Cited by 24Advanced Battery Technologies ResearchAdvancements in Battery MaterialsAdvanced Battery Materials and Technologies

Effect of High-temperature thermal management on degradation of li-ion battery for fast charging

Park, Sang-Jun, Song, Young-Woong, Kang, Byeongsu, Kang, Min-Jun, Kim, Min-Young, Choi, Yeong-Jun, Lim, Jinsun, Kim, Ho-Sung +1 more·2024·IEEE Transactions on Transportation Electrification

Abstract

There is a growing demand for electric vehicles and related technologies to promote low-carbon green growth. To meet this demand, charging technologies that can reduce charging times are becoming increasingly important. However, charging at high C-rates can lead to lithium plating or electrode damage because lithium ions cannot be inserted into the anode while being deposited on the surface, which could increase the irreversible capacity of the battery and pose safety risks. To address this issue, it is necessary to enhance the energy efficiency and safety of batteries, while also suppressing battery deterioration, by increasing the charge transfer and diffusion of lithium ions through thermal management of the battery prior to fast charging. This study analyses the fast charge/discharge characteristics and deterioration factors of cylindrical batteries under different thermal management conditions to establish an optimal thermal management control strategy. The total discharge energy up to the end of life of the battery increases by approximately 266% when the battery is fast charged at a minimum battery cell temperature of 54 °C. Optimal thermal management improves the lithium plating, internal resistance, and Coulombic efficiency during fast charging. Thus, the battery can be safely and efficiently used for an extended period.

Integrity signals

Registry

Crossref · 10.1109/tte.2023.3305640

Cites

1 of 1 references verified0 citation errors · 0 not checkable

Statistics

Recomputing p-values needs the paper’s full text.

Claims the paper makes

This paper’s full text isn’t openly available, so its claims and self-check weren’t run. The registry and citation checks still apply.

Claims other papers make about this one

Each is checked against this paper’s own text: does it say what the citing paper says it does?

  • Ambient temperature is a vital factor influencing the activation of lithium ions, especially at relatively high temperatures (>45°C) or low temperatures (<0°C).

    “Besides current input, the ambient temperature of a working battery is another vital factor influencing the activation of lithium ions, especially at relatively high temperatures (>45 • C) or low temperatures (<0 • C) [5][6][7][8][9].”

Authors
Park, S.-J., Song, Y.-W., Kang, B., Kang, M.-J., Kim, M.-Y., Choi, Y.-J., Lim, J., Kim, H.-S., & Hong, Y.
Affiliations
  • Korea Institute of Industrial Technology (KR)
  • Korea Institute of Industrial Technology (KITECH), Jeju, Jeju Province, Republic of Korea
  • Korea Institute of Industrial Technology (KITECH), Gwangju, Republic of Korea
  • Jeju National University (KR)
Venue
IEEE Transactions on Transportation Electrification
Published
2024-06
Volume
10
Issue
2
Pages
2912-2922
ISSN
  • 2332-7782 (ISSN-L)
  • 2372-2088
OpenAlex
W4385975687
Cited by
24
References
1
Citations by year
2026: 10 · 2025: 12 · 2024: 2
FWCI
1.74
Type
journal article
Language
en
Open access
closed
Locations
IEEE Transactions on Transportation Electrification (publishedVersion)
Funders
Korea Ministry of Trade, Industry, and Energy (MOTIE) through “Implementation of On-Board Grade Estimation for EV Battery Using Database and Verifying Re-Use Applications With Used Batteries” (P0021883)
Topics
  • Physical Sciences › Engineering › Automotive Engineering › Advanced Battery Technologies Research
  • Physical Sciences › Engineering › Electrical and Electronic Engineering › Advancements in Battery Materials
  • Physical Sciences › Engineering › Electrical and Electronic Engineering › Advanced Battery Materials and Technologies
Keywords
lithium-ion batteries, thermal management, fast charging, lithium plating, battery degradation, cylindrical batteries, charge transfer, lithium ion diffusion, Coulombic efficiency, internal resistance, irreversible capacity, electric vehicles, battery safety

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review