Coupled mechanical-chemical degradation of electrodes upon charging and discharging has been recognized as a major failure mechanism in lithium ion batteries. The instability of commonly employed electrolytes results in solid electrolyte interphase (SEI) formation. Although the SEI layer is necessary, as it passivates the electrode-electrolyte interface from further solvent decomposition, SEI formation consumes lithium and thus contributes to irreversible capacity loss. In this paper, we study irreversible capacity loss in a graphite-LiFePO 4 cell. Our results support the mechanism of irreversible capacity loss due to the consumption of lithium in forming SEI. We attribute irreversible capacity loss to diffusion induced stresses (DISs) that cause pre-existing cracks on the electrode surfaces to grow gradually upon cycling, leading to the growth of SEI on the newly exposed electrode surfaces. Because lithium is consumed in forming the new SEI, irreversible capacity loss continues with cycling. Along with the SEI formation upon newly exposed (cracked) surfaces, the existing SEI thickness also grows with cycling, resulting in additional loss of lithium. In this study, we provide, a simple mathematical model, based on the Paris’ Law formulation of mechanical fatigue, in combination with chemical degradation to explain battery life. We compare the predicted capacity at different temperatures with the experimental data obtained from electrochemical measurements on graphite-LiFePO 4 cells.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“which is why most physics-based models focus only on the most dominant mechanisms, such as the formation and growth of the solid electrolyte interphase (SEI) [11,12] or electronic contact loss through particle cracking [13,14].”
From Degradation diagnostics for lithium ion cells (2017) · cites this paper as [14]
Citations
Cites
Phospho‐olivines as Positive‐Electrode Materials for Rechargeable Lithium Batteries
Padhi, A. K., Nanjundaswamy, K. S., & Goodenough, J. B. (1997) · Journal of The Electrochemical Society · doi:10.1149/1.1837571 · Cited by 7,933
A Critical Analysis of Crack Propagation Laws
Paris, P., & Erdogan, F. (1963) · Journal of Basic Engineering · doi:10.1115/1.3656900 · Cited by 7,122
Lawn, B. (1993) · Cambridge University Press eBooks · doi:10.1017/cbo9780511623127 · Cited by 4,759
Suresh, S. (1998) · Cambridge University Press eBooks · doi:10.1017/cbo9780511806575 · Cited by 4,526
Battery materials for ultrafast charging and discharging
Kang, B., & Ceder, G. (2009) · Nature · doi:10.1038/nature07853 · Cited by 3,480
Insertion Electrode Materials for Rechargeable Lithium Batteries
Winter, M., Besenhard, J. O., Spahr, M. E., & Novák, P. (1998) · Advanced Materials · doi:10.1002/(sici)1521-4095(199807)10:10<808::aid-adma808>3.0.co;2-r · Cited by 2,998
Insertion Electrode Materials for Rechargeable Lithium Batteries
Winter, M., Besenhard, J. O., Spahr, M. E., & Novák, P. (1998) · Advanced Materials · doi:10.1002/(sici)1521-4095(199807)10:10<725::aid-adma725>3.0.co;2-z · Cited by 2,965
Electronically conductive phospho-olivines as lithium storage electrodes
Chung, S.-Y., Bloking, J. T., & Chiang, Y.-M. (2002) · Nature Materials · doi:10.1038/nmat732 · Cited by 2,939
Aurbach, D. (2000) · Journal of Power Sources · doi:10.1016/s0378-7753(00)00431-6 · Cited by 2,130
Fracture Mechanics: Fundamentals and Applications, Third Edition
Anderson, T. L., & Anderson, T. L. (2005) · CRC Press eBooks · doi:10.1201/9781420058215 · Cited by 1,854
Cycle-life model for graphite-LiFePO4 cells
Wang, J., Liu, P., Hicks-Garner, J., Sherman, E., Soukiazian, S., Verbrugge, M., Tataria, H., Musser, J., & Finamore, P. (2011) · Journal of Power Sources · doi:10.1016/j.jpowsour.2010.11.134 · Cited by 1,760
Self-citationColossal Reversible Volume Changes in Lithium Alloys
Beaulieu, L. Y., Eberman, K. W., Turner, R. L., Krause, L. J., & Dahn, J. R. (2001) · Electrochemical and Solid-State Letters · doi:10.1149/1.1388178 · Cited by 1,241
Main aging mechanisms in Li ion batteries
Broussely, M., Biensan, P., Bonhomme, F., Blanchard, P., Herreyre, S., Nechev, K., & Staniewicz, R. J. (2005) · Journal of Power Sources · doi:10.1016/j.jpowsour.2005.03.172 · Cited by 1,159
Numerical Simulation of Intercalation-Induced Stress in Li-Ion Battery Electrode Particles
Zhang, X., Shyy, W., & Marie Sastry, A. (2007) · Journal of The Electrochemical Society · doi:10.1149/1.2759840 · Cited by 893
Electroactivity of natural and synthetic triphylite
Ravet, N., Chouinard, Y., Magnan, J. F., Besner, S., Gauthier, M., & Armand, M. (2001) · Journal of Power Sources · doi:10.1016/s0378-7753(01)00727-3 · Cited by 844
Review of models for predicting the cycling performance of lithium ion batteries
Santhanagopalan, S., Guo, Q., Ramadass, P., & White, R. E. (2006) · Journal of Power Sources · doi:10.1016/j.jpowsour.2005.05.070 · Cited by 806
Stress generation and fracture in lithium insertion materials
Christensen, J., & Newman, J. (2006) · Journal of Solid State Electrochemistry · doi:10.1007/s10008-006-0095-1 · Cited by 727
An accelerated calendar and cycle life study of Li-ion cells
Bloom, I., Cole, B. W., Sohn, J. J., Jones, S. A., Polzin, E. G., Battaglia, V. S., Henriksen, G. L., Motloch, C., Richardson, R., Unkelhaeuser, T., et al. (2001) · Journal of Power Sources · doi:10.1016/s0378-7753(01)00783-2 · Cited by 619
Simulation of capacity fade in lithium-ion batteries
Spotnitz, R. (2003) · Journal of Power Sources · doi:10.1016/s0378-7753(02)00490-1 · Cited by 573
Qi, Y., Guo, H., Hector, L. G., & Timmons, A. (2010) · Journal of The Electrochemical Society · doi:10.1149/1.3327913 · Cited by 491
A Mathematical Model of Stress Generation and Fracture in Lithium Manganese Oxide
Christensen, J., & Newman, J. (2006) · Journal of The Electrochemical Society · doi:10.1149/1.2185287 · Cited by 485
Levi, M. D., & Aurbach, D. (1997) · The Journal of Physical Chemistry B · doi:10.1021/jp9701911 · Cited by 478
Cheng, Y.-T., & Verbrugge, M. W. (2009) · Journal of Power Sources · doi:10.1016/j.jpowsour.2009.01.021 · Cited by 469
Self-citation(2009) · doi:10.1007/978-0-387-76424-5 · Cited by 394
A generalized cycle life model of rechargeable Li-ion batteries
Ning, G., White, R. E., & Popov, B. N. (2006) · Electrochimica Acta · doi:10.1016/j.electacta.2005.06.033 · Cited by 372
Aging Mechanisms of LiFePO[sub 4] Batteries Deduced by Electrochemical and Structural Analyses
Liu, P., Wang, J., Hicks-Garner, J., Sherman, E., Soukiazian, S., Verbrugge, M., Tataria, H., Musser, J., & Finamore, P. (2010) · Journal of The Electrochemical Society · doi:10.1149/1.3294790 · Cited by 358
Self-citationIntercalation-Induced Stress and Heat Generation within Single Lithium-Ion Battery Cathode Particles
Zhang, X., Sastry, A. M., & Shyy, W. (2008) · Journal of The Electrochemical Society · doi:10.1149/1.2926617 · Cited by 334
A Mathematical Model for the Lithium-Ion Negative Electrode Solid Electrolyte Interphase
Christensen, J., & Newman, J. (2004) · Journal of The Electrochemical Society · doi:10.1149/1.1804812 · Cited by 330
Tin and tin-based intermetallics as new anode materials for lithium-ion cells
Wachtler, M., Besenhard, J. O., & Winter, M. (2001) · Journal of Power Sources · doi:10.1016/s0378-7753(00)00585-1 · Cited by 318
Modeling diffusion-induced stress in nanowire electrode structures
Deshpande, R., Cheng, Y.-T., & Verbrugge, M. W. (2010) · Journal of Power Sources · doi:10.1016/j.jpowsour.2010.02.021 · Cited by 303
Self-citationThe influence of surface mechanics on diffusion induced stresses within spherical nanoparticles
Cheng, Y.-T., & Verbrugge, M. W. (2008) · Journal of Applied Physics · doi:10.1063/1.3000442 · Cited by 302
Self-citationCapacity fade analysis of a lithium ion cell
Zhang, Q., & White, R. E. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.01.028 · Cited by 286
Real-time stress measurements in lithium-ion battery negative-electrodes
Sethuraman, V. A., Van Winkle, N., Abraham, D. P., Bower, A. F., & Guduru, P. R. (2012) · Journal of Power Sources · doi:10.1016/j.jpowsour.2012.01.036 · Cited by 219
Deshpande, R., Qi, Y., & Cheng, Y.-T. (2010) · Journal of The Electrochemical Society · doi:10.1149/1.3454762 · Cited by 171
Self-citationSolomon, H., Halford, G., Kaisand, L., & Leis, B. (1988) · doi:10.1520/stp942-eb · Cited by 162
Ionothermal Synthesis of Tailor-Made LiFePO4 Powders for Li-Ion Battery Applications
Recham, N., Dupont, L., Courty, M., Djellab, K., Larcher, D., Armand, M. B., & Tarascon, J. ‐. (2009) · Chemistry of Materials · doi:10.1021/cm803259x · Cited by 155
Markervich, E., Salitra, G., Levi, M. D., & Aurbach, D. (2005) · Journal of Power Sources · doi:10.1016/j.jpowsour.2005.03.107 · Cited by 150
Electrochemical Analysis of Lithiated Graphite Anodes
Verbrugge, M. W., & Koch, B. J. (2003) · Journal of The Electrochemical Society · doi:10.1149/1.1553788 · Cited by 141
Self-citationDiffusion Induced Stresses and Strain Energy in a Phase-Transforming Spherical Electrode Particle
Deshpande, R., Cheng, Y.-T., Verbrugge, M. W., & Timmons, A. (2011) · Journal of The Electrochemical Society · doi:10.1149/1.3565183 · Cited by 138
Self-citationBoyer, H. E. (1986) · CERN Document Server (European Organization for Nuclear Research) · Cited by 136
Life-Prediction Methods for Lithium-Ion Batteries Derived from a Fatigue Approach
Safari, M., Morcrette, M., Teyssot, A., & Delacourt, C. (2010) · Journal of The Electrochemical Society · doi:10.1149/1.3374634 · Cited by 117
Calendar life performance of pouch lithium-ion cells
Ramasamy, R. P., White, R. E., & Popov, B. N. (2004) · Journal of Power Sources · doi:10.1016/j.jpowsour.2004.09.024 · Cited by 104
Calendar life study of Li-ion pouch cells
Zhang, Q., & White, R. E. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.08.044 · Cited by 100
Harris, S. J., Deshpande, R. D., Qi, Y., Dutta, I., & Cheng, Y. (2010) · Journal of materials research/Pratt's guide to venture capital sources · doi:10.1557/jmr.2010.0183 · Cited by 94
Self-citationYan, J. W., Xia, B., Su, Y., Zhou, X., Zhang, J., & Zhang, X. (2008) · Electrochimica Acta · doi:10.1016/j.electacta.2008.05.032 · Cited by 94
Simulation of capacity loss in carbon electrode for lithium-ion cells during storage
Ramasamy, R. P., Lee, J., & Popov, B. N. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2006.12.086 · Cited by 82
Calendar life study of Li-ion pouch cells
Zhang, Q., & White, R. E. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.12.022 · Cited by 54
Cycle life performance of lithium-ion pouch cells
Kumaresan, K., Guo, Q., Ramadass, P., & White, R. E. (2005) · Journal of Power Sources · doi:10.1016/j.jpowsour.2005.08.058 · Cited by 54
Life Prediction Methods for Lithium-Ion Batteries Derived from a Fatigue Approach
Safari, M., Morcrette, M., Teyssot, A., & Delacourt, C. (2010) · Journal of The Electrochemical Society · doi:10.1149/1.3432560 · Cited by 49
Wang, T., Kiebele, A., Ma, J., Mhaisalkar, S. G., & Gruner, G. (2010) · Journal of The Electrochemical Society · doi:10.1149/1.3505994 · Cited by 43
Research works printed but not linked: 1
- Ragab A. R. Bayoumi S. B. , Engineering Solid Mechanics- Fundamental and Applications. (CRC Press, Boca Ranton, FL, 1999).
Cited by
Degradation diagnostics for lithium ion cells
Birkl, C. R., Roberts, M. R., McTurk, E., Bruce, P. G., & Howey, D. A. (2017) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.12.011 · Cited by 1,945
A review on the key issues of the lithium ion battery degradation among the whole life cycle
Han, X., Lu, L., Zheng, Y., Feng, X., Li, Z., Li, J., & Ouyang, M. (2019) · eTransportation · doi:10.1016/j.etran.2019.100005 · Cited by 1,745
Temperature dependent ageing mechanisms in Lithium-ion batteries – A Post-Mortem study
Waldmann, T., Wilka, M., Kasper, M., Fleischhammer, M., & Wohlfahrt-Mehrens, M. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2014.03.112 · Cited by 1,203
Xiong, R., Li, L., & Tian, J. (2018) · Journal of Power Sources · doi:10.1016/j.jpowsour.2018.10.019 · Cited by 1,017
Calendar and cycle life study of Li(NiMnCo)O2-based 18650 lithium-ion batteries
Ecker, M., Nieto, N., Käbitz, S., Schmalstieg, J., Blanke, H., Warnecke, A., & Sauer, D. U. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2013.09.143 · Cited by 782
Metadata
- Authors
- Deshpande, R., Verbrugge, M., Cheng, Y.-T., Wang, J., & Liu, P.
- Affiliations
- University of Kentucky (US)
- General Motors (United States) (US)
- HRL Laboratories (United States) (US)
- Venue
- Journal of The Electrochemical Society
- Publisher
- The Electrochemical Society
- Published
- 2012
- Volume
- 159
- Issue
- 10
- Pages
- A1730-A1738
- ISSN
- 0013-4651 (ISSN-L)
- 1945-7111
- OpenAlex
- W2021615999
- Cited by
- 389
- References
- 49
- Citations by year
- 2026: 33 · 2025: 30 · 2024: 33 · 2023: 31 · 2022: 27 · 2021: 29 · 2020: 31 · 2019: 25 · 2018: 25 · 2017: 30 · 2016: 28 · 2015: 29 · 2014: 21 · 2013: 17
- FWCI
- 38.54
- Type
- journal article
- Language
- en
- Open access
- closed
- Locations
- Journal of The Electrochemical Society (publishedVersion)
- Funders
- National Science Foundation
- Topics
- Physical Sciences › Engineering › Automotive Engineering › Battery Modeling and Management
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Advancements in Battery Materials
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Advanced Battery Materials and Technologies
- Keywords
- lithium-ion batteries, irreversible capacity, solid electrolyte interphase, lithium consumption, diffusion-induced stress, electrode cracking, Paris law, temperature effects, electrode-electrolyte interface
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.