Nanometre-scale evidence for interfacial dissolution–reprecipitation control of silicate glass corrosion
The DOI matches its Crossref record; 30 of the 31 references it cites were found in a registry or an index.
Abstract
Silicate glasses are durable solids, and yet they are chemically unstable in contact with aqueous fluids-this has important implications for numerous industrial applications related to the corrosion resistance of glasses, or the biogeochemical weathering of volcanic glasses in seawater. The aqueous dissolution of synthetic and natural glasses results in the formation of a hydrated, cation-depleted near-surface alteration zone and, depending on alteration conditions, secondary crystalline phases on the surface. The long-standing accepted model of glass corrosion is based on diffusion-coupled hydration and selective cation release, producing a surface-altered zone. However, using a combination of advanced atomic-resolution analytical techniques, our data for the first time reveal that the structural and chemical interface between the pristine glass and altered zone is always extremely sharp, with gradients in the nanometre to sub-nanometre range. These findings support a new corrosion mechanism, interfacial dissolution-reprecipitation. Moreover, they also highlight the importance of using analytical methods with very high spatial and mass resolution for deciphering the nanometre-scale processes controlling corrosion. Our findings provide evidence that interfacial dissolution-reprecipitation may be a universal reaction mechanism that controls both silicate glass corrosion and mineral weathering.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“The emergence of silica-rich 'leached layers' during metal silicate mineral dissolution in contact with bulk aqueous solution that can act as passivating layers is a well-known phenomenon, though debate continues regarding the deposition and polymerization mechanism.200,201”
From Molecular-scale mechanisms of CO2 mineralization in nanoscale interfacial water films (2022) · cites this paper as [200]
Citations
Cites
Miller, M. K. (2006) · Handbook of Microscopy for Nanotechnology · doi:10.1007/1-4020-8006-9_8 · Cited by 1,252
Kelly, T. F., & Miller, M. K. (2007) · Review of Scientific Instruments · doi:10.1063/1.2709758 · Cited by 867
Molecular mechanisms for corrosion of silica and silicate glasses
Bunker, B. C. (1994) · Journal of Non-Crystalline Solids · doi:10.1016/0022-3093(94)90708-0 · Cited by 635
(1967) · CaltechAUTHORS (California Institute of Technology) · Cited by 586
Insight into silicate-glass corrosion mechanisms
Cailleteau, C., Angeli, F., Devreux, F., Gin, S., Jestin, J., Jollivet, P., & Spalla, O. (2008) · Nature Materials · doi:10.1038/nmat2301 · Cited by 488
The mechanism of reequilibration of solids in the presence of a fluid phase
Putnis, A., & Putnis, C. V. (2007) · Journal of Solid State Chemistry · doi:10.1016/j.jssc.2007.03.023 · Cited by 403
Frugier, P., Gin, S., Minet, Y., Chave, T., Bonin, B., Godon, N., Lartigue, J.-E., Jollivet, P., Ayral, A., De Windt, L., et al. (2008) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2008.06.044 · Cited by 395
Mineral–water interfacial structures revealed by synchrotron X-ray scattering
Fenter, P., & Sturchio, N. C. (2004) · Progress in Surface Science · doi:10.1016/j.progsurf.2004.12.001 · Cited by 392
Interdiffusion of hydrogen and alkali ions in a glass surface
Doremus, R. H. (1975) · Journal of Non-Crystalline Solids · doi:10.1016/0022-3093(75)90079-4 · Cited by 366
Hellmann, R., Wirth, R., Daval, D., Barnes, J.-P., Penisson, J.-M., Tisserand, D., Epicier, T., Florin, B., & Hervig, R. L. (2012) · Chemical Geology · doi:10.1016/j.chemgeo.2011.12.002 · Cited by 327
Self-citation
Research works printed but not linked: 1
- Dran, J-C., Della Mea, G., Paccagnella, A., Petit, J-C. & Trotignon, L. The aqueous dissolution of alkali silicate glasses: Reappraisal of mechanisms by H and Na depth profiling with high energy ion beams. Phys. Chem. Glasses 29, 249–255 (1988).
Cited by
Items 201–300 of 331
Sessegolo, L., Verney‐Carron, A., Valle, N., Ausset, P., Narayanasamy, S., Nowak, S., Fourdrin, C., Saheb, M., & Chabas, A. (2021) · Journal of Non-Crystalline Solids · doi:10.1016/j.jnoncrysol.2021.121020 · Cited by 8
Water corrosion mechanisms in ternary sodium borosilicate glass under varied pH conditions
Bai, K., Qin, K., Jin, Z., Zhang, B., Wang, Y., Hu, H., Ejaz, A., Lv, P., Wang, T., & Peng, H. (2025) · Ceramics International · doi:10.1016/j.ceramint.2025.01.352 · Cited by 7
Carrière, C., Neff, D., Martin, C., Tocino, F. Y., Delanoë, A., Gin, S., Michau, N., Linard, Y., & Dillmann, P. (2020) · Materials and Corrosion · doi:10.1002/maco.202011766 · Cited by 8
Liu, X., Qiao, Y., Qian, Z., Zhou, S., Li, L., Ma, J., Wang, S., Qin, Q., & Zhang, Q. (2021) · Journal of Hazardous Materials Advances · doi:10.1016/j.hazadv.2021.100027 · Cited by 7
Diffusive processes in aqueous glass dissolution
Goût, T. L., Misra, S., Tipper, E. T., Bohlin, M. S., Guo, R., & Farnan, I. (2019) · npj Materials Degradation · doi:10.1038/s41529-019-0102-5 · Cited by 7
Etschmann, B. E., Verdugo, L., Kalintsev, A., Abdus-Salam, M., Ram, R., Vollert, L., O’Callaghan, J., Liu, Y., Williams, T., Guagliardo, P. R., et al. (2025) · Geoscience Frontiers · doi:10.1016/j.gsf.2025.102119 · Cited by 6
Compositional changes by SIMS and XPS analyses on fresh and aged Roman-like glass
Zanini, R., Franceschin, G., Cattaruzza, E., Prato, M., Barozzi, M., & Traviglia, A. (2022) · Journal of Non-Crystalline Solids · doi:10.1016/j.jnoncrysol.2023.122356 · Cited by 6
Liu, Y., Zhang, H., Zhang, Z., Jing, L., & Liu, K. (2024) · Fractal and Fractional · doi:10.3390/fractalfract8060335 · Cited by 6
Wang, R., Hu, L., Xu, Y., Chen, S., & Ren, J. (2024) · Acta Materialia · doi:10.1016/j.actamat.2024.120164 · Cited by 11
Advancing Sodium-Ion Battery Cathode Analysis With Cryogenic Ag-coated APT Specimens
Yadav, P., Aota, L. S., Woods, E., Schwarz, T. M., Joshi, Y., Singh, M. P., & Gault, B. (2025) · Microscopy and Microanalysis · doi:10.1093/mam/ozaf041 · Cited by 6
Chemical Reactivity and Surface Chemistry of Porous Silicon
Sailor, M. J. (2017) · Springer eBooks · doi:10.1007/978-3-319-04508-5_37-2 · Cited by 6
Silicon Oxynitride Coatings Are Very Promising for Inert and Durable Pharmaceutical Glass Vials
Topka, K. C., Diallo, B., Puyo, M., Chesneau, E., Inoubli, F., Ponton, S., Genevois, C., Samélor, D., Laloo, R., Sadowski, D., et al. (2023) · ACS Applied Engineering Materials · doi:10.1021/acsaenm.3c00584 · Cited by 6
Chen, S., Luo, L., Sun, H., Peng, T., Lei, J. H., Jin, Y., & Xian, Z. (2024) · Ceramics International · doi:10.1016/j.ceramint.2024.12.091 · Cited by 6
Wang, Z., Li, X., Chen, C., Lou, M., Wu, J., Gao, K., Li, Z., Sun, K., Li, Z., Xiao, Z., et al. (2024) · Advanced Science · doi:10.1002/advs.202412397 · Cited by 6
Chemical Reactivity and Surface Chemistry of Porous Silicon
Sailor, M. J. (2018) · Springer eBooks · doi:10.1007/978-3-319-71381-6_37 · Cited by 6
Simplifying a solution to a complex puzzle
Gin, S., Ryan, J. V., Kerisit, S., & Du, J. (2018) · npj Materials Degradation · doi:10.1038/s41529-018-0057-y · Cited by 6
Freedman, V. L., USDOE, Ryan, J., & Bacon, D. H. (2015) · OSTI OAI (U.S. Department of Energy Office of Scientific and Technical Information) · doi:10.2172/1515180 · Cited by 6
“…mechanisms such as reactive transport through an altered layer (Frugier et al. 2009) or a dissolution reprecipitation couple (Geisler et al. 2010; Hellman et al. 2015), each of these models (and others) includes a solution-affinity term in some form, pointing to a more general acceptance of the…”
BackgroundImpact of Chemical Corrosion on Mechanical Properties of Boroaluminosilicate Pharmaceutical Glasses
Ma, X., Liu, J., Zhang, J., Su, Y., Yi, K., Zhang, Y., Ding, L., & Zheng, Q. (2024) · Materials · doi:10.3390/ma17133120 · Cited by 5
“The microstructure of the alteration layer is extremely complex and very different from the original glass, such as “hydrated glass” or “mutual diffusion layer”, amorphous layer rich in silica, precipitate layer formed by secondary minerals and so on [23–26].”
BackgroundCagnon, B., Gin, S., Cabié, M., & Daval, D. (2025) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2025.155796 · Cited by 5
Self-citationMarcial, J., Chesnutt, J. M., Neeway, J. J., Gichon, E., Thorpe, C. L., Zhu, Z., Golovchak, R., Cebulski, J., Niedzielski, P., Szostek, M., et al. (2025) · npj Materials Degradation · doi:10.1038/s41529-025-00624-4 · Cited by 5
“Atomic scale measurements are crucial for future interpretations of the mechanisms of alteration 95,111 – 113 .”
Self-citationZhai, Y., QingDong, Z., Hellmann, R., ShanKe, L., JianMing, L., & Nan, J. (2020) · Acta Petrologica Sinica · doi:10.18654/1000-0569/2020.09.14 · Cited by 6
Self-citationGeochemical applications of mineral-water interactions
Ruíz-Agudo, E., & Ruiz‐Agudo, C. (2024) · Elsevier eBooks · doi:10.1016/b978-0-323-99762-1.00051-6 · Cited by 6
Delaye, J., Tiwari, S., Brun, E., Fossati, P. C. M., & Gin, S. (2024) · Journal of the American Ceramic Society · doi:10.1111/jace.20167 · Cited by 5
Taron, M., Gin, S., Kaya, H., Delaye, J., & Kim, S. H. (2025) · npj Materials Degradation · doi:10.1038/s41529-025-00576-9 · Cited by 5
“From the B pro fi les, it is thus possible to determine the thickness of the gel, with the midpoint depth of the B gradient indicating the interface between the gel and the pristine glass as explained in former articles dedicated to this analytical technique applied to glass corrosion 12,13 .”
Zhang, D., Zhang, X., Zeng, X., Zhu, C., Meng, F., & Yan, Q. (2025) · Scripta Materialia · doi:10.1016/j.scriptamat.2025.116818 · Cited by 5
Evaluation of Glass Coatings with Various Silica Content Corrosion in a 0.5 M HCl Water Solution
Wang, H., Zhang, C., Jiang, C., Zhu, L., Cui, J., Han, L., Chen, M., Geng, S., & Wang, F. (2021) · Crystals · doi:10.3390/cryst11040346 · Cited by 5
Decreasing Hygroscopicity Slows Forsterite Carbonation under Low-Water Conditions
Rajan, B. P., Mergelsberg, S. T., Bowden, M., Peterson, K. A., Burton, S., Bowers, G. M., Wietsma, T., Graham, T. R., Qafoku, O. S., Thompson, C. J., et al. (2025) · Environmental Science & Technology · doi:10.1021/acs.est.5c01695 · Cited by 5
Atomistic origin of kinetics in hydrated aluminosilicate gels upon precipitation
Zhao, C. B., Yu, J., Chen, X., Wu, Q., Zhou, W. H., & Bauchy, M. (2023) · The Journal of Chemical Physics · doi:10.1063/5.0165937 · Cited by 4
Zheng, Q., Ma, X., Ma, Y., Yu, J., Yue, Y., & He, H. (2024) · npj Materials Degradation · doi:10.1038/s41529-024-00431-3 · Cited by 4
Wang, K., Chen, Y., Findling, N., Charlot, F., Charlet, L., Liu, J., & Zhang, Z. T. (2024) · npj Materials Degradation · doi:10.1038/s41529-024-00444-y · Cited by 4
“The formation of a gap parallel to SAL is commonly found indriedsamplesfromex-situexperiments 6,55 .”
Qin, Q., Stone‐Weiss, N., Shi, N., Mukherjee, P., Ren, J., & Goel, A. (2024) · Journal of the American Ceramic Society · doi:10.1111/jace.19806 · Cited by 4
Hsieh, E., Fischer, C., & Orillaneda, B. C. (2023) · Heritage Science · doi:10.1186/s40494-023-00953-0 · Cited by 4
Berlin, T. U., Kutzschbach, M., Potsdam, D. G., Guttmann, P., Energie, H.-Z. B. F. M. U., Marquardt, K. T., Bayreuth, U., Werner, S., Henzler, K. D., Institut, P. S., et al. (2018) · Physics and Chemistry of Glasses European Journal of Glass Science and Technology Part B · doi:10.13036/17533562.59.1.043 · Cited by 4
“Another possibility, is to use energy filtered TEM (EFTEM) or TEM electron energy loss spectroscopy (EELS), which both have been successfully applied to derive chemical information of altered silicate glasses at the nanometer scale (Hellman et al. 2015, Gin et al. 2013).”
BackgroundJiang, B., He, H., Zhang, Y., & Yu, J. (2018) · Journal of the American Ceramic Society · doi:10.1111/jace.16083 · Cited by 4
Alloteau, F. (2017) · theses.fr (ABES) · doi:10.70675/c2b59355z1dfcz46e2zbbcaz7a10309c0474 · Cited by 9
Hatori, T., Matsubara, R., Inagaki, Y., Ishida, K., & Ohkubo, T. (2024) · Journal of the American Ceramic Society · doi:10.1111/jace.19935 · Cited by 3
Corrosion studies on Tang dynasty opaque glaze celadon excavated from Qiong kiln, Sichuan, China
Wu, H. P., Wang, Y., Ma, Q., Wang, Y. H., & ZhiminLi (2025) · Materials Characterization · doi:10.1016/j.matchar.2025.114863 · Cited by 3
Senevirathna, T. C., Dharmapriya, P. L., Balasooriya, N. W. B., Pitawala, H. M. T. G. A., Wijayasinghe, H. W. M. A. C., Abeysinghe, M., & Sajeev, K. (2025) · Journal of Earth System Science · doi:10.1007/s12040-025-02559-5 · Cited by 3
Shen, F., Tang, J., Wang, Y., Liu, G., & Liu, C. (2025) · npj Materials Degradation · doi:10.1038/s41529-025-00672-w · Cited by 3
“This concept is consistent with the stepwise, site-speci fi c dissolution mechanisms proposed based on quantum chemical calculations 41 and is supported by experimental observations of interfacial dissolution – reprecipitation processes in silicates and aluminosilicates at the nanoscale 42 .”
Structural origin of high bioactivity in zirconia containing bioactive glasses
Xie, W., Pillai, D. V., Shi, Y., Youngman, R. E., Hufziger, K. T., Fu, Q., Zheng, Y., & Du, J. (2025) · Acta Biomaterialia · doi:10.1016/j.actbio.2025.11.014 · Cited by 3
Pathway of dolomite mimetically replacing calcite in nature
Huang, H., Meister, P. H., Li, G., Hu, W., Xu, W., Luo, Y., Lu, Y., & Yan, W. (2026) · Geological Society of America Bulletin · doi:10.1130/b38031.1 · Cited by 3
Remedial insight on ageing of glass through the study of ancient man‐made artefacts
Golovchak, R., Kovalskiy, A. P., Shpotyuk, Y., Mahlovanyi, B., Płoch, D., Ignatova, T., Kozdraś, A., Cebulski, J., & Czopek, S. (2020) · Archaeometry · doi:10.1111/arcm.12599 · Cited by 5
Lee, C. W., Kwon, Y. K., & Heo, J. (2021) · Journal of Radioanalytical and Nuclear Chemistry · doi:10.1007/s10967-021-07687-y · Cited by 3
Cao, W., Zhou, Z., Li, C., Wang, Q., Huang, Y. F., & Shen, S. (2020) · Ceramics International · doi:10.1016/j.ceramint.2020.09.007 · Cited by 3
Rumynin, V. G., Rozov, K., Nikulenkov, A. M., Sindalovskiy, L. N., Aloy, A. S., Karpovich, N. F., & Slastikhina, P. V. (2022) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2022.153895 · Cited by 3
Natural glass alteration under a hyperalkaline condition for about 4000 years
Kikuchi, R., Satō, T., Fujii, N., Shimbashi, M., & Arcilla, C. A. (2022) · Scientific Reports · doi:10.1038/s41598-022-20482-3 · Cited by 5
Glass alteration in 19th century glass photographic plates: Potential role in gelatin delamination
Hiebert, M. E., Oakman, S., Brogdon-Grantham, S. A., & Lam, T. F. (2022) · Journal of the American Ceramic Society · doi:10.1111/jace.18880 · Cited by 3
Diffusion models for the early-stage SON68 glass dissolution in a hyper-alkaline solution
Liu, S., Ferrand, K., Aertsens, M., Jacques, D., & Lemmens, K. (2019) · Applied Geochemistry · doi:10.1016/j.apgeochem.2019.104439 · Cited by 3
Carou, C. B. (2019) · Digital Library of Theses and Dissertations (Universidade de São Paulo) · doi:10.11606/d.8.2019.tde-11122019-171423 · Cited by 8
Corrosion of Natural Glasses in Seawater
Hellmann, R. (2021) · Wiley eBooks · doi:10.1002/9781118801017.ch7.3 · Cited by 5
Self-citationRadiation damage effects on the structure and properties of radioactive waste glasses
Rautiyal, P. (2021) · Sheffield Hallam University · doi:10.7190/shu-thesis-00378 · Cited by 3
Temperature dependent lithium isotope fractionation during glass dissolution
Goût, T. L., Bohlin, M. S., Tipper, E. T., Lampronti, G. I., & Farnan, I. (2021) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2021.09.005 · Cited by 2
Formation Mechanism of Crystalline Phase during Corrosion of Aluminum Phosphate Glasses
Wang, R., Hu, L., Tang, Y., Chen, S., Xu, Y., & Ren, J. (2024) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.3c08405 · Cited by 2
Lönartz, M. I., Stausberg, L., Müller, G., Dohmen, L., Lenting, C., Fritzsche, M. B. K., & Geisler, T. (2025) · Journal of Visualized Experiments · doi:10.3791/67763 · Cited by 2
Popel, A. J., Okhrimenko, D. V., Jensen, M., Rasmussen, K. H., Bøjesen, E. D., Ceccato, M., Sørensen, H. O., Lakshtanov, L. Z., Solvang, M., & Stipp, S. L. S. (2025) · Journal of Non-Crystalline Solids · doi:10.1016/j.jnoncrysol.2025.123692 · Cited by 3
Lönartz, M. I., Stausberg, L., Fritzsche, M. B. K., Trautmann, C., & Geisler, T. (2026) · npj Materials Degradation · doi:10.1038/s41529-026-00754-3 · Cited by 2
Element mobility and oxygen isotope systematics during submarine alteration of basaltic glass
He, M., Zhang, S., Zhang, L., Yang, F., Zhang, Y., Huang, X., & Wei, G. (2021) · American Mineralogist · doi:10.2138/am-2021-7831 · Cited by 3
Monitoring and Understanding VOC Induced Glass Corrosion Using Multi-modal Imaging Techniques
Sharma, D., Rothenhäusler, U., Schmidt-Ott, K., Nurit, M., Castro, Y., Goïc, G. L., Joseph, É., George, S., & Lombardo, T. (2022) · Lecture notes in mechanical engineering · doi:10.1007/978-3-031-17594-7_27 · Cited by 2
Sessegolo, L., Godon, N., Lossois, A., Cabié, M., Frugier, P., Tocino, F. Y., Michau, N., & Martin, C. (2024) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2024.155253 · Cited by 2
Self-citationBerezicka, A., Wojteczko, A., Sułowska, J., & Szumera, M. (2025) · Molecules · doi:10.3390/molecules30081790 · Cited by 2
Ji, W. A. N. G., Ma, X., Hanghao, G. U. O., Huixia, W. A. N. G., Yongping, Q. U., Weizhou, J. I. A. O., & Ma, Z. (2025) · Journal of Fuel Chemistry and Technology · doi:10.1016/s1872-5813(25)60566-4 · Cited by 2
Flame‐impingement‐induced superhydrophilicity of soda‐lime‐silica glass surface
Roy, B. K. D., Schmidt, A., Rosin, A., & Gerdes, T. (2024) · International Journal of Applied Glass Science · doi:10.1111/ijag.16695 · Cited by 1
Wu, H. P., Wang, Y., Ma, Q., Li, H., He, P., Wang, Y., & Xu, S. (2025) · npj Heritage Science · doi:10.1038/s40494-025-01648-4 · Cited by 1
Long, S., Han, H., Bai, W., Han, J., Zhou, J. K., Ma, Q., & Li, Z. (2025) · Journal of Non-Crystalline Solids · doi:10.1016/j.jnoncrysol.2025.123712 · Cited by 1
Shang, S., Zhang, W., & Zhang, J. (2025) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.5c05058 · Cited by 1
Composition‐Response Mapping of Dissolution and Ion Release in Multicomponent Borate Glasses
Andrea, C., & Boyd, D. (2026) · Journal of the American Ceramic Society · doi:10.1111/jace.70537 · Cited by 1
In-situ organic cation evolution driven sequential crystal transformation in hybrid metal halides
Han, W., Guan, J., Guo, X., Liu, W., Zhao, R., Wang, Z., Xu, L., Cheng, P., Chen, M., Li, Q., et al. (2026) · National Science Open · doi:10.1360/nso/20260013 · Cited by 1
Sly, J. J., & Mauro, J. C. (2026) · Journal of the American Ceramic Society · doi:10.1111/jace.70850 · Cited by 1
“Evidence for an alternative mechanism shows gel formation by precipitation of silica and additional glass components as solubility limits are reached over time [ 25, 29 ].”
Maeda, S., Funayama, I., Motegi, N., & Fujima, T. (2026) · Journal of Non-Crystalline Solids · doi:10.1016/j.jnoncrysol.2026.124256 · Cited by 1
Hiebert, M. E., Phaneuf, R. J., & Vicenzi, E. P. (2018) · Microscopy and Microanalysis · doi:10.1017/s1431927618011340 · Cited by 1
Utsunomiya, S., Fueda, K., Minomo, K., Horie, K., Takehara, M., Yamasaki, S., Shiotsu, H., Ohnuki, T., Law, G. T. W., Grambow, B., et al. (2022) · Royal Society of Chemistry eBooks · doi:10.1039/9781839166570-00015 · Cited by 1
Kordová, T., Mareška, A., & Havlík, M. M. (2022) · Koroze a ochrana materialu · doi:10.2478/kom-2022-0009 · Cited by 1
Echave, T. D. (2018) · theses.fr (ABES) · doi:10.70675/cedec676zdd02z4fd3z933az77472948ba49 · Cited by 1
Jan, A. (2020) · theses.fr (ABES) · doi:10.70675/99648d10z3288z4411z86e1z176378366e02 · Cited by 4
Skorina, T. (2015) · Resource-Efficient Technologies · doi:10.1016/j.reffit.2015.06.005
Bioalteration de verres basaltiques modèles : impact des sidérophores et rôle du fer
Pérez, A. (2015) · theses.fr (ABES) · doi:10.70675/a2cff8eaz147az4775z90a6zcc588b13b0b6 · Cited by 1
Hiebert, M. E., Phaneuf, R. J., & Vicenzi, E. P. (2017) · Microscopy and Microanalysis · doi:10.1017/s1431927617005918
Multiscale Expression Of Apatite Dissolution
Conde, A. (2019) · ScholarWorks -A service of University of Vermont Libraries (University of Vermont)
Lu, X. (2018) · University of North Texas Digital Library (University of North Texas) · doi:10.12794/metadc1404587
Preventing Glass Alteration in Museum Objects using ALD Deposited Amorphous Alumina CoatingsPreprint
Hiebert, M. E., Weaver, J. L., Lam, T. F., Little, N. C., Hyde, E., Vicenzi, E. P., & Phaneuf, R. J. (2020) · doi:10.21203/rs.3.rs-71473/v1
Zhong, Y., Huang, K., Zou, Q., Ye, L., & Yefang, L. (2022) · SSRN Electronic Journal · doi:10.2139/ssrn.4103100
Valbi, V. (2020) · theses.fr (ABES) · doi:10.70675/0156e3c1z9c35z4622z89d9zcb489504847d · Cited by 5
Stock, D., Linke, R., Heft, A., & Grünler, B. (2024) · The European Physical Journal B · doi:10.1140/epjb/s10051-024-00754-9
Reliability of Materials and Components for Solid Oxide Fuel Cells
Trejo, R. M., USDOE Office of Fossil Energy (FE), Shyam, A., Guo, Q., McClurg, D., Kirkham, M., Lance, M. J., Cakmak, E., & Lara‐Curzio, E. (2024) · OSTI OAI (U.S. Department of Energy Office of Scientific and Technical Information) · doi:10.2172/2429858
Effect of a cement-bentonite grout on AVM glass alteration and C-steel corrosion at nanometer scale
Carrière, C., Delanoë, A., Gin, S., Gardès, E., Monnet, I., Neff, D., Foy, E., Martin, C., Tocino, F. Y., Michau, N., et al. (2025) · Corrosion Engineering Science and Technology The International Journal of Corrosion Processes and Corrosion Control · doi:10.1177/1478422x241310412
“12,16 The self-reorganisation of such a gel leads to its densi fi cation, becoming a diffusion barrier which can limit the exchange of dissolved species at the interface.”
The effect of magnesia and lime on the durability of synthetic basaltic glasses
Mansfield, J. T., Tang, C., Thorpe, C. L., Corkhill, C. L., Harrison, M. T., & Hand, R. J. (2025) · Journal of Non-Crystalline Solids · doi:10.1016/j.jnoncrysol.2025.123500
Rimsza, J. (2016) · University of North Texas Digital Library (University of North Texas) · doi:10.12794/metadc849660
Zhou, B., Ma, Q., Li, Z., Zhang, Z., & Li, N. (2024) · Figshare · doi:10.6084/m9.figshare.26599307
Boron isotope tracers of diffusion during glass dissolution
Goût, T. L., Guo, R., Misra, S., Tipper, E. T., Bohlin, M. S., Hu, Y., & Farnan, I. (2025) · Environmental and Biogeochemical Processes · doi:10.48130/ebp-0025-0004
Wang, R., Ding, L., Liu, L., Ma, X., Ma, J., Zhang, J., Su, Y., Yi, K., Yu, J., Shan, Z., et al. (2026) · Journal of the American Ceramic Society · doi:10.1111/jace.70526
“…surface is not simply depleted or leached out of glass surface after corrosion for 192 h (Figure 2C) as the previous investigations reported; 7,9,14,16,17 instead, it shows a Na + -ion concentration gradient in the alteration layer where the Na ion concentration at the corrosion interface is…”
Chemical durability of chemically strengthened float silicate glasses
Kaur, D., & Sglavo, V. M. (2026) · Journal of Materials Science · doi:10.1007/s10853-026-12332-8
Pollet-Villard, M. (2016) · theses.fr (ABES) · doi:10.70675/6ae49837z0fc5z41d2za5fezd0819f15a563
“Chemical weathering spontaneously affects most solids including building and industrial materials (e.g. Nicoleau et al. 2013; King et al. 2014; Hellmann et al. 2015), biomaterials (e.”
BackgroundApport des verres basaltiques à la validation du modèle GRAAL sur le très long terme
Ducasse, T. (2017) · theses.fr (ABES) · doi:10.70675/2c1713f9zbf02z465azb041zea0a5e8426d5 · Cited by 2
Géochimie en milieu nanoporeux : application aux verres nucléaires
Collin, M. (2018) · theses.fr (ABES) · doi:10.70675/a031ccb3ze083z42e5z8426zf9c4a193eae6 · Cited by 6
Reactive transport modeling in fractured media of nuclear glass for industrial application
Repina, M. (2019) · theses.fr (ABES) · doi:10.70675/6eb1ce0dzc88fz4d9bz8efazde05c86a02ee
“2000) or precipitation (Jercinovic et al. 1990; Geisler et al. 2010; Hellmann et al. 2015) from elements released in solution by the hydrolysis of a glass network.”
BackgroundBouissonnié, A. (2019) · theses.fr (ABES) · doi:10.70675/0fc8aa0bz9643z45e6z85b5z0e57081b316e · Cited by 1
Metadata
- Authors
- Hellmann, R., Cotte, S., Cadel, E., Malladi, S., Karlsson, L. S., Lozano-Perez, S., Cabié, M., & Seyeux, A.
- Affiliations
- Centre National de la Recherche Scientifique (FR)
- Delft University of Technology (NL)
- Aix-Marseille Université (FR)
- Corresponding author
- Hellmann, Roland
- Venue
- Nature Materials
- Published
- 2015-01-05
- Volume
- 14
- Issue
- 3
- Pages
- 307-311
- ISSN
- 1476-1122 (ISSN-L)
- 1476-4660
- OpenAlex
- W2054790370
- Semantic Scholar
- 00f2749480774a8526d45e81d2bc514fca233140
- Cited by
- 315
- References
- 31
- Citations by year
- 2026: 21 · 2025: 29 · 2024: 24 · 2023: 19 · 2022: 25 · 2021: 35 · 2020: 36 · 2019: 29 · 2018: 35 · 2017: 24 · 2016: 23 · 2015: 14
- FWCI
- 25.44
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.springer.com/tdm (tdm)
- www.springer.com/tdm (vor)
- Locations
- Nature Materials (publishedVersion)
- PubMed (publishedVersion)
- HAL (submittedVersion)
- Funders
- European Commission
- Centre National de la Recherche Scientifique
- Agence Nationale pour la Gestion des Déchets Radioactifs
- Topics
- Physical Sciences › Materials Science › Ceramics and Composites › Glass properties and applications
- Social Sciences › Arts and Humanities › Archeology (arts and humanities) › Cultural Heritage Materials Analysis
- Physical Sciences › Earth and Planetary Sciences › Geochemistry and Petrology › Geochemistry and Elemental Analysis
- Keywords
- glass-water interface, mineral weathering
- MeSH terms
- Corrosion, Glass, Materials Testing, Particle Size, Solvents, Surface Properties, Water, Silicates, Nanostructures
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.