Abstract
The use of absorbable orthopedic implants has increased substantially during the last decade. Currently, most of them are fabricated from poly-L-lactide (PLLA), its co-polymers, or mixtures with other constituents. In vivo, PLLA persists for years after its surgical role has ended, which is confirmed by a long-term histological study of PLLA implanted in sheep either as functional interference screws or nonfunctional rods. The first tissue reaction is the sequestration of the implant within new bone during the initial 3 months. After a nonreactive period, a second tissue reaction is associated with the early signs of structural disintegration of the PLLA at 1 year. Subsequently, as the polymer mass reduces, it is replaced by a relatively avascular fibrous tissue containing macrophages and having an occasional multinucleated giant cell on the implant surface. After 3 years much of the polymer is still present, although as isolated fragments. The tissue reactions can be explained in terms of the physical chemistry of PLLA degradation. Though biocompatible, the excessive longevity of PLLA and the absence of its replacement by bone, indicates that despite being satisfactory clinically, it is not an ideal implant material, and that improved absorbable materials need to be developed.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Biodegradable polymers for use in surgery—polyglycolic/poly(actic acid) homo- and copolymers: 1
Gilding, D. K., & Reed, A. M. (1979) · Polymer · doi:10.1016/0032-3861(79)90009-0 · Cited by 1,345 · cited 1×
“The first medical use of absorbable materials was over 40 years ago in the manufacture of absorbable sutures [7] and following this, other absorbable products were slowly introduced almost entirely in the area of sutures, orthopedic sports medicine, soft tissue fixation devices, and orthopedic fracture fixation device…”
BackgroundLate degradation tissue response to poly(?-lactide) bone plates and screws
Bergsma, J. (1995) · Biomaterials · doi:10.1016/0142-9612(95)91092-d · Cited by 799
Orthopaedic applications for PLA‐PGA biodegradable polymers
Athanasiou, K., Agrawal, C., Barber, F., & Burkhart, S. (1998) · Arthroscopy · doi:10.1016/s0749-8063(98)70099-4 · Cited by 487
Cited by
Design of biodegradable, implantable devices towards clinical translation
Li, C., Guo, C., Fitzpatrick, V., Ibrahim, A., Zwierstra, M. J., Hanna, P., Lechtig, A., Nazarian, A., Lin, S. J., & Kaplan, D. L. (2019) · Nature Reviews Materials · doi:10.1038/s41578-019-0150-z · Cited by 808
Synthesis, properties and biomedical applications of poly(glycerol sebacate) (PGS): A review
Rai, R., Tallawi, M., Grigore, A., & Boccaccini, A. R. (2012) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2012.02.001 · Cited by 477
Control of Scaffold Degradation in Tissue Engineering: A Review
Zhang, H., Zhou, L., & Zhang, W. (2014) · Tissue Engineering Part B: Reviews · doi:10.1089/ten.teb.2013.0452 · Cited by 290
Electrospinning production of nanofibrous membranes
Mishra, R. K., Mishra, P., Verma, K., Mondal, A., Chaudhary, R. G., Abolhasani, M. M., & Loganathan, S. (2019) · Environmental Chemistry Letters · doi:10.1007/s10311-018-00838-w · Cited by 244
“2005a; Walton and Cotton 2007; Raghavendran et al.”
Farraro, K. F., Kim, K. E., Woo, S. L.-Y., Flowers, J. R., & McCullough, M. B. (2014) · Journal of Biomechanics · doi:10.1016/j.jbiomech.2013.12.003 · Cited by 214
“A 10-year follow-up study showed that an osseous cyst had formed after complete degradation of an interference screw (Walton and Cotton, 2007).”
BackgroundBiodegradable Piezoelectric Polymers: Recent Advancements in Materials and Applications
Ali, M., Bathaei, M. J., Istif, E., Karimi, S. N. H., & Beker, L. (2023) · Advanced Healthcare Materials · doi:10.1002/adhm.202300318 · Cited by 211
Degradation Behaviors of Electrospun Resorbable Polyester Nanofibers
Dong, Y., Liao, S., Ngiam, M., Chan, C. K., & Ramakrishna, S. (2009) · Tissue Engineering Part B: Reviews · doi:10.1089/ten.teb.2008.0619 · Cited by 200
“PLA polymers are used in a broad variety of medical applications, including bioresorbable sutures, 36 dental implants, 37 bone screws and plates, 38 and controlled drug delivery.”
Degradable piezoelectric biomaterials for wearable and implantable bioelectronics
Li, J., Long, Y., Yang, F., & Wang, X. (2020) · Current Opinion in Solid State and Materials Science · doi:10.1016/j.cossms.2020.100806 · Cited by 187
The osteogenesis of bacterial cellulose scaffold loaded with bone morphogenetic protein-2
Shi, Q., Li, Y., Sun, J., Zhang, H., Chen, L., Chen, B., Yang, H., & Wang, Z. (2012) · Biomaterials · doi:10.1016/j.biomaterials.2012.05.071 · Cited by 185
Layered chitosan-collagen hydrogel/aligned PLLA nanofiber construct for flexor tendon regeneration
Deepthi, S., Nivedhitha Sundaram, M., Deepti Kadavan, J., & Jayakumar, R. (2016) · Carbohydrate Polymers · doi:10.1016/j.carbpol.2016.07.124 · Cited by 164
“The degradation of PLLA takes very long time in vitro nd in vivo (Walton & Cotton, 2007), thus maintaining the structural ntegrity of the scaffold.”
BackgroundThe nanofibrous architecture of poly(l-lactic acid)-based functional copolymers
Liu, X., & Ma, P. X. (2010) · Biomaterials · doi:10.1016/j.biomaterials.2009.09.046 · Cited by 104
“First, PLLA is a relatively hydrophobic material and its degradation rate is too slow for some applications [19-21].”
BackgroundStructure-property relationships in 3D-printed poly(l-lactide-co-ε-caprolactone) degradable polymer
Bachtiar, E. O., Ritter, V. C., & Gall, K. (2021) · Journal of the Mechanical Behavior of Biomedical Materials · doi:10.1016/j.jmbbm.2021.104650 · Cited by 27
Metadata
- Authors
- Walton, M., & Cotton, N. J.
- Venue
- Journal of Biomaterials Applications
- Publisher
- SAGE Publications
- Published
- 2007-04
- Volume
- 21
- Issue
- 4
- Pages
- 395-411
- ISSN
- 0885-3282 (ISSN-L)
- 1530-8022
- OpenAlex
- W2075343185
- Cited by
- 101
- References
- 3
- FWCI
- 2.57
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.