Degradation of Well Cement by CO 2 under Geologic Sequestration Conditions
The DOI matches its Crossref record; 20 of the 20 references it cites were found in a registry or an index.
Abstract
Experiments were conducted to assess the durability of cements in wells penetrating candidate formations for geologic sequestration of CO2. These experiments showed a significant variation in the initial degradation (9 days of exposure) based on the curing conditions. The high-temperature (50 degrees C) and high-pressure (30.3 MPa) curing environment increased the degree of hydration and caused a change in the microstructure and distribution of the Ca(OH)2(s) phase within the cement. Cement cured at 50 degrees C and 30.3 MPa (representing sequestration conditions) proved to be more resistant to carbonic acid attack than cement cured at 22 degrees C and 0.1 MPa. The cement cured at 50 degrees C and 30.3 MPa exhibited a shallower depth of degradation and displayed a well-defined carbonated zone as compared to cement cured under ambient conditions. This is likely due to smaller, more evenly distributed Ca(OH)2(s) crystals that provide a uniform and effective barrier to CO2 attack.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“The importance of waterbearing CO2 for the stability and carbonation of steel, steel slag, cement, and fly ash is well etablished.153,239- 244”
From Molecular-scale mechanisms of CO2 mineralization in nanoscale interfacial water films (2022) · cites this paper as [242]
Citations
Cites
PROPERTIES OF CONCRETE. 4TH AND FINAL EDITION
Neville, A. M. (1968) · Virtual Defense Library (Ministerio de Defensa) · Cited by 5,477
Neville, A. M. (1968) · Virtual Defense Library (Ministerio de Defensa) · Cited by 5,444
Lea's Chemistry of Cement and Concrete
(1998) · Elsevier eBooks · doi:10.1016/b978-0-7506-6256-7.x5007-3 · Cited by 1,019
White, C. M., Strazisar, B. R., Granite, E. J., Hoffman, J. S., & Pennline, H. W. (2003) · Journal of the Air & Waste Management Association · doi:10.1080/10473289.2003.10466206 · Cited by 751
Self-citationCarey, J. W., Wigand, M., Chipera, S. J., WoldeGabriel, G., Pawar, R., Lichtner, P. C., Wehner, S. C., Raines, M. A., & Guthrie, G. D. (2007) · International Journal of Greenhouse Gas Control · doi:10.1016/s1750-5836(06)00004-1 · Cited by 503
Peer Reviewed: Safe Storage of CO2 in Deep Saline Aquifiers
Bruant, R. G., Jr., Jr., Celia, M. A., Guswa, A. J., & Peters, C. A. (2002) · Environmental Science & Technology · doi:10.1021/es0223325 · Cited by 269
An overview of the underground disposal of carbon dioxide
Holloway, S. (1997) · Energy Conversion and Management · doi:10.1016/s0196-8904(96)00268-3 · Cited by 241
Sedimentary basins and greenhouse gases: a serendipitous association
Hitchon, B., Gunter, W. D., Gentzis, T., & Bailey, R. T. (1999) · Energy Conversion and Management · doi:10.1016/s0196-8904(98)00146-0 · Cited by 210
Mitigation Strategies for the Risk of CO2 Migration Through Wellbores
Barlet-Gouédard, V., Rimmelé, G., Goffé, B., & Porcherie, O. (2006) · All Days · doi:10.2118/98924-ms · Cited by 167
Regulating the Ultimate Sink: Managing the Risks of Geologic CO2Storage
Wilson, E. J., Johnson, T. L., & Keith, D. W. (2003) · Environmental Science & Technology · doi:10.1021/es021038+ · Cited by 166
Research works printed but not linked: 14
- Holloway S, 1997, Energy Convers. Manage., 38, 198
- White C. M., 2003, J. Air Waste Manage. Assoc., 53, 715
- Wilson E. J., 2003, Environ. Sci. Technol., 37, 3483
- Scherer G. W., 2005, CO2 Capture Project Technical Results, 2, 848
- Duguid A., 2006, Proceedings of 8th International Conference on Greenhouse Gas Control Technologies; Gale, J., Rokke, J., Zweigel, P., Svenson, H., Eds.; Elsevier: Amsterdam
- Duguid A., 2006, Proceedings of the 4th Annual Conference on Carbon Capture and Sequestration
- Bearden W. G., 1959, Oil-Well Cementing Practices in the United States, 59
- Stutzman P. E., Proceedings of the 21st International Conference on Cement Microscopy; International Cement Microscopy Association: Las Vegas, NV
- Thaulow N., Proceedings of the 24th International Conference on Cement Microscopy; International Cement Microscopy Association: San Diego, CA
- Stutzman P. E., 2001, Calcium Hydroxide in Concrete, 72
- Glasser F. P., 2001, Calcium Hydroxide in Concrete, 36
- Thaulow N., 2001, Calcium Hydroxide in Concrete, 201
- Mindness S., 2001, Calcium Hydroxide in Concrete, 154
- Moritis G, 2001, Oil Gas J., 99, 73
Cited by
Items 401–500 of 682
CO2 Underground Storage and Wellbore Integrity
Gaurina-Medjimurec, N., & Pašić, B. (2013) · Advances in environmental engineering and green technologies book series · doi:10.4018/978-1-4666-4777-0.ch015 · Cited by 9
Sedić, K., Gaurina-Medjimurec, N., & Pašić, B. (2015) · International Conference on Offshore Mechanics and Arctic Engineering (OMAE) · doi:10.1115/omae2015-41561 · Cited by 9
“3 MPa) and brine solutions at increased pressure and temperature and decreased pH [17].”
BackgroundMaterials for sustainable development
(2012) · MRS Bulletin · doi:10.1557/mrs.2012.90 · Cited by 9
CO2 storage feasibility in the P18-2 depleted gas field
Neele, F. P., Wildenborg, T., Geel, K., Loeve, D., Peters, L., Kahrobaei, S., Candela, T., Koenen, M., Hopmans, P., der Valk, K. V., et al. (2020) · TNO Repository · Cited by 9
Williams, J., Roy, S., Pal, N., Bridger, P., Vishal, V., & Nag, K. (2025) · International journal of greenhouse gas control · doi:10.1016/j.ijggc.2025.104497 · Cited by 8
Jun, E. C. J., Foo, H. C. Y., Mahmud, H. K. B., Wei, L. S., & Bennour, Z. (2025) · Renewable and Sustainable Energy Reviews · doi:10.1016/j.rser.2025.116567 · Cited by 8
A decade of progress in understanding and managing legacy well integrity for geologic carbon storage
Lackey, G., Wolterbeek, T. K. T., Cahill, A. G., Cavanagh, A., Moghadam, A., Iyer, J., Jordan, P. D., & Pawar, R. J. (2026) · International journal of greenhouse gas control · doi:10.1016/j.ijggc.2026.104604 · Cited by 8
Cement Sheath Integrity in Oil and Gas Wells
Gu, C., Feng, Y., & Li, X. (2024) · IntechOpen eBooks · doi:10.5772/intechopen.113052 · Cited by 8
Gan, M., Zhang, L., Wang, Y., Qin, Q., Xiao, T., Yin, Y., & Wang, H. (2024) · International journal of greenhouse gas control · doi:10.1016/j.ijggc.2024.104267 · Cited by 8
Hajiabadi, S. H., Khalifeh, M., & van Noort, R. (2025) · Geoenergy Science and Engineering · doi:10.1016/j.geoen.2025.213919 · Cited by 8
Gan, M., Zhang, L., Wang, Y., Hakuzweyezu, T., Sun, Q., & Qin, Q. (2025) · Geoenergy Science and Engineering · doi:10.1016/j.geoen.2025.213970 · Cited by 8
van Noort, R., Svenningsen, G., & Li, K. (2025) · Geoenergy Science and Engineering · doi:10.1016/j.geoen.2025.214005 · Cited by 8
Zhang, L., Xue, Q., Mei, K., Li, X., Wang, Y., Cheng, X., & Fu, X. (2024) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2024.135127 · Cited by 8
Han, J., Carey, J. W., & Zhang, J. (2011) · NACE CORROSION Conference · doi:10.5006/c2011-11376 · Cited by 8
Reactive Flow Channelization in Fractured Cement-implications for Wellbore Integrity
Wenning, Q. C., Huerta, N. J., Hesse, M. A., & Bryant, S. L. (2013) · Energy Procedia · doi:10.1016/j.egypro.2013.06.500 · Cited by 8
Comparison of Portland Cement (KS and API Class G) on Cement Carbonation for Carbon Storage
Lee, S., Chae, G., Jo, M., & Kim, T. (2014) · Journal of Materials in Civil Engineering · doi:10.1061/(asce)mt.1943-5533.0001031 · Cited by 8
Chemical degradation of reinforced epoxy‐cement composites under CO2‐rich environments
Schütz, M. K., Baldissera, A. F., Coteskvisk, P. M., Vecchia, F. D., Menezes, S. C., de Miranda, C. R., & Einloft, S. (2017) · Polymer Composites · doi:10.1002/pc.24589 · Cited by 8
González-Estrella, J., Ellison, J., Stormont, J. C., Shaikh, N., Peterson, E. J., Lichtner, P. C., & Cerrato, J. M. (2020) · Environmental Engineering Science · doi:10.1089/ees.2020.0093 · Cited by 8
“…of cement (e.g., elastic moduli and hardness) (Huerta et al. , 2011; Spokas et al. , 2018), and increase the dissolution rates of portlandite (Baur et al. , 2004; Marty et al. , 2009), which increase the porosity of cement (Kutchko et al. , 2007; Huerta et al. , 2011; Mason et al. , 2013).”
Barría, J. C., Manzanal, D., Pereira, J., & Ghabezloo, S. (2020) · E3S Web of Conferences · doi:10.1051/e3sconf/202020502007 · Cited by 8
Rhino, K., Iyer, J., Walsh, S. D. C., Carroll, S. A., & Smith, M. M. (2021) · International journal of greenhouse gas control · doi:10.1016/j.ijggc.2021.103340 · Cited by 8
Emmel, B. U., Gaweł, K., Bhuiyan, M. H., Torsæter, M., & Edvardsen, L. (2022) · Energies · doi:10.3390/en15020542 · Cited by 8
“Portlandite and calcium silicate hydrates are dissolved upon carbonation and calcite is precipitated, whereby the porosity and permeability of the material decrease [42].”
BackgroundNakano, K., Mito, S., Xue, Z., & Ohbuchi, A. (2016) · e-Journal of Surface Science and Nanotechnology · doi:10.1380/ejssnt.2016.198 · Cited by 8
Bello, K. (2014) · Louisiana State University · doi:10.31390/gradschool_theses.269 · Cited by 8
Final Technical Report: Integrated Wellbore Integrity Analysis Program for CO2 Storage Applications
Battelle, C., Sminchak, J. R., & USDOE Office of Fossil Energy (FE) (2018) · OSTI OAI (U.S. Department of Energy Office of Scientific and Technical Information) · doi:10.2172/1481775 · Cited by 8
Li, H., Yuen, K., Ma, H., Shi, X., Li, Y., Yang, C., Zheng, X., Lei, Z., Fang, J., & Liang, R. (2026) · Applied Energy · doi:10.1016/j.apenergy.2026.127781 · Cited by 7
Carbonic Acid Resistance of Hydroxyapatite-Containing Cement
Srivastava, A., Ahmed, R. M., & Shah, S. N. (2019) · SPE Drilling & Completion · doi:10.2118/193585-pa · Cited by 7
Wang, Y., Wang, J., Liu, H., Lv, X., & Ji, Z. (2025) · Petroleum Science · doi:10.1016/j.petsci.2025.02.023 · Cited by 7
Wellbore Integrity Challenges in the Era of Energy Transition
Nassan, T. H., & Amro, M. M. (2025) · EAGE Conference and Exhibition incorporating SPE EUROPEC · doi:10.2118/225550-ms · Cited by 7
Thermodynamic Modeling of Carbonation of Cementitious Materials in Contact with Supercritical CO2
Minoo, H., & Ishida, T. (2013) · Energy Procedia · doi:10.1016/j.egypro.2013.06.495 · Cited by 7
Casing Failure Using Machine Learning Algorithms: Five Case Studies
Noshi, C. I., Noynaert, S. F., & Schubert, J. J. (2018) · SPE Thermal Well Integrity and Design Symposium · doi:10.2118/193373-ms · Cited by 7
Wolterbeek, T. K. T., & Hangx, S. J. T. (2021) · Energies · doi:10.3390/en14227507 · Cited by 7
THE INFLUENCE OF CO2 ON WELL CEMENT
Gaurina-Međimurec, N. (2010) · DOAJ (DOAJ: Directory of Open Access Journals) · Cited by 7
Understanding boundary condition effects on the corrosion kinetics of class H well cement
Matteo, E., Scherer, G. W., Huet, B., & Pel, L. (2011) · Energy Procedia · doi:10.1016/j.egypro.2011.02.520 · Cited by 7
“Batch [4-6] and flowthrough [7,8] studies have examined the bounds of cement attack rates.”
BackgroundLong Term Wellbore Isolation In a Corrosive Environment
Ilesanmi, O. R., Hilal, B., Gill, S., Brandl, A., & Abdullah, A. (2013) · SPE/IADC Middle East Drilling Technology Conference and Exhibition · doi:10.2118/166769-ms · Cited by 7
Avalia??o da degrada??o por CO2 supercr?tico da pasta de cimento empregada em po?os de petr?leo
Vecchia, F. D. (2009) · LA Referencia (Red Federada de Repositorios Institucionales de Publicaciones Científicas) · Cited by 7
Jobard, E. (2013) · theses.fr (ABES) · doi:10.70675/dba75305zd20cz421bzbadcz1835af8c43f0 · Cited by 7
On the Flow of CO2-Saturated Water in a Cement Fracture
Tafen, D. N., Kutchko, B. G., & Massoudi, M. (2023) · Geosciences · doi:10.3390/geosciences13100312 · Cited by 6
Self-citationZheng, Y., Mei, K., Wei, T., He, X., Liu, C., Zhang, C., & Cheng, X. (2025) · Geoenergy Science and Engineering · doi:10.1016/j.geoen.2025.213914 · Cited by 6
A Review on In Situ Hydrogen Generation in Hydrocarbon Reservoirs
Özyurtkan, M. H., Çetin, C., & Temizel, C. (2026) · Gases · doi:10.3390/gases6010009 · Cited by 6
“Moreover, hydrogen diffusion into cement and wellbore materials has been shown to degrade cement–casing bonding and increase porosity, thereby elevating the risk of leakage during long-term operations [35].”
Hydraulic-Chemical Coupling Associated With Injection and Storage of CO2 Into Subsurface
Pawar, R. J., & Guthrie, G. D. (2018) · Elsevier eBooks · doi:10.1016/b978-0-12-812752-0.00013-7 · Cited by 6
Flow patterns of a resin repair material in a vertical wellbore microannulus
Fernandez, S. G., & Stormont, J. C. (2023) · Gas Science and Engineering · doi:10.1016/j.jgsce.2023.204963 · Cited by 6
Guo, X., Zhang, Y., Song, Y., & Zhang, Y. (2024) · Geoenergy Science and Engineering · doi:10.1016/j.geoen.2024.213177 · Cited by 6
Zhang, Z., Bu, Y., Guo, S., Lu, C. H., Liu, H., Guo, X., & Wang, X. (2025) · Physics of Fluids · doi:10.1063/5.0266722 · Cited by 6
Novel ductile wellbore cementitious composite for geologic CO2 storage
Adeoye, J. T., Zhang, D., Li, V. C., & Ellis, B. R. (2019) · International journal of greenhouse gas control · doi:10.1016/j.ijggc.2019.102896 · Cited by 6
“…zone supports previous studies, which showed that exposure to CO2-acidified water does not result in distinct reaction zones in fly ash-amended cementitious materials (Adeoye et al., 2019; Crow et al., 2010; Zhang et al., 2014), whereas it does in neat Portland cement (Kutchko et al., 2007).”
ResultGiannoukos, K., Hall, M. R., Rochelle, C. A., Milodowski, A. E., & Rigby, S. P. (2014) · Energy Procedia · doi:10.1016/j.egypro.2014.10.364 · Cited by 6
“In contrast, the carbonated outer part has lost its original structure with Si-bearing compounds being the dominant ones [5, 8].”
BackgroundOmosebi, O. A. (2016) · SHAREOK (University of Oklahoma; Oklahoma State University; Central Oklahoma University) · Cited by 6
Mechanical and microscopic properties of API G cement after exposure to supercritical CO2
Kuo, C.-C., Wang, C.-L., & Hsiang, H. (2017) · Terrestrial Atmospheric and Oceanic Sciences · doi:10.3319/tao.2015.08.20.02(gsc · Cited by 6
Bagheri, M., Shariatipour, S. M., & Ganjian, E. (2020) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2020.121100 · Cited by 6
Kmieć, M., Karpiński, B., Antoszkiewicz, M., & Szkodo, M. (2018) · Applied Clay Science · doi:10.1016/j.clay.2018.04.028 · Cited by 6
Moreno, W. E. G., Ponzi, G. G. D., Henrique, A. A. M. P., & Andrade, J. J. D. O. (2019) · Materials and Geoenvironment · doi:10.2478/rmzmag-2019-0017 · Cited by 6
Min, Y., Montross, S. N., Spaulding, R. E., Brandi, M., Huerta, N., Thomas, R., & Kutchko, B. G. (2021) · Environmental Science & Technology · doi:10.1021/acs.est.1c02699 · Cited by 6
Self-citation“Wellbore Integrity...” Say What??
Cooper, J. (2009) · Energy Procedia · doi:10.1016/j.egypro.2009.02.157 · Cited by 6
Sulfate Promotes Compact CaCO3 Formation and Protects Portland Cement from Supercritical CO2 Attack
Zhu, Y., McWest, L., Steefel, C. I., Wang, Y., Li, Q., Gao, Z., Yang, J., & Jun, Y. (2025) · Environmental Science & Technology · doi:10.1021/acs.est.4c08259 · Cited by 5
Bhuvankar, P., & Cihan, A. (2025) · International journal of greenhouse gas control · doi:10.1016/j.ijggc.2025.104373 · Cited by 5
Yin, Y., Zhang, L., Mei, K., Cheng, X., Gan, M.-G., Wang, Y., & Zhang, C.-M. (2025) · Petroleum Science · doi:10.1016/j.petsci.2025.12.001 · Cited by 5
Safety and risk assessment frameworks for offshore CO2 storage
Shah, M. S., Zendehboudi, S., Duan, X., Saady, N. M. C., Mohamadi‐Baghmolaei, M., Heagle, D., Dusseault, M. B., & Khan, F. (2026) · Process Safety and Environmental Protection · doi:10.1016/j.psep.2026.108980 · Cited by 5
Understanding CO2-brine-wellbore Cement-rock Interactions for CO2 Storage
Farooqui, N. M., Liu, Q., Maroto‐Valer, M. M., Mosleh, M. H., Korre, A., & Durucan, Ş. (2017) · Energy Procedia · doi:10.1016/j.egypro.2017.03.1676 · Cited by 5
“Poorly cemented casing/well annulus, casing failure and well abandonment failures have been recognised as some of the main reasons for well leakage when carbon dioxide is stored in geological formations [1].”
Background3D zero-thickness interface model for fracture of cement-based materials with chemical degradation
Martínez, A., Liaudat, J., López, C. M., & Carol, I. (2021) · International Journal of Solids and Structures · doi:10.1016/j.ijsolstr.2021.111379 · Cited by 5
Geomechanics of Geological Carbon Sequestration
Feng, Y., & Shui, Z. (2022) · IntechOpen eBooks · doi:10.5772/intechopen.105412 · Cited by 5
Lian, J., Wu, Z., Yu, L., Gao, Q., Mei, K., Cai, J., & Cheng, X. (2021) · Frontiers in Materials · doi:10.3389/fmats.2022.995122 · Cited by 5
“Portland cement is usually used in CCUS cementing projects (Kutchko et al., 2008; Duguid, 2009; Brandão et al., 2017).”
MethodExploring CCUS Well Construction Using Fit-For-Purpose Cement Designs
Shine, J., Qasmi, U., & Elhancha, A. (2024) · International Petroleum Technology Conference · doi:10.2523/iptc-23771-ea · Cited by 5
The Relevance of Geochemical Tools to Monitor Deep Geological CO2 Storage Sites
Jeandel, É., & Sarda, P. (2012) · InTech eBooks · doi:10.5772/32098 · Cited by 5
“Some authors note that a carbonate layer can be formed at the interface between the CO2-rich brine and the cement, which forms a barrier to further cement degradation (Kutchko et al., 2007, 2008).”
BackgroundTime-dependent Fluid Migration From a Storage Formation via Leaky Wells
Huerta, N. J., Strazisar, B. R., Bryant, S. L., & Hesse, M. A. (2014) · Energy Procedia · doi:10.1016/j.egypro.2014.11.605 · Cited by 5
“However, experiments have shown significant reaction between freephase CO2 or CO2-saturated brine and cement both in the field and in the laboratory under static and dynamic conditions (Kutchko et al., 2007; Mason et al., 2013; Newell and Carey, 2013).”
Self-citationLong Term Wellbore Isolation In a Corrosive Environment
Ilesanmi, O. R., Hilal, B., Gill, S., Brandl, A., Mazrouei, M. A., & Abdullah, A. (2014) · International Petroleum Technology Conference · doi:10.3997/2214-4609-pdb.395.spe-166769-ms · Cited by 5
Chemo-mechanical composite layer model for CO2-attacked cement
Li, Y., Ahmed, R. M., Han, B., Lu, Y., & Jin, Y. (2020) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2020.119128 · Cited by 5
Boul, P. J., Shanmugam, S., & Johnson, K. D. (2021) · The Canadian Journal of Chemical Engineering · doi:10.1002/cjce.24282 · Cited by 5
Wasch, L. J., Koenen, M., Wollenweber, J., & Tambach, T. J. (2015) · Greenhouse Gases Science and Technology · doi:10.1002/ghg.1515 · Cited by 5
Boul, P. J., Rasner, D. K., Johnson, K. D., & Thaemlitz, C. J. (2019) · MRS Communications · doi:10.1557/mrc.2019.70 · Cited by 5
Geomechanical Simulation of CO2 Leakage and Cap Rock Remediation
Nygaard, R., Bai, B., & Eckert, A. P. (2012) · OSTI OAI (U.S. Department of Energy Office of Scientific and Technical Information) · doi:10.2172/1113759 · Cited by 5
Wellbore Seal Repair Using Nanocomposite Materials
Stormont, J. C. (2016) · OSTI OAI (U.S. Department of Energy Office of Scientific and Technical Information) · doi:10.2172/1337552 · Cited by 5
Emergence of Delamination Fractures around Casing and Its Stability
Wang, W. (2013) · Louisiana State University · doi:10.31390/gradschool_dissertations.264 · Cited by 5
Geomechanical Study of Underground Hydrogen Storage
Kumar, K. R. (2023) · Research Repository (Delft University of Technology) · doi:10.4233/uuid:b3d264ce-e7dc-4e67-b0e1-94f3cc7831ca · Cited by 5
Assessing the feasibility of retrofitting legacy wells for CO2 geological sequestration
Malki, M. L., Heimerl, J., Ma, Z., Chen, B., van Wijk, J. W., & Mehana, M. Z. (2025) · International journal of greenhouse gas control · doi:10.1016/j.ijggc.2025.104389 · Cited by 4
Wellbore Interface and Cement Defects in CO 2 Geological Storage: A Review
Citalingam, K., Zeinijahromi, A., Salmachi, A., & Xie, Q. (2025) · Greenhouse Gases Science and Technology · doi:10.1002/ghg.70012 · Cited by 4
Oliveira, N., Szklo, A. S., Couto, P., Veloso, F. M. L., & Gravaud, I. (2026) · ACS Omega · doi:10.1021/acsomega.5c09944 · Cited by 4
Granular Calcium Carbonate Reinforced the Cement Paste Cured by Elevated Temperatures
Li, Y., & Liu, K. (2023) · ACS Omega · doi:10.1021/acsomega.2c07090 · Cited by 4
Diffusive Leakage of scCO2 in Shaly Caprocks: Effect of Geochemical Reactivity and Anisotropy
Cruz, F., Dang, S. T., Curtis, M. E., & Rai, C. (2024) · SPE Journal · doi:10.2118/219763-pa · Cited by 4
Liu, Y., Hu, K., Kuru, E., Li, H., Lin, Z., Iremonger, S. S., & DeBruijn, G. (2024) · SPE Annual Technical Conference and Exhibition · doi:10.2118/220884-ms · Cited by 4
Li, Z., Yin, Z., Zhou, D., Wu, Z., Wang, D., Guan, S., & Du, G. (2025) · Materials · doi:10.3390/ma18020244 · Cited by 4
Riyanto, L., Kumar, A. K., Shahril, M. A., Lau, C. H., Sazali, Y. A., Amir, M. S. E., Jain, B., Kapoor, S., Yakovlev, A., Duong, A. T., et al. (2023) · SPE Asia Pacific Oil and Gas Conference and Exhibition · doi:10.2118/215277-ms · Cited by 4
Du, Y., Qi, Y., Zeng, Q., Zhan, L., Wang, J., & Zhang, Z. (2024) · Journal of CO2 Utilization · doi:10.1016/j.jcou.2024.102937 · Cited by 4
Ghanbari, S., Sefat, M. H., Davies, D. R., J, M., Bonfanti, R. O., & Martin, I. (2024) · Abu Dhabi International Petroleum Exhibition & Conference (ADIPEC) · doi:10.2118/222449-ms · Cited by 4
Nassan, T. H., Kummer, N.-A., Fogden, A., Solbakken, J., Aarra, M. G., Zamani, N., Burachok, O., & Amro, M. M. (2025) · EAGE Conference and Exhibition incorporating SPE EUROPEC · doi:10.2118/225602-ms · Cited by 4
Time dependent leakage of CO₂ saturated water along a cement fracture
Huerta, N. J. (2013) · Texas ScholarWorks (Texas Digital Library) · Cited by 4
Li, B., Guo, B., Li, H., & Zhou, Y. (2015) · Journal of Sustainable Energy Engineering · doi:10.7569/jsee.2014.629518 · Cited by 4
CO2 Storage related Groundwater Impacts and Protection
Fischer, S., Knopf, S., May, F., & Rebscher, D. (2016) · Grundwasser · doi:10.1007/s00767-015-0315-7 · Cited by 4
“This process could ultimately result in pure amorphous silica gel and an increased porosity compared to unaltered cement, strongly reducing cement sealing properties (Kutchko et al. 2007).”
BackgroundThompson, J. R., Freedman, A. J., Peet, K. C., & Franklin, J. (2018) · Elsevier eBooks · doi:10.1016/b978-0-12-812752-0.00012-5 · Cited by 4
A Study on the Chemo-Mechanical Alteration of Cement in CO2 Storage Sites
Bagheri, M., Shariatipour, S. M., & Ganjian, E. (2019) · EAGE Conference and Exhibition incorporating SPE EUROPEC · doi:10.2118/195520-ms · Cited by 4
Cement-Rock Interface Subjected to scCO2
Barría, J. C., Manzanal, D., Martin, C., Piqué, T. M., & Pereira, J. (2019) · Hispana · Cited by 4
García-Rios, M., & Gouze, P. (2018) · Geosciences · doi:10.3390/geosciences8080290 · Cited by 4
“Although some researchers have attempted to mitigate the limitations of conventional Portland cement during years [5,13,14], it is obvious that it still displays some identified weaknesses, such as its limited ability to penetrate into the formation matrix for distances larger than a few inches, shortcomings during se…”
BackgroundZhang, X., Wu, B., Zhang, J., Li, J., Wang, S., Dong, L., Liu, L., & Xiang, D. (2019) · International Journal of Electrochemical Science · doi:10.20964/2019.11.04 · Cited by 4
Hakuzweyezu, T., Gan, M., Zhang, L., Wang, Y., & Onyekwena, C. C. (2025) · Energy & Fuels · doi:10.1021/acs.energyfuels.5c00286 · Cited by 3
Effect of carbonation on concrete structure - a review
Chavan, P., & Mishra, C. (2025) · Journal of Physics Conference Series · doi:10.1088/1742-6596/3076/1/012008 · Cited by 3
Liu, Y., Hu, K., Kuru, E., Li, H., Lin, Z., Iremonger, S. S., & DeBruijn, G. (2025) · SPE Annual Technical Conference and Exhibition · doi:10.2118/227930-ms · Cited by 3
Carbonation in CCUS oil wells: A mini‐review and bibliometric analysis
Ventura, R. A., Braga, G. S., Moraes, E. P., Freitas, J. C. D. O., Galbiati, F., & Santiago, R. C. (2025) · Next research. · doi:10.1016/j.nexres.2025.101214 · Cited by 3
Zou, M., Liu, J.-H., & Li, K. (2025) · Journal of Central South University · doi:10.1007/s11771-025-6045-9 · Cited by 3
“The dissolution of Ca(OH) 2 increases porosity and enhances the leaching of Ca 2+ from the cement paste [24].”
Engelke, B. S., Pernites, R. B., Kapoor, S., Droger, N., Abad, C., Malik, S., Jain, B., Agostinho, B., & Rasheed, H. (2025) · SPE Conference at Oman Petroleum & Energy Show · doi:10.2118/225233-ms · Cited by 3
Zhang, L., Gan, M., Zhang, L., Zhang, C., Wang, Y., & Hakuzweyezu, T. (2025) · Geomechanics for Energy and the Environment · doi:10.1016/j.gete.2025.100728 · Cited by 3
Cements for CO 2 Capture and Storage Wells
Plank, J. (2022) · ACS symposium series · doi:10.1021/bk-2022-1412.ch008 · Cited by 3
A Review of Studies Examining the Potential for Groundwater Contamination From CO 2 Sequestration
Varadharajan, C., Tinnacher, R. M., Trautz, R., Zheng, L., Dafflon, B., Wu, Y., Reagan, M. T., Birkhölzer, J., & Carey, J. W. (2018) · Geophysical monograph · doi:10.1002/9781119118657.ch15 · Cited by 3
Metadata
- Authors
- Kutchko, B. G., Strazisar, B. R., Dzombak, D. A., Lowry, G. V., & Thaulow, N.
- Affiliations
- United States Department of Energy (US)
- Corresponding author
- Strazisar, Brian R.
- Venue
- Environmental Science & Technology
- Publisher
- American Chemical Society (ACS)
- Published
- 2007-05-19
- Volume
- 41
- Issue
- 13
- Pages
- 4787-4792
- ISSN
- 0013-936X (ISSN-L)
- 1520-5851
- OpenAlex
- W2055191938
- Semantic Scholar
- 80aef684d3df6e40776af4e00a94d8da9ef3c58d
- Cited by
- 604
- References
- 20
- Citations by year
- 2026: 60 · 2025: 45 · 2024: 43 · 2023: 28 · 2022: 29 · 2021: 39 · 2020: 31 · 2019: 40 · 2018: 37 · 2017: 31 · 2016: 36 · 2015: 28 · 2014: 31 · 2013: 39 · 2012: 19
- FWCI
- 17.05
- Type
- journal article
- Language
- en
- Open access
- closed
- Locations
- Environmental Science & Technology (publishedVersion)
- PubMed (publishedVersion)
- Funders
- U.S. Department of Energy
- Princeton University
- National Energy Technology Laboratory
- Topics
- Physical Sciences › Environmental Science › Environmental Engineering › CO2 Sequestration and Geologic Interactions
- Physical Sciences › Energy › Fuel Technology › Drilling and Well Engineering
- Physical Sciences › Engineering › Civil and Structural Engineering › Concrete and Cement Materials Research
- Keywords
- CO2 sequestration, cement hydration, curing conditions, carbonation, cement durability
- MeSH terms
- Carbon Dioxide, Geology, Microscopy, Electron, Scanning, Geological Phenomena
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.