Joining of engineering ceramics
The DOI matches its Crossref record; 324 of the 328 references it cites were found in a registry or an index.
Abstract
Engineering ceramics such as alumina, zirconia, silicon nitride and silicon carbide can now be manufactured reliably with reproducible properties. As such, they are of increasing interest to industry, particularly for use in demanding environments, where their thermomechanical performance is of critical importance, with applications ranging from fuel cells to cutting tools. One aspect common to virtually all applications of engineering ceramics is that eventually they must be joined with another material, most usually a metal. The joining of engineering ceramics to metals is not always easy. There are two main considerations. The first consideration is the basic difference in atomic bonding: the ionic or covalent bonding of the ceramic, compared to the metallic bond. The second consideration is the mismatch in the coefficient of thermal expansion. In general, ceramics have a lower coefficient of thermal expansion than metals and, if high tensile forces are produced in the ceramic, either as a consequence of operating conditions or from the joining procedure itself, failure can occur. The plethora of joining processes available will be reviewed in this article, placing them in context from both an academic and commercial perspective. Comment will be made on research reporting advances on known technology, as well as introducing ‘newer’ technologies developed over the last 10 years. Finally, reviews and commentary will be made on the potential applications of the various joining processes in the commercial environment.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“Ceramic joining techniques are numerous and technically challenging, and often subject the entire sample to extreme conditions, such as high temperatures and/or vacuums [223].”
From Ultrafast Laser Additive Manufacturing: A Review (2023) · cites this paper as [223]
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Structural Inorganic Chemistry
(1971) · Nature · doi:10.1038/229453c0 · Cited by 5,766
The Superalloys: Fundamentals and Applications
Reed, R. C. (2008) · Cited by 3,725
The Superalloys: Fundamentals and Applications
Reed, R. C. (2006) · Cambridge University Press eBooks · doi:10.1017/cbo9780511541285 · Cited by 2,369
Transformation Toughening in Zirconia‐Containing Ceramics
Hannink, R. H. J., Kelly, P., & Muddle, B. C. (2000) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2000.tb01221.x · Cited by 2,268
Silicon Nitride and Related Materials
Riley, F. L. (2000) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2000.tb01182.x · Cited by 1,566
CRC Materials Science and Engineering Handbook
Shackelford, J. F., Han, Y.-H., Kim, S., & Kwon, S.-H. (2016) · CRC Press eBooks · doi:10.1201/b18971 · Cited by 1,274
Wettability at High Temperatures
(1999) · Pergamon materials series · doi:10.1016/s1470-1804(99)x8001-1 · Cited by 1,042
Current ceramic materials and systems with clinical recommendations: A systematic review
Conrad, H. J., Seong, W.-J., & Pesun, I. J. (2007) · The Journal of Prosthetic Dentistry · doi:10.1016/s0022-3913(07)60124-3 · Cited by 981
The application of the specular reflection of neutrons to the study of surfaces and interfaces
Penfold, J., & Thomas, R. K. (1990) · Journal of Physics Condensed Matter · doi:10.1088/0953-8984/2/6/001 · Cited by 742
Handbook of Ceramic Composites
Bansal, N. P. (2005) · Springer eBooks · doi:10.1007/b104068 · Cited by 654
Sealants for solid oxide fuel cells
Fergus, J. W. (2005) · Journal of Power Sources · doi:10.1016/j.jpowsour.2005.05.002 · Cited by 616
Wyckoff, R. W. G., Qosim, W., Yuwariah, Y., Hamdani, J., Rachmadi, M., & Perdani, S. (1965) · Cited by 550
Ceramic microstructures : property control by processing
Lee, W. E., & Rainforth, W. M. (1994) · Chapman & Hall eBooks · Cited by 535
Chawla, K. K. (1998) · Springer eBooks · doi:10.1007/978-1-4757-2966-5_7 · Cited by 468
Berndt, A. F. (1969) · Journal of Chemical Education · doi:10.1021/ed046p594.1 · Cited by 432
TLP bonding: a new method for joining heat resistant alloys
Duvall, D. S., Owczarski, W. A., & Paulonis, D. F. (1974) · Welding Journal · Cited by 422
Ceramics for Prosthetic Hip and Knee Joint Replacement
Rahaman, M. N., Yao, A., Bal, B. S., Garino, J. P., & Ries, M. D. (2007) · Journal of the American Ceramic Society · doi:10.1111/j.1551-2916.2007.01725.x · Cited by 376
Ordered Liquid Aluminum at the Interface with Sapphire
Oh, S. H., Kauffmann, Y., Scheu, C., Kaplan, W. D., & Rühle, M. (2005) · Science · doi:10.1126/science.1118611 · Cited by 361
Formation of LanxideTM ceramic composite materials
Newkirk, M. S., Urquhart, A. W., Zwicker, H. R., & BREVAL, E. (1986) · Journal of materials research/Pratt's guide to venture capital sources · doi:10.1557/jmr.1986.0081 · Cited by 338
Dynamics of wetting in reactive metal/ ceramic systems
Eustathopoulos, N. (1998) · Acta Materialia · doi:10.1016/s1359-6454(98)80013-x · Cited by 307
Principles of soldering and brazing
(1994) · Choice Reviews Online · doi:10.5860/choice.31-2706 · Cited by 228
Humpston, G., & Jacobson, D. M. (2004) · ASM International eBooks · doi:10.31399/asm.tb.ps.9781627083522 · Cited by 226
Ridging effects on wetting and spreading of liquids on solids
Saiz, E., Tomsia, A. P., & Cannon, R. M. (1998) · Acta Materialia · doi:10.1016/s1359-6454(98)80016-5 · Cited by 214
Jacobson, D. M., & Humpston, G. (2005) · ASM International eBooks · doi:10.31399/asm.tb.pb.9781627083515 · Cited by 213
Current Concepts in Orthopaedic Biomaterials and Implant Fixation
FRIEDMAN, R. J., BLACK, J., GALANTE, J. O., JACOBS, J. J., & SKINNER, H. B. (1993) · The Journal of Bone & Joint Surgery · doi:10.2106/00004623-199307000-00017 · Cited by 210
Active metal brazing of zirconia
Hanson, W. B., Ironside, K. I., & Fernie, J. A. (2000) · Acta Materialia · doi:10.1016/s1359-6454(00)00256-1 · Cited by 210
Self-citationA review of sealing technologies applicable to solid oxide electrolysis cells
Lessing, P. A. (2007) · Journal of Materials Science · doi:10.1007/s10853-006-0409-9 · Cited by 209
Handbook of properties of technical and engineering ceramics
Morrell, R. (1989) · CERN Document Server (European Organization for Nuclear Research) · Cited by 201
Critical issues and current status of SiC/SiC composites for fusion
Hasegawa, A., Kohyama, A., Jones, R. H., Snead, L. L., Riccardi, B., & Fenici, P. (2000) · Journal of Nuclear Materials · doi:10.1016/s0022-3115(00)00374-3 · Cited by 199
Yang, Z.-G. (2003) · Solid State Ionics · doi:10.1016/s0167-2738(03)00160-7 · Cited by 191
Characterization of the electrostatic bonding of silicon and Pyrex glass
Cozma, A., & Puers, R. (1995) · Journal of Micromechanics and Microengineering · doi:10.1088/0960-1317/5/2/010 · Cited by 187
Sealing Technology for Solid Oxide Fuel Cells (SOFC)
Singh, R. N. (2007) · International Journal of Applied Ceramic Technology · doi:10.1111/j.1744-7402.2007.02128.x · Cited by 186
The relation between wetting and interfacial chemistry in the CuAgTi/alumina system
Voytovych, R., Robaut, F., & Eustathopoulos, N. (2006) · Acta Materialia · doi:10.1016/j.actamat.2005.11.048 · Cited by 185
Glass–ceramic seal to join Crofer 22 APU alloy to YSZ ceramic in planar SOFCs
Smeacetto, F., Salvo, M., Ferraris, M., Cho, J., & Boccaccini, A. R. (2007) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2007.05.006 · Cited by 184
High-temperature wettability measurements in metal/ceramic systems – Some methodological issues
Sobczak, N., Singh, M., & Asthana, R. (2005) · Current Opinion in Solid State and Materials Science · doi:10.1016/j.cossms.2006.07.007 · Cited by 171
Reactive spreading: adsorption, ridging and compound formation
Saiz, E., Cannon, R. M., & Tomsia, A. P. (2000) · Acta Materialia · doi:10.1016/s1359-6454(00)00231-7 · Cited by 167
BAS (BaO·Al2O3·SiO2)-glasses for high temperature applications
Eichler, K., Solow, G., Otschik, P., & Schaffrath, W. (1999) · Journal of the European Ceramic Society · doi:10.1016/s0955-2219(98)00382-3 · Cited by 157
Progress in understanding and modeling reactive wetting of metals on ceramics
Eustathopoulos, N. (2005) · Current Opinion in Solid State and Materials Science · doi:10.1016/j.cossms.2006.04.004 · Cited by 151
Blugan, G., Kuebler, J., Bissig, V., & Janczak‐Rusch, J. (2006) · Ceramics International · doi:10.1016/j.ceramint.2006.03.010 · Cited by 150
Microsystem technologies for implantable applications
Receveur, R. A. M., Lindemans, F. W., & de Rooij, N. F. (2007) · Journal of Micromechanics and Microengineering · doi:10.1088/0960-1317/17/5/r02 · Cited by 142
Knowles, K. M., & van Helvoort, A. T. J. (2006) · International Materials Reviews · doi:10.1179/174328006x102501 · Cited by 137
Self-citationPennock, A. T., Schmidt, A. H., & Bourgeault, C. A. (2002) · The Journal of Arthroplasty · doi:10.1054/arth.2002.33565 · Cited by 136
Chemical interaction between glass–ceramic sealants and interconnect steels in SOFC stacks
Batfalsky, P., Haanappel, V. A. C., Malzbender, J., Menzler, N. H., Shemet, V., Vinke, I. C., & Steinbrech, R. W. (2005) · Journal of Power Sources · doi:10.1016/j.jpowsour.2005.05.046 · Cited by 133
Pascual, M. J., Guillet, A., & Durán, A. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.01.040 · Cited by 132
Joining of reaction-bonded silicon carbide using a preceramic polymer
Colombo, P., Sglavo, V. M., Pippel, E., & Woltersdorf, J. (1998) · Journal of Materials Science · doi:10.1023/a:1004312109836 · Cited by 121
Bonding of zirconia to super alloy with the active brazing technique
Sciti, D., Bellosi, A., & Esposito, L. (2001) · Journal of the European Ceramic Society · doi:10.1016/s0955-2219(00)00162-x · Cited by 120
Reactive Air Brazing: A Novel Method of Sealing SOFCs and Other Solid-State Electrochemical Devices
Weil, K. S., Kim, J. Y., & Hardy, J. S. (2005) · Electrochemical and Solid-State Letters · doi:10.1149/1.1850391 · Cited by 116
Kim, J. Y., Hardy, J. S., & Weil, K. S. (2005) · Journal of the American Ceramic Society · doi:10.1111/j.1551-2916.2005.00492.x · Cited by 116
Joining of ceramic composites by microwave heating
Aravindan, S., & Krishnamurthy, R. (1999) · Materials Letters · doi:10.1016/s0167-577x(98)00166-9 · Cited by 115
Diffusion bonding of aluminium oxide to stainless steel using stress relief interlayers
Travessa, D. N., Ferrante, M., & den Ouden, G. (2002) · Materials Science and Engineering A · doi:10.1016/s0921-5093(02)00046-1 · Cited by 112
Atomic structure of epitaxial Nb-Al2O3interfaces I. Coherent regions
Gutekunst, G., Mayer, J., & Rühle, M. (1997) · Philosophical magazine. A/Philosophical magazine. A. Physics of condensed matter. Structure, defects and mechanical properties · doi:10.1080/01418619708209859 · Cited by 110
Mandal, S., Ray, A. K., & Ray, A. K. (2004) · Materials Science and Engineering A · doi:10.1016/j.msea.2004.06.002 · Cited by 109
Joints of carbon fiber-reinforced SiC composites to Ti-alloy brazed by Ag–Cu–Ti short carbon fibers
Lin, G., Huang, J., & Zhang, H. (2007) · Journal of Materials Processing Technology · doi:10.1016/j.jmatprotec.2007.01.031 · Cited by 109
Joining of SiC/SiCf ceramic matrix composites for fusion reactor blanket applications
Colombo, P., Riccardi, B., Donato, A., & Scarinci, G. (2000) · Journal of Nuclear Materials · doi:10.1016/s0022-3115(99)00268-8 · Cited by 109
Investigation of interaction of metal melts and zirconia
Дуров, О. В., Naidich, Y. V., & Kоstyuk, B. D. (2005) · Journal of Materials Science · doi:10.1007/s10853-005-1928-5 · Cited by 103
The Direct Bonding of Metals to Ceramics by the Gas‐Metal Eutectic Method
Burgess, J. F., Neugebauer, C. A., & Flanagan, G. (1975) · Journal of The Electrochemical Society · doi:10.1149/1.2134293 · Cited by 99
The reactive route to ceramic joining: Fabrication, interfacial chemistry and joint properties
dimitris, P. S., Paulasto, M., Ceccone, G., & Stamos, V. (1998) · Acta Materialia · doi:10.1016/s1359-6454(98)80023-2 · Cited by 97
New approaches to joining ceramics for high-temperature applications
Locatelli, M. R., Dalgleish, B. J., Nakashima, K., Tomsia, A. P., & Glaeser, A. M. (1997) · Ceramics International · doi:10.1016/s0272-8842(96)00024-7 · Cited by 96
Investigations of the chemistry and bonding at niobiumsapphire interfaces
Bruley, J., Brydson, R., Müllejans, H., Mayer, J., Gutekunst, G., Mader, W., Knauss, D., & Rühle, M. (1994) · Journal of materials research/Pratt's guide to venture capital sources · doi:10.1557/jmr.1994.2574 · Cited by 93
Joining of machined SiC/SiC composites for thermonuclear fusion reactors
Ferraris, M., Salvo, M., Casalegno, V., Ciampichetti, A., Smeacetto, F., & Zucchetti, M. (2008) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2008.02.020 · Cited by 92
A braze system for sealing metal-supported solid oxide fuel cells
Tucker, M. C., Jacobson, C. P., Jonghe, L. C. D., & Visco, S. J. (2006) · Journal of Power Sources · doi:10.1016/j.jpowsour.2006.02.067 · Cited by 91
Atomic structure of epitaxial Nb-Al2O3interfaces II. Misfit dislocations
Gutekunst, G., Mayer, J., Vítek, V., & Rühle, M. (1997) · Philosophical magazine. A/Philosophical magazine. A. Physics of condensed matter. Structure, defects and mechanical properties · doi:10.1080/01418619708209860 · Cited by 91
Cockeram, B. V. (2005) · Journal of the American Ceramic Society · doi:10.1111/j.1551-2916.2005.00381.x · Cited by 89
Reactions of Ti and Zr with AlN and Al2O3
Loehman, R. E., & Tomsia, A. P. (1992) · Acta Metallurgica et Materialia · doi:10.1016/0956-7151(92)90266-h · Cited by 87
Oxidation behavior of surface-modified titanium for titanium-ceramic restorations
Wang, R. R., & Fung, K. K. (1997) · Journal of Prosthetic Dentistry · doi:10.1016/s0022-3913(97)70168-9 · Cited by 87
Weil, K. S., Coyle, C. A., Darsell, J. T., Xia, G., & Hardy, J. S. (2005) · Journal of Power Sources · doi:10.1016/j.jpowsour.2005.01.053 · Cited by 84
Glass and composite seals for the joining of YSZ to metallic interconnect in solid oxide fuel cells
Smeacetto, F., Salvo, M., Ferraris, M., Casalegno, V., & Asinari, P. (2007) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2007.07.008 · Cited by 84
(2006) · Choice Reviews Online · doi:10.5860/choice.43-4045 · Cited by 83
Comparison between barium and strontium-glass composites for sealing SOFCs
Brochu, M., Gauntt, B. D., Shah, R., Miyake, G., & Loehman, R. E. (2005) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2005.08.002 · Cited by 82
Kinetics of high-temperature spreading
Saiz, E., & Tomsia, A. P. (2005) · Current Opinion in Solid State and Materials Science · doi:10.1016/j.cossms.2006.04.005 · Cited by 82
Armor and heat sink materials joining technologies development for ITER plasma facing components
Barabash, V., Akiba, M., CARDELLA, A., Mazul, I. V., Odegard, B. C., Plöchl, L., Tivey, R., & Vieider, G. (2000) · Journal of Nuclear Materials · doi:10.1016/s0022-3115(00)00120-3 · Cited by 82
Al2O3/Ti interlayer/AISI 304 diffusion bonded joint
Kliauga, A. M., Travessa, D. N., & Ferrante, M. (2001) · Materials Characterization · doi:10.1016/s1044-5803(00)00095-4 · Cited by 81
Synthesis, Properties, and Ternary Phase Stability of M 6 X Compounds in the Ti─Cu─O System
Kelkar, G. P., & Carim, A. H. (1993) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1993.tb06652.x · Cited by 81
Nanostructure of wetting triple line in a Ag–Cu–Ti/Si3N4 reactive system
Nomura, M., Iwamoto, C., & Tanaka, S. (1999) · Acta Materialia · doi:10.1016/s1359-6454(98)00375-9 · Cited by 80
Interfacial reactions in alumina/CuAgTi braze/CuNi system
Valette, C., Devismes, M. F., Voytovych, R., & Eustathopoulos, N. (2004) · Scripta Materialia · doi:10.1016/j.scriptamat.2004.09.008 · Cited by 79
Brazing of SiC to a wrought nickel-based superalloy using CoFeNi(Si, B)CrTi filler metal
Xiong, H., Mao, W., Xie, Y., Guo, W., Li, X., & Cheng, Y. (2007) · Materials Letters · doi:10.1016/j.matlet.2007.03.003 · Cited by 78
Singh, P., Yang, Z. G., Viswanathan, V. V., & Stevenson, J. W. (2004) · Journal of Materials Engineering and Performance · doi:10.1361/10599490419261 · Cited by 78
Glass-ceramic joining and coating of SiC/SiC for fusion applications
Ferraris, M., Salvo, M., Isola, C., Montorsi, M., & Kohyama, A. (1998) · Journal of Nuclear Materials · doi:10.1016/s0022-3115(98)00176-7 · Cited by 78
Novel Refractory Alkaline Earth Silicate Sealing Glasses for Planar Solid Oxide Fuel Cells
Chou, Y., Stevenson, J. W., & Singh, P. (2007) · Journal of The Electrochemical Society · doi:10.1149/1.2733868 · Cited by 76
Equilibrium Phase Diagrams in the Systems PbO–Ag and CuO–Ag
Shao, Z. B., Liu, K. R., Liu, L. Q., Liu, H., & Dou, S. X. (1993) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1993.tb03996.x · Cited by 76
A reaction forming method for joining of silicon carbide-based ceramics
Singh, M. (1997) · Scripta Materialia · doi:10.1016/s1359-6462(97)00233-9 · Cited by 75
Wetting, spreading and joining in the alumina–zirconia–Inconel 738 system
Muolo, M. L., Ferrera, E., Morbelli, L., & Passerone, A. (2003) · Scripta Materialia · doi:10.1016/j.scriptamat.2003.10.015 · Cited by 74
Lee, W., Kwon, B.-D., & Jung, S. (2005) · International Journal of Refractory Metals and Hard Materials · doi:10.1016/j.ijrmhm.2005.04.003 · Cited by 73
Adhesion of porcelain to titanium and a titanium alloy
Suansuwan, N. S., & Swain, M. V. (2003) · Journal of Dentistry · doi:10.1016/s0300-5712(03)00071-x · Cited by 72
Coatings and joining for SiC and SiC-composites for nuclear energy systems
Henager, C. H., Shin, Y., Blum, Y. D., Giannuzzi, L. A., Kempshall, B. W., & Schwarz, S. M. (2007) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2007.03.189 · Cited by 71
Pietrzak, K., Kaliński, D., & Chmielewski, M. (2006) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2006.04.102 · Cited by 70
Ceramic Matrix Composites: Microstructure, Properties and Applications
Low, I. (2006) · CRC Press eBooks · doi:10.1201/9781439823743 · Cited by 69
Direct bonding of copper to aluminum nitride
Entezarian, M., & Drew, R. A. L. (1996) · Materials Science and Engineering A · doi:10.1016/0921-5093(96)10190-8 · Cited by 68
Self-citationFunctionally graded electrical/thermal ceramic systems
Ruys, A. J., Popov, E. B., Sun, D., Russell, J. J., & Murray, C. C. J. (2001) · Journal of the European Ceramic Society · doi:10.1016/s0955-2219(01)00165-0 · Cited by 68
Structure at abrupt copper–alumina interfaces: An ab initio study
Hashibon, A., ELSASSER, C., & Rühle, M. (2005) · Acta Materialia · doi:10.1016/j.actamat.2005.07.036 · Cited by 67
Dual-atmosphere tolerance of Ag–CuO-based air braze
KIM, J., Hardy, J. S., & Weil, S. K. (2006) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2006.08.054 · Cited by 66
Joining of alumina via copper/niobium/copper interlayers
Marks, R. A., Chapman, D. R., Danielson, D. T., & Glaeser, A. M. (2000) · Acta Materialia · doi:10.1016/s1359-6454(00)00229-9 · Cited by 66
Silver-copper oxide based reactive air braze for joining yttria-stabilized zirconia
Kim, J. Y., Hardy, J. S., & Weil, K. S. (2005) · Journal of materials research/Pratt's guide to venture capital sources · doi:10.1557/jmr.2005.0088 · Cited by 66
Choi, S. R., Bansal, N. P., & Garg, A. (2007) · Materials Science and Engineering A · doi:10.1016/j.msea.2007.01.084 · Cited by 65
Structure and Bond Strength of a Copper–Alumina Interface
Yoshino, Y., & Shibata, T. (1992) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1992.tb05500.x · Cited by 65
Wetting and reaction between β′-sialon, stainless steel and Cu–Ag brazing alloys containing Ti
Abed, A. N., Jalham, I. S., & Hendry, A. (2001) · Journal of the European Ceramic Society · doi:10.1016/s0955-2219(00)00211-9 · Cited by 65
Proposal for a new technique to join CFC composites to copper
Appendino, P. M., Ferraris, M., Casalegno, V., Salvo, M., Merola, M., & Grattarola, M. (2005) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2005.09.007 · Cited by 65
Microwave joining of 48% alumina–32% zirconia–20% silica ceramics
Ahmed, A., & Siores, E. (2001) · Journal of Materials Processing Technology · doi:10.1016/s0924-0136(01)00892-5 · Cited by 65
Transient-liquid-phase and liquid-film-assisted joining of ceramics
Sugar, J. D., McKeown, J. T., Akashi, T., Hong, S. M., Nakashima, K., & Glaeser, A. M. (2005) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2005.06.034 · Cited by 64
A wettability study of Cu/Sn/Ti active braze alloys on alumina
Lin, C.-C., Chen, R.-B., & Shiue, R.-K. (2001) · Journal of Materials Science · doi:10.1023/a:1017531730604 · Cited by 63
Novel Metal-Ceramic Joining for Planar SOFCs
Kim, J. Y., Hardy, J. S., & Weil, K. S. (2005) · Journal of The Electrochemical Society · doi:10.1149/1.1896530 · Cited by 63
Joining Mixed Conducting Oxides Using an Air-Fired Electrically Conductive Braze
Hardy, J. S., Kim, J. Y., & Weil, K. S. (2004) · Journal of The Electrochemical Society · doi:10.1149/1.1764782 · Cited by 62
Joining of sintered silicon carbide ceramics for high-temperature applications
Singh, M. (1998) · Journal of Materials Science Letters · doi:10.1023/a:1006568124914 · Cited by 62
Wafer bonding by low-temperature soldering
Lee, C., Huang, W.-F., & Shie, J. (2000) · Sensors and Actuators A Physical · doi:10.1016/s0924-4247(00)00338-1 · Cited by 62
Meier, A. M., Chidambaram, P. R., & Edwards, G. R. (1995) · Journal of Materials Science · doi:10.1007/bf01154485 · Cited by 62
Interfacial Reactions in Glass–Ceramic‐to‐Metal Seals
Donald, I. W., Metcalfe, B. L., & Gerrard, L. A. (2007) · Journal of the American Ceramic Society · doi:10.1111/j.1551-2916.2007.02024.x · Cited by 61
A new method for preparation of direct bonding copper substrate on Al2O3
He, H., Fu, R., Wang, D., Song, X., & Jing, M. (2007) · Materials Letters · doi:10.1016/j.matlet.2007.01.036 · Cited by 61
Fracture properties of interfacially doped Nb-A12O3 bicrystals: I, fracture characteristics
Korn, D., Elßner, G., Cannon, R. M., & Rühle, M. (2002) · Acta Materialia · doi:10.1016/s1359-6454(02)00193-3 · Cited by 60
Metal substrate effects on the thermochemistry of active brazing interfaces
Arróyave, R., & Eagar, T. W. (2003) · Acta Materialia · doi:10.1016/s1359-6454(03)00330-6 · Cited by 59
Role of titanium on the reactive spreading of lead-free solders on alumina
Grémillard, L., Saiz, E., Radmilovic, V. R., & Tomsia, A. P. (2006) · Journal of materials research/Pratt's guide to venture capital sources · doi:10.1557/jmr.2006.0393 · Cited by 59
The role of adsorption and reaction in wetting in the CuAg–Ti/alumina system
Voytovych, R., Ljungberg, L. Y., & Eustathopoulos, N. (2004) · Scripta Materialia · doi:10.1016/j.scriptamat.2004.05.002 · Cited by 59
Ultrasonic welding of ceramics/metals using inserts
Matsuoka, S. (1998) · Journal of Materials Processing Technology · doi:10.1016/s0924-0136(97)00372-5 · Cited by 58
Li, J. Q., Zeng, X. R., Tang, J. N., & Xiao, P. (2003) · Journal of the European Ceramic Society · doi:10.1016/s0955-2219(02)00426-0 · Cited by 58
SEM/EDS evaluation of porcelain adherence to gold‐coated cast titanium
Lee, K. M., Cai, Z., Griggs, J. A., Guiatas, L., Lee, D. J., & Okabe, T. H. (2003) · Journal of Biomedical Materials Research Part B Applied Biomaterials · doi:10.1002/jbm.b.20017 · Cited by 57
An evaluation of the partial transient liquid phase bonding of Si3N4 using Au coated Ni22Cr foils
Ceccone, G., Nicholas, M. G., dimitris, P. S., Tomsia, A. P., Dalgleish, B. J., & Glaeser, A. M. (1996) · Acta Materialia · doi:10.1016/1359-6454(95)00187-5 · Cited by 57
Joining of AlN with metals and alloys
Kara-Slimane, A., Juvé, D., Leblond, E., & Treheux, D. (2000) · Journal of the European Ceramic Society · doi:10.1016/s0955-2219(00)00037-6 · Cited by 55
Microstructural characterization of SiC ceramic and SiC–metal active metal brazed joints
Prakash, P., Mohandas, T., & Raju, P. D. (2005) · Scripta Materialia · doi:10.1016/j.scriptamat.2005.01.034 · Cited by 55
The use of transient FGM interlayers for joining advanced ceramics
Glaeser, A. M. (1997) · Composites Part B Engineering · doi:10.1016/s1359-8368(97)00039-5 · Cited by 55
Green State Joining of SiC without Applied Pressure
Zheng, J., & Akinç, M. (2001) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2001.tb01039.x · Cited by 54
Singh, M. (1998) · Journal of Materials Science · doi:10.1023/a:1004489712447 · Cited by 53
Direct joining of CFC to copper
Appendino, P. M., Ferraris, M., Casalegno, V., Salvo, M., Merola, M., & Grattarola, M. (2004) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2004.04.313 · Cited by 53
Joining of C/C composites to copper
Appendino, P. M., Casalegno, V., Ferraris, M., Grattarola, M., Merola, M., & Salvo, M. (2003) · Fusion Engineering and Design · doi:10.1016/s0920-3796(03)00218-7 · Cited by 53
Triple line ridging and attachment in high-temperature wetting
Saiz, E., Tomsia, A. P., & Cannon, R. M. (2001) · Scripta Materialia · doi:10.1016/s1359-6462(00)00549-2 · Cited by 53
Brazing perovskite ceramics with silver/copper oxide braze alloys
Erskine, K. M., Meier, A. M., & Pilgrim, S. M. (2002) · Journal of Materials Science · doi:10.1023/a:1014912923977 · Cited by 52
Chen, Z., Cao, M., Zhao, Q., & Zou, J. (2004) · Materials Science and Engineering A · doi:10.1016/j.msea.2004.04.012 · Cited by 52
Interfacial microstructure of partial transient liquid phase bonded Si3N4-to-Inconel 718 joints
Kim, J. J., Park, J., & Eagar, T. W. (2002) · Materials Science and Engineering A · doi:10.1016/s0921-5093(02)00402-1 · Cited by 51
Transient liquid-phase bonding of alumina and metal matrix composite base materials
Zhai, Y., North, T. H., & SERRATO-RODRIGUES, J. (1997) · Journal of Materials Science · doi:10.1023/a:1018529228375 · Cited by 49
Wettability of Co–V, and PdNi–Cr–V system alloys on SiC ceramic and interfacial reactions
Xiong, H.-P., Chen, B., Kang, Y.-S., Mao, W., Kawasaki, A., Okamura, H., & Watanabe, R. (2006) · Scripta Materialia · doi:10.1016/j.scriptamat.2006.08.067 · Cited by 49
Lin, G. B., Huang, J., Zhang, H., & Liu, H. (2006) · Science and Technology of Welding & Joining · doi:10.1179/174329306x113235 · Cited by 49
Joining of AlN ceramic to metals using sputtered Al or Ti film
Zhu, S. F., & Włosiński, W. (2001) · Journal of Materials Processing Technology · doi:10.1016/s0924-0136(00)00814-1 · Cited by 48
Novel joining of dissimilar ceramics in the Si3N4–Al2O3 system using polytypoid functional gradients
Lee, C., Zhang, X. F., & Thomas, G. J. (2001) · Acta Materialia · doi:10.1016/s1359-6454(01)00269-5 · Cited by 47
European contribution to the development of the ITER divertor
Merola, M., Danner, W., Palmer, J., Vielder, G., & Wu, C. H. (2003) · Fusion Engineering and Design · doi:10.1016/s0920-3796(03)00214-x · Cited by 47
Ye, J., & Domínguez-Rodríguez, A. (1995) · Scripta Metallurgica et Materialia · doi:10.1016/0956-716x(95)00206-b · Cited by 46
Joining of silicon nitride with a titanium foil interlayer
Lemus-Ruiz, J., & Drew, R. A. L. (2003) · Materials Science and Engineering A · doi:10.1016/s0921-5093(02)00892-4 · Cited by 46
Self-citationExperimental Phase Diagram in the Ag‐Cu 2 O‐CuO System
Nishiura, H., Suzuki, R. O., Ono, K., & Gauckler, L. J. (1998) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1998.tb02604.x · Cited by 46
Wetting behavior of Co based active brazing alloys on SiC and the interfacial reactions
Xiong, H., Li, X., Mao, W., & Cheng, Y. (2003) · Materials Letters · doi:10.1016/s0167-577x(03)00087-9 · Cited by 45
Joining of zirconia to metal with Cu–Ga–Ti and Cu–Sn–Pb–Ti fillers
Дуров, О. В., Kоstyuk, B. D., Shevchenko, A. V., & Naidich, Y. V. (2000) · Materials Science and Engineering A · doi:10.1016/s0921-5093(00)00916-3 · Cited by 45
Ghosh, S., Sharma, A. D., Kundu, P. K., & Basu, R. N. (2008) · Journal of The Electrochemical Society · doi:10.1149/1.2883732 · Cited by 45
Joining of yttria-tetragonal stabilized zirconia polycrystals using nanocrystals
Gutiérrez‐Mora, F., Domínguez-Rodríguez, A., ROUTBORT, J. L., Chaim, R., & Guiberteau, F. (1999) · Scripta Materialia · doi:10.1016/s1359-6462(99)00190-6 · Cited by 45
Molecular dynamics simulations of reactive wetting in metal–ceramic systems
Swiler, T. P., & Loehman, R. E. (2000) · Acta Materialia · doi:10.1016/s1359-6454(00)00228-7 · Cited by 44
Ceramic Substrates For Microelectronic Packaging
Chowdhry, U., & Sleight, A. W. (1987) · Annual Review of Materials Science · doi:10.1146/annurev.ms.17.080187.001543 · Cited by 44
Relief of the Residual Stresses in Ceramic‐Metal Joints by a Layered Braze Structure
Galli, M., Botsis, J., & Janczak‐Rusch, J. (2006) · Advanced Engineering Materials · doi:10.1002/adem.200500233 · Cited by 43
Structure and composition of interlayers in joints between SiC bodies
Pippel, E., Woltersdorf, J., Colombo, P., & Donato, A. (1997) · Journal of the European Ceramic Society · doi:10.1016/s0955-2219(96)00228-2 · Cited by 42
Direct silver bonding – an alternative for substrates in power semiconductor packaging
Schüler, C. C., Stuck, A., Beck, N., Keser, H. E., & ̈ck, U. T. (2000) · Journal of Materials Science Materials in Electronics · doi:10.1023/a:1008942502309 · Cited by 41
Interface Nanostructure of Brazed Silicon Nitride
Iwamoto, C., & Tanaka, S. (1998) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1998.tb02342.x · Cited by 41
Metal–ceramic interfaces: joining silicon nitride–stainless steel
Polanco, R., Pablos, A. D., Miranzo, P., & Osendi, M. I. (2004) · Applied Surface Science · doi:10.1016/j.apsusc.2004.05.290 · Cited by 41
Influence of internal stresses in superplastic joining of zirconia toughened alumina
Gutiérrez‐Mora, F., Goretta, K. C., Majumdar, S., ROUTBORT, J. L., Grimdisch, M., & Domínguez-Rodríguez, A. (2002) · Acta Materialia · doi:10.1016/s1359-6454(02)00161-1 · Cited by 40
Thermal cyclic test of alumina/kovar joint brazed by Ni–Ti active filler
Qiao, G., Zhang, C. G., & Jin, Z. H. (2003) · Ceramics International · doi:10.1016/s0272-8842(02)00081-0 · Cited by 40
Effects of chromium on the interface and bond strength of metal–ceramic joints
Zhang, J. X., Chandel, R. S., & Seow, H. P. (2002) · Materials Chemistry and Physics · doi:10.1016/s0254-0584(02)00072-x · Cited by 40
Liu, H. J., Feng, J. C., & Qian, Y. (2000) · Scripta Materialia · doi:10.1016/s1359-6462(00)00360-2 · Cited by 40
Martinelli, A. E., Drew, R. A. L., Fancello, E. A., Rogge, R. B., & Root, J. H. (1999) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1999.tb02000.x · Cited by 39
Self-citationLee, C. S., Ahn, S., DeJonghe, L. C., & Thomas, G. J. (2006) · Materials Science and Engineering A · doi:10.1016/j.msea.2006.06.139 · Cited by 39
Strength and Microstructure of Silicon Nitride Ceramics Brazed with Nickel‐Chromium‐Silicon Alloys
Hadian, A. M., & Drew, R. A. L. (1996) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1996.tb07926.x · Cited by 39
Self-citationSolid state bonding of Al2O3 with Cu, Ni and Fe: characteristics and properties
Esposito, L., Bellosi, A., Guicciardi, S., & Portu, G. D. (1998) · Journal of Materials Science · doi:10.1023/a:1004397019927 · Cited by 39
Heterogeneous junction of yttria partially stabilized zirconia by superplastic flow
Domínguez-Rodríguez, A., Guiberteau, F., & Jiménez-Melendo, M. (1998) · Journal of materials research/Pratt's guide to venture capital sources · doi:10.1557/jmr.1998.0224 · Cited by 39
Taranets, N. Y., & Jones, H. (2004) · Materials Science and Engineering A · doi:10.1016/j.msea.2004.02.021 · Cited by 38
Bonding at copper–alumina interfaces established by different surface treatments: a critical review
Scheu, C., Gao, M., Oh, S. H., Dehm, G., Klein, S., Tomsia, A. P., & Rühle, M. (2006) · Journal of Materials Science · doi:10.1007/s10853-006-0073-0 · Cited by 38
Wetting of silicon carbide by chromium containing alloys
Xiao, P., & Derby, B. (1998) · Acta Materialia · doi:10.1016/s1359-6454(98)00037-8 · Cited by 38
An investigation into the bonding of orthodontic attachments to porcelain
Larmour, C. J., Bateman, G., & Stirrups, D. R. (2005) · European Journal of Orthodontics · doi:10.1093/ejo/cji072 · Cited by 38
Current understanding of superplastic deformation of Y-TZP and its application to joining
Domínguez-Rodríguez, A., Gutiérrez‐Mora, F., Jiménez-Melendo, M., ROUTBORT, J. L., & Chaim, R. (2001) · Materials Science and Engineering A · doi:10.1016/s0921-5093(00)01368-x · Cited by 37
Ultrasonic welding of ceramic/metal
Matsuoka, S. (1994) · Journal of Materials Processing Technology · doi:10.1016/0924-0136(94)90094-9 · Cited by 36
Rogers, T., Aitken, N., Stribley, K., & Boyd, J. G. (2005) · Sensors and Actuators A Physical · doi:10.1016/j.sna.2005.03.009 · Cited by 36
Joining of alumina using a V-Active filler metal
Rijnders, M. R., & dimitris, P. S. (1999) · Scripta Materialia · doi:10.1016/s1359-6462(99)00273-0 · Cited by 36
Joining alumina/zirconia ceramics
Goretta, K. C., Gutiérrez‐Mora, F., Picciolo, J. J., & ROUTBORT, J. L. (2002) · Materials Science and Engineering A · doi:10.1016/s0921-5093(02)00212-5 · Cited by 36
Effects of a hydrophilic surface in anodic bonding
Lee, D., Ju, B., Jang, J. H., Lee, K.-B., & Oh, M.-H. (1999) · Journal of Micromechanics and Microengineering · doi:10.1088/0960-1317/9/4/305 · Cited by 35
Thermodynamic modelling of wetting at silicon nitride/NiCrSi alloy interfaces
Hadian, A. M., & Drew, R. A. L. (1994) · Materials Science and Engineering A · doi:10.1016/0921-5093(94)90417-0 · Cited by 35
Self-citationReaction products and growth kinetics during diffusion bonding of SiC ceramic to Ni–Cr alloy
Feng, J. C., Liu, H. J., Naka, M., & Schuster, J. C. (2003) · Materials Science and Technology · doi:10.1179/174328413x13789825316707 · Cited by 34
Brazing of alumina ceramics modified by pulsed plasma beams combined with arc PVD treatment
Piekoszewski, J., Krajewski, A., Prokert, F., Senkara, J., Stanisławski, J., Walis, L., Werner, Z., & Włosiński, W. (2003) · Vacuum · doi:10.1016/s0042-207x(02)00660-7 · Cited by 34
Diffusion-limited reactive wetting: effect of interfacial reaction behind the advancing triple line
Hodaj, F., Dezellus, O., Barbier, J. N., Mortensen, A., & Eustathopoulos, N. (2007) · Journal of Materials Science · doi:10.1007/s10853-007-1915-0 · Cited by 33
Reactions of Hf-Ag and Zr-Ag alloys with Al2O3 at elevated temperatures
Loehman, R. E., Hosking, F. M., Gauntt, B. D., Kotula, P. G., & Lu, P. (2005) · Journal of Materials Science · doi:10.1007/s10853-005-1952-5 · Cited by 33
Seamless Joining of Silicon Nitride Ceramics
Gopal, M., Sixta, M. E., Jonghe, L. C. D., & Thomas, G. J. (2001) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2001.tb00730.x · Cited by 33
Reactive brazing study of a silicon nitride to metal joining
Chaumat, G., Drevet, B., & Vernier, L. (1997) · Journal of the European Ceramic Society · doi:10.1016/s0955-2219(97)00059-9 · Cited by 33
Ceramic-metal interfaces and the spreading of reactive liquids
Meier, A. M., Javernick, D. A., & Edwards, G. R. (1999) · JOM · doi:10.1007/s11837-999-0209-1 · Cited by 33
Ag–Cu–Ti Braze Materials for Sealing SOFCs
Kobsiriphat, W., & Barnett, S. A. (2008) · Journal of Electrochemical Energy Conversion and Storage · doi:10.1115/1.2784279 · Cited by 33
Anodic bonding of glass to aluminium
Schjølberg‐Henriksen, K., Poppe, E. U., Moe, S. T., Storås, P., Taklo, M. M. V., Wang, D. T., & Jakobsen, H. (2005) · Microsystem Technologies · doi:10.1007/s00542-005-0040-8 · Cited by 32
Bissig, V., Galli, M., & Janczak‐Rusch, J. (2006) · Advanced Engineering Materials · doi:10.1002/adem.200500234 · Cited by 32
Interdiffusion involved in SHS welding of SiC ceramic to itself and to Ni-based superalloy
Li, S., Duan, H., Liu, S., Zhang, Y., Dang, Z., Zhang, Y., & Wu, C. (2000) · International Journal of Refractory Metals and Hard Materials · doi:10.1016/s0263-4368(00)00008-1 · Cited by 32
The determination of element diffusion in connecting SAE 1040/WC material by brazing
Uzkut, M., Köksal, N. S., & Ünlü, B. S. (2005) · Journal of Materials Processing Technology · doi:10.1016/j.jmatprotec.2005.05.001 · Cited by 32
Microstructure of diffusional zirconia–titanium and zirconia–(Ti–6 wt% Al–4 wt% V) alloy joints
Correia, R. N., Emiliano, J., & Moretto, P. (1998) · Journal of Materials Science · doi:10.1023/a:1004378520526 · Cited by 32
Joining of sialon ceramics by a stainless steel interlayer
Abed, A. N., Hussain, P., Jalham, I. S., & Hendry, A. (2001) · Journal of the European Ceramic Society · doi:10.1016/s0955-2219(01)00227-8 · Cited by 31
Naidich, Y. V. (2005) · Current Opinion in Solid State and Materials Science · doi:10.1016/j.cossms.2005.11.001 · Cited by 31
Comparison Between Micrometer‐ and Nano‐Scale Glass Composites for Sealing Solid Oxide Fuel Cells
Brochu, M., Gauntt, B. D., Shah, R., & Loehman, R. E. (2006) · Journal of the American Ceramic Society · doi:10.1111/j.1551-2916.2005.00804.x · Cited by 31
Li, S., Zhou, Y. Z., Duan, H., Qiu, J., & Zhang, Y. (2003) · Journal of Materials Science · doi:10.1023/a:1026135220737 · Cited by 31
Interfacial reactions in ceramic-metal systems
Loehman, R. E. (1988) · OSTI OAI (U.S. Department of Energy Office of Scientific and Technical Information) · Cited by 30
Reaction kinetics and mechanical properties in the reactive brazing of copper to aluminum nitride
Palit, D., & Meier, A. M. (2006) · Journal of Materials Science · doi:10.1007/s10853-006-0920-z · Cited by 30
Requirements for engineering ceramics in gas turbine engines
Bennett, A. (1986) · Materials Science and Technology · doi:10.1179/mst.1986.2.9.895 · Cited by 30
Effect of Thickness on Direct Bonding of Silicon Nitride to Steel
Suganuma, K., Okamoto, T., Koizumi, M., & Shimada, M. (1985) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1985.tb10139.x · Cited by 30
Mishra, P., Athavale, S. N., Pappachan, A. L., Grover, A. K., Suri, A. K., Sengupta, P., Kale, G. B., Bhanumurthy, K., & De, P. K. (2005) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-005-0240-y · Cited by 30
Joining ZrB2-SiC composites using glass interlayers
Esposito, L., & Bellosi, A. (2005) · Journal of Materials Science · doi:10.1007/s10853-005-2813-y · Cited by 30
The effect of TiO2 on the wetting behavior of silver–copper oxide braze filler metals
Weil, K. S., Kim, J. Y., Hardy, J. S., & Darsell, J. T. (2005) · Scripta Materialia · doi:10.1016/j.scriptamat.2005.12.003 · Cited by 30
Novel methods of brazing dissimilar materials
Suryanarayana, C., Moore, J. J., & Radtke, R. P. (2001) · AM&P Technical Articles · Cited by 30
Effects of thin film Nb interlayer in Cu/sapphire bonds
Liu, W., Elßner, G., & Rühle, M. (2001) · Materials Science and Engineering A · doi:10.1016/s0921-5093(01)01158-3 · Cited by 29
Diffusion bonding of Ti3AlC2 ceramic via a Si interlayer
Yin, X., Li, M., Li, T. P., & Zhou, Y. (2007) · Journal of Materials Science · doi:10.1007/s10853-006-1491-8 · Cited by 29
Cannon, R. M., Korn, D., Elßner, G., & Rühle, M. (2002) · Acta Materialia · doi:10.1016/s1359-6454(02)00194-5 · Cited by 29
Superplastic joining of alumina and zirconia ceramics
Boniecki, M., Kaliński, D., Librant, Z., & Wesołowski, W. (2006) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2006.05.055 · Cited by 28
Substrate effects on the high-temperature oxidation behavior of a gold-based braze filler metal
Weil, K. S., & Rice, J. P. (2005) · Scripta Materialia · doi:10.1016/j.scriptamat.2005.02.010 · Cited by 28
Novel compressive seals for solid oxide fuel cells
Le, S., Sun, K., Zhang, N., An, M., Zhou, D., Zhang, J., & Li, D. (2006) · Journal of Power Sources · doi:10.1016/j.jpowsour.2006.05.016 · Cited by 28
Xiong, H., Dong, W., Chen, B., Kang, Y.-S., Kawasaki, A., Okamura, H., & Watanabe, R. (2007) · Materials Science and Engineering A · doi:10.1016/j.msea.2007.04.026 · Cited by 28
Application of ion implantation to ceramic/metal joining
Samandi, M., Gudze, M., & Evans, P. J. (1997) · Nuclear Instruments and Methods in Physics Research Section B Beam Interactions with Materials and Atoms · doi:10.1016/s0168-583x(96)01152-4 · Cited by 27
Levay, A., Möbus, G., VITEK, V., Rühle, M., & Tichy, G. (1999) · Acta Materialia · doi:10.1016/s1359-6454(99)00273-6 · Cited by 27
Research works printed but not linked: 31
- M. F. Ashby: ‘Cambridge engineering selector v4’; 2007, Cambridge, Granta Design Limited.
- Fernie J. A., 1999, Ind Ceram, 19, 172
- Imai H., 2006, JSME Int. J. Ser. A, 49, 450
- Lindner P., 2004, Solid State Technol, 47, 55
- Ito M., 1991, US Patent 5073085
- Duvall D. S., 1974, Weld, 1, 203
- 10.1016/j.ijrmhm.2004.01.003 · doi:10.1016/j.ijrmhm.2004.01.003
- Fernie J. A., 1999, Mater. World, 7, 686
- Loehman R. E., 1989, Am. Ceram. Soc. Bull, 68, 891
- Eustathopoulos N., 1998, Acta Mater, 46, 2319
- Sobczak N., 2005, Curr. Opin. Solid State Mater. Set, 9, 241 — 253
- Derby B., 2004, Interf Set, 12, 29
- Ormston D. R., 2001, ‘The particulate reinforcement of active broze alloys for joining silicon carbide’, Cambridge
- Knowles K. M., 2002, Ceram. Trans, 138, 103
- Nolte H. J., 1954, US Patent 2667432
- Kim J. Y., 2005, J. Electrochem. Soc, 152, J52—J58
- Paulasto M., 1997, Ceram. Trans, 77, 91
- Peteves S. D., 1998, Acta. Mater, 46, 2407
- Reichel U., 1999, Z. Metallkd, 90, 699
- Gasse A., 1997, World Patent WO 9747568
- Chaumat G., 2001, European Patent EP 806402
- Gasse A., 2008, US Patent 7318547
- Pask J. A., 1971, Proc. Porcelain Enamel Inst. Tech. Forum, 33, 1
- Pask J. A., 1987, Am. Ceram. Soc. Bull, 66, 1587
- Ghosh S., 2008, J. Electrochem. Soc, 155, B473—B478
- Kobsiriphat W., 2008, J. Fuel Cell Set Technot, 011002
- Henager C. H., J. Nucl. Mater, 2007, 367
- Appendino P., 1563, J. Nucl. Mater, 2004, 329
- Barabash V., J. Nucl. Mater, 2000, 283
- Ferraris M., 1546, J. Nucl. Mater, 1998, 258
- Suryanarayana C., 2001, Adv. Mater. Processes, 159, 29
Cited by
Advanced ceramic components: Materials, fabrication, and applications
Ayode Otitoju, T., Ugochukwu Okoye, P., Chen, G., Li, Y., Onyeka Okoye, M., & Li, S. (2020) · Journal of Industrial and Engineering Chemistry · doi:10.1016/j.jiec.2020.02.002 · Cited by 368
Ultrafast laser welding of ceramics
Penilla, E. H., Devia-Cruz, L. F., Wieg, A. T., Martinez-Torres, P., Cuando-Espitia, N., Sellappan, P., Kodera, Y., Aguilar, G., & Garay, J. E. (2019) · Science · doi:10.1126/science.aaw6699 · Cited by 224
Ultra-high temperature ceramics: Aspiration to overcome challenges in thermal protection systems
Nisar, A., Hassan, R., Agarwal, A. K., & Balani, K. (2021) · Ceramics International · doi:10.1016/j.ceramint.2021.12.199 · Cited by 197
Room-temperature exceptional plasticity in defective Bi 2 Te 3 -based bulk thermoelectric crystals
Deng, T., Gao, Z., Li, Z., Qiu, P., Li, Z., Yuan, X., Ming, C., Wei, T.-R., Chen, L., & Shi, X. (2024) · Science · doi:10.1126/science.adr8450 · Cited by 186
Ali, M., Knowles, K. M., Mallinson, P. M., & Fernie, J. A. (2015) · Acta Materialia · doi:10.1016/j.actamat.2015.05.048 · Cited by 161
Self-citation
Metadata
- Authors
- Fernie, J. A., Drew, R. A. L., & Knowles, K. M.
- Venue
- International Materials Reviews
- Publisher
- SAGE Publications
- Published
- 2009-09
- Volume
- 54
- Issue
- 5
- Pages
- 283-331
- ISSN
- 0950-6608 (ISSN-L)
- 1743-2804
- OpenAlex
- W1985755219
- Cited by
- 282
- References
- 328
- FWCI
- 10.33
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.