Electrically conducting diamond powder was prepared by coating insulating diamond powder ( 8 - 12 μ m diam, ∼ 2 m 2 ∕ g ) with a thin boron-doped layer using microwave plasma-assisted chemical vapor deposition. Deposition times from 1 to 6 h were evaluated. Scanning electron microscopy (SEM) revealed that the diamond powder particles become more faceted and more secondary growths form with increasing deposition time. Fusion of neighboring particles was also observed with increasing growth time. The first-order diamond phonon line appeared in the Raman spectrum at ca. 1331 cm − 1 for deposition times up to 4 h, and was downshifted to as low as 1317 cm − 1 for some particles after the 6-h growth. Electrical resistance measurements of the bulk powder (no binder) confirmed that a conductive diamond overlayer formed, as the conductivity increased from near zero (insulating, < 10 − 5 S ∕ cm ) for the uncoated powder to 1.5 S ∕ cm after the 6-h growth. Ohmic behavior was seen in current-voltage curves recorded for the 4-h powder between ± 10 V . Cyclic voltammetric i-E curves for Fe ( CN ) 6 3 − ∕ 4 − and Ru ( NH 3 ) 6 3 + ∕ 2 + were recorded to evaluate the electrochemical properties of the conductive powder when mixed with a polytetrafluoroethylene binder. At scan rates between 10 and 500 mV ∕ s , Δ E p for both redox systems was high, ranging from 140 to 350 mV, consistent with significant ohmic resistance within the powder/binder electrode. Our results at this point suggest that the resistance is mainly due to poor particle-particle connectivity. Anodic polarization at 1.6 V vs Ag ∕ AgCl for 1 h (25°C) was performed to evaluate the morphological and microstructural stability of the conductive diamond in comparison with graphite and glassy carbon (GC) powders. The total charge passed during polarization was largest for the GC powder ( 0.88 C ∕ cm 2 ) and smallest for conductive diamond powder ( 0.18 C ∕ cm 2 ) . SEM images taken of conductive diamond powder after polarization showed no evidence of microstructural degradation, while significant morphological and microstructural changes were seen for the GC powder.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Carbons as supports for industrial precious metal catalysts
Auer, E., Freund, A., Pietsch, J., & Tacke, T. (1998) · Applied Catalysis A: General · doi:10.1016/s0926-860x(98)00184-7 · Cited by 792
Cited by
Carbon supports for low-temperature fuel cell catalysts
Antolini, E. (2009) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2008.09.030 · Cited by 1,295
Multifunctional 3D nanoarchitectures for energy storage and conversion
Rolison, D. R., Long, J. W., Lytle, J. C., Fischer, A. E., Rhodes, C. P., McEvoy, T. M., Bourg, M. E., & Lubers, A. M. (2009) · Chem. Soc. Rev. · doi:10.1039/b801151f · Cited by 812
Self-citationNovel catalyst support materials for PEMfuelcells: current status and future prospects
Shao, Y., Liu, J., Wang, Y., & Lin, Y. (2009) · J. Mater. Chem. · doi:10.1039/b808370c · Cited by 660
Design criteria for stable Pt/C fuel cell catalysts
Meier, J. C., Galeano, C., Katsounaros, I., Witte, J., Bongard, H. J., Topalov, A. A., Baldizzone, C., Mezzavilla, S., Schüth, F., & Mayrhofer, K. J. J. (2014) · Beilstein Journal of Nanotechnology · doi:10.3762/bjnano.5.5 · Cited by 559
Electrode Materials in Modern Organic Electrochemistry
Heard, D. M., & Lennox, A. J. J. (2020) · Angewandte Chemie International Edition · doi:10.1002/anie.202005745 · Cited by 523
Metadata
- Authors
- Fischer, A. E., & Swain, G. M.
- Venue
- Journal of The Electrochemical Society
- Publisher
- The Electrochemical Society
- Published
- 2005
- Volume
- 152
- Issue
- 9
- Pages
- B369
- ISSN
- 0013-4651 (ISSN-L)
- OpenAlex
- W1573150005
- Cited by
- 85
- References
- 1
- FWCI
- 3.83
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.