The DOI matches its Crossref record; 39 of the 39 references it cites were found in a registry or an index.
Current Understanding and Remaining Challenges in Modeling Long‐Term Degradation of Borosilicate Nuclear Waste Glasses
Abstract
Chemical durability is not a single material property that can be uniquely measured. Instead, it is the response to a host of coupled material and environmental processes whose rates are estimated by a combination of theory, experiment and modeling. High‐level nuclear waste ( HLW ) glass is perhaps the most studied of any material yet there remain significant technical gaps regarding their chemical durability. The phenomena affecting the long‐term performance of HLW glasses in their disposal environment include surface reactions, transport properties to and from the reacting glass surface, and ion exchange between the solid glass and the surrounding solution and alteration products. The rates of these processes are strongly influenced and are coupled through the solution chemistry, which is in turn influenced by the reacting glass and also by reaction with the near‐field materials and precipitation of alteration products. Therefore, those processes must be understood sufficiently well to estimate or bound the performance of HLW glass in its disposal environment over geologic time scales. This article summarizes the current state of understanding of surface reactions, transport properties and ion exchange along with the near‐field materials and alteration products influences on solution chemistry and glass reaction rates. Also summarized are the remaining technical gaps along with recommended approaches to fill those technical gaps.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Roy, R., Leamy, H. J., White, C. W., Kaufmann, E. N., Schwoebel, R. L., Taylor, K. C., & Northrup, C. J. (1984) · Physics Today · doi:10.1063/1.2916117 · Cited by 1,010
Aagaard, P., & Helgeson, H. C. (1982) · American Journal of Science · doi:10.2475/ajs.282.3.237 · Cited by 894
Steefel, C. I., & Van Cappellen, P. (1990) · Geochimica et Cosmochimica Acta · doi:10.1016/0016-7037(90)90003-4 · Cited by 548
An international initiative on long-term behavior of high-level nuclear waste glass
Gin, S., Abdelouas, A., Criscenti, L. J., Ebert, W. L., Ferrand, K., Geisler, T., Harrison, M. T., Inagaki, Y., Mitsui, S., Mueller, K. T., et al. (2013) · Materials Today · doi:10.1016/j.mattod.2013.06.008 · Cited by 546
Self-citationGislason, S. R., & Oelkers, E. H. (2003) · Geochimica et Cosmochimica Acta · doi:10.1016/s0016-7037(03)00176-5 · Cited by 503
Oelkers, E. H., & Gislason, S. R. (2001) · Geochimica et Cosmochimica Acta · doi:10.1016/s0016-7037(01)00664-0 · Cited by 498
Oelkers, E. H., Schott, J., & Devidal, J.-L. (1994) · Geochimica et Cosmochimica Acta · doi:10.1016/0016-7037(94)90281-x · Cited by 493
Insight into silicate-glass corrosion mechanisms
Cailleteau, C., Angeli, F., Devreux, F., Gin, S., Jestin, J., Jollivet, P., & Spalla, O. (2008) · Nature Materials · doi:10.1038/nmat2301 · Cited by 488
Self-citationFrugier, P., Gin, S., Minet, Y., Chave, T., Bonin, B., Godon, N., Lartigue, J.-E., Jollivet, P., Ayral, A., De Windt, L., et al. (2008) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2008.06.044 · Cited by 395
Self-citationInterdiffusion of hydrogen and alkali ions in a glass surface
Doremus, R. H. (1975) · Journal of Non-Crystalline Solids · doi:10.1016/0022-3093(75)90079-4 · Cited by 366
A General Rate Equation for Nuclear Waste Glass Corrosion
Grambow, B. (1984) · MRS Proceedings · doi:10.1557/proc-44-15 · Cited by 291
First-order dissolution rate law and the role of surface layers in glass performance assessment
Grambow, B., & Müller, R. (2001) · Journal of Nuclear Materials · doi:10.1016/s0022-3115(01)00619-5 · Cited by 243
Aqueous corrosion of borosilicate glass under acidic conditions: A new corrosion mechanism
Geisler, T., Janssen, A., Scheiter, D., Stephan, T., Berndt, J., & Putnis, A. (2010) · Journal of Non-Crystalline Solids · doi:10.1016/j.jnoncrysol.2010.04.033 · Cited by 240
Fundamental approaches in describing mineral dissolution and precipitation rates
Lasaga, A. C. (1995) · Reviews in Mineralogy and Geochemistry · Cited by 224
Durable Glass for Thousands of Years
Jantzen, C. M., Brown, K. G., & Pickett, J. B. (2010) · International Journal of Applied Glass Science · doi:10.1111/j.2041-1294.2010.00007.x · Cited by 204
Nuclear Waste Glasses - How Durable?
Grambow, B. (2006) · Elements · doi:10.2113/gselements.2.6.357 · Cited by 194
The structure of Na2O–Al2O3–SiO2 glass: impact on sodium ion exchange in H2O and D2O
McGrail, B. P., Icenhower, J. P., Shuh, D. K., Liu, P., Darab, J. G., Baer, D. R., Thevuthasen, S., Shutthanandan, V., Engelhard, M. H., Booth, C. H., et al. (2001) · Journal of Non-Crystalline Solids · doi:10.1016/s0022-3093(01)00890-0 · Cited by 173
Jégou, C., Gin, S., & Lärché, F. (2000) · Journal of Nuclear Materials · doi:10.1016/s0022-3115(00)00039-8 · Cited by 152
Self-citationNuclear Glass Durability: New Insight into Alteration Layer Properties
Gin, S., Guittonneau, C., Godon, N., Neff, D., Rébiscoul, D., Cabié, M., & Mostefaoui, S. (2011) · The Journal of Physical Chemistry C · doi:10.1021/jp205477q · Cited by 146
Self-citationKaolinite dissolution and precipitation kinetics at 22°C and pH 4
Yang, L., & Steefel, C. I. (2007) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2007.10.011 · Cited by 144
Curti, E., Crovisier, J. L., Morvan, G., & Karpoff, A. M. (2006) · Applied Geochemistry · doi:10.1016/j.apgeochem.2006.03.010 · Cited by 143
The effect of composition on the leaching of three nuclear waste glasses: R7T7, AVM and VRZ
Frugier, P., Martin, C., Ribet, I., Advocat, T., & Gin, S. (2005) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2005.06.023 · Cited by 142
Self-citationGin, S., Ryan, J. V., Schreiber, D. K., Neeway, J. J., & Cabié, M. (2013) · Chemical Geology · doi:10.1016/j.chemgeo.2013.04.001 · Cited by 133
Self-citationGlass–water interphase reactivity with calcium rich solutions
Chave, T., Frugier, P., Gin, S., & Ayral, A. (2011) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2011.05.005 · Cited by 122
Self-citationPoinssot, C., & Gin, S. (2011) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2011.09.012 · Cited by 120
Self-citationForward dissolution rate of silicate glasses of nuclear interest in clay-equilibrated groundwater
Jollivet, P., Gin, S., & Schumacher, S. (2012) · Chemical Geology · doi:10.1016/j.chemgeo.2012.09.012 · Cited by 111
Self-citationBourcier, W. L., Peiffer, D. W., Knauss, K. G., McKeegan, K. D., & Smith, D. K. (1989) · MRS Proceedings · doi:10.1557/proc-176-209 · Cited by 105
Consistency between kinetics and thermodynamics
Boudart, M. (1976) · The Journal of Physical Chemistry · doi:10.1021/j100567a012 · Cited by 96
Long-term modeling of alteration-transport coupling: Application to a fractured Roman glass
Verney‐Carron, A., Gin, S., Frugier, P., & Libourel, G. (2010) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2010.01.001 · Cited by 93
Self-citationInvestigation of gel porosity clogging during glass leaching
Jollivet, P., Angeli, F., Cailleteau, C., Devreux, F., Frugier, P., & Gin, S. (2008) · Journal of Non-Crystalline Solids · doi:10.1016/j.jnoncrysol.2008.07.023 · Cited by 91
Self-citationGin, S., Jégou, C., Frugier, P., & Minet, Y. (2008) · Chemical Geology · doi:10.1016/j.chemgeo.2008.05.004 · Cited by 81
Self-citationThe dual effect of Mg on the long-term alteration rate of AVM nuclear waste glasses
Thien, B., Godon, N., Ballestero, A., Gin, S., & Ayral, A. (2012) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2012.05.025 · Cited by 68
Self-citationSorption of silicon on magnetite and other corrosion products of iron
Philippini, V., Naveau, A., Catalette, H., et al. (2005) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2005.09.002 · Cited by 63
Corrosion of alkali–borosilicate waste glass K-26 in non-saturated conditions
Ojovan, M. I., Hand, R. J., Ojovan, N. V., & Lee, W. E. (2004) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2004.10.095 · Cited by 63
Knauss, K. G., Bourcier, W. L., McKeegan, K. D., Merzbacher, C. I., Nguyen, S. N., Ryerson, F. J., Smith, D. K., Weed, H. C., & Newton, L. D. (1989) · MRS Proceedings · doi:10.1557/proc-176-176 · Cited by 52
Trotignon, L., Petit, J.-C., Mea, G. D., & Dran, J.-C. (1992) · Journal of Nuclear Materials · doi:10.1016/0022-3115(92)90088-3 · Cited by 33
Morlok, A., & Libourel, G. (2012) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2012.10.030 · Cited by 29
Pierce, E. M., McGrail, B. P., Bagaasen, L. M., Rodriguez, E. A., Wellman, D. M., Geiszler, K. N., Baum, S. R., Reed, L. R., Crum, J. V., & Schaef, H. T. (2006) · OSTI OAI (U.S. Department of Energy Office of Scientific and Technical Information) · doi:10.2172/908206 · Cited by 14
Lab., C. (. S. L. L. N., & Konynenburg, R. V. (1986) · doi:10.2172/59943 · Cited by 11
Cited by
Origin and consequences of silicate glass passivation by surface layers
Gin, S., Jollivet, P., Fournier, M., Angeli, F., Frugier, P., & Charpentier, T. (2015) · Nature Communications · doi:10.1038/ncomms7360 · Cited by 303
Self-citationA comparative review of the aqueous corrosion of glasses, crystalline ceramics, and metals
Frankel, G. S., Vienna, J. D., Lian, J., Scully, J. R., Gin, S., Ryan, J. V., Wang, J., Kim, S. H., Windl, W., & Du, J. (2018) · npj Materials Degradation · doi:10.1038/s41529-018-0037-2 · Cited by 276
Self-citationDevelopment of boron oxide potentials for computer simulations of multicomponent oxide glasses
Deng, L., & Du, J. (2019) · Journal of the American Ceramic Society · doi:10.1111/jace.16082 · Cited by 261
Chemical evolution of lead in ancient artifacts -A case study of early Chinese lead-silicate glaze
Yin, X., Huang, T. J., & Gong, H. (2020) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2020.01.002 · Cited by 22
Metadata
- Authors
- Vienna, J. D., Ryan, J. V., Gin, S., & Inagaki, Y.
- Venue
- International Journal of Applied Glass Science
- Publisher
- Wiley
- Published
- 2013-11-11
- Volume
- 4
- Issue
- 4
- Pages
- 283-294
- ISSN
- 2041-1286 (ISSN-L)
- 2041-1294
- OpenAlex
- W2134644154
- Cited by
- 266
- References
- 39
- FWCI
- 11.80
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.