Al2O3 and TiO2 Atomic Layer Deposition on Copper for Water Corrosion Resistance
Abstract
Al(2)O(3) and TiO(2) atomic layer deposition (ALD) were employed to develop an ultrathin barrier film on copper to prevent water corrosion. The strategy was to utilize Al(2)O(3) ALD as a pinhole-free barrier and to protect the Al(2)O(3) ALD using TiO(2) ALD. An initial set of experiments was performed at 177 °C to establish that Al(2)O(3) ALD could nucleate on copper and produce a high-quality Al(2)O(3) film. In situ quartz crystal microbalance (QCM) measurements verified that Al(2)O(3) ALD nucleated and grew efficiently on copper-plated quartz crystals at 177 °C using trimethylaluminum (TMA) and water as the reactants. An electroplating technique also established that the Al(2)O(3) ALD films had a low defect density. A second set of experiments was performed for ALD at 120 °C to study the ability of ALD films to prevent copper corrosion. These experiments revealed that an Al(2)O(3) ALD film alone was insufficient to prevent copper corrosion because of the dissolution of the Al(2)O(3) film in water. Subsequently, TiO(2) ALD was explored on copper at 120 °C using TiCl(4) and water as the reactants. The resulting TiO(2) films also did not prevent the water corrosion of copper. Fortunately, Al(2)O(3) films with a TiO(2) capping layer were much more resilient to dissolution in water and prevented the water corrosion of copper. Optical microscopy images revealed that TiO(2) capping layers as thin as 200 Å on Al(2)O(3) adhesion layers could prevent copper corrosion in water at 90 °C for ~80 days. In contrast, the copper corroded almost immediately in water at 90 °C for Al(2)O(3) and ZnO films by themselves on copper. Ellipsometer measurements revealed that Al(2)O(3) films with a thickness of ~200 Å and ZnO films with a thickness of ~250 Å dissolved in water at 90 °C in ~10 days. In contrast, the ellipsometer measurements confirmed that the TiO(2) capping layers with thicknesses of ~200 Å on the Al(2)O(3) adhesion layers protected the copper for ~80 days in water at 90 °C. The TiO(2) ALD coatings were also hydrophilic and facilitated H(2)O wetting to copper wire mesh substrates.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cited by
Next-Generation Lithium Metal Anode Engineering via Atomic Layer Deposition
Kozen, A. C., Lin, C.-F., Pearse, A. J., Schroeder, M. A., Han, X., Hu, L., Lee, S.-B., Rubloff, G. W., & Noked, M. (2015) · ACS Nano · doi:10.1021/acsnano.5b02166 · Cited by 816
Bio-Inspired Titanium Dioxide Materials with Special Wettability and Their Applications
Liu, K., Cao, M., Fujishima, A., & Jiang, L. (2014) · Chemical Reviews · doi:10.1021/cr4006796 · Cited by 571
Li, C., Cauwe, M., Yang, Y., Schaubroeck, D., Mader, L., & Op de Beeck, M. (2019) · Coatings · doi:10.3390/coatings9090579 · Cited by 46
Implantable Device Fabrication and Packaging
Stieglitz, T. (2023) · Handbook of Neuroengineering · doi:10.1007/978-981-16-5540-1_102 · Cited by 7
Metadata
- Authors
- Abdulagatov, A. I., Yan, Y., Cooper, J. R., Zhang, Y., Gibbs, Z. M., Cavanagh, A. S., Yang, R. G., Lee, Y. C., & George, S. M.
- Venue
- ACS Applied Materials & Interfaces
- Publisher
- American Chemical Society (ACS)
- Published
- 2011-11-16
- Volume
- 3
- Issue
- 12
- Pages
- 4593-4601
- ISSN
- 1944-8244 (ISSN-L)
- 1944-8252
- OpenAlex
- W1995326391
- Cited by
- 300
- References
- 0
- FWCI
- 10.47
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: Al2O3 and TiO2 Atomic Layer Deposition on Copper for Water Corrosion Resistance. https://app.cochat.ai/papers/10.1021/am2009579
- The paper
- Abdulagatov, A. I., Yan, Y., Cooper, J. R., Zhang, Y., Gibbs, Z. M., Cavanagh, A. S., Yang, R. G., Lee, Y. C., & George, S. M. (2011). Al2O3 and TiO2 Atomic Layer Deposition on Copper for Water Corrosion Resistance. ACS Applied Materials & Interfaces. https://doi.org/10.1021/am2009579
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.