating this process for a non-collinear g , all components of the projected displacement field can be measured which are then differentiated to get the strain [13].”
BackgroundInfluentialMoiré enhanced charge density wave state in twisted 1T-TiTe2/1T-TiSe2 heterostructures
Zhao, W.-M., Zhu, L. Q., Nie, Z., Li, Q., Wang, Q., Dou, L.-G., Hu, J.-G., Xian, L., Meng, S., & Li, S. (2021) · Nature Materials · doi:10.1038/s41563-021-01167-0 · Cited by 93
Core–Shell Layered Oxide Cathode for High-Performance Sodium-Ion Batteries
Chen, C., Han, Z., Chen, S., Qi, S., Lan, X., Zhang, C., Chen, L., Wang, P., & Wei, W. F. (2020) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.9b19260 · Cited by 92
Engineering Phase Transformation of MoS2/RGO by N-doping as an Excellent Microwave Absorber
Guo, H., Wang, L., You, W., Yang, L., Li, X., Chen, G., Wu, Z., Xiang, Q., Wang, M., & Che, R. (2020) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.0c01998 · Cited by 94
Atomic Defects and Doping of Monolayer NbSe2
Nguyen, L. T. T., Komsa, H., Khestanova, E., Kashtiban, R. J., Peters, J. J. P., Lawlor, S. D., Sánchez, A. M., Sloan, J., Gorbachev, R., Grigorieva, I. V., et al. (2017) · ACS Nano · doi:10.1021/acsnano.6b08036 · Cited by 97
The structural properties of GaN/AlN core–shell nanocolumn heterostructures
Hestroffer, K., Mata, R., Camacho‐Mojica, D. C., Leclère, C., Tourbot, G., Niquet, Y., Cros, A., Bougerol, C., Renevier, H., & Daudin, B. (2010) · Nanotechnology · doi:10.1088/0957-4484/21/41/415702 · Cited by 91
Flexoelectric Thin-Film Photodetectors
Wu, M., Jiang, Z., Lou, X., Zhang, F., Song, D., Ning, S., Guo, M., Pennycook, S. J., Dai, J., & Wen, Z. (2021) · Nano Letters · doi:10.1021/acs.nanolett.1c00055 · Cited by 91
Structural transition and migration of incoherent twin boundary in diamond
Tong, K., Zhang, X., Li, Z., Wang, Y., Luo, K., Li, C., Jin, T., Chang, Y., Zhao, S., Wu, Y., et al. (2024) · Nature · doi:10.1038/s41586-023-06908-6 · Cited by 94
Grédiac, M., Blaysat, B., & Sur, F. (2017) · Experimental Mechanics · doi:10.1007/s11340-017-0279-x · Cited by 91
“ux and uy can be retrieved from these equations by using several approaches, for instance the Geometric Phase Analysis (GPA) [41], its windowed version [43], or the localized spectrum analysis [17] used in the present study.”
MethodRoom-temperature epitaxial welding of 3D and 2D perovskites
Zhu, Z., Zhu, C., Yang, L., Chen, Q., Zhang, L., Dai, J., Cao, J., Zeng, S., Wang, Z., Wang, Z., et al. (2022) · Nature Materials · doi:10.1038/s41563-022-01311-4 · Cited by 93
Yang, L., Wei, C., Jiang, F., Liang, D., Yan, K., Cheng, Z., Li, Z., & Ren, F. (2023) · Acta Materialia · doi:10.1016/j.actamat.2023.119526 · Cited by 90
Imaging moiré deformation and dynamics in twisted bilayer graphene
de Jong, T. A., Benschop, T., Chen, X., Krasovskii, E. E., de Dood, M. J. A., Tromp, R. M., Allan, M. P., & van der Molen, S. J. (2022) · Nature Communications · doi:10.1038/s41467-021-27646-1 · Cited by 101
Gong, Y., Chen, Y., Zhang, Q., Meng, F., Shi, J., Liu, X., Liu, X., Zhang, J., Wang, H., Wang, J., et al. (2018) · Nature Communications · doi:10.1038/s41467-018-05833-x · Cited by 88
Song, Y., Cui, Y., Li, B., Geng, L., Yan, J., Zhu, D., Zhou, P., Zhou, J. P., Yan, Z., Xue, Q., et al. (2023) · Nano Energy · doi:10.1016/j.nanoen.2023.108846 · Cited by 88
A route for a strong increase of critical current in nanostrained iron-based superconductors
Ozaki, T., Wu, L., Zhang, C., Jaroszynski, J. J., Si, W., Zhou, J., Zhu, Y., & Li, Q. (2016) · Nature Communications · doi:10.1038/ncomms13036 · Cited by 88
Linden, Y., Pinkas, M., Munitz, A., & Meshi, L. (2017) · Scripta Materialia · doi:10.1016/j.scriptamat.2017.06.015 · Cited by 88
Shamsi, J., Dang, Z., Ijaz, P., Abdelhady, A. L., Bertoni, G., Moreels, I., & Manna, L. (2017) · Chemistry of Materials · doi:10.1021/acs.chemmater.7b04827 · Cited by 88
Atomic-scale strain manipulation of a charge density wave
Gao, S., Flicker, F., Sankar, R., Zhao, H., Ren, Z., Rachmilowitz, B., Balachandar, S., Chou, F. C., Burch, K. S., Wang, Z., et al. (2018) · Proceedings of the National Academy of Sciences · doi:10.1073/pnas.1718931115 · Cited by 87
Strain distribution in GaN∕AlN quantum-dot superlattices
Sarigiannidou, E., Monroy, E., Daudin, B., Rouvière, J., & Andreev, A. D. (2005) · Applied Physics Letters · doi:10.1063/1.2123394 · Cited by 87
Wu, Y., Ciston, J., Kräemer, S., Bailey, N., Odette, G. R., & Hosemann, P. (2016) · Acta Materialia · doi:10.1016/j.actamat.2016.03.031 · Cited by 86
“5% in the ferrite matrix as determined by GPA as shown in Supplemental Fig.”
Qin, H., Lin, G., Zhang, J., Cao, X., Xia, W., Yang, H., Yuan, K., Jin, T., Wang, Q., & Jiao, L. (2025) · Advanced Materials · doi:10.1002/adma.202417593 · Cited by 85
Atomic-Scale Observation of O1 Faulted Phase-Induced Deactivation of LiNiO 2 at High Voltage
Wang, C., Zhang, R., Kisslinger, K., & Xin, H. L. (2021) · Nano Letters · doi:10.1021/acs.nanolett.1c00862 · Cited by 85
Grieb, T., Müller‐Caspary, K., Fritz, R., Schowalter, M., Neugebohrn, N., Knaub, N., Volz, K., & Rosenauer, A. (2012) · Ultramicroscopy · doi:10.1016/j.ultramic.2012.03.014 · Cited by 86
“Strain field measurements from STEM images were done for various alloys [22–25], by either real space methods (peak finding, or peak pair [26,27]) or the geometric phase analysis [28] in Fourier space.”
MethodTaraci, J. L., Hÿtch, M., Clement, T., Peralta, P. D., McCartney, M. R., Drucker, J. S., & Picraux, S. T. (2005) · Nanotechnology · doi:10.1088/0957-4484/16/10/062 · Cited by 85
Self-citationA Microdot Multilayer Oxide Device: Let Us Tune the Strain-Ionic Transport Interaction
Schweiger, S., Kubicek, M., Messerschmitt, F., Murer, C., & Rupp, J. L. M. (2014) · ACS Nano · doi:10.1021/nn501128y · Cited by 84
Zheng, X., Han, W., Yang, K., Wong, L. W., Tsang, C. S., Lai, K. H., Zheng, F., Yang, T., Lau, S. P., Ly, T. H., et al. (2022) · Science Advances · doi:10.1126/sciadv.abo0773 · Cited by 84
Dynamic reconfiguration of van der Waals gaps within GeTe–Sb 2 Te 3 based superlattices
Momand, J., Wang, R., Boschker, J. E., Verheijen, M. A., Calarco, R., & Kooi, B. J. (2017) · Nanoscale · doi:10.1039/c7nr01684k · Cited by 84
Accurate Control of Core–Shell Upconversion Nanoparticles through Anisotropic Strain Engineering
Zhao, J., Chen, X., Chen, B., Luo, X. G., Sun, T., Zhang, W., Wang, C., Lin, J., Su, D., Qiao, X., et al. (2019) · Advanced Functional Materials · doi:10.1002/adfm.201903295 · Cited by 83
Paull, O. H. C., Xu, C., Cheng, X., Zhang, Y., Xu, B., Kelley, K. P., de Marco, A., Vasudevan, R. K., Bellaïche, L., Nagarajan, V., et al. (2021) · Nature Materials · doi:10.1038/s41563-021-01098-w · Cited by 88
Heusler-alloy films for spintronic devices
Hirohata, A., Sagar, J. T., Lari, L., Fleet, L. R., & Lazarov, V. K. (2013) · Applied Physics A · doi:10.1007/s00339-013-7679-2 · Cited by 86
Huang, Z., Wang, S., Guo, X. W., Marlton, F. P., Fan, Y., Pang, W. K., Huang, T., Xiao, J., Li, D., Liu, H., et al. (2024) · Advanced Materials · doi:10.1002/adma.202410857 · Cited by 82
Atomically Intimate Contact between Solid Electrolytes and Electrodes for Li Batteries
Li, F., Li, J., Zhu, F., Liu, T., Xu, B., Kim, T., Kramer, M. J., Ma, C., Zhou, L., & Nan, C. (2019) · Matter · doi:10.1016/j.matt.2019.05.004 · Cited by 81
Xu, J., Han, Z., Jiang, K., Bai, P., Liang, Y., Zhang, X., Wang, P., Guo, S., & Zhou, H. S. (2019) · Small · doi:10.1002/smll.201904388 · Cited by 81
Chu, S., Liu, P., Zhang, Y., Wang, X., Song, S., Zhu, T., Zhang, Z., Han, X., Sun, B., & Chen, M. W. (2022) · Nature Communications · doi:10.1038/s41467-022-31800-8 · Cited by 81
Jiang, Q., Li, M., Li, J., Wang, J., Zhang, G., Wang, J., Zuo, J., Cao, G., Duan, R., Hao, Y., et al. (2025) · Advanced Materials · doi:10.1002/adma.202417620 · Cited by 81
Conductivity and Local Structure of LaNiO 3 Thin Films
Fowlie, J., Gibert, M., Tieri, G., Gloter, A., Íñiguez, J., Filippetti, A., Catalano, S., Gariglio, S., Schober, A., Guennou, M., et al. (2017) · Advanced Materials · doi:10.1002/adma.201605197 · Cited by 80
Li, M., Sun, Q., Xu, S., Hong, M., Lyu, W., Liu, J. Y., Wang, Y., Dargusch, M. S., Zou, J., & Chen, Z. (2021) · Advanced Materials · doi:10.1002/adma.202102575 · Cited by 80
Jia, Z., Zhao, Q., Zhang, Y., Xu, Y., Chen, Y., Deng, X., Zhang, F., Wang, L., & Guo, D. (2022) · Materials Science and Engineering A · doi:10.1016/j.msea.2022.144543 · Cited by 80
Liang, G., Yang, L., Han, Q., Chen, G., Lin, C., Chen, Y., Luo, L., Liu, X., Li, Y., & Che, R. (2020) · Advanced Energy Materials · doi:10.1002/aenm.201904267 · Cited by 79
Fujisawa, K., Carvalho, B. R., Zhang, T., Perea‐López, N., Lin, Z., Carôzo, V., Ramos, S. L. L. M., Kahn, E., Bolotsky, A., Liu, H., et al. (2021) · ACS Nano · doi:10.1021/acsnano.0c10897 · Cited by 79
Resolving strain in carbon nanotubes at the atomic level
Warner, J. H., Young, N. P., Kirkland, A. I., & Briggs, G. A. D. (2011) · Nature Materials · doi:10.1038/nmat3125 · Cited by 86
Zhang, S., Huang, Z., Wen, Z., Zhang, L., Jin, J. H., Shahbazian‐Yassar, R., & Yang, J. (2017) · Nano Letters · doi:10.1021/acs.nanolett.7b00603 · Cited by 80
Geng, W., Guo, X., Zhu, Y., Tang, Y., Feng, Y., Zou, M., Wang, Y., Han, M., Ma, J., Wu, B., et al. (2018) · ACS Nano · doi:10.1021/acsnano.8b05449 · Cited by 84
Diffusional-displacive transformation in a metastable β titanium alloy and its strengthening effect
Qi, L., He, S., Chen, C., Jiang, B., Hao, Y., Ye, H., Yang, R., & Du, K. (2020) · Acta Materialia · doi:10.1016/j.actamat.2020.05.058 · Cited by 78
Dislocation and oxygen-release driven delithiation in Li2MnO3
Nakayama, K., Ishikawa, R., Kobayashi, S., Shibata, N., & Ikuhara, Y. (2020) · Nature Communications · doi:10.1038/s41467-020-18285-z · Cited by 78
Effects of solar irradiation on thermally driven CO2 methanation using Ni/CeO2–based catalyst
Golovanova, V., Spadaro, M. C., Arbiol, J., Golovanov, V., Rantala, T. T., Andreu, T., & Morante, J. R. (2021) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2021.120038 · Cited by 80
“In order to analyze the possible strain influence of the Ni nanoparticles embedded in the CeO2 mesoporous channels, we used the Geometrical Phase Analysis (GPA) routines in the Digital Micrograph software [48].”
MethodKoch, C. T., Özdöl, V. B., & van Aken, P. A. (2010) · Applied Physics Letters · doi:10.1063/1.3337090 · Cited by 78
STEM_CELL: A software tool for electron microscopy. Part 2 analysis of crystalline materials
Grillo, V., & Rossi, F. (2012) · Ultramicroscopy · doi:10.1016/j.ultramic.2012.10.009 · Cited by 78
MacLaren, I., & Ramasse, Q. M. (2014) · International Materials Reviews · doi:10.1179/1743280413y.0000000026 · Cited by 94
Semiconductor–Ferromagnetic Insulator–Superconductor Nanowires: Stray Field and Exchange Field
Liu, Y., Vaitiekėnas, S., Martí‐Sánchez, S., Koch, C., Hart, S., Cui, Z., Kanne, T., Khan, S. A., Tanta, R., Upadhyay, S., et al. (2019) · Nano Letters · doi:10.1021/acs.nanolett.9b04187 · Cited by 86
Strain states and unique properties in cold-rolled TiNi shape memory alloys
Liang, Q., Zhao, S., Liang, C., Zhao, T., Wang, D., Ding, X., Li, S., Wang, Y., Zheng, Y., Ren, X., et al. (2022) · Acta Materialia · doi:10.1016/j.actamat.2022.117890 · Cited by 77
Paolella, A., Bertoni, G., Dilena, E., Marras, S., Ansaldo, A., Manna, L., & George, C. (2014) · Nano Letters · doi:10.1021/nl4046697 · Cited by 77
Jabar, B., Qin, X., Li, D., Zhang, J., Mansoor, A., Xin, H., Song, C., & Huang, L. (2019) · Journal of Materials Chemistry A · doi:10.1039/c9ta05798f · Cited by 76
Mukherjee, D., Gamler, J. T. L., Skrabalak, S. E., & Unocic, R. R. (2020) · ACS Catalysis · doi:10.1021/acscatal.0c00224 · Cited by 80
Jabar, B., Qin, X., Mansoor, A., Ming, H., Huang, L., Danish, M. H., Zhang, J., Li, D., Zhu, C., Xin, H., et al. (2020) · Nano Energy · doi:10.1016/j.nanoen.2020.105512 · Cited by 77
Tang, Y., Zhu, Y., & Ma, X. (2015) · Ultramicroscopy · doi:10.1016/j.ultramic.2015.09.014 · Cited by 76
Equilibrium and stability of phase-separating Au–Pt nanoparticles
Braidy, N., Purdy, G. R., & Botton, G. A. (2008) · Acta Materialia · doi:10.1016/j.actamat.2008.08.024 · Cited by 76
Nanoscale diffractive probing of strain dynamics in ultrafast transmission electron microscopy
Feist, A., da Silva, N. R., Liang, W., Ropers, C., & Schäfer, S. (2018) · Structural Dynamics · doi:10.1063/1.5009822 · Cited by 76
Role of crystal defects on brittleness of C15 Cr2Nb Laves phase
Yang, Z., Chisholm, M. F., Yang, B., Ma, X., Wang, Y., Zhuo, M. J., & Pennycook, S. J. (2012) · Acta Materialia · doi:10.1016/j.actamat.2012.01.030 · Cited by 75
Mapping stress and strain in nanostructures by high-resolution transmission electron microscopy
Hÿtch, M., & Houdellier, F. (2006) · Microelectronic Engineering · doi:10.1016/j.mee.2006.10.062 · Cited by 75
Self-citationBals, S., Goris, B., Liz‐Marzán, L. M., & Tendeloo, G. V. (2014) · Angewandte Chemie International Edition · doi:10.1002/anie.201401059 · Cited by 75
Kim, H., Lee, S., Shin, J. H., Zhu, M., Akl, M., Lu, K., Han, N. M., Baek, Y., Chang, C. S., Suh, J. M., et al. (2022) · Nature Nanotechnology · doi:10.1038/s41565-022-01200-6 · Cited by 74
Copper lattice tension boosts full-cell CO electrolysis to multi-carbon olefins and oxygenates
Ma, W., Xie, S., Zhang, B., He, X., Liu, X., Mei, B., Sun, F., Jiang, Z. R., Li, L., Zhang, Q., et al. (2023) · Chem · doi:10.1016/j.chempr.2023.03.022 · Cited by 74
Nanostructure and strain in InGaN/GaN superlattices grown in GaN nanowires
Kehagias, T., Dimitrakopulos, G. P., Becker, P., Kioseoglou, J., Furtmayr, F., Koukoula, T., Häusler, I., Chernikov, A., Chatterjee, S., Karakostas, T., et al. (2013) · Nanotechnology · doi:10.1088/0957-4484/24/43/435702 · Cited by 74
Spurgeon, S. R., Sloppy, J. D. R., Kepaptsoglou, D. M., Balachandran, P. V., Nejati, S., Karthik, J., Damodaran, A. R., Johnson, C. L., Ambaye, H., Goyette, R. J., et al. (2013) · ACS Nano · doi:10.1021/nn405636c · Cited by 74
“1% accuracy down to the nanometer scale.(50,51) In all samples the in-plane strain is essentially uniform over the 3 5 nm integration window, varying by <0.”
BackgroundLiu, Y., Wang, Y., Zhu, Y., Lei, C.-H., Tang, Y., Li, S., Zhang, S., Li, J., & Ma, X. (2017) · Nano Letters · doi:10.1021/acs.nanolett.7b02615 · Cited by 74
Metal–ferroelectric supercrystals with periodically curved metallic layers
Hadjimichael, M., Li, Y., Zatterin, E. M., Chahine, G., Conroy, M., Moore, K., O’Connell, E. N., Ondrejkovič, P., Márton, P., Hlinka, J., et al. (2021) · Nature Materials · doi:10.1038/s41563-020-00864-6 · Cited by 74
Tripathy, A., Saravanakumar, B., Mohanty, S., NAYAK, S. K., & Ramadoss, A. (2021) · ACS Applied Electronic Materials · doi:10.1021/acsaelm.1c00267 · Cited by 73
Ming, H., Zhu, G., Zhu, C., Qin, X., Chen, T., Zhang, J., Li, D., Xin, H., & Jabar, B. (2021) · ACS Nano · doi:10.1021/acsnano.1c03120 · Cited by 73
High‐Entropy Engineering for Broadband Infrared Radiation
Wang, W., Liu, B., He, C., Zhao, P. C., Zhao, S., Wang, Z., Lu, Z., Guo, H., Ren, G., Liu, G., et al. (2023) · Advanced Functional Materials · doi:10.1002/adfm.202303197 · Cited by 103
High-Entropy Strategy to Achieve Electronic Band Convergence for High-Performance Thermoelectrics
Li, K., Sun, L., Bai, W. Y., Ma, N., Zhao, C., Zhao, J., Xiao, C., & Xie, Y. (2024) · Journal of the American Chemical Society · doi:10.1021/jacs.4c04048 · Cited by 75
Ductilization of single-phase refractory high-entropy alloys via activation of edge dislocation
Wang, Y. W., He, Q., Ye, Z. H., Liao, Y. C., Li, C., Wang, Q., & Gu, J. (2024) · Acta Materialia · doi:10.1016/j.actamat.2024.120614 · Cited by 73
Zhang, X., Yin, H., Dang, C., Nie, H., Huang, Z., Zheng, S., Du, M., Gu, Z., Cao, J., & Wu, X. (2025) · Angewandte Chemie International Edition · doi:10.1002/anie.202425569 · Cited by 73
Tilt boundaries and associated solute segregation in a Mg–Gd alloy
Zhu, Y., Bian, M., & Nie, J. (2017) · Acta Materialia · doi:10.1016/j.actamat.2016.12.032 · Cited by 73
Hu, Q., Qiu, W., Chen, L., Chen, J., Yang, L., & Tang, J. (2021) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.1c12722 · Cited by 72
Metadata
- Authors
- Hÿtch, M. J., Snoeck, E., & Kilaas, R.
- Affiliations
- Centre National de la Recherche Scientifique (FR)
- Lawrence Berkeley National Laboratory (US)
- Corresponding author
- Hÿtch, M.J.
- Venue
- Ultramicroscopy
- Publisher
- Elsevier BV
- Published
- 1998-08
- Volume
- 74
- Issue
- 3
- Pages
- 131-146
- ISSN
- 0304-3991 (ISSN-L)
- OpenAlex
- W1970014398
- Semantic Scholar
- 7f38bb189a356c5a9f9438c2e0567a2d47f21065
- Cited by
- 2,752
- References
- 27
- Citations by year
- 2026: 234 · 2025: 347 · 2024: 276 · 2023: 194 · 2022: 164 · 2021: 156 · 2020: 158 · 2019: 126 · 2018: 98 · 2017: 120 · 2016: 105 · 2015: 105 · 2014: 91 · 2013: 96 · 2012: 87
- FWCI
- 11.67
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.elsevier.com/tdm/userlicense/1.0/ (tdm)
- Locations
- Ultramicroscopy (publishedVersion)
- Funders
- U.S. Department of Energy
- Basic Energy Sciences
- Topics
- Life Sciences › Biochemistry, Genetics and Molecular Biology › Structural Biology › Advanced Electron Microscopy Techniques and Applications
- Physical Sciences › Materials Science › General Materials Science › Advanced Materials Characterization Techniques
- Physical Sciences › Materials Science › Materials Chemistry › Ferroelectric and Piezoelectric Materials
- Keywords
- displacement field measurement, strain mapping, inverse Fourier transform, domain walls, ferroelectric-ferroelastic coupling, lead titanate
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.