The DOI matches its Crossref record; 29 of the 29 references it cites were found in a registry or an index.
Indentation-induced subsurface tunneling cracks as a means for evaluating fracture toughness of brittle coatings
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“The glass plate shows several long radial cracks emanating from the tip of the needle, many of them reaching the edge of the plate”
From Fabrication, testing and modeling of a new flexible armor inspired from natural fish scales and osteoderms (2014) · cites this paper as [22]
In the citing paper
“Our system consisted of a thin plate on a soft substrate, so that failure from flexural stresses always prevailed over failure from contact stress [21, 22].”
From Fabrication, testing and modeling of a new flexible armor inspired from natural fish scales and osteoderms (2014) · cites this paper as [22]
Citations
Cites
Timoshenko, S. P., & Woinowsky-Krieger, S. (1959) · UCLA Biblioteca de Ingenieria Civil · Cited by 12,112
Anstis, G. R., Chantikul, P., Lawn, B. R., & Marshall, D. B. (1981) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1981.tb10320.x · Cited by 5,653 · cited 3×
“Note in the former case the standard deviation is arbitrarily taken as 25% of the mean (Antis et al. 1981).”
BackgroundInfluentialIndentation fracture: principles and applications
Lawn, B., & Wilshaw, R. (1975) · Journal of Materials Science · doi:10.1007/bf00823224 · Cited by 1,321 · cited 3×
“where δ is a dimensionless quantity, P the applied load and cthemeancracklength(Fig.1b).ItisInterestingto note that a similar power-law relation also governs the behavior of other important indentation crack systems in monolithic materials, e.g., top-surface cone or radial cracks ( Lawn and Wilshaw 1975 ) as well as c…”
BackgroundInfluentialCracking of thin bonded films in residual tension
Beuth, J. L. (1992) · International Journal of Solids and Structures · doi:10.1016/0020-7683(92)90015-l · Cited by 643 · cited 2×
“6, we find from Beuth (1992) for the cases of (porcelain, glass, silicon,Y-TZP, alumina) coatings on polycarbonate g = (7.”
BackgroundFracture modes in brittle coatings with large interlayer modulus mismatch
Chai, H., Lawn, B., & Wuttiphan, S. (1999) · Journal of Materials Research · doi:10.1557/jmr.1999.0514 · Cited by 170
Self-citationThe mechanical performance of DLC films on steel substrates
Wang, J. S., Sugimura, Y., Evans, A. G., & Tredway, W. K. (1998) · Thin Solid Films · doi:10.1016/s0040-6090(98)00418-0 · Cited by 160 · cited 1×
“As an example consider the case of a DLC film on steel substrate, where the fracture is generally dominated by ring cracking at the top surface of the coating ( Wang et al. 1998; Michler and Blank 2001).”
Chai, H., & Lawn, B. R. (2007) · Acta Materialia · doi:10.1016/j.actamat.2006.10.061 · Cited by 144
Self-citationEricson, F., Johansson, S. A. I., & Schweitz, J. (1988) · Materials Science and Engineering A · doi:10.1016/0025-5416(88)90489-2 · Cited by 122 · cited 1×
“Material constants for glass, alumina, Y-TZP and porcelain are from Kim et al. (2001), those for silicon from Ericson (1988) Material E [GPa] ν KC [MPa m 1/2 ] KC [MPa m 1/2 ]”
BackgroundMichler, J., & Blank, E. (2001) · Thin Solid Films · doi:10.1016/s0040-6090(00)01340-7 · Cited by 113 · cited 2×
“As an example consider the case of a DLC film on steel substrate, where the fracture is generally dominated by ring cracking at the top surface of the coating (Wang et al. 1998; Michler and Blank 2001).”
BackgroundJungk, J. M., Boyce, B. L., Buchheit, T., Friedmann, T. A., Yang, D., & Gerberich, W. W. (2006) · Acta Materialia · doi:10.1016/j.actamat.2006.05.003 · Cited by 89
Cited by
Chintapalli, R. K., Mirkhalaf, M., Dastjerdi, A. K., & Barthelat, F. (2014) · Bioinspiration & Biomimetics · doi:10.1088/1748-3182/9/3/036005 · Cited by 128
“Our system consisted of a thin plate on a soft substrate, so that failure from flexural stresses always prevailed over failure from contact stress [21, 22].”
BackgroundMethodFracture toughness measurement on TiN hard coatings using internal energy induced cracking
Wang, A., Yu, G., & Huang, J. (2013) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2013.11.010 · Cited by 49
On the mechanical properties of tooth enamel under spherical indentation
Chai, H. (2014) · Acta Biomaterialia · doi:10.1016/j.actbio.2014.07.003 · Cited by 39
“The UTS was determined using the bilayer test, an approach especially suitable to small-size materials [15].”
MethodSelf-citationEvaluation of fracture toughness of ZrN hard coatings by internal energy induced cracking method
Huang, J., Chen, Y.-H., Wang, A., Yu, G., & Chen, H. (2014) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2014.09.026 · Cited by 25
Osorio, J. D., Maya, D., Barrios, A. C., Lopera-Valle, A., Navas, F. J., Meza, J. M., Hernandez-Ortiz, J. P., & Toro, A. (2013) · Journal of the American Ceramic Society · doi:10.1111/jace.12621 · Cited by 23
Metadata
- Authors
- Chai, H.
- Affiliations
- Tel Aviv University (IL)
- Corresponding author
- Chai, Herzl
- ORCID
- Chai, Herzl
- Venue
- International Journal of Fracture
- Published
- 2009-06-10
- Volume
- 158
- Issue
- 1
- Pages
- 15-26
- ISSN
- 0020-7268 (ISSN-L)
- 0376-9429
- 1573-2673
- OpenAlex
- W2006775486
- Semantic Scholar
- 67372af3eda51f998acdcbbdaa8a62720ce53ff9
- Cited by
- 9
- References
- 29
- Citations by year
- 2024: 1 · 2014: 4 · 2013: 2
- FWCI
- 1.06
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.springer.com/tdm (tdm)
- Locations
- International Journal of Fracture (publishedVersion)
- Topics
- Physical Sciences › Engineering › Mechanics of Materials › Metal and Thin Film Mechanics
- Physical Sciences › Engineering › Mechanics of Materials › Fatigue and fracture mechanics
- Physical Sciences › Engineering › Mechanics of Materials › Mechanical Behavior of Composites
- Keywords
- fracture toughness, brittle coatings, indentation, stress intensity factor, compliant substrates, transparent substrates, thin films
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: Indentation-induced subsurface tunneling cracks as a means for evaluating fracture toughness of brittle coatings. https://app.cochat.ai/papers/10.1007/s10704-009-9362-3
- The paper
- Chai, H. (2009). Indentation-induced subsurface tunneling cracks as a means for evaluating fracture toughness of brittle coatings. International Journal of Fracture. https://doi.org/10.1007/s10704-009-9362-3
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.