Battery Cycle Life Prediction with Coupled Chemical Degradation and Fatigue Mechanics
The DOI matches its Crossref record; 50 of the 50 references it cites were found in a registry or an index.
Abstract
Coupled mechanical-chemical degradation of electrodes upon charging and discharging has been recognized as a major failure mechanism in lithium ion batteries. The instability of commonly employed electrolytes results in solid electrolyte interphase (SEI) formation. Although the SEI layer is necessary, as it passivates the electrode-electrolyte interface from further solvent decomposition, SEI formation consumes lithium and thus contributes to irreversible capacity loss. In this paper, we study irreversible capacity loss in a graphite-LiFePO 4 cell. Our results support the mechanism of irreversible capacity loss due to the consumption of lithium in forming SEI. We attribute irreversible capacity loss to diffusion induced stresses (DISs) that cause pre-existing cracks on the electrode surfaces to grow gradually upon cycling, leading to the growth of SEI on the newly exposed electrode surfaces. Because lithium is consumed in forming the new SEI, irreversible capacity loss continues with cycling. Along with the SEI formation upon newly exposed (cracked) surfaces, the existing SEI thickness also grows with cycling, resulting in additional loss of lithium. In this study, we provide, a simple mathematical model, based on the Paris’ Law formulation of mechanical fatigue, in combination with chemical degradation to explain battery life. We compare the predicted capacity at different temperatures with the experimental data obtained from electrochemical measurements on graphite-LiFePO 4 cells.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“which is why most physics-based models focus only on the most dominant mechanisms, such as the formation and growth of the solid electrolyte interphase (SEI) [11,12] or electronic contact loss through particle cracking [13,14].”
From Degradation diagnostics for lithium ion cells (2017) · cites this paper as [14]
Citations
Cites
Phospho‐olivines as Positive‐Electrode Materials for Rechargeable Lithium Batteries
Padhi, A. K., Nanjundaswamy, K. S., & Goodenough, J. B. (1997) · Journal of The Electrochemical Society · doi:10.1149/1.1837571 · Cited by 7,933
A Critical Analysis of Crack Propagation Laws
Paris, P., & Erdogan, F. (1963) · Journal of Basic Engineering · doi:10.1115/1.3656900 · Cited by 7,122
Lawn, B. (1993) · Cambridge University Press eBooks · doi:10.1017/cbo9780511623127 · Cited by 4,759
Suresh, S. (1998) · Cambridge University Press eBooks · doi:10.1017/cbo9780511806575 · Cited by 4,526
Battery materials for ultrafast charging and discharging
Kang, B., & Ceder, G. (2009) · Nature · doi:10.1038/nature07853 · Cited by 3,480
Insertion Electrode Materials for Rechargeable Lithium Batteries
Winter, M., Besenhard, J. O., Spahr, M. E., & Novák, P. (1998) · Advanced Materials · doi:10.1002/(sici)1521-4095(199807)10:10<808::aid-adma808>3.0.co;2-r · Cited by 2,998
Insertion Electrode Materials for Rechargeable Lithium Batteries
Winter, M., Besenhard, J. O., Spahr, M. E., & Novák, P. (1998) · Advanced Materials · doi:10.1002/(sici)1521-4095(199807)10:10<725::aid-adma725>3.0.co;2-z · Cited by 2,965
Electronically conductive phospho-olivines as lithium storage electrodes
Chung, S.-Y., Bloking, J. T., & Chiang, Y.-M. (2002) · Nature Materials · doi:10.1038/nmat732 · Cited by 2,939
Aurbach, D. (2000) · Journal of Power Sources · doi:10.1016/s0378-7753(00)00431-6 · Cited by 2,130
Fracture Mechanics: Fundamentals and Applications, Third Edition
Anderson, T. L., & Anderson, T. L. (2005) · CRC Press eBooks · doi:10.1201/9781420058215 · Cited by 1,854
Research works printed but not linked: 1
- Ragab A. R. Bayoumi S. B. , Engineering Solid Mechanics- Fundamental and Applications. (CRC Press, Boca Ranton, FL, 1999).
Cited by
Degradation diagnostics for lithium ion cells
Birkl, C. R., Roberts, M. R., McTurk, E., Bruce, P. G., & Howey, D. A. (2017) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.12.011 · Cited by 1,945
A review on the key issues of the lithium ion battery degradation among the whole life cycle
Han, X., Lu, L., Zheng, Y., Feng, X., Li, Z., Li, J., & Ouyang, M. (2019) · eTransportation · doi:10.1016/j.etran.2019.100005 · Cited by 1,745
Temperature dependent ageing mechanisms in Lithium-ion batteries – A Post-Mortem study
Waldmann, T., Wilka, M., Kasper, M., Fleischhammer, M., & Wohlfahrt-Mehrens, M. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2014.03.112 · Cited by 1,203
Xiong, R., Li, L., & Tian, J. (2018) · Journal of Power Sources · doi:10.1016/j.jpowsour.2018.10.019 · Cited by 1,017
Calendar and cycle life study of Li(NiMnCo)O2-based 18650 lithium-ion batteries
Ecker, M., Nieto, N., Käbitz, S., Schmalstieg, J., Blanke, H., Warnecke, A., & Sauer, D. U. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2013.09.143 · Cited by 782
Calendar Aging of Lithium-Ion Batteries: I. Impact of the Graphite Anode on Capacity Fade
Keil, P., Schuster, S. F., Wilhelm, J., Travi, J., Hauser, A., Karl, R. C., & Jossen, A. (2016) · Journal of The Electrochemical Society · doi:10.1149/2.0411609jes · Cited by 669
Li, J., Adewuyi, K., Lotfi, N., Landers, R. G., & Park, J. (2018) · Applied Energy · doi:10.1016/j.apenergy.2018.01.011 · Cited by 623
Wang, J., Purewal, J., Liu, P., Hicks-Garner, J., Soukazian, S., Sherman, E., Sorenson, A., Vu, L., Tataria, H., & Verbrugge, M. W. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2014.07.030 · Cited by 514
Self-citationReniers, J. M., Mulder, G., & Howey, D. A. (2019) · Journal of The Electrochemical Society · doi:10.1149/2.0281914jes · Cited by 462
Schroder, K., Alvarado, J., Yersak, T. A., Li, J., Dudney, N., Webb, L. J., Meng, Y. S., & Stevenson, K. J. (2015) · Chemistry of Materials · doi:10.1021/acs.chemmater.5b01627 · Cited by 454
Lithium-ion battery degradation: how to model it
O'Kane, S. E. J., Ai, W., Madabattula, G., Alonso-Alvarez, D., Timms, R., Sulzer, V., Edge, J. S., Wu, B., Offer, G. J., & Marinescu, M. (2022) · Physical Chemistry Chemical Physics · doi:10.1039/d2cp00417h · Cited by 400
Laresgoiti, I., Käbitz, S., Ecker, M., & Sauer, D. U. (2015) · Journal of Power Sources · doi:10.1016/j.jpowsour.2015.09.033 · Cited by 377
Yang, F., Wang, D., Zhao, Y., Tsui, K.-L., & Bae, S. J. (2018) · Energy · doi:10.1016/j.energy.2017.12.144 · Cited by 349
Waldmann, T., Iturrondobeitia, A., Kasper, M., Ghanbari, N., Aguesse, F., Bekaert, E., Daniel, L., Genies, S., Gordon, I. J., Löble, M. W., et al. (2016) · Journal of The Electrochemical Society · doi:10.1149/2.1211609jes · Cited by 328
Lu, P., Li, C., Schneider, E. W., & Harris, S. J. (2014) · The Journal of Physical Chemistry C · doi:10.1021/jp4111019 · Cited by 326
Yildirim, H., Kinaci, A., Chan, M. K. Y., & Greeley, J. P. (2015) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.5b02904 · Cited by 306
Han, X., Ouyang, M., Lu, L., & Li, J. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2014.06.111 · Cited by 302
Hsieh, A. G., Bhadra, S., Hertzberg, B. J., Gjeltema, P. J., Goy, A., Fleischer, J. W., & Steingart, D. A. (2015) · Energy & Environmental Science · doi:10.1039/c5ee00111k · Cited by 293
Lin, Y.-X., Liu, Z., Leung, K., Chen, L.-Q., Lu, P., & Qi, Y. (2016) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.01.078 · Cited by 287
State of health and charge measurements in lithium-ion batteries using mechanical stress
Cannarella, J., & Arnold, C. B. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2014.07.003 · Cited by 278
Franco, A. A. (2013) · RSC Advances · doi:10.1039/c3ra23502e · Cited by 262
Prada, E., Di Domenico, D., Creff, Y., Bernard, J., Sauvant-Moynot, V., & Huet, F. (2013) · Journal of The Electrochemical Society · doi:10.1149/2.053304jes · Cited by 242
Ouyang, M., Feng, X., Han, X., Lu, L., Li, Z., & He, X. (2016) · Applied Energy · doi:10.1016/j.apenergy.2015.12.063 · Cited by 239
A continuum of physics-based lithium-ion battery models reviewed
Brosa Planella, F., Ai, W., Boyce, A. M., Ghosh, A., Korotkin, I., Sahu, S., Sulzer, V, Timms, R., Tranter, T. G., Zyskin, M., et al. (2022) · Progress in Energy · doi:10.1088/2516-1083/ac7d31 · Cited by 217
“Physics-based models have been developed using the fatigue crack model of Paris’ law [28], which shows better accuracy for battery cells at high C-rates.”
Electrode Side Reactions, Capacity Loss and Mechanical Degradation in Lithium-Ion Batteries
Xu, J., Deshpande, R. D., Pan, J., Cheng, Y.-T., & Battaglia, V. S. (2015) · Journal of The Electrochemical Society · doi:10.1149/2.0291510jes · Cited by 220
Self-citationShin, H., Park, J., Han, S., Sastry, A. M., & Lu, W. (2015) · Journal of Power Sources · doi:10.1016/j.jpowsour.2014.11.120 · Cited by 217
Intercalation of Layered Materials from Bulk to 2D
Stark, M. S., Kuntz, K. L., Martens, S. J., & Warren, S. C. (2019) · Advanced Materials · doi:10.1002/adma.201808213 · Cited by 216
Ladpli, P., Kopsaftopoulos, F., & Chang, F.-K. (2018) · Journal of Power Sources · doi:10.1016/j.jpowsour.2018.02.056 · Cited by 214
Life prediction model for grid-connected Li-ion battery energy storage system
Smith, K., Saxon, A., Keyser, M., Lundstrom, B., Cao, Z., & Roc, A. (2017) · 2017 American Control Conference (ACC) · doi:10.23919/acc.2017.7963578 · Cited by 186
Physics-Informed Neural Networks for Prognostics and Health Management of Lithium-Ion Batteries
Wen, P., Ye, Z.-S., Li, Y., Chen, S., Xie, P., & Zhao, S. (2024) · IEEE Transactions on Intelligent Vehicles · doi:10.1109/tiv.2023.3315548 · Cited by 205
“For instance, based on SEI formation and the growth process on both the initial and cracked surface [18], [19], (3) can be specified as where t l represents the monitoring time earlier than t k and Θ = { θ 1 , θ 2 , . . . , θ 6 } are composite parameters.”
BackgroundMethodInfluentialVoltage hysteresis of lithium ion batteries caused by mechanical stress
Lu, B., Song, Y., Zhang, Q., Pan, J., Cheng, Y.-T., & Zhang, J. (2016) · Physical Chemistry Chemical Physics · doi:10.1039/c5cp06179b · Cited by 210
Self-citationTagade, P., Hariharan, K. S., Ramachandran, S., Khandelwal, A., Naha, A., Kolake, S. M., & Han, S. H. (2020) · Journal of Power Sources · doi:10.1016/j.jpowsour.2019.227281 · Cited by 204
Alipour, M., Ziebert, C., Conte, F. V., & Kizilel, R. (2020) · Batteries · doi:10.3390/batteries6030035 · Cited by 200
Challenges and opportunities toward long-life lithium-ion batteries
Xu, X., Han, X., Lu, L., Wang, F., Yang, M., Liu, X., Wu, Y., Tang, S., Hou, Y., Hou, J., et al. (2024) · Journal of Power Sources · doi:10.1016/j.jpowsour.2024.234445 · Cited by 195
Measurements of the Fracture Energy of Lithiated Silicon Electrodes of Li-Ion Batteries
Pharr, M., Suo, Z., & Vlassak, J. J. (2013) · Nano Letters · doi:10.1021/nl403197m · Cited by 196
Feng, X., He, X., Ouyang, M., Wang, L., Lu, L., Ren, D., & Santhanagopalan, S. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0311816jes · Cited by 194
Battery management strategies: An essential review for battery state of health monitoring techniques
Pradhan, S. K., & Chakraborty, B. (2022) · Journal of Energy Storage · doi:10.1016/j.est.2022.104427 · Cited by 194
Accelerated cycle life testing and capacity degradation modeling of LiCoO2-graphite cells
Diao, W., Saxena, S., & Pecht, M. (2019) · Journal of Power Sources · doi:10.1016/j.jpowsour.2019.226830 · Cited by 187
A Comprehensive Review on Lithium-Ion Battery Lifetime Prediction and Aging Mechanism Analysis
Madani, S. S., Shabeer, Y., Allard, F., Fowler, M., Ziebert, C., Wang, Z., Panchal, S., Chaoui, H., Mekhilef, S., Dou, S. X., et al. (2025) · Batteries · doi:10.3390/batteries11040127 · Cited by 171
Impact of Particle Size Distribution on Performance of Lithium‐Ion Batteries
Bläubaum, L., Röder, F., Nowak, C., Chan, H. S., Kwade, A., & Krewer, U. (2020) · ChemElectroChem · doi:10.1002/celc.202001249 · Cited by 179
Kumar, R., Tokranov, A., Sheldon, B. W., Xiao, X., Huang, Z., Li, C., & Mueller, T. (2016) · ACS Energy Letters · doi:10.1021/acsenergylett.6b00284 · Cited by 176
Modeling crack growth during Li insertion in storage particles using a fracture phase field approach
Klinsmann, M., Rosato, D., Kamlah, M., & McMeeking, R. M. (2016) · Journal of the Mechanics and Physics of Solids · doi:10.1016/j.jmps.2016.04.004 · Cited by 176
Recycling and Reusing of Graphite from Retired Lithium‐ion Batteries: A Review
Tian, H., Graczyk‐Zajac, M., Kessler, A., Weidenkaff, A., & Riedel, R. (2024) · Advanced Materials · doi:10.1002/adma.202308494 · Cited by 170
Ai, W., Wu, B., & Martínez‐Pañeda, E. (2022) · Journal of Power Sources · doi:10.1016/j.jpowsour.2022.231805 · Cited by 160
Differential thermal voltammetry for tracking of degradation in lithium-ion batteries
Wu, B., Yufit, V., Merla, Y., Martinez-Botas, R. F., Brandon, N. P., & Offer, G. J. (2015) · Journal of Power Sources · doi:10.1016/j.jpowsour.2014.09.127 · Cited by 151
Modeling the SEI-Formation on Graphite Electrodes in LiFePO4Batteries
Li, D., Danilov, D. L., Zhang, Z., Chen, H., Yang, Y., & Notten, P. H. L. (2015) · Journal of The Electrochemical Society · doi:10.1149/2.0161506jes · Cited by 161
An Effective Relithiation Process for Recycling Lithium‐Ion Battery Cathode Materials
Yang, T., Lu, Y., Li, L., Ge, D., Yang, H., Leng, W., Zhou, H., Han, X., Schmidt, N., Ellis, M., et al. (2019) · Advanced Sustainable Systems · doi:10.1002/adsu.201900088 · Cited by 159
A review on state of health estimation for lithium ion batteries in photovoltaic systems
Tian, J., Xiong, R., & Shen, W. (2019) · eTransportation · doi:10.1016/j.etran.2019.100028 · Cited by 151
Electrochemical Thermal-Mechanical Modelling of Stress Inhomogeneity in Lithium-Ion Pouch Cells
Ai, W., Kraft, L., Sturm, J., Jossen, A., & Wu, B. (2019) · Journal of The Electrochemical Society · doi:10.1149/2.0122001jes · Cited by 152
Vennam, G., Sahoo, A., & Ahmed, S. M. F. (2022) · Journal of Energy Storage · doi:10.1016/j.est.2022.104720 · Cited by 156
Deshpande, R. D., & Bernardi, D. M. (2017) · Journal of The Electrochemical Society · doi:10.1149/2.0841702jes · Cited by 154
Self-citationCracking predictions of lithium-ion battery electrodes by X-ray computed tomography and modelling
Boyce, A. M., Martínez‐Pañeda, E., Wade, A., Zhang, Y. S., Bailey, J. J., Heenan, T. M. M., Brett, D. J. L., & Shearing, P. R. (2022) · Journal of Power Sources · doi:10.1016/j.jpowsour.2022.231119 · Cited by 145
“Fracture of electrode particles contributes to the general degradation of the LIBs through mechanisms such as: build-up of solid-electrolyte-interphase (SEI) on newly cracked surfaces, leading to capacity fade [12]; loss of contact between particles and carbon binder, resulting in electrical isolation of particles, an…”
BackgroundHan, X., Ouyang, M., Lu, L., & Li, J. (2014) · Energies · doi:10.3390/en7084895 · Cited by 138
“This model is in good agreement with the experiment results [1,8,21].”
BackgroundResultSchroder, K., Dylla, A. G., Harris, S., Webb, L. J., & Stevenson, K. (2014) · ACS Applied Materials and Interfaces · doi:10.1021/am506517j · Cited by 131
Takahashi, K., & Srinivasan, V. (2015) · Journal of The Electrochemical Society · doi:10.1149/2.0281504jes · Cited by 133
Battery capacity fading estimation using a force-based incremental capacity analysis
Samad, N. A., Kim, Y., Siegel, J. B., & Stefanopoulou, A. G. (2016) · Journal of The Electrochemical Society · doi:10.1149/2.0511608jes · Cited by 130
“5,14,34 The method plots the differential of voltage over capacity with respect to capacity (dV/dQ versus Q).”
Non-uniform effect on the thermal/aging performance of Lithium-ion pouch battery
Song, W., Chen, M., Bai, F., Lin, S., Chen, Y., & Feng, Z. (2017) · Applied Thermal Engineering · doi:10.1016/j.applthermaleng.2017.09.090 · Cited by 133
Pharr, M., Suo, Z., & Vlassak, J. J. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2014.07.153 · Cited by 135
Prognostics of Li(NiMnCo)O2-based lithium-ion batteries using a novel battery degradation model
Yang, F., Wang, D., Xing, Y., & Tsui, K. (2017) · Microelectronics Reliability · doi:10.1016/j.microrel.2017.02.002 · Cited by 134
Understanding Full-Cell Evolution and Non-chemical Electrode Crosstalk of Li-Ion Batteries
Knehr, K. W., Hodson, T., Bommier, C., Davies, G., Kim, A., & Steingart, D. A. (2018) · Joule · doi:10.1016/j.joule.2018.03.016 · Cited by 127
Guo, W., Sun, Z., Vilsen, S. B., Meng, J., & Stroe, D. I. (2022) · Journal of Energy Storage · doi:10.1016/j.est.2022.105992 · Cited by 126
Purewal, J. J., Wang, J. J., Graetz, J., Soukiazian, S., Tataria, H., & Verbrugge, M. W. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2014.07.028 · Cited by 131
Self-citationYüksel, T., Litster, S., Viswanathan, V., & Michalek, J. J. (2016) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.10.104 · Cited by 141
Charging Optimization for Li-Ion Battery in Electric Vehicles: A Review
Chen, C., Wei, Z., & Knoll, A. (2021) · IEEE Transactions on Transportation Electrification · doi:10.1109/tte.2021.3135525 · Cited by 137
“disordering and exfoliation [102], [116], [117], side reactions,”
BackgroundHao, F., & Fang, D. (2013) · Journal of The Electrochemical Society · doi:10.1149/2.054304jes · Cited by 119
Klinsmann, M., Rosato, D., Kamlah, M., & McMeeking, R. M. (2015) · Journal of The Electrochemical Society · doi:10.1149/2.0281602jes · Cited by 115
A modeling and experimental study of capacity fade for lithium-ion batteries
Carnovale, A., & Li, X. (2020) · Energy and AI · doi:10.1016/j.egyai.2020.100032 · Cited by 124
Zhang, Y., Zhao, C., & Guo, Z. (2019) · International Journal of Mechanical Sciences · doi:10.1016/j.ijmecsci.2019.02.042 · Cited by 117
Dong, G., & Wei, J. (2021) · Electrochimica Acta · doi:10.1016/j.electacta.2021.139133 · Cited by 116
A comprehensive single-particle-degradation model for battery state-of-health prediction
Li, J., Landers, R. G., & Park, J. (2020) · Journal of Power Sources · doi:10.1016/j.jpowsour.2020.227950 · Cited by 116
Edouard, C., Petit, M., Forgez, C., Bernard, J., & Revel, R. (2016) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.06.030 · Cited by 118
Fang, D., Wu, W., Li, J., Yuan, W., Liu, T., Dai, C., Wang, Z., & Zhao, M. (2023) · Green Energy and Intelligent Transportation · doi:10.1016/j.geits.2023.100082 · Cited by 111
Measurement Techniques for Online Battery State of Health Estimation in Vehicle-to-Grid Applications
Landi, M., & Gross, G. (2014) · IEEE Transactions on Instrumentation and Measurement · doi:10.1109/tim.2013.2292318 · Cited by 111
Saxena, S., Ward, L. T., Kubal, J., Lu, W., Babinec, S., & Paulson, N. H. (2022) · Journal of Power Sources · doi:10.1016/j.jpowsour.2022.231736 · Cited by 112
Silicon Nanowire Degradation and Stabilization during Lithium Cycling by SEI Layer Formation
Cho, J., & Picraux, S. T. (2014) · Nano Letters · doi:10.1021/nl500130e · Cited by 109
Overcharge and Aging Analytics of Li-Ion Cells
Robles, D. J., Vyas, A. A., Fear, C., Jeevarajan, J. A., & Mukherjee, P. P. (2020) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ab9569 · Cited by 118
Liang, J., Gan, Y., Yao, M., & Li, Y. (2020) · International Journal of Heat and Mass Transfer · doi:10.1016/j.ijheatmasstransfer.2020.120615 · Cited by 100
Quantifying economic benefits of second life batteries of gridable vehicles in the smart grid
Debnath, U. K., Ahmad, I., & Habibi, D. (2014) · International Journal of Electrical Power & Energy Systems · doi:10.1016/j.ijepes.2014.05.077 · Cited by 103
Dai, Y., Cai, L., & White, R. E. (2013) · Journal of Power Sources · doi:10.1016/j.jpowsour.2013.08.113 · Cited by 103
Fracture behavior in battery materials
Li, P., Zhao, Y., Shen, Y., & Bo, S. (2020) · Journal of Physics Energy · doi:10.1088/2515-7655/ab83e1 · Cited by 98
Performance degradation due to anodic failure mechanisms in lithium-ion batteries
Sarkar, A., Nlebedim, C. I., & Shrotriya, P. (2020) · Journal of Power Sources · doi:10.1016/j.jpowsour.2020.229145 · Cited by 97
A design optimization methodology for Li+ batteries
Golmon, S., Maute, K. K., & Dunn, M. L. (2013) · Journal of Power Sources · doi:10.1016/j.jpowsour.2013.12.025 · Cited by 95
Stochastic Analysis of Diffusion Induced Damage in Lithium-Ion Battery Electrodes
Barai, P., & Mukherjee, P. P. (2013) · Journal of The Electrochemical Society · doi:10.1149/2.132306jes · Cited by 98
Selective recovery of lithium from spent LiFePO4 battery via a self-catalytic air oxidation method
Jin, H., Zhang, J., Yang, C., Ma, L., Chen, Y., & Wang, C. (2023) · Chemical Engineering Journal · doi:10.1016/j.cej.2023.141805 · Cited by 94
Ruan, J., Walker, P. D., Watterson, P. A., & Zhang, N. (2016) · Applied Energy · doi:10.1016/j.apenergy.2016.09.057 · Cited by 94
“With the increasing working temperature, higher DOD and discharging rate, the life cycles declines to lower than 1000 [57,58].”
BackgroundPerformance of commercial Li-Ion cells for future NASA missions and aerospace applications
Krause, F. C., Ruiz, J. P., Jones, S. C., Brandon, E. J., Darcy, E. C., Iannello, C. J., & Bugga, R. V. (2021) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/abf05f · Cited by 90
Mechanical Degradation of Graphite/PVDF Composite Electrodes: A Model-Experimental Study
Takahashi, K., Higa, K., Mair, S., Chintapalli, M., Balsara, N. P., & Srinivasan, V. (2015) · Journal of The Electrochemical Society · doi:10.1149/2.0271603jes · Cited by 92
Effect of thermal gradients on inhomogeneous degradation in lithium-ion batteries
Shen, L., Zhang, C., Zhao, Y., Offer, G. J., & Marinescu, M. (2023) · Communications Engineering · doi:10.1038/s44172-023-00124-w · Cited by 102
“In order to reduce complexity, models are normally used either without a thermal component 4,25 , or with a single temperature and state of health (SoH) for the entire cell 26,27 .”
BackgroundLi, Y., Guo, W., Stroe, D., Zhao, H., Kristensen, P. K., Jensen, L. R., Pedersen, K., & Gurevich, L. (2024) · Chemical Engineering Journal · doi:10.1016/j.cej.2024.155588 · Cited by 96
Lucu, M., Martinez-Laserna, E., Gandiaga, I., Liu, K., Camblong, H., Widanage, W. D., & Marco, J. (2020) · Journal of Energy Storage · doi:10.1016/j.est.2020.101410 · Cited by 84
“In the negative electrode, the particle cracking reveals fresh anode surface, which react with electrolyte reforming SEI and augmenting capacity loss [28,29].”
Electrochemomechanics of Electrodes in Li-Ion Batteries: A Review
Xu, R., & Zhao, K. (2016) · Journal of Electrochemical Energy Conversion and Storage · doi:10.1115/1.4035310 · Cited by 86
Crawford, A., Huang, Q., Kintner-Meyer, M. C., Zhang, J., Reed, D. M., Sprenkle, V., Viswanathan, V., & Choi, D. (2018) · Journal of Power Sources · doi:10.1016/j.jpowsour.2018.01.080 · Cited by 84
Lucu, M., Martinez-Laserna, E., Gandiaga, I., Liu, K., Camblong, H., Widanage, W. D., & Marco, J. (2020) · Journal of Energy Storage · doi:10.1016/j.est.2020.101409 · Cited by 79
Multi-Scale Mechanical Behavior of the Li3PS4 Solid-Phase Electrolyte
Baranowski, L. L., Heveran, C. M., Ferguson, V. L., & Stoldt, C. R. (2016) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.6b06612 · Cited by 78
Shi, Q., Liu, W., Qu, Q., Gao, T., Wang, Y., Liu, G., Battaglia, V., & Zheng, H. (2016) · Carbon · doi:10.1016/j.carbon.2016.10.008 · Cited by 77
Tracking degradation in lithium iron phosphate batteries using differential thermal voltammetry
Shibagaki, T., Merla, Y., & Offer, G. J. (2018) · Journal of Power Sources · doi:10.1016/j.jpowsour.2017.11.011 · Cited by 74
“The trickle charging at 100% SOC may have induced lithium plating which would spontaneously react with the electrolyte to form SEI.”
BackgroundInfluentialZheng, H., Tan, L., Zhang, L., Qu, Q., Wan, Z., Wang, Y., Shen, M., & 郑洪河 (2015) · Electrochimica Acta · doi:10.1016/j.electacta.2015.05.039 · Cited by 74
Wassiliadis, N., Kriegler, J., Gamra, K. A., & Lienkamp, M. (2023) · Journal of Power Sources · doi:10.1016/j.jpowsour.2022.232586 · Cited by 83
de Vasconcelos, L. S., Sharma, N., Xu, R., & Zhao, K. (2018) · Experimental Mechanics · doi:10.1007/s11340-018-00451-6 · Cited by 72
“The constant disruption of the solid interfaces leads to Li depletion, increase of ohmic and thermal resistances, and steady fade of cyclic efficiency, while the isolation of the active materials results in a mostly immediate loss in capacity of batteries [12, 13].”
Leng, Y., Ge, S., Marple, D., Yang, X., Bauer, C., Lamp, P., & Wang, C. (2017) · Journal of The Electrochemical Society · doi:10.1149/2.0451706jes · Cited by 76
Metadata
- Authors
- Deshpande, R., Verbrugge, M., Cheng, Y.-T., Wang, J., & Liu, P.
- Affiliations
- University of Kentucky (US)
- General Motors (United States) (US)
- HRL Laboratories (United States) (US)
- Venue
- Journal of The Electrochemical Society
- Publisher
- The Electrochemical Society
- Published
- 2012
- Volume
- 159
- Issue
- 10
- Pages
- A1730-A1738
- ISSN
- 0013-4651 (ISSN-L)
- 1945-7111
- OpenAlex
- W2021615999
- Cited by
- 389
- References
- 49
- Citations by year
- 2026: 33 · 2025: 30 · 2024: 33 · 2023: 31 · 2022: 27 · 2021: 29 · 2020: 31 · 2019: 25 · 2018: 25 · 2017: 30 · 2016: 28 · 2015: 29 · 2014: 21 · 2013: 17
- FWCI
- 38.54
- Type
- journal article
- Language
- en
- Open access
- closed
- Locations
- Journal of The Electrochemical Society (publishedVersion)
- Funders
- National Science Foundation
- Topics
- Physical Sciences › Engineering › Automotive Engineering › Battery Modeling and Management
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Advancements in Battery Materials
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Advanced Battery Materials and Technologies
- Keywords
- lithium-ion batteries, irreversible capacity, solid electrolyte interphase, lithium consumption, diffusion-induced stress, electrode cracking, Paris law, temperature effects, electrode-electrolyte interface
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.