Corrosion in high-temperature and supercritical water and aqueous solutions: a review
The DOI matches its Crossref record; 202 of the 210 references it cites were found in a registry or an index.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“Nickel exhibits a low Ni-Ni2S3 eutectic point at 645°C explaining the high sensitivity of high nickel materials to sulfides at atmospheric pressure 67 , while chromium 68 and molybdenum 69 are known to increase corrosion resistance towards sulfides.”
From Continuous Extraction of Black Liquor Salts under Hydrothermal Conditions (2021) · cites this paper as [69]
In the citing paper
“The solubility of hydroxide and carbonate salts are typically very low, which probably explains their observed inhibition of corrosion in supercritical water 69 .”
From Continuous Extraction of Black Liquor Salts under Hydrothermal Conditions (2021) · cites this paper as [69]
Citations
Cites
Pitting Corrosion of Metals: A Review of the Critical Factors
Frankel, G. S. (1998) · Journal of The Electrochemical Society · doi:10.1149/1.1838615 · Cited by 2,135
Organic Chemical Reactions in Supercritical Water
Savage, P. E. (1999) · Chemical Reviews · doi:10.1021/cr9700989 · Cited by 1,416
Reactions at supercritical conditions: Applications and fundamentals
Savage, P. E., Gopalan, S., Mizan, T. I., Martino, C. J., & Brock, E. E. (1995) · AIChE Journal · doi:10.1002/aic.690410712 · Cited by 945
Corrosion mechanisms in theory and practice
(1996) · Choice Reviews Online · doi:10.5860/choice.34-0946 · Cited by 930
Homogeneous Catalysis in Supercritical Fluids
Jessop, P. G., Ikariya, T., & Noyori, R. (1999) · Chemical Reviews · doi:10.1021/cr970037a · Cited by 825
Mishra, V. S., Mahajani, V. V., & Joshi, J. B. (1995) · Industrial & Engineering Chemistry Research · doi:10.1021/ie00040a001 · Cited by 758
Supercritical Fluids in Heterogeneous Catalysis
Baiker, A. (1999) · Chemical Reviews · doi:10.1021/cr970090z · Cited by 751
Cellulose hydrolysis in subcritical and supercritical water
Sasaki, M., Kabyemela, B., Malaluan, R., Hirose, S., Takeda, N., Adschiri, T., & Arai, K. (1998) · The Journal of Supercritical Fluids · doi:10.1016/s0896-8446(98)00060-6 · Cited by 644
Advances in Corrosion Science and Technology
Fontana, M. G., & Staehle, R. W. (1972) · Springer eBooks · doi:10.1007/978-1-4615-8255-7 · Cited by 619
New Directions in Inorganic and Metal-Organic Coordination Chemistry in Supercritical Fluids
Darr, J. A., & Poliakoff, M. (1999) · Chemical Reviews · doi:10.1021/cr970036i · Cited by 597
Research works printed but not linked: 25
- Hayashi, 1998, An energy balance study of a newly developed recycling system for waste plastics, Papers of Ship Res. Inst., 35, 133
- Fujii, 1976, Electrochemical study on the corrosion behavior of metals and alloys in aqueous solutions at high temperature and high pressure, Trans. Nat. Res. Inst. Metals, 18, 101
- Cragnolino, 1990, A review of pitting corrosion in high-temperature aqueous solutions, 413
- Stellwag, 1986, Electrode potential monitoring in hot water systems—a method to identify critical corrosion conditions, Dechema Monographs, 101, 17
- J.R. Galvele Present state of understanding of the breakdown of passivity and repassivation, in: R.P. Frankenthal, J. Kruger (Eds.), Passivity of Metals, Proceedings of the 4th International Symposium on Passivity, Warrenton, VA, 1977, p. 285.
- Cragnolino, 1990, A review of pitting corrosion in high-temperature aqueous solutions, 413
- Lichi, 1984, A comparison of pitting corrosion and stress corrosion cracking characteristics of some engineering alloys, Met. Australasia, 16, 4
- Lin, 1981, Stress corrosion cracking of sensitized type 304 stainless steel in high temperature chloride solutions, Corrosion, 37, 616, 10.5006/1.3577548 · DOI
- Garnsey, 1979, Corrosion of PWR steam generators, Nucl. Energy, 18, 117
- Kehr, 1993, Die neuen 800-MW-Braunkohlenbloecke der VEAG Vereinigte Energiewerke AG in Boxberg und Schwarze Pumpe, VGB Kraftwerkstechnik, 73, 941
- G. Scheffknecht, Q. Chen, Material issues for supercritical boilers, in: A. Strang, W.M. Banks, R.D. Conroy, G.M. McColvin, J.C. Neal, S. Simpson (Eds.), Parsons 2000 Conference—Advanced Materials for 21st Century Turbines and Power Plant, Proceeding of the 5th International Charles Parsons Turbine Conference, Cambridge, UK, 2000, p. 249.
- Vajnman, 1999, Failures of steam lines at thermal power stations due to corrosion surroundings, Teploenergetika, 46, 35
- Y. Katsumura, Y. Oka (Eds.), The 1st International Symposium on Supercritical-Cooled Water Reactors, Design and Technology, The University of Tokyo Press, Tokyo, Japan, 2000.
- Joshi, 1985, Engineering aspects of the treatment of aqueous waste streams, Indian Chem. Eng., 27, 2/3
- Tester, 1999, Hydrolysis and oxidation in subcritical and supercritical water: connecting process engineering science to molecular interactions, Corrosion, 55, 1088, 10.5006/1.3283946 · DOI · Paper page
- Han, 1999, Materials degregation in supercritical water oxidation system, Corrosion Sci. Prot. Technol. China, 11, 44
- D.B. Mitton, J.C. Orzalli, R.M. Latanision, Corrosion phenomena associated with SCWO systems, in: G. Brunner, M. Perrut (Eds.), Proceedings of the 3rd International Symposium on Supercritical Fluids, Strasbourg, France, 1994, p. 43.
- A.G. Robertson, Corrosion evaluation of selected materials under acidic hydrothermal oxidation conditions, Master thesis, University of Texas in Austin, Austin, TX, 1996, 148 pp.
- R.M. Latanision, D.B. Mitton, S.H. Zhang, J.A. Cline, N. Caputy, T.A. Arias, A. Rigos, Corrosion and corrosion mechanisms in supercritical water oxidation systems for hazardous waste diposal, Proceedings of the 4th International Symposium on Supercritical Fluids, Sendai, Japan, 1997, p. 865.
- S. Fodi, J. Konys, J. Hausselt, H. Schmidt, V. Casal, Corrosion of high temperature alloys in supercritical water oxidation systems, Corrosion 98, NACE National Association of Corrosion Engineers, Houston, TX, Paper No. 416, 1998, 10 pp. · DOI
- A. Ruck, J. Novotny, J. Konys, J. Hausselt, Effect of iron in nickel based alloys for SCWO plants, Eurocorr '98, European Federation of Corrosion, Event no. 221, Utrecht, The Netherlands, 1998, electronic proceedings.
- A. Ruck, J. Novotny, J. Konys, J. Hausselt, Comparison of nickel, iron and cobalt based alloys for supercritical water oxidation plants, Eurocorr '98, European Federation of Corrosion, Event no. 221, Utrecht, The Netherlands, 1998, electronic proceedings.
- G.L. D'Arcy, Corrosion behavior of titanium alloys exposed to supercritical water oxidation conditions, Master thesis, University of Texas in Austin, Austin, TX, 1996, 174 pp.
- Rafalsky, 1983, Interaction of sulfur and water under high temperatures, Geokhimia, 5, 665
- Dadze, 1993, Experimental determination of the concentrations of H2S, HSO4−, SO2aq, H2S2O3, S0aq, and Stot in the aqueous phase in the S–H2O system at elevated temperatures, Geochem. Int., 30, 36
Cited by
Items 601–674 of 674
Aqueous and High‐Temperature Corrosion
GHALI, E. L. (2010) · Wiley eBooks · doi:10.1002/9780470531778.ch2
Interactions of Si 3 N 4 ‐Based Ceramics in Water Environment under Sub‐Critical Conditions
Šajgalík, P., Galusková, D., Hnatko, M., & Galusek, D. (2011) · Ceramic engineering and science proceedings · doi:10.1002/9781118095379.ch5
Role of Dissolved Hydrogen in Water in Corrosion of Alloy 600 in High Temperature Water
Peng, Q., Shoji, T., Hou, J., Sakaguchi, K., & Takeda, Y. (2011) · Springer eBooks · doi:10.1007/978-3-319-48760-1_112
Comparison of the Corrosion Behavior of the 14CR ODS Alloy in Steam and Supercritical Water
Bischoff, J., & Motta, A. T. (2011) · Springer eBooks · doi:10.1007/978-3-319-48760-1_116
Supercritical water use in energetic - Corrosion issues
Zychová, M., & Růžičková, M. (2011) · Proceedings of the 2011 3rd International Youth Conference on Energetics (IYCE)
ВПЛИВ НЕОРГАНІЧНИХ МАТЕРІАЛІВ НА ПОВЕДІНКУ НАДКРИТИЧНОЇ ВОДИ ПОБЛИЗУ ПСЕВДОСПІНОДАЛІ
Артеменко, C. В. (2014) · Refrigeration Engineering and Technology · doi:10.15673/0453-8307.3/2014.32569
Structural mechanism of scale for 12Cr–W–Mo–Co steels with enhanced oxidation resistance
Wang, S. S., Li, C., Wu, Y., Wang, T., Chen, X. H., & Hui, X. (2014) · Corrosion Engineering Science and Technology The International Journal of Corrosion Processes and Corrosion Control · doi:10.1179/1743278214y.0000000170
Mild Wet Torrefaction and Characterization of Woody Biomass from Mozambique for Thermal Applications
Cuvilas, C. A. (2015) · KTH Publication Database DiVA (KTH Royal Institute of Technology) · Cited by 1
Ubah, C. G. (2010) · cIRcle (University of British Columbia) · doi:10.14288/1.0071276
“A delineation of the electrochemical and chemical processes in corrosion in terms of electrochemical and pH values [2] is depicted in Figure 1.”
BackgroundLeybros, A., Roubaud, A., Turc, H.-A., & Fournel, B. (2008) · HAL
Anzelj, D. (2016) · Saint Mary's University Institutional Repository (Saint Mary's University)
The effect of water quality on steel corrosion
Rajakovic-Ognjanovic, V. N. (2011) · doi:10.2298/bg20110617rajakovicognjanovic · Cited by 1
Ojea, R. B. (2011) · TDX (Tesis Doctorals en Xarxa)
Gaseificação de vinhaça em água supercrítica.
da Silva, S. C. F. (2016) · Digital Library of Theses and Dissertations (Universidade de São Paulo) · doi:10.11606/d.3.2016.tde-30062016-085815
GASEIFICAÇÃO DE VINHAÇA EM ÁGUA SUPERCRÍTICA
Química, E., & Giudici, R. (2016)
Characterization of Alloy 214 After Exposure to Superheated Steam at 800 °C
Tepylo, N., Sanchez, R. G., & Huang, X. (2017) · Journal of Nuclear Engineering and Radiation Science · doi:10.1115/1.4037718
Microwave Technique for the Corrosion Detection
(2018) · International Journal of Microwaves Applications · doi:10.30534/ijma/2018/03722018
Echocardiography for Assessing Acute Myocardial Infarction and Complications
Kamp, O. (2018) · Springer eBooks · doi:10.1007/978-3-319-71617-6_20
Neutralization of poultry waste by thermohydrolysis in near-critical water
Janas, M., & Zawadzka, A. (2019) · Acta Innovations · doi:10.32933/actainnovations.30.3
“In addition, the products of thermohydrolysis show a significantly milder action on the apparatus walls than the products of supercritical water oxidation [8-10, 13, 14].”
BackgroundHydrogen evolution and corrosion behavior of zirconium tubing in sub‐ and supercritical water
Choudhry, K. I., & Svishchev, I. M. (2019) · Materials and Corrosion · doi:10.1002/maco.201911082
Degradation Kinetics of Organic Amines in Supercritical Water
Namilakonda, P. K. (2005) · SHAREOK (University of Oklahoma; Oklahoma State University; Central Oklahoma University)
Wu, X., Sun, M., & Han, E. (2010) · NACE CORROSION Conference · doi:10.5006/c2010-10197
Design, Fabrication, and Operational Parameters of a Supercritical Water Oxidation Reactor
Moore, S. J. (2020) · ResearchWorks at the University of Washington (University of Washington) · Cited by 2
Corrosion in Supercritical Water—Waste Destruction Environments
(2006) · ASM International eBooks · doi:10.31399/asm.hb.v13c.a0004132
High temperature electrochemical studies on nickel: glycerol and nickel electro-oxidation
Borsboom-Hanson, T. (2021) · UVic’s Research and Learning Repository (University of Victoria)
Xu, D., & Guo, S. (2021) · Springer eBooks · doi:10.1007/978-981-16-5525-8_1
Corrosion Behavior of Alloys in Supercritical Water Oxidation Processes
Xu, D., & Guo, S. (2021) · Springer eBooks · doi:10.1007/978-981-16-5525-8_5
7 Gas Processing, Purification, and Upgrading
Shah, Y. T. (2017) · CRC Press eBooks · doi:10.1201/9781315302355-8
Synthetic Gas Production by Co-Gasification
(2015) · Green chemistry and chemical engineering · doi:10.1201/b19100-4
Purohit, A. L., Misquith, J., Moore, S., Pinkard, B. R., Kramlich, J. C., Reinhall, P. G., & Novosselov, I. V. (2020) · ChemRxiv · doi:10.26434/chemrxiv.13173278 · Cited by 1
Behaviour of Ni-based coating alloys in supercritical water
Qian, Y. (2011) · Carleton University's Institutional Repository (MacOdrum Library, Carleton University) · doi:10.22215/etd/2011-07397
(2018) · Elsevier eBooks · doi:10.1016/b978-0-12-812992-0.00021-2
Role of Dissolved Hydrogen in Water in Corrosion of Alloy 600 in High Temperature Water
Peng, Q., Shoji, T., Hou, J., Sakaguchi, K., & Takeda, Y. (2012) · Wiley eBooks · doi:10.1002/9781118456835.ch192
Comparison of the Corrosion Behavior of the 14CR ODS Alloy in Steam and Supercritical Water
Bischoff, J., & Motta, A. T. (2012) · Wiley eBooks · doi:10.1002/9781118456835.ch200
Włodarczyk, R., Kobyłecki, R., & Bis, Z. (2010) · Wiley eBooks · doi:10.1002/9783527628148.hoc039
(2013) · Elsevier eBooks · doi:10.1016/b978-0-12-396488-5.00028-9
Resource utilization of thermoplastics in supercritical water
Jin, H., Bai, B., Wang, W., Cao, C., Lu, B., Shi, J., & Guo, L. (2023) · Elsevier eBooks · doi:10.1016/b978-0-323-95402-0.00003-3
Oxidation Study of Incoloy 800H Tubes Exposed to Super-Heated Steam and Supercritical Water
Nazarali, Q. (2023) · Carleton University's Institutional Repository (MacOdrum Library, Carleton University) · doi:10.22215/etd/2023-15631
Black liquor gasification for chemical recovery and hydrogen gas production in supercritical water
Hawangchu, Y. (2016) · Chula Digiverse · doi:10.58837/chula.the.2016.1573
Wang, J. (2023) · SSRN Electronic Journal · doi:10.2139/ssrn.4639591
Wei, S., Wang, X., Li, X., Xu, J., & Shoji, T. (2024) · SSRN Electronic Journal · doi:10.2139/ssrn.4860882
Chen, J., Lin, Z., Tang, X., Zhu, R., Chen, S., Wang, Y., & Yang, J. (2024) · SSRN Electronic Journal · doi:10.2139/ssrn.4884877
Cao, A., & Li, Z. (2024) · International Conference on Design Science (ICDS) · doi:10.1109/icds62420.2024.10751726
“The circumferential crack defects generated by pipes in harsh environments can easily cause pipe bursts and explosions, posing a great threat to the normal use of small-diameter pipes[1,2].”
Mpofu, P., Malatji, N., Shongwe, M. B., & Kanyane, L. R. (2025) · Metallography Microstructure and Analysis · doi:10.1007/s13632-025-01211-4
“Cr is commonly employed for corrosion resistance, but it also adds to high-temperature oxidation resistance, which is required for prolonged exposure to severe environments [18, 19].”
Korpelin, V., Nevalaita, J., Melander, M., Honkala, K., & Koskinen, P. (2025) · The Journal of Chemical Physics · doi:10.1063/5.0268814
Combined Corrosion and Fatigue Damage in an Additive-Manufactured Hpdc Tooling InsertPreprint
Marchini, L., Gelfi, M., Solazzi, L., & Pola, A. (2025) · SSRN Electronic Journal · doi:10.2139/ssrn.5387361
Excellent High‐Temperature Oxidation Resistance of a 9Cr–6W–0.3N Heat‐Resistant Martensitic Steel
Shang, H., Sun, D., Liu, Z., Ning, B., Chen, Y., & Dong, Z. (2025) · steel research international · doi:10.1002/srin.202500646
Li, K., Chen, J., Xie, G., Tang, X., Xu, D., & Yang, J. (2025) · Corrosion Science · doi:10.1016/j.corsci.2025.113397 · Cited by 1
Chemical bioadaptability of biodegradable metals
Zheng, Y. (2025) · Elsevier eBooks · doi:10.1016/b978-0-443-22133-0.00005-9
One-pot enzymatic resolution/separation of enantiomers using green solvents
Pinto, J. J. B. F. (2013) · Portuguese National Funding Agency for Science, Research and Technology (RCAAP Project by FCT)
Crack Injection as a Mechanism for Stress Corrosion Cracking
(2020) · Arizona State University Library Digital Repository (Arizona State University)
Bhuiyan, M. S. H., Meesungnoen, J., Sultana, A., & Jay‐Gerin, J. (2025) · Nuclear Engineering and Design · doi:10.1016/j.nucengdes.2025.114479
Experimental evidence on the bitumen role of the metal enrichment in the Erdaokan Ag-Pb-Zn deposit
Yan, S.-F., Zheng, X.-M., Li, L., Zheng, H.-Y., Yuan, M., Santosh, M., & Li, S. (2026) · Organic Geochemistry · doi:10.1016/j.orggeochem.2026.105128
An, Z., Zhang, S., Han, Y., Li, Y., Zhu, C., Ge, Z., Feng, X., & Yang, Y. (2026) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2026.156531 · Cited by 1
Role of Coexisting Substances in the Hydrothermal Dechlorination of Polyvinyl Chloride (PVC)
Yamasaki, Y., Hosokawa, S., & Hungwe, D. (2026) · Journal of the Japan Society of Material Cycles and Waste Management · doi:10.3985/jjsmcwm.37.1
Yu, Q. M. W. (2012) · theses.fr (ABES) · doi:10.70675/b26e5af7zf79dz4aaczb602z6f67257e7409 · Cited by 12
Synthèse solvothermale supercritique de nanostructures d'oxyde de cérium
Slostowski, C. (2012) · theses.fr (ABES) · doi:10.70675/b8449f00z262ez42a8z84e7z0400271fe391 · Cited by 3
Piolet, R. (2014) · theses.fr (ABES) · doi:10.70675/ee9965d8za32bz4c17za923ze80475a5bc98 · Cited by 3
“Différents auteurs ont révélé que les solubilités de différents matériaux dont ZnO augmentaient avec la température pour des températures inférieures à la température critique (dans d’autres milieux que ceux étudiés dans cette étude) (Dirkse, 1954; Laudise, 1963; Martynova, 1976; Plyasunov, 1988; Yokoyama, 1993; Wesol…”
Lemoine, G. (2017) · theses.fr (ABES) · doi:10.70675/4f7caed2z1195z4fbez84b9z03aa22784048
“De nombreux travaux ont été menés afin de trouver des matériaux résistants à la corrosion à haute pression et haute température [37-40].”
BackgroundParticle design and coating of pharmaceutical ingredients using supercritical fluid techniques
Djerafi, R. (2017) · theses.fr (ABES) · doi:10.70675/35ceb9a7z46c3z459fz9e97z55d8bf24b613
Study of the stabilization mechanisms of tetragonal ZrO2 nanocrystals in supercritical fluids
Auxéméry, A. (2019) · theses.fr (ABES) · doi:10.70675/3d586820z07aez4a7ez9439z943e8f3b0dbb
Combinatorial Evaluation of Corrosion Resistance of Ru-Based Alloys in Supercritical Acidic Fluids
Murakami, R., Naveenkarthik, M., Kamada, K., & Yoshikawa, A. (2026) · Materials · doi:10.3390/ma19091844
“As a result, the dissociation equilibria of acids, bases, and salts, the behavior of dissolved gases, and the stability of passive films also change, giving rise to corrosion mechanisms different from those under ambient conditions [7,8].”
Ahovan, H. R., Akbari, A., & Afsharmanesh, M. (2026) · Chemistry Africa · doi:10.1007/s42250-026-01873-9
“However, it is highly susceptible to corrosion, particularly in aggressive acidic environments encountered during industrial operations such as acid pickling, chemical cleaning, descaling, and acid stimulation [2, 3].”
Ghule, B., Sundaresan, C., & Raja, V. S. (2026) · Corrosion Science · doi:10.1016/j.corsci.2026.114292
Microstructure–Surface Properties Correlation of LPBF–Manufactured Alloys
Marchini, L. (n.d.) · Institutional Research Information System (Università degli Studi di Brescia)
Li, Z., & Cheng, Z. (2026) · The Journal of Physical Chemistry B · doi:10.1021/acs.jpcb.6c03930
Wen, X., Zhou, T., Liu, Y., 郑晓军, Guo, J., Huang, X., Liu, Q., Zou, X., Wei, Q., & Xie, Y. (2026) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2026.157227
Xu, X., Liu, S., He, L., Tan, Y., Hu, S., Ouyang, X., & Zhou, Q. (2026) · Journal of Radioanalytical and Nuclear Chemistry · doi:10.1007/s10967-026-11254-8
Metadata
- Authors
- Kritzer, P.
- Affiliations
- Freudenberg (Germany) (DE)
- Corresponding author
- Kritzer, Peter
- Venue
- The Journal of Supercritical Fluids
- Publisher
- Elsevier BV
- Published
- 2004-04
- Volume
- 29
- Issue
- 1-2
- Pages
- 1-29
- ISSN
- 0896-8446 (ISSN-L)
- OpenAlex
- W2056290266
- Semantic Scholar
- 756bbb8a0c2e4081004a4768c600ad9bedb486a2
- Cited by
- 660
- References
- 210
- Citations by year
- 2026: 15 · 2025: 39 · 2024: 31 · 2023: 16 · 2022: 42 · 2021: 42 · 2020: 29 · 2019: 56 · 2018: 33 · 2017: 41 · 2016: 43 · 2015: 38 · 2014: 45 · 2013: 31 · 2012: 33
- FWCI
- 7.65
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.elsevier.com/tdm/userlicense/1.0/ (tdm)
- www.elsevier.com/legal/tdmrep-license (tdm)
- Locations
- The Journal of Supercritical Fluids (publishedVersion)
- Topics
- Physical Sciences › Chemical Engineering › Process Chemistry and Technology › Subcritical and Supercritical Water Processes
- Physical Sciences › Materials Science › Materials Chemistry › Corrosion Behavior and Inhibition
- Physical Sciences › Materials Science › Metals and Alloys › Hydrogen embrittlement and corrosion behaviors in metals
- Keywords
- corrosion, supercritical water, high-temperature water, aqueous solutions, corrosion mechanism, intergranular corrosion, pitting corrosion, general corrosion, stress corrosion cracking, ionic products, ion solubility, ion dissociation, corrosion products, alloy composition, heat treatment, pH
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.