Recent progress in ultra-low formaldehyde emitting adhesive systems and formaldehyde scavengers in wood-based panels: a review
The DOI matches its Crossref record; 91 of the 91 references it cites were found in a registry or an index.
Abstract
Traditional wood-based panels are produced with synthetic, formaldehyde-based adhesives, commonly made from fossil-derived constituents, such as urea, phenol, melamine, etc. Along with their numerous advantages, such as chemical versatility, high reactivity and excellent adhesive performance, these adhesives are characterized by certain problems, connected with the hazardous volatile organic compounds (VOCs), mostly free formaldehyde in the adhesives and the formaldehyde emission from the finished wood composites, which is carcinogenic to humans and harmful to the environment. The growing environmental concerns and stringent legislative requirements to the formaldehyde emission from wood-based panels have posed new challenges to researchers and industrial practice, related to the development of sustainable, eco-friendly wood-based panels with close-to-zero formaldehyde emission. The most common methods to reduce the formaldehyde emission from wood-based panels have been to decrease the free formaldehyde in the adhesive by modifying the adhesive (like lowering the molar ratio of formaldehyde to urea in UF resin) or by using formaldehyde scavengers, one group of scavengers being for adhesives by mixing or reacting and the second one scavengers for wood-based panels as post-treatments. Another way is to use alternative bio-based adhesives, however, there are still substantial challenges for the complete replacement of formaldehyde-based adhesives with bio-based adhesives, mainly because of their relatively low bonding strength, poor water resistance, etc. This article presents a review and analysis of the current state of research in the field of low formaldehyde emission wood adhesives and formaldehyde scavengers for manufacturing low-toxic, eco-friendly wood composites.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Silk grafting with methacrylic monomers: Process optimization and comparison
Ferrero, F., Periolatto, M., & Luraschi, M. (2006) · Journal of Applied Polymer Science · doi:10.1002/app.25555 · Cited by 692
Urea–formaldehyde (UF) adhesive resins for wood
Dunky, M. (1998) · International Journal of Adhesion and Adhesives · doi:10.1016/s0143-7496(97)00054-7 · Cited by 479 · cited 7×
“are colourless and easy to handle (Dunky 1998).”
BackgroundInfluentialMelamine formaldehyde: curing studies and reaction mechanism
Merline, D. J., Vukusic, S., & Abdala, A. A. (2012) · Polymer Journal · doi:10.1038/pj.2012.162 · Cited by 479
Handbook of Adhesive Technology, Revised and Expanded
(2003) · CRC Press eBooks · doi:10.1201/9780203912225 · Cited by 439 · cited 8×
“The reaction of melamine (a 1,3,5 amino-substituted triazine derivative) with formaldehyde in pure MF resins is usually performed in an aqueous solution, and it is slightly like the reaction of urea and formaldehyde in UF resins (Pizzi 2003).”
BackgroundInfluentialPreparation of activated carbons from coffee residue for the adsorption of formaldehyde
Boonamnuayvitaya, V., Sae-ung, S., & Tanthapanichakoon, W. (2005) · Separation and Purification Technology · doi:10.1016/j.seppur.2004.07.007 · Cited by 306 · cited 1×
“Many recent studies reported effective formaldehyde adsorption by activated carbons (Rong et al. 2003; Boonamnuayvitaya et al. 2005; Song et al. 2007) and other carbonbased nanomaterials (Kumar et al. 2013b; Kumar et al. 2017; Suresh and Bandosz 2018).”
BackgroundFormaldehyde sources, formaldehyde concentrations and air exchange rates in European housings
Salthammer, T. (2019) · Building and Environment · doi:10.1016/j.buildenv.2018.12.042 · Cited by 245 · cited 2×
“Global trends have shown strictly reductions in allowable formaldehyde emissions from wood-based panels, targeting lower formaldehyde released from hydrolytically unstable formaldehyde-based wood adhesives (Salthammer 2019).”
BackgroundAdhesive systems used in the European particleboard, MDF and OSB industries
Mantanis, G. I., Athanassiadou, E. T., Barbu, M. C., & Wijnendaele, K. (2018) · Wood Material Science & Engineering · doi:10.1080/17480272.2017.1396622 · Cited by 216
Wood Composites and Their Polymer Binders
Pizzi, A., Papadopoulos, A. N., & Policardi, F. (2020) · Polymers · doi:10.3390/polym12051115 · Cited by 208
Self-citationResearch status, industrial application demand and prospects of phenolic resin
Xu, Y., Guo, L., Zhang, H., Zhai, H., & Ren, H. (2019) · RSC Advances · doi:10.1039/c9ra06487g · Cited by 206 · cited 8×
“Scheme of addition-condensation reaction of phenol-formaldehyde resins (adapted from Christiansen and Gollob (1985) Xu et al. (2019) Park and Riedl (2000)).”
BackgroundMethodInfluentialVolatile organic compounds and formaldehyde in nature, wood and wood based panels
Roffael, E. (2006) · European Journal of Wood and Wood Products · doi:10.1007/s00107-005-0061-0 · Cited by 193 · cited 4×
“…and relative humidity), inherent wood-based panels properties, air exchange rate and air velocity at the emitting surface, loading factor (ratio of emitting surface to room dimensions), as well as the availability of reactive materials, removing formaldehyde (Roffael 2006; Kumar and Pizzi 2019a).”
BackgroundInfluentialKim, S. (2009) · Bioresource Technology · doi:10.1016/j.biortech.2008.06.062 · Cited by 181 · cited 7×
“Porous materials like pozzolan (Kim 2009b), charcoal (Eom et al. 2006; Kim et al. 2006; Kowaluk et al. 2016), zeolite (Camlibel 2020), sepiolite Xu et al. 2019), and calcite mineral (Camlibel 2021), due to rough and irregular surface with porous form, provide some scavenging ability.”
BackgroundMethodInfluentialHow mole ratio of UF resin affects formaldehyde emission and other properties: a literature critique
Myers, G. E. (1984) · Forest Products Journal · Cited by 171
Removal of formaldehyde on carbon -based materials: A review of the recent approaches and findings
Suresh, S., & Bandosz, T. J. (2018) · Carbon · doi:10.1016/j.carbon.2018.05.023 · Cited by 169 · cited 1×
“Many recent studies reported effective formaldehyde adsorption by activated carbons (Rong et al. 2003; Boonamnuayvitaya et al. 2005; Song et al. 2007) and other carbonbased nanomaterials (Kumar et al. 2013b; Kumar et al. 2017; Suresh and Bandosz 2018).”
BackgroundBoran, S., Usta, M., & Gümüşkaya, E. (2011) · International Journal of Adhesion and Adhesives · doi:10.1016/j.ijadhadh.2011.06.011 · Cited by 151 · cited 6×
“…et al. 2013) or other compounds such as starch derivatives, charcoal, pozzolan, zeolites, and urea (Basta et al. 2006;Park et al. 2008; Kim 2009b; Kmec et al. 2010; Boran et al. 2011; Costa et al. 2013a) is an environmentally friendly way to reduce formaldehyde emission from wood-based panels.”
BackgroundMethodInfluentialPark, B., & Jeong, H.-W. (2011) · International Journal of Adhesion and Adhesives · doi:10.1016/j.ijadhadh.2011.05.001 · Cited by 150
Synthesis, characterization and thermal analysis of urea–formaldehyde/nanoSiO2 resins
Roumeli, E., Papadopoulou, E., Pavlidou, E., Vourlias, G., Bikiaris, D. Ν., Paraskevopoulos, K. M., & Chrissafis, K. (2011) · Thermochimica Acta · doi:10.1016/j.tca.2011.10.007 · Cited by 147 · cited 1×
“Al2O3 and SiO2 nanoparticles have a very strong absorbability, and they can react with the active group of the UF resin and absorb free formaldehyde (de Cademartori et al. 2019; Dudkin et al. 2006, Lin et al. 2006, Roumeli et al. 2012).”
BackgroundUtilization of pine (Pinus pinea L.) cone in manufacture of wood based composite
Ayrılmış, N., Büyüksarı, Ü., Avcı, E., & Koç, E. (2009) · Forest Ecology and Management · doi:10.1016/j.foreco.2009.09.043 · Cited by 135 · cited 2×
“The addition of pine cone flour (Ayrilmis et al. 2009; Buyuksari et al. 2010), rice husk flour and wheat flour (Kim et al. 2006), hemp flour (Kawalerczyk et al. 2020), soy flour, and wollastonite (Taghiyari et al. 2020a), chestnut shell powder (Ayrilmis and Kaymakci 2012), chestnut bur (Liang et…”
BackgroundScavengers for achieving zero formaldehyde emission of wood-based panels
Costa, N. A., Pereira, J., Ferra, J. M. M., Cruz, P., Martins, J. M., Magalhães, F. D., Mendes, A. M. M., & Carvalho, L. (2013) · Wood Science and Technology · doi:10.1007/s00226-013-0573-4 · Cited by 131 · cited 8×
“…et al. 2013) or other compounds such as starch derivatives, charcoal, pozzolan, zeolites, and urea (Basta et al. 2006;Park et al. 2008; Kim 2009b; Kmec et al. 2010; Boran et al. 2011; Costa et al. 2013a) is an environmentally friendly way to reduce formaldehyde emission from wood-based panels.”
BackgroundMethodInfluentialRemoval of formaldehyde at low concentration using various activated carbon fibers
Song, Y. L., Qiao, W., Yoon, S., Mochida, I., Guo, Q., & Liu, L. (2007) · Journal of Applied Polymer Science · doi:10.1002/app.26368 · Cited by 122 · cited 1×
“Many recent studies reported effective formaldehyde adsorption by activated carbons (Rong et al. 2003; Boonamnuayvitaya et al. 2005; Song et al. 2007) and other carbonbased nanomaterials (Kumar et al. 2013b; Kumar et al. 2017; Suresh and Bandosz 2018).”
BackgroundPirayesh, H., Khanjanzadeh, H., & Salari, A. (2012) · Composites Part B Engineering · doi:10.1016/j.compositesb.2012.05.008 · Cited by 120
Thermal behavior of modified urea–formaldehyde resins
Samaržija‐Jovanović, S., Jovanović, V., Konstantinovic, S. S., Marković, G., & Marinović-Cincović, M. T. (2010) · Journal of Thermal Analysis and Calorimetry · doi:10.1007/s10973-010-1143-8 · Cited by 118
Theory and Practice of the Preparation of Low Formaldehyde Emission UF Adhesives
Pizzi, A., Lipschitz, L., & Valenzuela, J. (1994) · Holzforschung · doi:10.1515/hfsg.1994.48.3.254 · Cited by 118 · cited 1×
“Since urea has four reactive sites, there is a possibility to use higher initial F/U mole ratios up to 4.0; but no results have been reported on the presence of tetra-hydroxymethyl urea (Pizzi et al. 1994).”
BackgroundInfluentialSelf-citationThermal behaviour of urea-formaldehyde resins during curing
Siimer, K., Kaljuvee, T., & Christjanson, P. (2003) · Journal of Thermal Analysis and Calorimetry · doi:10.1023/a:1024590019244 · Cited by 116 · cited 1×
“…the resin synthesis (Smythe 1952, Smythe 1951), structure (Marvel et al. 1946), kinetic studies (Crowe and Lynch 1948), morphology (Nuryawan et al. 2016), curing reaction (Dongbin et al. 2006), thermal and hydrolytic stability (Siimer et al. 2003, Abdullah and Park 2009, Park and Jeong 2011b).”
BackgroundRowell, R. M. (2012) · CRC Press eBooks · doi:10.1201/b12487-13 · Cited by 110 · cited 1×
“…of approximately 11 million tons worldwide (Kumar and Pizzi 2019a), is due to their high reactivity, excellent adhesion properties, solubility in water, rather low curing temperatures, short press time, ease of handling, and relatively low cost (Dunky 2003, Frihart 2012, Mantanis et al. 2018).”
BackgroundInfluence of nanoclay on urea‐formaldehyde resins for wood adhesives and its model
Lei, H., Du, G., Pizzi, A., & Celzard, A. (2008) · Journal of Applied Polymer Science · doi:10.1002/app.28359 · Cited by 109 · cited 1×
“In several studies, UF adhesive has been modified with nanoaluminum oxide (de Cademartori et al. 2019; Dudkin et al. 2006), nanosilica (Lei et al. 2008; Lin et al. 2005a, 2005b; Roumeli et al. 2010; Samarzija-Jovanovic et al. 2011), and nanocrystalline cellulose (Zhang et al. 2011), to decrease FEs.”
BackgroundSelf-citationPreparation and characterisation of bioplastics made from cottonseed protein
Yue, H., Cui, Y., Shuttleworth, P. S., & Clark, J. H. (2012) · Green Chemistry · doi:10.1039/c2gc35509d · Cited by 104 · cited 2×
“The amine groups and side chains of amino acids of proteins were able to cross-link with formaldehyde to reduce formaldehyde release (Yue et al. 2012).”
BackgroundEco-Friendly, High-Density Fiberboards Bonded with Urea-Formaldehyde and Ammonium Lignosulfonate
Antov, P., Savov, V., Krišťák, Ľ., Réh, R., & Mantanis, G. I. (2021) · Polymers · doi:10.3390/polym13020220 · Cited by 104 · cited 1×
“…al. 2006; Moubarik et al. 2010; Boran et al. 2012; Gangi et al. 2013, Pizzi et al. (2020); Selakjani et al. 2021) to the UF resin or wood furnish (Antov et al. 2021a, 2021b, 2021c; Bekhta et al. 2021a; Bekhta et al. 2021b; Lorenz et al. 1999; Kim 2009a; Hematabadi et al. 2012; Gangi et al. 2013;…”
BackgroundSelf-citationGindl‐Altmutter, W., Dessipri, E., & Wimmer, R. (2002) · Holzforschung · doi:10.1515/hf.2002.017 · Cited by 103 · cited 1×
“In addition to wood adhesives, MF resins have now found applications in flooring and decorative laminates, moulding compounds, and coatings (Gindl et al. 2002, Merline et al. 2013).”
BackgroundImam, S. H., Mao, L., Chen, L., & Greene, R. V. (1999) · Starch - Stärke · doi:10.1002/(sici)1521-379x(199906)51:6<225::aid-star225>3.0.co;2-f · Cited by 98 · cited 2×
“annual renewability, abundance, comparatively low cost, and eco-friendliness (Imam et al. 1999).”
BackgroundBüyüksarı, Ü., Ayrılmış, N., Avcı, E., & Koç, E. (2009) · Bioresource Technology · doi:10.1016/j.biortech.2009.08.038 · Cited by 95 · cited 2×
“The addition of pine cone flour (Ayrilmis et al. 2009; Buyuksari et al. 2010), rice husk flour and wheat flour (Kim et al. 2006), hemp flour (Kawalerczyk et al. 2020), soy flour, and wollastonite (Taghiyari et al. 2020a), chestnut shell powder (Ayrilmis and Kaymakci 2012), chestnut bur (Liang et…”
BackgroundSynthesis and Thermal Degradation Studies of Melamine Formaldehyde Resins
Ullah, S., Bustam, M. A., Nadeem, M., Naz, M. Y., Tan, W. L., & Shariff, A. M. (2014) · The Scientific World JOURNAL · doi:10.1155/2014/940502 · Cited by 95
Réh, R., Krišťák, Ľ., Sedliačik, J., Bekhta, P., Božíková, M., Kunecová, D., Vozárová, V., Tudor, E. M., Antov, P., & Savov, V. (2021) · Polymers · doi:10.3390/polym13040511 · Cited by 95 · cited 3×
“…exhibited formaldehyde scavenging properties when added to the adhesive mixtures for bonding plywood (Aydin et al. 2017; Kawalerczyk et al. 2019; Réh et al. 2021; Ružiak et al. 2017; Wang et al. 2012b), particleboard (Medved et al. 2019; Nemli and Colakoğlu 2005; Sari et al. 2012), MDF (Boran…”
BackgroundSelf-citationPark, B., Kim, Y. S., Singh, A. P., & Lim, K. P. (2003) · Journal of Applied Polymer Science · doi:10.1002/app.12115 · Cited by 87 · cited 1×
“However, most of the low F/U mole ratio UF resins tend to have longer gelation time, slow curing, and low cross-linking density (Park and Kim 2008, Park et al. 2003), resulting in a poor strength at the expense of lower formaldehyde emission (Myers and Koutsky 1990, Myers 1986a).”
BackgroundFormaldehyde Liberation and Cure Behavior of Urea-Formaldehyde Resins
Myers, G. E., & Koutsky, J. A. (1990) · Holzforschung · doi:10.1515/hfsg.1990.44.2.117 · Cited by 86 · cited 2×
“…2006, Park et al. 2008, Gonçalves et al. 2019) 90–92; 1–2 80–90; 3–4 200–300 8.5–9.0 12.0–13.0 8.0–8.2 (Liang et al. 2018) 3 90–92; 1–2 80–90; 3–4 200–300 7.8–8.2 4.6–6.0 8.0–8.2 (Myers and Koutsky 1990, Lubis and Park 2020a, Chuang and Gary 1992) 42 2.0 1.1–1.3 2 90–92; 1 80–85; 3–4 200–250…”
BackgroundInfluentialZhang, H., Zhang, J., Song, S., Wu, G., & Pu, J. (2011) · BioResources · doi:10.15376/biores.6.4.4430-4438 · Cited by 82 · cited 2×
“A work by Zhang et al. (2011) presented significant improvements in bond strength (an increase by 23.6”
BackgroundInfluentialResearch Progress on Formaldehyde Emission of Wood-Based Panel
Zhang, J., Song, F., Tao, J., Zhang, Z., & Shi, S. Q. (2018) · International Journal of Polymer Science · doi:10.1155/2018/9349721 · Cited by 82 · cited 1×
“The environmental conditions under which the woodbased panels are tested, i.e. relative humidity and temperature, are defined as the main exogenic factors (Sundin et al. 1992; Roffael 2006, Zhang et al. 2018).”
BackgroundAntov, P., Savov, V., Trichkov, N., Krišťák, Ľ., Réh, R., Papadopoulos, A. N., Taghiyari, H. R., Pizzi, A., Kunecová, D., & Pachikova, M. (2021) · Polymers · doi:10.3390/polym13162775 · Cited by 80 · cited 1×
“…al. 2006; Moubarik et al. 2010; Boran et al. 2012; Gangi et al. 2013, Pizzi et al. (2020); Selakjani et al. 2021) to the UF resin or wood furnish (Antov et al. 2021a, 2021b, 2021c; Bekhta et al. 2021a; Bekhta et al. 2021b; Lorenz et al. 1999; Kim 2009a; Hematabadi et al. 2012; Gangi et al. 2013;…”
BackgroundSelf-citationCosta, N. A., Pereira, J., Martins, J. M., Ferra, J. M. M., Cruz, P., Magalhães, F. D., Mendes, A. M. M., & Carvalho, L. (2011) · International Journal of Adhesion and Adhesives · doi:10.1016/j.ijadhadh.2011.11.003 · Cited by 80 · cited 1×
“Promising results in reducing the formaldehyde emission from wood-based panels were obtained by adding sodium sulfite (Wang et al. 2012a), sodium metabisulfite and ammonium bisulfite (Costa et al. 2012, 2013a, 2013b, 2014) to the resin.”
MethodAyrılmış, N., Lee, Y., Kwon, J. H., Han, T.-H., & Kim, H. (2015) · Building and Environment · doi:10.1016/j.buildenv.2015.12.009 · Cited by 80 · cited 1×
“…to manufacture furniture products and construction materials; but most of those products emit formaldehyde from formaldehyde-based adhesives which are one the most negative aspects of wood-based panels particularly in indoor environments (Park et al. 2016, Salthammer 2019, Ayrilmis et al. 2016).”
BackgroundBekhta, P., Sedliačik, J., Нощенко, Г. В., Kačík, F., & Bekhta, N. (2021) · European Journal of Wood and Wood Products · doi:10.1007/s00107-020-01632-8 · Cited by 78 · cited 2×
“…Boran et al. 2012; Gangi et al. 2013, Pizzi et al. (2020); Selakjani et al. 2021) to the UF resin or wood furnish (Antov et al. 2021a, 2021b, 2021c; Bekhta et al. 2021a; Bekhta et al. 2021b; Lorenz et al. 1999; Kim 2009a; Hematabadi et al. 2012; Gangi et al. 2013; Moubarik et al. 2013) or other…”
BackgroundSelf-citationFilho, R. M. D. B., Mendes, L. M., Novack, K. M., Aprelini, L. O., & Botaro, V. R. (2010) · Industrial Crops and Products · doi:10.1016/j.indcrop.2010.11.007 · Cited by 76 · cited 8×
“Reference UF F/U: 0.9–1.0 58–61 200–300* 180–250 0.2–0.4 (Hong et al. 2020, Lubis et al. 2020, Park et al. 2006, Park et al. 2008) F/U: 1.2–1.6 52–56 50–165* 250–575 0.41–0.75 MF F/M: 1.0–2.0 50–65 50–150* 100–500 0.2–0.3 (Dunky 2003, 2004, Merline et al. 2013, Monteiro et al. 2011) MUF F/(M+U): 0.7–1.0 57–65 60–200*…”
InfluentialVolatile Organic Compounds (VOCs) Emitted from Coated Furniture Units
Ülker, Ö. C., Ülker, O., & Hızıroǧlu, S. (2021) · Coatings · doi:10.3390/coatings11070806 · Cited by 75
de Cademartori, P. H. G., Artner, M. A., de Freitas, R. A., & Magalhães, W. L. E. (2019) · Composites Part B Engineering · doi:10.1016/j.compositesb.2019.107281 · Cited by 75 · cited 3×
“Al2O3 and SiO2 nanoparticles have a very strong absorbability, and they can react with the active group of the UF resin and absorb free formaldehyde (de Cademartori et al. 2019; Dudkin et al. 2006, Lin et al. 2006, Roumeli et al. 2012).”
BackgroundHydrolytic Removal of Cured Urea–Formaldehyde Resins in Medium-Density Fiberboard for Recycling
Lubis, M. A. R., Hong, M.-K., & Park, B.-D. (2018) · Journal of Wood Chemistry and Technology · doi:10.1080/02773813.2017.1316741 · Cited by 71 · cited 1×
“The hydrolysis reaction depends onmany factors, such as the molar ratio of the monomers, chemical structure, degree of crystallinity, degree of cross-linking, and hydrolysis conditions (Lubis and Park 2018, Lubis et al. 2018).”
BackgroundSelf-citationEco-Friendly Fiberboard Panels from Recycled Fibers Bonded with Calcium Lignosulfonate
Antov, P., Krišťák, Ľ., Réh, R., Savov, V., & Papadopoulos, A. N. (2021) · Polymers · doi:10.3390/polym13040639 · Cited by 71 · cited 1×
“…al. 2006; Moubarik et al. 2010; Boran et al. 2012; Gangi et al. 2013, Pizzi et al. (2020); Selakjani et al. 2021) to the UF resin or wood furnish (Antov et al. 2021a, 2021b, 2021c; Bekhta et al. 2021a; Bekhta et al. 2021b; Lorenz et al. 1999; Kim 2009a; Hematabadi et al. 2012; Gangi et al. 2013;…”
BackgroundSelf-citationKim, S., Kim, H., Kim, H., & Lee, H. H. (2006) · Macromolecular Materials and Engineering · doi:10.1002/mame.200600213 · Cited by 71 · cited 16×
“The use of bio-based scavengers such as tannins, lignin, starch, wheat flour, rice husk flour added to the resin (Cameron and Pizzi 1985, Eom et al. 2006; Kim et al. 2006; Moubarik et al. 2010; Gangi et al. 2013, Selakjani et al. 2021) or wood furnish (Lorenz et al.”
BackgroundMethodInfluentialInvestigation of melamine-formaldehyde cure by Fourier transform Raman spectroscopy
Scheepers, M. L., Gelan, J. M. J. V., Carleer, R., Adriaensens, P., Vanderzande, D. J. M., Kip, B. J., & Brandts, P. M. (1993) · Vibrational Spectroscopy · doi:10.1016/0924-2031(93)87022-l · Cited by 68 · cited 1×
“…30 95–100; 30 75–100 9.0–10.0 9.0–10.0 9.0–10.0 (Pizzi 2003) 2.0–6.0 – – 95–100; 30 95–100; 30 75–100 8.5–9.0 8.5–9.0 8.5–9.0 (Merline et al. 2013, Tomita and Ono 1979, Scheepers et al. 1993) MUF 1.5 1.0–1.6 2 90–92; 1 90–92; 1 75–100 8.2–8.5 6.5–7.0 9.0–9.2 (Jeong et al. 2019, Lubis et al.…”
InfluentialKim, S. (2008) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2008.11.008 · Cited by 67 · cited 7×
“Porous materials like pozzolan (Kim 2009b), charcoal (Eom et al. 2006; Kim et al. 2006; Kowaluk et al. 2016), zeolite (Camlibel 2020), sepiolite Xu et al. 2019), and calcite mineral (Camlibel 2021), due to rough and irregular surface with porous form, provide some scavenging ability.”
BackgroundMethodInfluentialSteinhof, O., Kibrik, É. J., Scherr, G., & Hasse, H. (2014) · Magnetic Resonance in Chemistry · doi:10.1002/mrc.4044 · Cited by 66 · cited 3×
“Recent studies prove that these intermediates exist in UF reaction mixtures (Steinhof et al. 2014, Liang et al. 2018).”
BackgroundMethodInfluentialChuang, I.-S., & Maciel, G. E. (1992) · Macromolecules · doi:10.1021/ma00038a029 · Cited by 64 · cited 4×
“However, most of the low F/U mole ratio UF resins tend to have longer gelation time, slow curing, and low cross-linking density (Park and Kim 2008, Park et al. 2003), resulting in a poor strength at the expense of lower formaldehyde emission (Myers and Koutsky 1990, Myers 1986a).”
InfluentialAmmonium Lignosulfonate Adhesives for Particleboards with pMDI and Furfuryl Alcohol as Crosslinkers
Hemmilä, V., Αδαμόπουλος, Σ., Hosseinpourpia, R., & Ahmed, S. A. (2019) · Polymers · doi:10.3390/polym11101633 · Cited by 63 · cited 1×
“The most acceptable and effective procedure of reducing formaldehyde emission in wood-based panels is using formaldehyde scavengers, often referred to as formaldehyde catchers (Bertaud et al. 2012; Mantanis et al. 2018; Hemmilä et al. 2019).”
BackgroundDeveloping Environmentally Friendly Wood Composite Panels by Nanotechnology
Candan, Z., & Akbulut, T. (2013) · BioResources · doi:10.15376/biores.8.3.3590-3598 · Cited by 60 · cited 1×
“Candan and Akbulut (2012, 2013) reported that the addition of 1% and 3% Al2O3, SiO2 and ZnO particles had significantly reduced the FEs from the UF-bonded particleboard and plywood panels.”
BackgroundFormaldehyde Release from Wood Products
Meyer, B., Andrews, B. A. K., & Reinhardt, R. M. (1986) · ACS symposium series · doi:10.1021/bk-1986-0316 · Cited by 60
Adhesives based on formaldehyde – environmental problems
Łebkowska, M., Załęska‐Radziwiłł, M., & Tabernacka, A. (2017) · Biotechnologia · doi:10.5114/bta.2017.66617 · Cited by 59
Utilization of bark flours as additive in plywood manufacturing
Aydın, İ., Demirkır, C., Çolak, S., & Çolakoğlu, G. (2016) · European Journal of Wood and Wood Products · doi:10.1007/s00107-016-1096-0 · Cited by 58 · cited 1×
“Bark flours obtained from different tree species having high polyphenol content (walnut, chestnut, fir, and spruce) also exhibited formaldehyde scavenging properties when added to the adhesive mixtures for bonding plywood (Aydin et al. 2017; Kawalerczyk et al. 2019; Réh et al. 2021; Ružiak et al. 2017; Wang et al. 201…”
BackgroundInvestigation of thermal insulation panels made of black locust tree bark
Pásztory, Z., Ronyecz, I., & Börcsök, Z. (2017) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2017.04.204 · Cited by 58
Lubis, M. A. R., & Park, B. (2020) · The Journal of Adhesion · doi:10.1080/00218464.2020.1753515 · Cited by 52
Self-citationAnalysis of Larch-Bark Capacity for Formaldehyde Removal in Wood Adhesives
Tudor, E. M., Barbu, M. C., Petutschnigg, A. J., Réh, R., & Krišťák, Ľ. (2020) · International Journal of Environmental Research and Public Health · doi:10.3390/ijerph17030764 · Cited by 50 · cited 4×
“2012), decorative panels (Tudor et al. 2020), and thermal insulation panels using bark and bark extractives (Pásztory et al.”
BackgroundMethodInfluentialSelakjani, P. P., Dorieh, A., Pizzi, A., Shahavi, M. H., Hasankhah, A., Shekarsaraee, S., Ashouri, M., Movahed, S. G., & Abatari, M. N. (2021) · International Journal of Adhesion and Adhesives · doi:10.1016/j.ijadhadh.2021.102962 · Cited by 48 · cited 2×
“…flour (Cameron and Pizzi 1985, Eom et al. 2006; Kim et al. 2006; Moubarik et al. 2010; Boran et al. 2012; Gangi et al. 2013, Pizzi et al. (2020); Selakjani et al. 2021) to the UF resin or wood furnish (Antov et al. 2021a, 2021b, 2021c; Bekhta et al. 2021a; Bekhta et al. 2021b; Lorenz et al.…”
BackgroundSelf-citationMueller, J. U., Bruckner, T. M., & Triebig, G. (2012) · International Archives of Occupational and Environmental Health · doi:10.1007/s00420-012-0745-9 · Cited by 45
Antov, P., Jivkov, V., Savov, V., Simeonova, R., & Yavorov, N. (2020) · Applied Sciences · doi:10.3390/app10217526 · Cited by 45 · cited 1×
“Several studies and reviews have addressed the issue of reducing formaldehyde emission in various ways (Antov et al. 2020b; Antov et al. 2020a, 2020b, 2020a; İstek et al. 2018; Kariuki et al. 2019; Myers 1984, 1986b).”
BackgroundSelf-citationHoong, Y. B., Tahir, P. M., Loh, Y. F., Koh, M.-S., Abdullah, L. C., & Ashaari, Z. (2010) · Journal of Adhesion Science and Technology · doi:10.1163/016942410x507740 · Cited by 45 · cited 2×
“Urea (CH₄N₂O), applied mainly as an aqueous solution, often in combination with ammonium chloride, was reported to improve the stability and control the pH of the UF resin, forming cross-linked UF polymer (Hoong et al. 2010).”
BackgroundFormaldehyde Use and Alternative Biobased Binders for Particleboard Formulation: A Review
Kariuki, S. W., Wachira, J. M., Kawira, M., & Murithi, G. (2019) · Journal of Chemistry · doi:10.1155/2019/5256897 · Cited by 44 · cited 1×
“Several studies and reviews have addressed the issue of reducing formaldehyde emission in various ways (Antov et al. 2020b; Antov et al. 2020a, 2020b, 2020a; İstek et al. 2018; Kariuki et al. 2019; Myers 1984, 1986b).”
BackgroundPark, B., Kang, E., & Park, J. (2008) · Journal of Applied Polymer Science · doi:10.1002/app.28748 · Cited by 44 · cited 8×
“…200–250 8.0–8.2 4.6–5.0 8.0–8.5 (Lubis and Park 2020a, Chuang and Gary 1992) 2.0 1.0–1.2 2 90–92; 1–2 80–90; 3–4 200–300 7.8–8.5 4.6–6.0 8.0–8.2 (Park et al. 2006, Park et al. 2008, Gonçalves et al. 2019) 90–92; 1–2 80–90; 3–4 200–300 8.5–9.0 12.0–13.0 8.0–8.2 (Liang et al. 2018) 3 90–92; 1–2…”
BackgroundMethodInfluentialLubis, M. A. R., & Park, B.-D. (2018) · Holzforschung · doi:10.1515/hf-2018-0010 · Cited by 43 · cited 2×
“(Lubis and Park 2018).”
BackgroundSelf-citationDuan, H., Qiu, T., Guo, L., Ye, J., & Li, X. (2015) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2015.03.037 · Cited by 43 · cited 1×
“A new kind of long-term effective bio-scavenger in the microcapsule form was developed by using an intraliquid desiccation method (Duan et al. 2015).”
MethodFlour fillers with urea-formaldehyde resin in plywood
Kawalerczyk, J., Dziurka, D., Mirski, R., & Trociński, A. (2019) · BioResources · doi:10.15376/biores.14.3.6727-6735 · Cited by 43 · cited 1×
“…fir, and spruce) also exhibited formaldehyde scavenging properties when added to the adhesive mixtures for bonding plywood (Aydin et al. 2017; Kawalerczyk et al. 2019; Réh et al. 2021; Ružiak et al. 2017; Wang et al. 2012b), particleboard (Medved et al. 2019; Nemli and Colakoğlu 2005; Sari…”
BackgroundGonçalves, C., Paiva, N. T., Ferra, J. M. M., Martins, J. M., Magalhães, F. D., Barros-Timmons, A. M., & Carvalho, L. (2018) · Holzforschung · doi:10.1515/hf-2017-0182 · Cited by 42 · cited 1×
“These resins are produced by numerous companies worldwide, as the technologies are well known requiring low capital investments (Gonçalves et al. 2018, Mantanis et al. 2018).”
BackgroundNanotechnology for wood quality improvement and protection
Taghiyari, H. R., Tajvidi, M., Taghiyari, R., Mantanis, G. I., Esmailpour, A., & Hosseinpourpia, R. (2020) · Elsevier eBooks · doi:10.1016/b978-0-12-817852-2.00019-6 · Cited by 42 · cited 3×
“…2013a, Bekhta et al. 2018), and (v) mixing of UF resin with other resins (H’ng et al. 2011) or the use of alternative adhesive systems based on carbon materials, modified amide–containing biopolymer, carboxymethyl cellulose and soy flour (Basta et al. 2006; Gui et al. 2016; Taghiyari et al. 2020a).”
BackgroundSelf-citationHong, M.-K., Lubis, M. A. R., Park, B.-D., Sohn, C. H., & Roh, J. (2020) · Wood Material Science & Engineering · doi:10.1080/17480272.2018.1528479 · Cited by 41 · cited 3×
“Reference UF F/U: 0.9–1.0 58–61 200–300* 180–250 0.2–0.4 (Hong et al. 2020, Lubis et al. 2020, Park et al. 2006, Park et al. 2008) F/U: 1.2–1.6 52–56 50–165* 250–575 0.41–0.75 MF F/M: 1.0–2.0 50–65 50–150* 100–500 0.2–0.3 (Dunky 2003, 2004, Merline et al. 2013, Monteiro et al. 2011) MUF F/(M+U):…”
BackgroundInfluentialSelf-citationHemp flour as a formaldehyde scavenger for melamine-urea-formaldehyde adhesive in plywood production
Kawalerczyk, J., Siuda, J., Mirski, R., & Dziurka, D. (2020) · BioResources · doi:10.15376/biores.15.2.4052-4064 · Cited by 41 · cited 4×
“The addition of pine cone flour (Ayrilmis et al. 2009; Buyuksari et al. 2010), rice husk flour and wheat flour (Kim et al. 2006), hemp flour (Kawalerczyk et al. 2020), soy flour, and wollastonite (Taghiyari et al. 2020a), chestnut shell powder (Ayrilmis and Kaymakci 2012), chestnut bur (Liang et…”
BackgroundInfluentialMechanisms of Formaldehyde Release from Bonded Wood Products
Myers, G. E. (1986) · ACS symposium series · doi:10.1021/bk-1986-0316.ch008 · Cited by 40 · cited 6×
“However, most of the low F/U mole ratio UF resins tend to have longer gelation time, slow curing, and low cross-linking density (Park and Kim 2008, Park et al. 2003), resulting in a poor strength at the expense of lower formaldehyde emission (Myers and Koutsky 1990, Myers 1986a).”
BackgroundInfluentialPotential of pulp and paper sludge as a formaldehyde scavenger agent in MDF resins
Migneault, S., Koubaa, A., Riedl, B., Nadji, H., Deng, J., & Zhang, T. (2011) · Holzforschung · doi:10.1515/hf.2011.039 · Cited by 39 · cited 3×
“The scavenging activity of pulp and paper sludge was studied by several researchers (Bekhta et al. 2019; Migneault et al. 2011; Xing et al. 2013).”
BackgroundKumar, A., Gupta, A., Sharma, K. V., & Nasir, M. (2013) · European Journal of Wood and Wood Products · doi:10.1007/s00107-013-0664-9 · Cited by 38 · cited 4×
“Many recent studies reported effective formaldehyde adsorption by activated carbons (Rong et al. 2003; Boonamnuayvitaya et al. 2005; Song et al. 2007) and other carbonbased nanomaterials (Kumar et al. 2013b; Kumar et al. 2017; Suresh and Bandosz 2018).”
BackgroundInfluentialEffect of natural compounds on reducing formaldehyde emission from plywood
Uchiyama, S., Matsushima, E., Kitao, N., Tokunaga, H., Ando, M., & Otsubo, Y. (2007) · Atmospheric Environment · doi:10.1016/j.atmosenv.2007.09.046 · Cited by 37
Hematabadi, H., Behrooz, R., Shakibi, A., & Arabi, M. (2011) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2011.09.018 · Cited by 37 · cited 2×
“…2021) to the UF resin or wood furnish (Antov et al. 2021a, 2021b, 2021c; Bekhta et al. 2021a; Bekhta et al. 2021b; Lorenz et al. 1999; Kim 2009a; Hematabadi et al. 2012; Gangi et al. 2013; Moubarik et al. 2013) or other compounds (starch derivatives, charcoal, pozzolan, zeolites, and urea) that…”
BackgroundTaghiyari, H. R., Hosseini, S. B., Ghahri, S., Ghofrani, M., & Papadopoulos, A. N. (2020) · Applied Sciences · doi:10.3390/app10196709 · Cited by 35 · cited 3×
“…2013a, Bekhta et al. 2018), and (v) mixing of UF resin with other resins (H’ng et al. 2011) or the use of alternative adhesive systems based on carbon materials, modified amide–containing biopolymer, carboxymethyl cellulose and soy flour (Basta et al. 2006; Gui et al. 2016; Taghiyari et al. 2020a).”
BackgroundSelf-citationKhalaf, Y., Hage, P. E., Mihajlova, J. D., Bergeret, A., Lacroix, P., & Hage, R. E. (2021) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2021.123071 · Cited by 35 · cited 1×
“Chitosan, the second most abundant polysaccharide in nature after cellulose, has an excellent potential to adsorb formaldehyde from panels due to the availability of free amine (NH2) groups (Khalaf et al. 2021).”
BackgroundYamanaka, S., Oiso, T., Kurahashi, Y., Abe, H., Hara, K., Fujimoto, T., & Kuga, Y. (2014) · Journal of Nanoparticle Research · doi:10.1007/s11051-014-2266-9 · Cited by 29 · cited 1×
“Yamanaka et al. (2014) employed a scalable and template-free production strategy to synthesize mesoporous calcium carbonate, and it was observed that the mesoporous calcium carbonate powder adsorbed formaldehyde gas.”
MethodDazmiri, M. K., Kiamahalleh, M. V., Kiamahalleh, M. V., Mansouri, H. R., & Moazami, V. (2018) · European Journal of Wood and Wood Products · doi:10.1007/s00107-018-1375-z · Cited by 28
Sodium metabisulphite as a scavenger of air pollutants for wood-based building materials
Costa, N. A., Pereira, J., Ferra, J. M. M., Cruz, P., Martins, J. M., Magalhães, F. D., Mendes, A. M. M., & Carvalho, L. (2013) · International Wood Products Journal · doi:10.1179/2042645313y.0000000037 · Cited by 26 · cited 8×
“…et al. 2013) or other compounds such as starch derivatives, charcoal, pozzolan, zeolites, and urea (Basta et al. 2006;Park et al. 2008; Kim 2009b; Kmec et al. 2010; Boran et al. 2011; Costa et al. 2013a) is an environmentally friendly way to reduce formaldehyde emission from wood-based panels.”
BackgroundMethodInfluentialBekhta, P., Sedliačik, J., & Bekhta, N. (2020) · Polymers · doi:10.3390/polym12030593 · Cited by 26 · cited 3×
“…1984; Dunky 1998), (ii) alteration of hot pressing parameters, i.e. pressing temperature and pressing time applied (Petinarakism and Kavvouras 2006, Bekhta et al. 2020), (iii) addition of formaldehyde scavengers, such as tannins, lignin, starch, wheat flour, and rice husk flour (Cameron and Pizzi…”
BackgroundInfluentialSelf-citationKumar, A., Sharma, K. V., Gupta, A. K., Tywoniak, J., & Hájek, P. (2016) · European Journal of Wood and Wood Products · doi:10.1007/s00107-016-1106-2 · Cited by 23
H`ng, P. S., Lee, S. H., Loh, Y. W., Lum, W. C., & Tan, B. (2011) · Asian Journal of Scientific Research · doi:10.3923/ajsr.2011.264.270 · Cited by 20 · cited 2×
“2018), and (v) mixing of UF resin with other resins (H’ng et al. 2011) or”
BackgroundEffect of aluminum oxide nanoparticles on the properties of urea-formaldehyde resin
Дудкин, Б. Н., Krivoshapkin, P. V., & Krivoshapkina, E. F. (2006) · Russian Journal of Applied Chemistry · doi:10.1134/s1070427206090254 · Cited by 19 · cited 3×
“Al2O3 and SiO2 nanoparticles have a very strong absorbability, and they can react with the active group of the UF resin and absorb free formaldehyde (de Cademartori et al. 2019; Dudkin et al. 2006, Lin et al. 2006, Roumeli et al. 2012).”
BackgroundMethodSteinhof, O., Scherr, G., & Hasse, H. (2015) · Magnetic Resonance in Chemistry · doi:10.1002/mrc.4274 · Cited by 18 · cited 2×
“Formation of urea-formaldehyde oligomers during the condensation reaction (adapted from Steinhof et al. (2014, 2015)).”
BackgroundMethodInfluentialAct, A. (2015) · Cited by 18
Reduction of formaldehyde emission from light MDF panels by adding chestnut shell flour
Ayrılmış, N., & Kaymakçı, A. (2011) · Holzforschung · doi:10.1515/hf.2011.170 · Cited by 15 · cited 1×
“…wheat flour (Kim et al. 2006), hemp flour (Kawalerczyk et al. 2020), soy flour, and wollastonite (Taghiyari et al. 2020a), chestnut shell powder (Ayrilmis and Kaymakci 2012), chestnut bur (Liang et al. 2021), walnut/almond particle (Pirayesh et al. 2013), into the wood-based panels…”
BackgroundXing, S., Riedl, B., Deng, J., Nadji, H., & Koubaa, A. (2013) · European Journal of Wood and Wood Products · doi:10.1007/s00107-013-0729-9 · Cited by 14
Diatomaceous earth as an inorganic additive to reduce formaldehyde emissions from particleboards
Funk, M., Wimmer, R., & Αδαμόπουλος, Σ. (2015) · Wood Material Science and Engineering · doi:10.1080/17480272.2015.1040066 · Cited by 11 · cited 1×
“Funk et al. (2017) found that particleboard produced with nano-mesoporous diatomaceous earth additive scavenged about 45% of the formaldehyde.”
BackgroundAntioxidant Activity of Keratin Hydrolysates Studied by DSC
Matyašovský, J., Sedliačik, J., Šimon, P., Novák, I., Krystofiak, T., JURKOVIČ, P., Duchovič, P., Sedliačiková, M., Cibulková, Z., Mičušík, M., et al. (2019) · Journal of the American Leather Chemists Association · Cited by 8
Cited by
Particleboard from agricultural biomass and recycled wood waste: a review
Lee, S. H., Lum, W. C., Boon, J. G., Kristak, L., Antov, P., Pędzik, M., Rogoziński, T., Taghiyari, H. R., Lubis, M. A. R., Fatriasari, W., et al. (2022) · Journal of Materials Research and Technology · doi:10.1016/j.jmrt.2022.08.166 · Cited by 248
Self-citationLatest advancements in high-performance bio-based wood adhesives: A critical review
Hussin, M. H., Abd Latif, N. H., Hamidon, T. S., Idris, N. N., Hashim, R., Appaturi, J. N., Brosse, N., Ziegler-Devin, I., Chrusiel, L., Fatriasari, W., et al. (2022) · Journal of Materials Research and Technology · doi:10.1016/j.jmrt.2022.10.156 · Cited by 197
Self-citationWronka, A., & Kowaluk, G. (2022) · Materials · doi:10.3390/ma15238487 · Cited by 38
Savov, V., Antov, P., Panchev, C., Lubis, M. A. R., Taghiyari, H. R., Lee, S. H., Krišťák, Ľ., & Todorova, M. (2023) · Fibers · doi:10.3390/fib11120103 · Cited by 18
“This is also supported by the fact that the main type of adhesives used in the production of wood-based panels is the urea-formaldehyde (UF) resin [24–28], which is highly unresistant to hydrolysis [29–35].”
Self-citation
Metadata
- Authors
- Kristak, L., Antov, P., Bekhta, P., Lubis, M. A. R., Iswanto, A. H., Reh, R., Sedliacik, J., Savov, V., Taghiyari, H. R., Papadopoulos, A. N., Pizzi, A., & Hejna, A.
- Venue
- Wood Material Science & Engineering
- Publisher
- Informa UK Limited
- Published
- 2022-04-07
- Volume
- 18
- Issue
- 2
- Pages
- 763-782
- ISSN
- 1748-0272 (ISSN-L)
- 1748-0280
- OpenAlex
- W4226220972
- Cited by
- 203
- References
- 91
- FWCI
- 18.64
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.