Quantitative measurement of displacement and strain fields from HREM micrographs
The DOI matches its Crossref record; 27 of the 27 references it cites were found in a registry or an index.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Citations
Cites
Physical Properties of Crystals
(2007) · Materials Today · doi:10.1016/s1369-7021(07)70138-4 · Cited by 7,769
Fourier-transform method of fringe-pattern analysis for computer-based topography and interferometry
Takeda, M., Ina, H., & Kobayashi, S. (1982) · Journal of the Optical Society of America · doi:10.1364/josa.72.000156 · Cited by 4,277
The correlation averaging of a regularly arranged bacterial cell envelope protein
Saxton, W. O., & Baumeister, W. (1982) · Journal of Microscopy · doi:10.1111/j.1365-2818.1982.tb00405.x · Cited by 872
Physical properties of crystals, their representation by tensors and matrices
Boas, W. (1958) · Journal of the Mechanics and Physics of Solids · doi:10.1016/0022-5096(58)90012-7 · Cited by 689
Hirsch, P. B., & Whelan, M. J. (1960) · Philosophical Transactions of the Royal Society of London. Series A, Mathematical and Physical Sciences · doi:10.1098/rsta.1960.0013 · Cited by 453
Digital image processing: The semper system
Saxton, W. O., Pitt, T., & Horner, M. (1979) · Ultramicroscopy · doi:10.1016/s0304-3991(79)80044-3 · Cited by 350
A review of phase unwrapping techniques in fringe analysis
Judge, T. R., & Bryanston-Cross, P. J. (1994) · Optics and Lasers in Engineering · doi:10.1016/0143-8166(94)90073-6 · Cited by 286
Direct measurement of local lattice distortions in strained layer structures by HREM
Bierwolf, R., Hohenstein, M., Phillipp, F., Brandt, O., Crook, G. E., & Ploog, K. (1993) · Ultramicroscopy · doi:10.1016/0304-3991(93)90234-o · Cited by 213
Atomistic structure of 90° domain walls in ferroelectric PbTiO3thin films
Stemmer, S., Streiffer, S. K., Ernst, F., & Rüuhle, M. (1995) · Philosophical magazine. A/Philosophical magazine. A. Physics of condensed matter. Structure, defects and mechanical properties · doi:10.1080/01418619508244477 · Cited by 158
Treacy, M. M. J., & Gibson, J. M. (1986) · Journal of Vacuum Science & Technology B Microelectronics Processing and Phenomena · doi:10.1116/1.583473 · Cited by 128
Research works printed but not linked: 8
- Frank, 1982, Optik, 63, 67
- Saxton, 1992, Scanning Microscopy Supplement, 6, 53
- Hetherington, 1992, Scanning Microscopy Supplement, 6, 405
- Amelinckx, 1993, 2, 334
- Gabor, 1946, Proc. Inst. Electr. Eng., 93, 429
- Olmo, 1988, Ferroelectrics, 81, 1257
- F.M. Ross, R. Kilaas, E. Snoeck, M.J. Hÿtch, A. Thorel, L. Normand, Mater. Res. Soc. Proc. (1996), in press.
- Hawkes, 1992, Scanning Microscopy Supplement, 6, 179
Cited by
Items 801–900 of 1,001
Chu, S., Zhang, F., Chen, D., Chen, M. W., & Liu, P. (2024) · Nano Letters · doi:10.1021/acs.nanolett.3c04516 · Cited by 26
Li, Z., Zhang, L., Svendsen, B., Xue, Q., Tang, S., Ma, Y., & Liu, W. (2024) · International Journal of Plasticity · doi:10.1016/j.ijplas.2024.104156 · Cited by 26
Wang, Y., Ruterana, P., Kret, S., Kazzi, S. E., Desplanque, L., & Wallart, X. (2013) · Applied Physics Letters · doi:10.1063/1.4790296 · Cited by 29
Stoichiometry of LaAlO3 films grown on SrTiO3 by pulsed laser deposition
Golalikhani, M., Lei, Q., Chen, G., Spanier, J. E., Ghassemi, H., Johnson, C. L., Taheri, M. L., & Xi, X. X. (2013) · Journal of Applied Physics · doi:10.1063/1.4811821 · Cited by 26
Tikhomirov, V. G., Zemlyakov, V. E., Volkov, V. V., Parnes, Y. M., Vyuginov, V. N., Lundin, W. V., Sakharov, A. V., Zavarin, E. E., Tsatsul’nikov, A. F., Cherkashin, N. A., et al. (2016) · Semiconductors · doi:10.1134/s1063782616020263 · Cited by 26
Chen, X., Lei, B., Zhu, Y. S., Zhou, J., Liu, Z., Ji, W., & Zhou, W. (2020) · Nanoscale · doi:10.1039/d0nr03530k · Cited by 26
On the formation mechanisms of intragranular shear bands in olivine by stress-induced amorphization
Idrissi, H., Béché, A., Gauquelin, N., Haq, I. U., Bollinger, C., Demouchy, S., Verbeeck, J., Pardoen, T., Schryvers, D., & Cordier, P. (2022) · Acta Materialia · doi:10.1016/j.actamat.2022.118247 · Cited by 26
Markovskyi, A., Gorbenko, V., Yokosawa, T., Will, J., Spiecker, E., Batentschuk, M., Elia, J., Fedorov, A. G., Pakuła, M., Kaczmarek, M., et al. (2022) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2022.167159 · Cited by 26
Li, Q., Wang, C., Lin, Z., Wang, L., Xiao, Y., Zhang, P., Cao, X., Fang, Y., Liao, Q., Yang, J. B., et al. (2022) · Acta Materialia · doi:10.1016/j.actamat.2022.118664 · Cited by 26
Peters, J. J. P., Mullarkey, T., Hedley, E., Müller, K. H., Porter, A. E., Mostaed, A., & Jones, L. (2023) · Nature Communications · doi:10.1038/s41467-023-40875-w · Cited by 26
Effect of interfacial stress on microchemistry and coercivity in 2:17-type SmCo sintered magnets
Yang, L., Zuo, S., Guan, C., Liu, Z., Hu, M., Kang, D., Zhao, M., Liu, B., Liu, J., Peng, Y. L., et al. (2023) · Acta Materialia · doi:10.1016/j.actamat.2023.119580 · Cited by 26
Ribet, S. M., Varnavides, G., Pedroso, C. C. S., Cohen, B. E., Ercius, P. A., Scott, M. C., & Ophus, C. (2024) · Applied Physics Letters · doi:10.1063/5.0206814 · Cited by 26
Sun, H., Wang, Y., Liu, Y., Wu, R., Chang, A., Zhao, P., & Zhang, B. (2024) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.4c00187 · Cited by 26
Dual-phase ceramics based on multi-cation boride and carbide: Investigations at the nanoscale
Smith, S. M., Gilli, N., Fahrenholtz, W. G., Hilmas, G. E., García-González, S., Jiménez‐Piqué, E., Stefano Curtarolo, A., & Silvestroni, L. (2024) · Journal of Materiomics · doi:10.1016/j.jmat.2024.06.002 · Cited by 26
Pd-Assisted Growth of InAs Nanowires
Heun, S., Radha, B., Ercolani, D., Kulkarni, G. U., Rossi, F., Grillo, V., Salviati, G., Beltram, F., & Sorba, L. (2010) · Crystal Growth & Design · doi:10.1021/cg1008335 · Cited by 26
Wang, Y. Y., Li, J., Domenicucci, A., & Bruley, J. (2012) · Ultramicroscopy · doi:10.1016/j.ultramic.2012.08.008 · Cited by 26
Nakamura, A., Furutsuki, S., Nishimura, S., Tohei, T., Sato, Y., Shibata, N., Yamada, A., & Ikuhara, Y. (2014) · Chemistry of Materials · doi:10.1021/cm5024986 · Cited by 28
Klinger, M., Polívka, L., Jäger, A., & Tyunina, M. (2016) · Journal of Applied Crystallography · doi:10.1107/s1600576716003800 · Cited by 26
“State-ofthe-art HRTEM combined with geometric phase analysis (GPA) (Hÿtch et al., 1998, 2003; Diercks et al., 2011; Hÿtch, 1997; Johnson et al., 2004) allows for mapping lattice parameters or lattice strains, typically with a precision of approximately 0.2% and spatial resolution of 0.2 nm for the field of view of 1…”
BackgroundMethodInfluentialAn, Y., & Zhang, S. (2017) · Applied Optics · doi:10.1364/ao.56.005418 · Cited by 26
Impact of a van der Waals interface on intrinsic and extrinsic defects in an MoSe 2 monolayer
Alvarez, C., Dau, M. T., Marty, A., Vergnaud, C., Poche, H. L., Pochet, P., Jamet, M., & Okuno, H. (2018) · Nanotechnology · doi:10.1088/1361-6528/aad66f · Cited by 26
“To further explore the effect of defect formation on the vdW heterostructure, we used geometric phase analysis (GPA) to calculate the displacement in graphene and MoSe2 [51, 52].”
MethodFerreiro‐Vila, E., Blanco-Canosa, S., Lucas, I., Vasili, H. B., Magén, C., Ibarra, A., Rubio‐Zuazo, J., Castro, G. R., Morellón, L., & Rivadulla, F. (2019) · Advanced Functional Materials · doi:10.1002/adfm.201901984 · Cited by 26
Inlaid ReS2 Quantum Dots in Monolayer MoS2
Wang, Z., Luo, R., Johnson, I., Kashani, H., & Chen, M. (2019) · ACS Nano · doi:10.1021/acsnano.9b08186 · Cited by 26
Zhang, J., Wang, W., Wang, T., Jiang, L., Wang, N., Dai, Y., Wang, M., & Qi, Y. (2020) · Ceramics International · doi:10.1016/j.ceramint.2020.11.233 · Cited by 26
Periodic Polarization Waves in a Strained, Highly Polar Ultrathin SrTiO3
Tang, Y., Zhu, Y., Wu, B., Wang, Y., Yang, L., Feng, Y., Zou, M., Geng, W., & Ma, X. (2021) · Nano Letters · doi:10.1021/acs.nanolett.1c02117 · Cited by 26
Residual stress assessment of interconnects by slot milling with FIB and geometric phase analysis
Wang, Q., Xie, H., Liu, Z., Lou, X., Wang, J., Xu, K., Zhang, Z., Liao, J., & Gu, C. (2010) · Optics and Lasers in Engineering · doi:10.1016/j.optlaseng.2009.12.006 · Cited by 26
Partial dislocations in wurtzite GaN
Komninou, P., Kioseoglou, J., Dimitrakopulos, G. P., Kehagias, T., & Karakostas, T. (2005) · physica status solidi (a) · doi:10.1002/pssa.200521263 · Cited by 26
Liu, R., Liang, W., Miao, Q., Zhao, H., Zhang, X., Zhang, M., Yan, R., Ramasubramanian, B., & Ramakrishna, S. (2024) · Journal of Advanced Ceramics · doi:10.26599/jac.2024.9220969 · Cited by 25
Exceptionally low thermal conductivity in distorted high entropy alloy
Wang, H., Ma, S., Zhao, W., He, Q., Liu, Y., Zhao, S., & Yang, Y. G. (2024) · Materials Research Letters · doi:10.1080/21663831.2024.2413101 · Cited by 25
“Geometric phase analyses (GPA) [24] were employed to assess lattice strain, utilizing the open source program Strain ++ .”
Shan, Y., Zhang, Y., Zhang, C., Jiang, F., Huang, B., Zhao, S., & Song, K. (2025) · Materials & Design · doi:10.1016/j.matdes.2025.113935 · Cited by 25
Chen, R., & Dayeh, S. A. (2015) · Nano Letters · doi:10.1021/acs.nanolett.5b00327 · Cited by 31
Cheng, S., Li, J., Han, M., Deng, S., Tan, G., Zhang, X., Zhu, J., & Zhu, Y. (2017) · Physical Review Letters · doi:10.1103/physrevlett.118.145501 · Cited by 25
Li, C., Wang, L., Chen, W., Lu, L., Nan, H., Wang, D., Zhang, Y., Yang, Y., & Jia, C. (2017) · Advanced Materials Interfaces · doi:10.1002/admi.201700972 · Cited by 25
Plasma-assisted molecular beam epitaxy of NiO on GaN(00.1)
Budde, M., Remmele, T., Tschammer, C., Feldl, J., Franz, P., Lähnemann, J., Cheng, Z., Hanke, M., Ramsteiner, M., Albrecht, M., et al. (2020) · Journal of Applied Physics · doi:10.1063/1.5129881 · Cited by 25
Rajak, P., Knez, D., Chaluvadi, S. K., Orgiani, P., Rossi, G., Méchin, L., & Ciancio, R. (2021) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.1c15599 · Cited by 25
Martí‐Sánchez, S., Botifoll, M., Oksenberg, E., Koch, C., Borja, C., Spadaro, M. C., Giulio, V. D., Ramasse, Q. M., de Abajo, F. J. G., Joselevich, E., et al. (2022) · Nature Communications · doi:10.1038/s41467-022-31778-3 · Cited by 25
Raising the solubility of Gd yields superior thermoelectric performance in n-type PbSe
Deng, Q., Zhong, Y., Zhao, C., Zhang, F., Xia, C., Chen, Y., & Ang, R. (2022) · Journal of Materials Chemistry A · doi:10.1039/d2ta06161a · Cited by 25
A Review on Strain Study of Cuprate Superconductors
Zhang, J., Wu, H., Zhao, G., Han, L., & Zhang, J. (2022) · Nanomaterials · doi:10.3390/nano12193340 · Cited by 25
Trivedi, V., Tiadi, M., Murty, B. S., Satapathy, D. K., Battabyal, M., & Gopalan, R. (2022) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.2c13747 · Cited by 25
Yang, J., Wang, M., Lu, B., Hou, H., Zhang, X., Xu, Z., Liu, J., Liu, G., & Qiao, G. (2023) · Chemical Engineering Journal · doi:10.1016/j.cej.2023.143559 · Cited by 25
Zhang, Z., Hao, Z., Wang, H., Zhang, D., & Zhang, D. (2023) · Materials Science and Engineering A · doi:10.1016/j.msea.2023.145564 · Cited by 25
Wang, D., Li, Y., Yang, Y., Ding, C., Wei, Y., Liu, D., Li, H. L., Bì, H., Chen, S., Ji, S., et al. (2024) · eScience · doi:10.1016/j.esci.2024.100279 · Cited by 25
Jiang, H., Gong, Q., Peterlechner, M., Daum, L., Rösner, H., & Wilde, G. (2024) · Materials Science and Engineering A · doi:10.1016/j.msea.2024.146758 · Cited by 25
der Jeught, S. V., Sijbers, J., & Dirckx, J. (2015) · Journal of Imaging · doi:10.3390/jimaging1010031 · Cited by 27
“In order to solve (2) without prior knowledge of the true unwrapped phase φ( ), the authors define the complex quantity ( ) = φ ( ) = φ( ) − 2π ( ) = φ( ) and recognize that (1/ )∇ = ∇ φ [38], where (.”
BackgroundImaging and thickness measurement of amorphous intergranular films using TEM
MacLaren, I. (2003) · Ultramicroscopy · doi:10.1016/j.ultramic.2003.10.002 · Cited by 25
Interface structure and strain state of InAs nano-clusters embedded in silicon
Wu, M., Trampert, A., AlZoubi, T., Benyoucef, M., & Reithmaier, J. P. (2015) · Acta Materialia · doi:10.1016/j.actamat.2015.02.042 · Cited by 25
Microstructure and deformation mechanisms in nanocrystalline Ni–Fe. Part I. Microstructure
Petegem, S. V., Zimmermann, J., Brandstetter, S., Sauvage, X., Legros, M., & Swygenhoven, H. V. (2013) · Acta Materialia · doi:10.1016/j.actamat.2013.06.031 · Cited by 25
Highly strained AlAs-type interfaces in InAs/AlSb heterostructures
Vallet, M., Claveau, Y., Warot-Fonrose, B., Gatel, C., Nicolaï, J., Combe, N., Magén, C., Teissier, R., Baranov, A. N., & Ponchet, A. (2016) · Applied Physics Letters · doi:10.1063/1.4952951 · Cited by 25
Baniecki, J. D., Yamazaki, T., Ricinschi, D., Overmeere, Q. V., Aso, H., Miyata, Y., Yamada, H., Fujimura, N., Maran, R., Anazawa, T., et al. (2017) · Scientific Reports · doi:10.1038/srep41725 · Cited by 25
González, D., Braza, V., Utrilla, A. D., Gonzalo, A., Reyes, D. F., Ben, T., Guzmán, Á., Hierro, A., & Ulloa, J. M. (2017) · Nanotechnology · doi:10.1088/1361-6528/aa83e2 · Cited by 25
Oxygen Stoichiometry Effect on Polar Properties of LaAlO3/SrTiO3
Sharma, P. K., Huang, Z., Li, M., Li, C., Hu, S., Lee, H., Lee, J., Eom, C., Pennycook, S. J., Seidel, J., et al. (2018) · Advanced Functional Materials · doi:10.1002/adfm.201707159 · Cited by 25
Mun, H., Lee, K. H., Yoo, S. J., Kim, H., Jeong, J., Oh, S. H., Snyder, G. J., Lee, Y. H., Kim, Y., & Kim, S. W. (2018) · Acta Materialia · doi:10.1016/j.actamat.2018.08.027 · Cited by 25
“7(b)) [39], it is clearly visualized that the periodic distribution of misfit dislocation cores are represented as strain dipoles shown in Fig.”
BackgroundQian, W., Li, J., Zhu, J., Hao, W., & Chen, L. (2019) · Optics and Lasers in Engineering · doi:10.1016/j.optlaseng.2019.105804 · Cited by 25
Effect of precipitate coherency on the corrosion-induced hydrogen trapping in 2024 aluminum alloy
Kamoutsi, H., Haidemenopoulos, G. N., Mavros, H., Karantonidis, C., Floratos, P., Alhosani, Z., Cho, P., Anjum, D. H., Ravaux, F., & Polychronopoulou, K. (2021) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2021.08.005 · Cited by 25
Characterization and modeling of structural properties of SiGe/Si superlattices upon annealing
Py, M., Barnes, J., Rivallin, P., Pakfar, A., Denneulin, T., Cooper, D., & Hartmann, J. (2011) · Journal of Applied Physics · doi:10.1063/1.3622622 · Cited by 25
Electron microscopy by specimen design: application to strain measurements
Cherkashin, N. A., Denneulin, T., & Hÿtch, M. (2017) · Scientific Reports · doi:10.1038/s41598-017-12695-8 · Cited by 25
Self-citationKret, S., PawelDlużewski, Dłużewski, P., & Sobczak, E. (2000) · Journal of Physics Condensed Matter · doi:10.1088/0953-8984/12/49/334 · Cited by 25
Zhou, J., Cui, H., Liu, Y., Ming, H., Yu, Y., Dravid, V. P., Luo, Z., Yan, Q., Zou, Z., & Kanatzidis, M. G. (2025) · Nature Communications · doi:10.1038/s41467-025-60571-1 · Cited by 24
“Geometric phase analysis was performed using the Strain++ program 59 .”
Bonef, B., López‐Haro, M., Amichi, L., Beeler, M., Grenier, A., Robin, É., Jouneau, P., Mollard, N., Mouton, I., Haas, B., et al. (2016) · Nanoscale Research Letters · doi:10.1186/s11671-016-1668-2 · Cited by 24
“For ternary or quaternary alloys, methods based on the analysis of the lattice parameters, such as X-ray diffraction, nanobeam electron diffraction [1], or geometrical phase analysis of high-resolution transmission electron microscopy images [2], cannot discriminate between strain and composition effects.”
MethodSong, L., Liu, S., & Mao, X. (2017) · RSC Advances · doi:10.1039/c7ra05079h · Cited by 24
Yun, H., Prakash, A., Birol, T., Jalan, B., & Mkhoyan, K. A. (2021) · Nano Letters · doi:10.1021/acs.nanolett.1c00966 · Cited by 24
Bian, Z., Yang, C., Zhu, H., Zhao, D., Wang, M., Zhang, H., Chen, Z., & Wang, H. (2022) · Materials Research Letters · doi:10.1080/21663831.2022.2136016 · Cited by 24
“Furthermore, an HRTEM image of the Al/Al9FeNi interface with interface precipitates (Position 2) (Positions 1 and 3 are Al matrix) is shown (Figure 4(f)), and related lattice strains are calculated by GPA (Geometric Phase Analysis, Figure 4(g–h)).”
MethodInfluentialKruk, A., & Cempura, G. (2022) · Materials Characterization · doi:10.1016/j.matchar.2022.112560 · Cited by 24
The ill-defined π(AlFeMgSi) phase intermetallics formed in an automotive Al-Si-Mg alloy
Xi, H. H., Xu, J. J., Yuan, X., Ming, W. Q., Zhang, Z., & Chen, J. H. (2023) · Materials Characterization · doi:10.1016/j.matchar.2023.112839 · Cited by 24
Zhao, J., Wei, Z., Chen, N., Meng, F., Tian, R., Zeng, Y., & Du, F. (2023) · Energy storage materials · doi:10.1016/j.ensm.2023.103127 · Cited by 37
Han, Y., Guo, N., Deng, C., Han, H., Li, W., Collieus, L. L., Wang, S., Li, Y., Chen, Y., Peng, S., et al. (2024) · Advanced Functional Materials · doi:10.1002/adfm.202315579 · Cited by 24
Mao, Y., Sheng, Y., Gao, Y., Yang, H. J., Liu, J., Tam, K. C., Fu, S., Chen, W., & Tang, C. (2024) · Carbon · doi:10.1016/j.carbon.2024.119412 · Cited by 25
Li, S., Li, S., Liu, H., Liu, L., Pan, D. M., Li, G., Wang, Z., Hou, X., Gao, J., Zhang, X., et al. (2024) · Materials Characterization · doi:10.1016/j.matchar.2024.114132 · Cited by 24
Stable lithium storage with strong-grain sustained pinning-reinforced nanocrystalline silicon
Hu, T., Zhou, H., Tang, J., Chen, S., Li, Z., Yu, X., Zhang, Y., Yang, J., & Zhou, X. (2024) · Energy & Environmental Science · doi:10.1039/d4ee02202e · Cited by 24
High vertical yield InP nanowire growth on Si(111) using a thin buffer layer
Fonseka, H. A., Tan, H. H., Wong‐Leung, J., Kang, J. H., Parkinson, P., & Jagadish, C. (2013) · Nanotechnology · doi:10.1088/0957-4484/24/46/465602 · Cited by 28
Cooper, D., Denneulin, T., Barnes, J., Hartmann, J., Hutin, L., Royer, C. L., Béché, A., & Rouvière, J. (2012) · Journal of Applied Physics · doi:10.1063/1.4767925 · Cited by 24
Nicolaï, J., Warot-Fonrose, B., Gatel, C., Teissier, R., Baranov, A. N., Magén, C., & Ponchet, A. (2015) · Journal of Applied Physics · doi:10.1063/1.4926786 · Cited by 24
InAs/GaAs Sharply Defined Axial Heterostructures in Self-Assisted Nanowires
Scarpellini, D., Somaschini, C., Fedorov, A., Bietti, S., Frigeri, C., Grillo, V., Esposito, L., Salvalaglio, M., Marzegalli, A., Montalenti, F., et al. (2015) · Nano Letters · doi:10.1021/nl504690r · Cited by 24
The bi-layered precipitate phase ζ in the Al-Ag alloy system
Zhang, Z., BOURGEOIS, L. N., Rosalie, J. M., & Medhekar, N. V. (2017) · Acta Materialia · doi:10.1016/j.actamat.2017.04.061 · Cited by 24
“Geometric phase analysis (GPA) filters a lattice image according to the peaks in its fast Fourier transform (FFT) and compares that image to a reference lattice to resolve local strain in real space [48].”
BackgroundStrain analysis from nano-beam electron diffraction: Influence of specimen tilt and beam convergence
Grieb, T., Krause, F. F., Schowalter, M., Zillmann, D., Sellin, R. L., Müller‐Caspary, K., Mahr, C., Mehrtens, T., Bimberg, D., & Rosenauer, A. (2018) · Ultramicroscopy · doi:10.1016/j.ultramic.2018.03.013 · Cited by 24
Atomic Scale Investigation on Precipitates and Defects of Mg–RE Alloys: A Review
Zhu, C., & Chen, B. (2018) · Advanced Engineering Materials · doi:10.1002/adem.201800734 · Cited by 24
Chen, J., Zhou, S., Wen, Y., Ryu, G. H., Allen, C. S., Lu, Y., Kirkland, A. I., & Warner, J. H. (2019) · Nanoscale · doi:10.1039/c8nr08821g · Cited by 24
Evolution of β Mg17Al12 in Mg Al Zn Ag alloy over time
Li, Y., Tan, C., Yu, X., Nie, Z., Zhao, X., Han, J., Yuan, S., Zhao, M., Guo, C., & Wang, F. (2019) · Materials Science and Engineering A · doi:10.1016/j.msea.2019.03.094 · Cited by 24
Direct observation of an electrically degenerate interface layer in a GaN/sapphire heterostructure
Kim, Y., Lee, S. B., Lee, J., & Oh, S. H. (2019) · Nanoscale · doi:10.1039/c9nr01803d · Cited by 24
Measuring strain on HR-STEM images: application to threading dislocations in Al0.8In0.2N
Rouvière, J., Mouti, A., & Stadelmann, P. (2011) · Journal of Physics Conference Series · doi:10.1088/1742-6596/326/1/012022 · Cited by 24
Growth of platinum ultrathin films on Al2O3(0001)
Benamara, O., Snoeck, E., Respaud, M., & Blon, T. (2011) · Surface Science · doi:10.1016/j.susc.2011.07.002 · Cited by 24
Self-citationTwinning and lattice distortions in the epitaxy of La0.67Sr0.33MnO3 thin films on (0 0 1) SrTiO3
Pailloux, F., Lyonnet, R., Maurice, J.-L., & Contour, J. P. (2001) · Applied Surface Science · doi:10.1016/s0169-4332(01)00218-5 · Cited by 24
Experimental examination of displacement field in an edge dislocation core in aluminum
Zhao, C., Xing, Y., & Bai, P. C. (2007) · Physics Letters A · doi:10.1016/j.physleta.2007.07.034 · Cited by 24
Nonlinear FE analysis of residual stresses induced by dislocations in heterostructures
Dluzewski, P. H., Maciejewski, G., Jurczak, G., Kret, S., & Laval, J. Y. (2003) · Computational Materials Science · doi:10.1016/j.commatsci.2003.10.012 · Cited by 24
“This method is based upon a centering of a small aperture around the strong reflection in the Fourier transform of the image, see [ 14 ].”
MethodAnisotropic strain relaxation in a-plane GaN quantum dots
Founta, S., Coraux, J., Jalabert, D., Bougerol, C., Rol, F., Mariette, H., Renevier, H., Daudin, B., Oliver, R. A., Humphreys, C. J., et al. (2007) · Journal of Applied Physics · doi:10.1063/1.2713937 · Cited by 24
Kret, S., Dłużewski, P., Szczepańska, A., Żak, M., Czernecki, R., Krysko, M., Leszczyński, M., & Maciejewski, G. (2007) · Nanotechnology · doi:10.1088/0957-4484/18/46/465707 · Cited by 24
Scarisoreanu, N. D., Craciun, F., Birjega, R., Ion, V., Teodorescu, V. S., Ghica, C., Negrea, R., & Dinescu, M. (2016) · Scientific Reports · doi:10.1038/srep25535 · Cited by 23
Local-strain-induced CO2 adsorption geometries and electrochemical reduction pathway shift
Liu, C., Bu, Y., Xu, Y., Mahmood, A., Xie, J., Fu, Y., Li, S., Cheng, P., Wu, Y., Liang, X., et al. (2024) · National Science Review · doi:10.1093/nsr/nwae191 · Cited by 23
Chen, J., Ma, X., Gong, L., Zhou, C., Chen, J., Lu, Y., Zhou, M., He, H., & Ye, Z. (2024) · Journal of Materials Chemistry C · doi:10.1039/d4tc02339k · Cited by 23
Jia, Z. P., Guan, X., Shi, F., & Li, X. (2025) · Materials Science and Engineering A · doi:10.1016/j.msea.2025.148344 · Cited by 23
A novel method to repair and upgrade spent LFP cathode material by inherent Al impurity doping
Yu, H., Zhao, D., Chen, K., Huang, M., Yang, H., Yang, L., Wang, Z., Chen, L., Ding, X., Lv, H., et al. (2025) · Resources Conservation and Recycling · doi:10.1016/j.resconrec.2025.108523 · Cited by 23
Ortiz, G., García-García, A., Bizière, N., Boust, F., Bobo, J. F., & Snoeck, E. (2013) · Journal of Applied Physics · doi:10.1063/1.4789801 · Cited by 23
Self-citationZhou, Z., Chai, Y. W., Ikuta, Y., Lee, Y., Lin, Y., & Kimura, Y. (2020) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.0c02549 · Cited by 23
Wilde, G., Rösner, H., & Divinski, S. V. (2023) · MATERIALS TRANSACTIONS · doi:10.2320/matertrans.mt-mf2022009 · Cited by 23
Nucleation of Threading Dislocations in 4H-SiC at Early Physical-Vapor-Transport Growth Stage
Shao, Q., Geng, W., Xu, S., Chen, P., Zhang, X., Shen, R., Tian, H., Pi, X., Yang, D., & Wang, R. (2023) · Crystal Growth & Design · doi:10.1021/acs.cgd.3c00416 · Cited by 23
Zhang, W., Tian, R., Wang, J., Liu, Y., & Mai, W. (2023) · Applied Surface Science · doi:10.1016/j.apsusc.2023.158066 · Cited by 23
Structural and vibrational study of porous CeO2 nanoparticles
Ascencio, F., Rangel‐Gamboa, L., Maqueda-Cabrera, B., Zorrilla, C., Herrera, R., & Mendoza‐Cruz, R. (2023) · Materials Chemistry and Physics · doi:10.1016/j.matchemphys.2023.128492 · Cited by 23
Scanning transmission electron microscopy for advanced characterization of ferroic materials
Cabral, M. J., Chen, Z., & Liao, X. (2023) · Microstructures · doi:10.20517/microstructures.2023.39 · Cited by 23
Local strain evolution near α/β interface in TC11 titanium alloy under electroshocking treatment
Liu, C., Yu, Y., Sun, H., Yin, F., Xie, L., Qian, D., Song, Y., Wang, L., Zhang, L., & Hua, L. (2024) · Materials Characterization · doi:10.1016/j.matchar.2024.113689 · Cited by 23
Low-fatigue large elastocaloric effect in NiTi shape memory alloy enabled by two-step transition
Liang, Q., Wang, D., Liang, C., Ding, X., & Wang, Y. (2024) · Scripta Materialia · doi:10.1016/j.scriptamat.2024.116239 · Cited by 23
Preserving surface strain in nanocatalysts via morphology control
Shi, C., Cheng, Z., Leonardi, A., Yang, Y., Engel, M., Jones, M. R., & Han, Y. (2024) · Science Advances · doi:10.1126/sciadv.adp3788 · Cited by 25
“Different from conventional geometric phase analysis ( 5 , 20 ), which requires atomic-resolution images and typically offers a limited field of view with high noise, we use a nanobeam 4D-STEM approach ( 21 , 22 ), which affords us a remarkable ( 0.18”
MethodInfluential
Metadata
- Authors
- Hÿtch, M. J., Snoeck, E., & Kilaas, R.
- Affiliations
- Centre National de la Recherche Scientifique (FR)
- Lawrence Berkeley National Laboratory (US)
- Corresponding author
- Hÿtch, M.J.
- Venue
- Ultramicroscopy
- Publisher
- Elsevier BV
- Published
- 1998-08
- Volume
- 74
- Issue
- 3
- Pages
- 131-146
- ISSN
- 0304-3991 (ISSN-L)
- OpenAlex
- W1970014398
- Semantic Scholar
- 7f38bb189a356c5a9f9438c2e0567a2d47f21065
- Cited by
- 2,752
- References
- 27
- Citations by year
- 2026: 234 · 2025: 347 · 2024: 276 · 2023: 194 · 2022: 164 · 2021: 156 · 2020: 158 · 2019: 126 · 2018: 98 · 2017: 120 · 2016: 105 · 2015: 105 · 2014: 91 · 2013: 96 · 2012: 87
- FWCI
- 11.67
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.elsevier.com/tdm/userlicense/1.0/ (tdm)
- Locations
- Ultramicroscopy (publishedVersion)
- Funders
- U.S. Department of Energy
- Basic Energy Sciences
- Topics
- Life Sciences › Biochemistry, Genetics and Molecular Biology › Structural Biology › Advanced Electron Microscopy Techniques and Applications
- Physical Sciences › Materials Science › General Materials Science › Advanced Materials Characterization Techniques
- Physical Sciences › Materials Science › Materials Chemistry › Ferroelectric and Piezoelectric Materials
- Keywords
- displacement field measurement, strain mapping, inverse Fourier transform, domain walls, ferroelectric-ferroelastic coupling, lead titanate
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.