Joining of engineering ceramics
The DOI matches its Crossref record; 324 of the 328 references it cites were found in a registry or an index.
Abstract
Engineering ceramics such as alumina, zirconia, silicon nitride and silicon carbide can now be manufactured reliably with reproducible properties. As such, they are of increasing interest to industry, particularly for use in demanding environments, where their thermomechanical performance is of critical importance, with applications ranging from fuel cells to cutting tools. One aspect common to virtually all applications of engineering ceramics is that eventually they must be joined with another material, most usually a metal. The joining of engineering ceramics to metals is not always easy. There are two main considerations. The first consideration is the basic difference in atomic bonding: the ionic or covalent bonding of the ceramic, compared to the metallic bond. The second consideration is the mismatch in the coefficient of thermal expansion. In general, ceramics have a lower coefficient of thermal expansion than metals and, if high tensile forces are produced in the ceramic, either as a consequence of operating conditions or from the joining procedure itself, failure can occur. The plethora of joining processes available will be reviewed in this article, placing them in context from both an academic and commercial perspective. Comment will be made on research reporting advances on known technology, as well as introducing ‘newer’ technologies developed over the last 10 years. Finally, reviews and commentary will be made on the potential applications of the various joining processes in the commercial environment.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“Ceramic joining techniques are numerous and technically challenging, and often subject the entire sample to extreme conditions, such as high temperatures and/or vacuums [223].”
From Ultrafast Laser Additive Manufacturing: A Review (2023) · cites this paper as [223]
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Items 201–324 of 324
Influence of Ti on wetting of AlN by Ni-base alloys
Koltsov, A. V., Dumont, M., Hodaj, F., & Eustathopoulos, N. (2005) · Materials Science and Engineering A · doi:10.1016/j.msea.2005.09.003 · Cited by 27
Olesińska, W., Kaliński, D., Chmielewski, M., Diduszko, R., & Włosiński, W. (2006) · Journal of Materials Science Materials in Electronics · doi:10.1007/s10854-006-0024-1 · Cited by 27
Barlak, M., Olesińska, W., Piekoszewski, J., Werner, Z., Chmielewski, M., JAGIELSKI, J., Kaliński, D., Sartowska, B., & Borkowska, K. (2007) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2006.01.090 · Cited by 27
Meier, A. M., Chidambaram, P. R., & Edwards, G. R. (1998) · Acta Materialia · doi:10.1016/s1359-6454(98)00100-1 · Cited by 27
Yost, F. G. (2000) · Scripta Materialia · doi:10.1016/s1359-6462(00)00298-0 · Cited by 27
Design, Fabrication, and Testing of Ceramic Joints for High Temperature SiC/SiC Composites
Singh, M., & Lara‐Curzio, E. (2000) · Journal of Engineering for Gas Turbines and Power · doi:10.1115/1.1362664 · Cited by 27
Xiong, H., Mao, W., Xie, Y., Chen, B., Guo, W.-L., Li, X., & Cheng, Y. (2007) · Journal of materials research/Pratt's guide to venture capital sources · doi:10.1557/jmr.2007.0370 · Cited by 26
Joining of ceramics using oxide and oxynitride glasses in the Y-Sialon system
Weldon, L. M., Hampshire, S., & Pomeroy, M. J. (1997) · Journal of the European Ceramic Society · doi:10.1016/s0955-2219(97)00056-3 · Cited by 26
Microstructure and mechanical strength of diffusion-bonded silicon nitride–molybdenum joints
Martinelli, A. E., & Drew, R. A. L. (1999) · Journal of the European Ceramic Society · doi:10.1016/s0955-2219(99)00027-8 · Cited by 26
Self-citationInfluence of oxygen on the joining between copper and aluminium nitride
Jarrige, J., Joyeux, T., Lecompte, J. P., & Labbe, J. C. (2006) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2006.02.028 · Cited by 26
Mechanical behavior and microstructural analysis of alumina–titanium brazed interfaces
Nono, M. D. C. D. A., Barroso, J. J., & Castro, P. J. (2006) · Materials Science and Engineering A · doi:10.1016/j.msea.2006.07.113 · Cited by 25
An upgraded brazing technique to manufacture ceramic-metal joints for UHV applications
Murari, A., Albrecht, H., Barzon, A., Curiotto, S., & Lotto, L. (2002) · Vacuum · doi:10.1016/s0042-207x(02)00504-3 · Cited by 25
Constrained yielding in niobium single crystals bonded to sapphire
Soyez, G., Elßner, G., Rühle, M., & Raj, R. (1998) · Acta Materialia · doi:10.1016/s1359-6454(98)00028-7 · Cited by 25
High-temperature tolerance of the silver-copper oxide braze in reducing and oxidizing atmospheres
Kim, J. Y., Hardy, J. S., & Weil, K. S. (2006) · Journal of materials research/Pratt's guide to venture capital sources · doi:10.1557/jmr.2006.0178 · Cited by 25
Kruzic, J. J., Marks, R. A., Yoshiya, M., Glaeser, A. M., Cannon, R. M., & Ritchie, R. O. (2002) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2002.tb00491.x · Cited by 24
Transient liquid phase bonding of alumina to alumina via boron oxide interlayer
Chang, L.-S., & Huang, C.-F. (2004) · Ceramics International · doi:10.1016/j.ceramint.2003.11.018 · Cited by 24
Lessing, P. A., Erickson, A. W., & Kunerth, D. C. (2000) · Journal of Materials Science · doi:10.1023/a:1004766424209 · Cited by 23
Fabrication and characterisation of silicon carbide/superalloy interfaces
Li, J., & Xiao, P. (2003) · Journal of the European Ceramic Society · doi:10.1016/s0955-2219(03)00369-8 · Cited by 23
Status of CFC development in Europe for ITER
Peacock, A. T., Merola, M., Pick, M. A., & Tivey, R. (2007) · Physica Scripta · doi:10.1088/0031-8949/2007/t128/005 · Cited by 23
Joining of advanced ceramics in green state
Wang, L., & Aldinger, F. (2002) · Materials Letters · doi:10.1016/s0167-577x(01)00536-5 · Cited by 23
Ion implantation as a pre-treatment method of AlN substrate for direct bonding with copper
Barlak, M., Olesińska, W., Piekoszewski, J., Chmielewski, M., JAGIELSKI, J., Kaliński, D., Werner, Z., & Sartowska, B. (2005) · Vacuum · doi:10.1016/j.vacuum.2005.01.027 · Cited by 22
Joining of Alumina Ceramics Using Nanocrystalline Tape Cast Interlayer
Chaim, R., & Ravi, B. G. (2000) · Journal of materials research/Pratt's guide to venture capital sources · doi:10.1557/jmr.2000.0248 · Cited by 22
Silver–Glass Composite for High Temperature Sealing
Deng, X., Duquette, J., & Petric, A. (2007) · International Journal of Applied Ceramic Technology · doi:10.1111/j.1744-7402.2007.02131.x · Cited by 22
Kim, J. Y., & Weil, K. S. (2007) · Journal of the American Ceramic Society · doi:10.1111/j.1551-2916.2007.02075.x · Cited by 22
Anodic oxidation during electrostatic bonding
van Helvoort, A. T. J., Knowles, K. M., Holmestad, R., & Fernie, J. A. (2004) · The Philosophical Magazine A Journal of Theoretical Experimental and Applied Physics · doi:10.1080/14786430310001637015 · Cited by 22
Self-citationDing, W., Xu, J., Shen, M., Fu, Y., & Xiao, B. (2006) · Materials Science and Technology · doi:10.1179/174328406x79315 · Cited by 21
Ceramic joining through reactive wetting of alumina with calcium aluminate refractory cements
Geetha, K., Umarji, A. M., & Kutty, T. R. N. (2000) · Bulletin of Materials Science · doi:10.1007/bf02720077 · Cited by 21
High temperature wetting: Insights from atomistic simulations
Webb, E. B., Hoyt, J. J., & Grest, G. S. (2005) · Current Opinion in Solid State and Materials Science · doi:10.1016/j.cossms.2006.03.003 · Cited by 21
CMC integration and demonstration for gas turbine engines (CINDERS)
Barnard, P. A., Henderson, M. B., & Rhodes, N. (2004) · Applied Thermal Engineering · doi:10.1016/j.applthermaleng.2003.11.019 · Cited by 21
Advanced Structural Ceramics --From Research to Applications--
Mizutani, T., Matsuhiro, K., & YAMAMOTO, N. (2006) · Journal of the Ceramic Society of Japan · doi:10.2109/jcersj.114.905 · Cited by 21
Deposition of solder for micro-joining on M.E.M.S. components by means of magnetron sputtering
Lugscheider, E., Bobzin, K., & Lake, M. K. (2001) · Surface and Coatings Technology · doi:10.1016/s0257-8972(01)01182-3 · Cited by 21
Liquid‐Film‐Assisted Formation of Alumina/Niobium Interfaces
Sugar, J. D., McKeown, J. T., Marks, R. A., & Glaeser, A. M. (2002) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2002.tb00490.x · Cited by 21
The Al2O3-t itanium adhesion in the view of the diffusion bonding process
Travessa, D. N., & Ferrante, M. (2002) · Journal of Materials Science · doi:10.1023/a:1020669022776 · Cited by 20
Experimental determination of phase equilibria in the silver–copper oxide system at high temperature
Darsell, J. T., & Weil, K. S. (2007) · Scripta Materialia · doi:10.1016/j.scriptamat.2007.01.050 · Cited by 20
Nascimento, R. M., Martinelli, A. E., Buschinelli, A. J. A., & Sigismund, E. (2007) · Materials Science and Engineering A · doi:10.1016/j.msea.2007.02.033 · Cited by 20
Hardy, J. S., Kim, J. Y., Thomsen, E. C., & Weil, K. S. (2007) · Journal of The Electrochemical Society · doi:10.1149/1.2430691 · Cited by 20
PTLPB of Si3N4 to FA-129 using nickel as a core interlayer
Brochu, M., Pugh, M., & Drew, R. A. L. (2004) · International Journal of Refractory Metals and Hard Materials · doi:10.1016/s0263-4368(04)00004-6 · Cited by 20
Self-citationEffects of adhesive composition on bond strength of joined silicon nitride ceramics
Xie, R., Huang, L., Fu, X., & Chen, Y. (1998) · Journal of the European Ceramic Society · doi:10.1016/s0955-2219(98)80011-3 · Cited by 19
Scanning acoustic microscopy study of titanium-ceramic interface of dental restorations
Wang, R. R., Meyers, E., & Katz, J. L. (1998) · Journal of Biomedical Materials Research · doi:10.1002/(sici)1097-4636(19981215)42:4<508::aid-jbm5>3.0.co;2-v · Cited by 19
Pan, W., Li, J., & Chen, J. (2002) · Thin Solid Films · doi:10.1016/s0040-6090(02)00950-1 · Cited by 19
Öztürk, K., Basu, R. N., Randall, C. A., & Mayo, M. J. (1999) · Scripta Materialia · doi:10.1016/s1359-6462(99)00271-7 · Cited by 19
Development of silver–metal oxide reactive air braze alloys for electroding PZT ceramics
Pavlina, E. J., Meier, A. M., Monteleone, P., & Weigner, J. D. (2006) · Journal of Materials Science · doi:10.1007/s10853-006-1381-0 · Cited by 19
The effect of composition on the microwave bonding of alumina ceramics
Binner, J. G. P., Fernie, J. A., Whitaker, P. A., & Cross, T. E. (1998) · Journal of Materials Science · doi:10.1023/a:1004319100692 · Cited by 19
Self-citationJoining of ceramic oxides by liquid wetting and capillarity
Esposito, L., & Bellosi, A. (2001) · Scripta Materialia · doi:10.1016/s1359-6462(01)01092-2 · Cited by 18
Jiménez‐Piqué, E., Domínguez-Rodríguez, A., Martínez-Fernández, J., Lara‐Curzio, E., & Singh, M. (2000) · Journal of the European Ceramic Society · doi:10.1016/s0955-2219(99)00154-5 · Cited by 18
Direct Welding of Metals and Ceramics by Ultrasonic Vibration
Imai, H., & Matsuoka, S.-I. (2006) · JSME International Journal Series A · doi:10.1299/jsmea.49.444 · Cited by 18
Zhou, F., Suh, C., & Kim, S. (2002) · Materials Letters · doi:10.1016/s0167-577x(01)00619-x · Cited by 18
Nanostructures at Electrostatic Bond Interfaces
van Helvoort, A. T. J., Knowles, K. M., & Fernie, J. A. (2003) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2003.tb03553.x · Cited by 18
Self-citationJoining of silicon nitride ceramic composites with Y2O3–Al2O3–SiO2 mixtures
Zhou, F. (2002) · Journal of Materials Processing Technology · doi:10.1016/s0924-0136(02)00277-7 · Cited by 17
Comparison between two processes using oxygen in the Cu/AlN bonding
Jarrige, J., Joyeux, T., Lecompte, J. P., & Labbe, J. C. (2006) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2006.04.037 · Cited by 17
Bonding of silicon nitride ceramics using Fe–Ni/Cu/Ni/Cu/Fe–Ni interlayers
Fang, F., Chen, Z., Lou, H., & Sui, R. (2001) · Materials Letters · doi:10.1016/s0167-577x(00)00232-9 · Cited by 17
Microstructure of brazed joints between mechanically metallized Si3N4 and stainless steel
Nascimento, R. M., Martinelli, A. E., Buschinelli, A. J. A., Reisgen, U., & Remmel, J. (2005) · Journal of Materials Science · doi:10.1007/s10853-005-0920-4 · Cited by 17
Non-destructive characterization of carbon fiber composite/Cu joints for nuclear fusion applications
Casalegno, V., Salvo, M., Ferraris, M., Smeacetto, F., Merola, M., & Bettuzzi, M. (2008) · Fusion Engineering and Design · doi:10.1016/j.fusengdes.2008.04.005 · Cited by 17
Nanostructured gamma-alumina formed during anodic bonding of Al/Glass
Xing, Q., & Sasaki, G. (2007) · Solid State Ionics · doi:10.1016/j.ssi.2006.12.012 · Cited by 17
Reactive brazing of ceria to an ODS ferritic stainless steel
Khan, T. I., & Al-Badri, A. (2003) · Journal of Materials Science · doi:10.1023/a:1023917504820 · Cited by 16
CHEMICAL REACTIONS AND ADHERENCE AT GLASS-METAL INTERFACES
Pask, J. A. (1971) · eScholarship (California Digital Library) · Cited by 16
Reaction and bonding of Hf and Zr containing alloys to alumina and silica
Loehman, R. E., Gauntt, B. D., Hosking, F. M., Kotula, P. G., Rhodes, S. K., & Stephens, J. J. (2003) · Journal of the European Ceramic Society · doi:10.1016/s0955-2219(03)00292-9 · Cited by 16
A capacitor discharge technique with optimized energy for joining ceramics
Takaki, K., Fujimaki, Y., Takada, Y., Itagaki, M., Fujiwara, T., Ohshima, S., Oyama, K., Takahashi, I., & Kuwashima, T. (2002) · Vacuum · doi:10.1016/s0042-207x(01)00456-0 · Cited by 16
Hu, Y.-Q., Zhao, Y.-P., & Yu, T. (2007) · Materials Science and Engineering A · doi:10.1016/j.msea.2006.09.155 · Cited by 16
Capacitor‐Discharge Joining of Oxide Ceramics
Turan, S., Bucklow, I. A., & Wallach, E. R. (1999) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1999.tb01902.x · Cited by 16
Evaluation of Si3N4 joints: bond strength and microstructure
Xie, R., Huang, L., Chen, Y., & Fu, X. (1999) · Journal of Materials Science · doi:10.1023/a:1004507124881 · Cited by 15
Joining ceramic to metal using a powder metallurgy method for high temperature applications
Li, J., & Xiao, P. (2001) · Journal of Materials Science · doi:10.1023/a:1017503503711 · Cited by 15
A fritless copper conductor system for power electronic applications
Reicher, R., Smetana, W., Schuster, J. C., & Adlaßnig, A. (2001) · Microelectronics Reliability · doi:10.1016/s0026-2714(00)00264-x · Cited by 15
Ab initio study of electronic densities of states at copper–alumina interfaces
Hashibon, A., ELSASSER, C., & Rühle, M. (2007) · Acta Materialia · doi:10.1016/j.actamat.2006.10.026 · Cited by 15
Ag–Al based air braze for high temperature electrochemical devices
KIM, J., Hardy, J. S., & Weil, K. S. (2006) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2006.08.055 · Cited by 15
Application of Ceramics to Turbocharger Rotors for Passenger Cars
Katano, Y., Ando, M., Itoh, T., & Sasaki, M. (1993) · Journal of Engineering for Gas Turbines and Power · doi:10.1115/1.2906692 · Cited by 15
An investigation into microwave bonding mechanisms via a study of silicon carbide and zirconia
Binner, J. G. P., Fernie, J. A., & Whitaker, P. A. (1998) · Journal of Materials Science · doi:10.1023/a:1004367016622 · Cited by 14
Self-citationDiffusion bonding of silicon nitride to titanium
Lemus-Ruiz, J., & Drew, R. A. L. (2000) · British Ceramic Transactions · doi:10.1179/096797800680947 · Cited by 14
Self-citationChou, Y., Stevenson, J. W., Hardy, J. S., & Singh, P. (2006) · Journal of The Electrochemical Society · doi:10.1149/1.2210571 · Cited by 14
Joining particulate and whisker ceramic composites by plastic flow
Chen, N., Gutiérrez‐Mora, F., Koritala, R. E., Goretta, K. C., ROUTBORT, J. L., & Pan, J. (2002) · Composite Structures · doi:10.1016/s0263-8223(02)00077-6 · Cited by 14
The Triple Line in Reactive Wetting
Yost, F. G. (1998) · Scripta Materialia · doi:10.1016/s1359-6462(98)00030-x · Cited by 13
Taranets, N. Y., & Jones, H. (2005) · Journal of Materials Science · doi:10.1007/s10853-005-1958-z · Cited by 13
Loehman, R. E., & Kotula, P. G. (2004) · Journal of the American Ceramic Society · doi:10.1111/j.1551-2916.2004.00055.x · Cited by 13
Influence of Metal Foil Width on Bonding Strength in Capacitor Discharge Ceramics Joining
Takaki, K., Mikami, Y., Itagaki, M., Mukaigawa, S., Fujiwara, T., & Nakamura, S. (2006) · IEEE Transactions on Plasma Science · doi:10.1109/tps.2006.883409 · Cited by 13
Development of Brazing Technology for Ceramic Turbocharger Rotors
Ito, M., Ishida, N., & Kato, N. (1988) · SAE technical papers on CD-ROM/SAE technical paper series · doi:10.4271/880704 · Cited by 13
Wang, J., Li, Y., & Gerasimov, S. A. (2007) · Bulletin of Materials Science · doi:10.1007/s12034-007-0067-9 · Cited by 12
Identification and characterization of (Ti, Cu, A1)6N, a new η nitride phase
Carim, A. H. (1989) · Journal of materials research/Pratt's guide to venture capital sources · doi:10.1557/jmr.1989.1456 · Cited by 12
Development of a Copper Oxide‐Silver Braze for Ceramic Joining
Kim, J. Y., & Weil, K. S. (2006) · Ceramic transactions /Ceramic transactions · doi:10.1002/9781118405802.ch6 · Cited by 11
Texture change in Ni and Cu foils on diffusion bonding to zirconia
Mun, J., Derby, B., & Sutton, A. P. (1997) · Scripta Materialia · doi:10.1016/s1359-6462(96)00330-2 · Cited by 11
Effect of adhesive composition on bonding of silicon nitride ceramic
Zhou, F. (2003) · Ceramics International · doi:10.1016/s0272-8842(02)00118-9 · Cited by 11
Taranets, N. Y., & Jones, H. (2004) · Journal of Materials Science · doi:10.1023/b:jmsc.0000040082.16505.be · Cited by 11
Use of aluminum in air-brazing aluminum oxide
Kim, J. Y., Hardy, J. S., & Weil, K. S. (2004) · Journal of materials research/Pratt's guide to venture capital sources · doi:10.1557/jmr.2004.0221 · Cited by 11
Mullite/Mo interfaces formed by intrusion bonding
Bartolomé, J. F., Díaz, M., Moya, J. S., Saiz, E., & Tomsia, A. P. (2003) · Journal of the European Ceramic Society · doi:10.1016/s0955-2219(03)00339-x · Cited by 10
Diffusion bonding of SiC ceramic to TiAl-based alloy
Huijie, L., & Jicai, F. (2001) · Journal of Materials Science Letters · doi:10.1023/a:1010950427079 · Cited by 10
Effects of interlayer composition on joining of 25%CePO4/ZrO2–ZrO2 ceramics on green state
Gao, H. Y., Liu, J., Du, H., Liu, M., Wang, L., & Huo, W. (2004) · Ceramics International · doi:10.1016/j.ceramint.2003.09.017 · Cited by 10
Bonding strength of alumina tiles joined using capacitor discharge technique
Takaki, K., Takada, Y., Itagaki, M., Mukaigawa, S., Fujiwara, T., Ohshima, S., Oyama, K., Takahashi, I., & Kuwashima, T. (2003) · Surface and Coatings Technology · doi:10.1016/s0257-8972(03)00167-1 · Cited by 10
Iijima, M., & Watanabe, Y. (2001) · Japanese Journal of Applied Physics · doi:10.1143/jjap.40.3789 · Cited by 10
Effect of Pd additions on the invariant reactions in the Ag−CuOx system
Darsell, J. T., & Weil, K. S. (2006) · Journal of Phase Equilibria and Diffusion · doi:10.1361/105497106x92862 · Cited by 10
Neutron reflection studies of titanium segregation to metal–ceramic interfaces
Derby, B., Xiao, P., & Webster, J. R. P. (1998) · Physica B Condensed Matter · doi:10.1016/s0921-4526(98)00254-3 · Cited by 10
Winn, A. J., Derby, B., Webster, J. R. P., & Holt, S. A. (2004) · Journal of the American Ceramic Society · doi:10.1111/j.1551-2916.2004.00279.x · Cited by 10
Reichel, U., & Warlimont, H. (1999) · International Journal of Materials Research (formerly Zeitschrift fuer Metallkunde) · doi:10.1515/ijmr-1999-900909 · Cited by 10
The interfacial microstructure of zirconia and MaCor™ joined using spin-on interlayers
Zeng, L., Case, E. D., & Crimp, M. A. (2001) · Materials Science and Engineering A · doi:10.1016/s0921-5093(00)01955-9 · Cited by 9
Ultrasonic Welding of Thin Alumina and Aluminum Using Inserts
ISHIKURO, T., & Matsuoka, S. (2005) · JSME International Journal Series A · doi:10.1299/jsmea.48.317 · Cited by 9
High-temperature capillarity and interfacial phenomena
Sobczak, N., Singh, M., & Asthana, R. (2005) · Current Opinion in Solid State and Materials Science · doi:10.1016/j.cossms.2006.07.006 · Cited by 9
Vacuum diffusion bonding of TiB2cermet to TiAl based alloys
Li, Z. R., Feng, J. C., & Cao, J. X. (2004) · Materials Science and Technology · doi:10.1179/026708304225016798 · Cited by 9
Characterisation of the join of electric discharge pulse welded ceramics
Binner, J. G. P., Davis, P. A., Fernie, J. A., & Dubovetskü, I. D. (1995) · Journal of the European Ceramic Society · doi:10.1016/0955-2219(95)00076-7 · Cited by 9
Self-citationJoining Si 3 N 4 ‐Based Ceramics with Oxidation‐Formed Surface Layers
Plucknett, K. P. (2000) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2000.tb01662.x · Cited by 9
Bonding of stabilised zirconia (Y-TZP) by means of nano Y-TZP particles
Cina, B., & Eldror, I. (2001) · Materials Science and Engineering A · doi:10.1016/s0921-5093(00)01815-3 · Cited by 9
High-temperature brazing for reliable tungsten–CFC joints
Koppitz, T., Pintsuk, G., Reisgen, U., Remmel, J., Hirai, T., Sievering, R., Rojas, Y. A., & Casalegno, V. (2007) · Physica Scripta · doi:10.1088/0031-8949/2007/t128/034 · Cited by 9
Vila, M., Prieto, C., Miranzo, P., Osendi, M. I., Río, J. M. D., & Pérez-Castellanos, J. L. (2005) · Journal of the American Ceramic Society · doi:10.1111/j.1551-2916.2005.00485.x · Cited by 9
Joining of ZrO2-4.5 wt% Y2O3 (Y-TZP) ceramics using nanocrystalline tape cast interlayers
Ravi, B. G., & Chaim, R. (2002) · Journal of Materials Science · doi:10.1023/a:1013804301381 · Cited by 9
Interface structure and strain development during compression tests of Al2O3/Nb/Al2O3 sandwiches
Scheu, C., Liu, Y., Oh, S. H., Brunner, D., & Rühle, M. (2006) · Journal of Materials Science · doi:10.1007/s10853-006-0728-x · Cited by 8
Derby, B., & Holt, S. A. (2004) · Interface Science · doi:10.1023/b:ints.0000012292.19049.e2 · Cited by 8
The characterization of metal/ceramic interfaces using specular neutron reflection
Xiao, P., Derby, B., Webster, J. R. P., & Penfold, J. (1997) · Acta Materialia · doi:10.1016/s1359-6454(96)00170-x · Cited by 8
Development of Ceramic Turbocharger Rotors for High-Temperature Use
KAWASE, H., Kato, K., MATSUHISA, T., & Mizuno, T. (1993) · Journal of Engineering for Gas Turbines and Power · doi:10.1115/1.2906681 · Cited by 7
Bonding of alumina to steel using copper interlayer
Włosiński, W., Olesińska, W., & Pietrzak, K. (1996) · Journal of Materials Processing Technology · doi:10.1016/0924-0136(96)85102-8 · Cited by 7
Bonding and Integration of Silicon Carbide Based Materials for Multifunctional Applications
Singh, M., & Halbig, M. C. (2007) · Key engineering materials · doi:10.4028/www.scientific.net/kem.352.201 · Cited by 7
Corrosion Behaviour of Metal/Ceramic Interfaces in Physiological Solutions
Rocha, L. A., Ferreira, T. O., & Monteiro, A. (2002) · Key engineering materials · doi:10.4028/www.scientific.net/kem.230-232.479 · Cited by 7
Vila, M., Martínez, M., Prieto, C., Miranzo, P., Osendi, M. I., Terry, A. E., & Vaughan, G. (2004) · Powder Technology · doi:10.1016/j.powtec.2004.09.035 · Cited by 6
Characterisation of liquid metal/solid ceramic interfaces by neutron reflection
Derby, B., Edwards, R., Webster, J. R. P., & Xiao, P. (1998) · Acta Materialia · doi:10.1016/s1359-6454(98)80020-7 · Cited by 6
High temperature neutron reflection spectroscopy of liquid metal/ceramic interfaces
Edwards, R., Derby, B., Xiao, P., & Webster, J. P. R. (1998) · Physica B Condensed Matter · doi:10.1016/s0921-4526(98)00256-7 · Cited by 6
Grain growth and texture changes in a Ni foil during diffusion bonding to ZrO2
Mun, J., Sutton, A. P., & Derby, B. (1997) · Philosophical magazine. A/Philosophical magazine. A. Physics of condensed matter. Structure, defects and mechanical properties · doi:10.1080/01418619708209975 · Cited by 6
Reactive Joining of Alumina by Oxidation of Al Interlayers
Bengisu, M., & Fahrenholtz, W. G. (2004) · Key engineering materials · doi:10.4028/www.scientific.net/kem.264-268.655 · Cited by 5
High-temperature neutron reflectometry of liquid metal-ceramic interfaces
Edwards, R., Derby, B., Webster, J. R. P., & Xiao, P. (1999) · Journal of Physics D Applied Physics · doi:10.1088/0022-3727/32/18/302 · Cited by 5
Dielectric window for reactor like ICRF vacuum transmission line
Heikinheimo, L., Heikkinen, J. A., Linden, J., Kaye, A., Orivuori, S., Saarelma, S., Tähtinen, S., Walton, R., & Wasastjerna, F. (2001) · Fusion Engineering and Design · doi:10.1016/s0920-3796(01)00216-2 · Cited by 5
Mechanical properties of the Ni filler metal layer in Si 3 N 4 joints measured by nanoindentation
Miranzo, P., Osendi, M. I., & Vergara, I. (2004) · Surface and Interface Analysis · doi:10.1002/sia.1912 · Cited by 5
Measurement of dielectric properties of alumina at high temperature while exposed to microwaves
Aguilar, J. A., & Pearce, J. A. (2003) · British Ceramic Transactions · doi:10.1179/096797803225009274 · Cited by 4
Ceramics in engines – process requirements and research activity
Riley, F. L., & Milsom, S. J. (1986) · Materials Science and Technology · doi:10.1179/mst.1986.2.9.891 · Cited by 4
Modelling of the Current-Time Characteristics in Anodic Bonding
Knowles, K. M. (2006) · Advances in science and technology · doi:10.4028/www.scientific.net/ast.45.1558 · Cited by 2
Self-citationRequirements for ceramics in reciprocating engines
Parker, D. A. (1986) · Materials Science and Technology · doi:10.1179/mst.1986.2.9.900 · Cited by 2
The Effect of Metal Coating on the Strength of Capacitor-Discharge Joining of Oxide Ceramics
Turan, S., Turan, D., Bucklow, I. A., & Wallach, E. R. (2004) · Key engineering materials · doi:10.4028/www.scientific.net/kem.264-268.687 · Cited by 2
Organization and financing of ceramics research and development – an overview
Sinclair, T. J. (1986) · Materials Science and Technology · doi:10.1179/mst.1986.2.9.889 · Cited by 2
Active soft solder deposition by magnetron-sputter-ion-plating (MSIP)-PVD-process
Lugscheider, E., Bobzin, K., & Erdle, A. (2003) · Thin Solid Films · doi:10.1016/s0040-6090(03)01110-6 · Cited by 2
Rogers, T., Aitken, N., Stribley, K., & Boyd, J. (2004) · Cited by 1
Research works printed but not linked: 31
- M. F. Ashby: ‘Cambridge engineering selector v4’; 2007, Cambridge, Granta Design Limited.
- Fernie J. A., 1999, Ind Ceram, 19, 172
- Imai H., 2006, JSME Int. J. Ser. A, 49, 450
- Lindner P., 2004, Solid State Technol, 47, 55
- Ito M., 1991, US Patent 5073085
- Duvall D. S., 1974, Weld, 1, 203
- 10.1016/j.ijrmhm.2004.01.003 · doi:10.1016/j.ijrmhm.2004.01.003
- Fernie J. A., 1999, Mater. World, 7, 686
- Loehman R. E., 1989, Am. Ceram. Soc. Bull, 68, 891
- Eustathopoulos N., 1998, Acta Mater, 46, 2319
- Sobczak N., 2005, Curr. Opin. Solid State Mater. Set, 9, 241 — 253
- Derby B., 2004, Interf Set, 12, 29
- Ormston D. R., 2001, ‘The particulate reinforcement of active broze alloys for joining silicon carbide’, Cambridge
- Knowles K. M., 2002, Ceram. Trans, 138, 103
- Nolte H. J., 1954, US Patent 2667432
- Kim J. Y., 2005, J. Electrochem. Soc, 152, J52—J58
- Paulasto M., 1997, Ceram. Trans, 77, 91
- Peteves S. D., 1998, Acta. Mater, 46, 2407
- Reichel U., 1999, Z. Metallkd, 90, 699
- Gasse A., 1997, World Patent WO 9747568
- Chaumat G., 2001, European Patent EP 806402
- Gasse A., 2008, US Patent 7318547
- Pask J. A., 1971, Proc. Porcelain Enamel Inst. Tech. Forum, 33, 1
- Pask J. A., 1987, Am. Ceram. Soc. Bull, 66, 1587
- Ghosh S., 2008, J. Electrochem. Soc, 155, B473—B478
- Kobsiriphat W., 2008, J. Fuel Cell Set Technot, 011002
- Henager C. H., J. Nucl. Mater, 2007, 367
- Appendino P., 1563, J. Nucl. Mater, 2004, 329
- Barabash V., J. Nucl. Mater, 2000, 283
- Ferraris M., 1546, J. Nucl. Mater, 1998, 258
- Suryanarayana C., 2001, Adv. Mater. Processes, 159, 29
Cited by
Advanced ceramic components: Materials, fabrication, and applications
Ayode Otitoju, T., Ugochukwu Okoye, P., Chen, G., Li, Y., Onyeka Okoye, M., & Li, S. (2020) · Journal of Industrial and Engineering Chemistry · doi:10.1016/j.jiec.2020.02.002 · Cited by 368
Ultrafast laser welding of ceramics
Penilla, E. H., Devia-Cruz, L. F., Wieg, A. T., Martinez-Torres, P., Cuando-Espitia, N., Sellappan, P., Kodera, Y., Aguilar, G., & Garay, J. E. (2019) · Science · doi:10.1126/science.aaw6699 · Cited by 224
Ultra-high temperature ceramics: Aspiration to overcome challenges in thermal protection systems
Nisar, A., Hassan, R., Agarwal, A. K., & Balani, K. (2021) · Ceramics International · doi:10.1016/j.ceramint.2021.12.199 · Cited by 197
Room-temperature exceptional plasticity in defective Bi 2 Te 3 -based bulk thermoelectric crystals
Deng, T., Gao, Z., Li, Z., Qiu, P., Li, Z., Yuan, X., Ming, C., Wei, T.-R., Chen, L., & Shi, X. (2024) · Science · doi:10.1126/science.adr8450 · Cited by 186
Ali, M., Knowles, K. M., Mallinson, P. M., & Fernie, J. A. (2015) · Acta Materialia · doi:10.1016/j.actamat.2015.05.048 · Cited by 161
Self-citation
Metadata
- Authors
- Fernie, J. A., Drew, R. A. L., & Knowles, K. M.
- Venue
- International Materials Reviews
- Publisher
- SAGE Publications
- Published
- 2009-09
- Volume
- 54
- Issue
- 5
- Pages
- 283-331
- ISSN
- 0950-6608 (ISSN-L)
- 1743-2804
- OpenAlex
- W1985755219
- Cited by
- 282
- References
- 328
- FWCI
- 10.33
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.