Abstract
The effect of feature size, geometry, and roughness on the settlement of zoospores of the ship fouling alga Ulva was evaluated using engineered microtopographies in polydimethylsiloxane elastomer. The topographies studied were designed at a feature spacing of 2 microm and all significantly reduced spore settlement compared to a smooth surface. An indirect correlation between spore settlement and a newly described engineered roughness index (ERI) was identified. ERI is a dimensionless ratio based on Wenzel's roughness factor, depressed surface fraction, and the degree of freedom of spore movement. Uniform surfaces of either 2 mum diameter circular pillars (ERI=5.0) or 2 microm wide ridges (ERI=6.1) reduced settlement by 36% and 31%, respectively. A novel multi-feature topography consisting of 2 mum diameter circular pillars and 10 microm equilateral triangles (ERI=8.7) reduced spore settlement by 58%. The largest reduction in spore settlement, 77%, was obtained with the Sharklet AF topography (ERI=9.5).
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Wettability of porous surfaces
Cassie, A. B. D., & Baxter, S. (1944) · Transactions of the Faraday Society · doi:10.1039/tf9444000546 · Cited by 13,807
RESISTANCE OF SOLID SURFACES TO WETTING BY WATER
Wenzel, R. N. (1936) · Industrial & Engineering Chemistry · doi:10.1021/ie50320a024 · Cited by 13,316
Bico, J., Thiele, U., & Quéré, D. (2002) · Colloids and Surfaces A: Physicochemical and Engineering Aspects · doi:10.1016/s0927-7757(02)00061-4 · Cited by 1,390
Recent developments in superhydrophobic surfaces and their relevance to marine fouling: a review
Genzer, J., & Efimenko, K. (2006) · Biofouling · doi:10.1080/08927010600980223 · Cited by 1,134
Bico, J., Marzolin, C., & Quéré, D. (1999) · Europhysics Letters (EPL) · doi:10.1209/epl/i1999-00548-y · Cited by 953
Bico, J., Tordeux, C., & Quéré, D. (2001) · Europhysics Letters (EPL) · doi:10.1209/epl/i2001-00402-x · Cited by 650
Quéré, D. (2002) · Physica A: Statistical Mechanics and its Applications · doi:10.1016/s0378-4371(02)01033-6 · Cited by 533
Engineered antifouling microtopographies – correlating wettability with cell attachment
Carman, M. L., Estes, T. G., Feinberg, A. W., Schumacher, J. F., Wilkerson, W., Wilson, L. H., Callow, M. E., Callow, J. A., & Brennan, A. B. (2006) · Biofouling · doi:10.1080/08927010500484854 · Cited by 478
Self-citationEngineering Shark skin and other solutions
Ball, P. (1999) · Nature · doi:10.1038/22883 · Cited by 388
Cell-to-Cell Communication Across the Prokaryote-Eukaryote Boundary
Joint, I., Tait, K., Callow, M. E., Callow, J. A., Milton, D., Williams, P., & Cámara, M. (2002) · Science · doi:10.1126/science.1077075 · Cited by 298
Self-citationMicrotopographic Cues for Settlement of Zoospores of the Green Fouling Alga Enteromorpha
Callow, M. E., Jennings, A. R., Brennan, A. B., Seegert, C. E., Gibson, A., Wilson, L., Feinberg, A., Baney, R., & Callow, J. A. (2002) · Biofouling · doi:10.1080/08927010290014908 · Cited by 297
Self-citationFinlay, J. A. (2002) · Integrative and Comparative Biology · doi:10.1093/icb/42.6.1116 · Cited by 283
Self-citationSuper-hydrophobicity fundamentals: implications to biofouling prevention
Marmur, A. (2006) · Biofouling · doi:10.1080/08927010600562328 · Cited by 226
Chaudhury, M. K., Finlay, J. A., Chung, J. Y., Callow, M. E., & Callow, J. A. (2005) · Biofouling · doi:10.1080/08927010500044377 · Cited by 212
Self-citationHoipkemeier-Wilson, L., Schumacher, J. F., Carman, M. L., Gibson, A. L., Feinberg, A. W., Callow, M. E., Finlay, J. A., Callow, J. A., & Brennan, A. B. (2004) · Biofouling · doi:10.1080/08927010410001662689 · Cited by 200
Self-citationSmith, A. M., & Callow, J. A. (2006) · Springer eBooks · doi:10.1007/978-3-540-31049-5 · Cited by 144
Self-citationWheeler, G. L., Tait, K., Taylor, A. R., Brownlee, C., & Joint, I. R. (2005) · Plant Cell & Environment · doi:10.1111/j.1365-3040.2005.01440.x · Cited by 121
Surface elastic modulus of barnacle adhesive and release characteristics from silicone surfaces
Sun, Y., Guo, S., Walker, G. C., Kavanagh, C. J., & Swain, G. W. (2004) · Biofouling · doi:10.1080/08927010400026383 · Cited by 116
Cited by
Banerjee, I., Pangule, R. C., & Kane, R. S. (2011) · Advanced Materials · doi:10.1002/adma.201001215 · Cited by 2,749
Trends in the development of environmentally friendly fouling-resistant marine coatings
Callow, J. A., & Callow, M. E. (2011) · Nature Communications · doi:10.1038/ncomms1251 · Cited by 1,288
Self-citationFouling Release Coatings: A Nontoxic Alternative to Biocidal Antifouling Coatings
Lejars, M., Margaillan, A., & Bressy, C. (2012) · Chemical Reviews · doi:10.1021/cr200350v · Cited by 1,268
Natural Bactericidal Surfaces: Mechanical Rupture of Pseudomonas aeruginosa Cells by Cicada Wings
Ivanova, E. P., Hasan, J., Webb, H. K., Truong, V. K., Watson, G. S., Watson, J. A., Baulin, V. A., Pogodin, S., Wang, J. Y., Tobin, M. J., et al. (2012) · Small · doi:10.1002/smll.201200528 · Cited by 1,019
Advances in polymers for anti-biofouling surfaces
Krishnan, S., Weinman, C. J., & Ober, C. K. (2008) · Journal of Materials Chemistry · doi:10.1039/b801491d · Cited by 824
Metadata
- Authors
- Schumacher, J. F., Carman, M. L., Estes, T. G., Feinberg, A. W., Wilson, L. H., Callow, M. E., Callow, J. A., Finlay, J. A., & Brennan, A. B.
- Venue
- Biofouling
- Publisher
- Informa UK Limited
- Published
- 2007-01
- Volume
- 23
- Issue
- 1
- Pages
- 55-62
- ISSN
- 0892-7014 (ISSN-L)
- 1029-2454
- OpenAlex
- W2068298719
- Cited by
- 453
- References
- 18
- FWCI
- 56.49
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.