Speciation and Crystal Chemistry of Iron(III) Chloride Hydrolyzed in the Presence of SiO4 Ligands. 1. An Fe K-Edge EXAFS Study

Doelsch, Emmanuel, Rose, Jérome, Masion, Armand, Bottero, Jean Yves, Nahon, Daniel, Bertsch, Paul M.·2000·Langmuir

Abstract

The hydrolysis of Fe−Si systems with Si/Fe ratios between 0 and 4 leads to the formation of poorly crystalline or, more frequently, of long-range disorganized precipitates. The increase of Si/Fe molar ratios results in an dramatic change of Fe polymerization. The formation of double and single corner-sharing Fe linkages is reduced compared to pure Fe hydrolysis products. The growth regime depends on the Si concentration in the system. Three-dimensional and two-dimensional growth of Fe colloids occurs at low and high Si/Fe ratios, respectively, systems with Si/Fe ratios around 1 representing a crossover between these two regimes. Though Si neighbors cannot be detected unequivocally by Fe K-edge EXAFS, their presence in the close environment of Fe atoms is evident from the change in Fe speciation.

Integrity signals

Registry

Crossref · 10.1021/la991378h

Cites

27 of 27 references verified0 citation errors · 0 not checkable

Statistics

Recomputing p-values needs the paper’s full text.

Claims the paper makes

This paper’s full text isn’t openly available, so its claims and self-check weren’t run. The registry and citation checks still apply.

Cites

Flagged first, then by citations

Cited by

Sorted by citations

Authors
Doelsch, E., Rose, J., Masion, A., Bottero, J. Y., Nahon, D., & Bertsch, P. M.
Affiliations
  • CEREGE (UMR 6635, CNRS-Aix-Marseille III), Europole Méditerranéen de l'Arbois, BP 80, 13545 Aix-en-Provence Cedex 04, France, and Savannah River Ecology Laboratory, AACES, University of Georgia, PO Drawer E, Aiken, South Carolina 29802
  • Centre National de la Recherche Scientifique (FR)
Venue
Langmuir
Published
2000-04-21
Volume
16
Issue
10
Pages
4726-4731
ISSN
  • 0743-7463 (ISSN-L)
  • 1520-5827
OpenAlex
W1986293997
Cited by
101
References
27
Citations by year
2026: 1 · 2025: 3 · 2024: 1 · 2023: 2 · 2022: 4 · 2021: 2 · 2020: 5 · 2019: 8 · 2018: 4 · 2017: 8 · 2016: 6 · 2015: 5 · 2014: 4 · 2013: 4 · 2012: 4
FWCI
4.88
Type
journal article
Language
en
Open access
closed
Locations
  • Langmuir (publishedVersion)
  • HAL AMU (submittedVersion)
Funders
U.S. Department of Energy (FC09-96SR18546)
Topics
  • Physical Sciences › Energy › Renewable Energy, Sustainability and the Environment › Iron oxide chemistry and applications
  • Physical Sciences › Physics and Astronomy › Radiation › X-ray Spectroscopy and Fluorescence Analysis
  • Physical Sciences › Environmental Science › Water Science and Technology › Coagulation and Flocculation Studies
Keywords
Fe-Si system, crystal chemistry, Fe K-edge EXAFS, precipitate morphology

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review