The DOI matches its Crossref record.
Fracture modes in brittle coatings with large interlayer modulus mismatch
Abstract
Fracture modes in a model glass–polymer coating–substrate system indented with hard spheres are investigated. The large modulus mismatch between the glass and polymer results in distinctive transverse fracture modes within the brittle coating: exaggerated circumferential (C) ring cracks that initiate at the upper coating surface well outside the contact (as opposed to the near-contact Hertzian cone fractures observed in monolithic brittle materials); median–radial (M) cracks that initiate at the lower surface (i.e., at the substrate interface) on median planes containing the contact axis. Bonding between the coating and substrate is sufficiently strong as to preclude delamination in our system. The transparency of the constituent materials usefully enables in situ identification and quantification of the two transverse fracture modes during contact. The morphologies of the cracks and the corresponding critical indentation loads for initiation are measured over a broad range of coating thicknesses (20 mm to 5.6 mm), on coatings with like surface flaw states, here ensured by a prebonding abrasion treatment. There is a well-defined, broad intermediate range where the indented coating responds more like a flexing plate than a Hertzian contact, and where the M and C cracks initiate in close correspondence with a simple critical stress criterion, i.e., when the maximum tensile stresses exceed the bulk strength of the (abraded) glass. In this intermediate range the M cracks generally form first—only when the flaws on the lower surface are removed (by etching) do the C cracks form first. Finite element modeling is used to evaluate the critical stresses at crack initiation and the surface locations of the crack origins. Departures from the critical stress condition occur at the extremes of very thick coatings (monolith limit) and very thin coatings (thin-film limit), where stress gradients over the flaw dimension are large. Implications of the results concerning practical coating systems are considered.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cited by
Fracture mode transitions in brittle coatings on compliant substrates as a function of thickness
Chai, H., & Lawn, B. R. (2004) · Journal of Materials Research · doi:10.1557/jmr.2004.0219 · Cited by 81
Self-citationDesigning damage-resistant brittle-coating structures: I. Bilayers
Miranda, P., Pajares, A., Guiberteau, F., Deng, Y., & Lawn, B. R. (2003) · Acta Materialia · doi:10.1016/s1359-6454(03)00290-8 · Cited by 57
Self-citationChai, H. (2009) · International Journal of Fracture · doi:10.1007/s10704-009-9362-3 · Cited by 9
Self-citation
Metadata
- Authors
- Chai, H., Lawn, B., & Wuttiphan, S.
- Venue
- Journal of Materials Research
- Published
- 1999-09
- Volume
- 14
- Issue
- 9
- Pages
- 3805-3817
- ISSN
- 0884-1616 (ISSN-L)
- 0884-2914
- 2044-5326
- OpenAlex
- W2116792350
- Cited by
- 170
- References
- 0
- FWCI
- 15.92
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: Fracture modes in brittle coatings with large interlayer modulus mismatch. https://app.cochat.ai/papers/10.1557/jmr.1999.0514
- The paper
- Chai, H., Lawn, B., & Wuttiphan, S. (1999). Fracture modes in brittle coatings with large interlayer modulus mismatch. Journal of Materials Research. https://doi.org/10.1557/jmr.1999.0514
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.