Averting cracks caused by insertion reaction in lithium–ion batteries
Abstract
In a lithium-ion battery, both electrodes are atomic frameworks that host mobile lithium ions. When the battery is being charged or discharged, lithium ions diffuse from one electrode to the other. Such an insertion reaction deforms the electrodes and may cause the electrodes to crack. This paper uses fracture mechanics to determine the critical conditions to avert insertion-induced cracking. The method is applied to cracks induced by the mismatch between phases in LiFePO 4.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Stress generation and fracture in lithium insertion materials
Christensen, J., & Newman, J. (2006) · Journal of Solid State Electrochemistry · doi:10.1007/s10008-006-0095-1 · Cited by 727
First-principles study of Li ion diffusion inLiFePO4
Ouyang, C., Shi, S., Wang, Z., Huang, X., & Chen, L. (2004) · Physical Review B · doi:10.1103/physrevb.69.104303 · Cited by 297 · cited 1×
“In the b direction of the framework are tunnels, in which lithium ions diffuse.(9,17,18,28) The crystal has two phases: the lithium-rich phase noted as LiFePO4, and the lithium-poor phase noted as FePO4.”
Cited by
Size-Dependent Fracture of Silicon Nanoparticles During Lithiation
Liu, X. H., Zhong, L., Huang, S., Mao, S. X., Zhu, T., & Huang, J. Y. (2012) · ACS Nano · doi:10.1021/nn204476h · Cited by 2,376
McDowell, M. T., Lee, S. W., Nix, W. D., & Cui, Y. (2013) · Advanced Materials · doi:10.1002/adma.201301795 · Cited by 1,670
Yan, P., Zheng, J., Gu, M., Xiao, J., Zhang, J.-G., & Wang, C.-M. (2017) · Nature Communications · doi:10.1038/ncomms14101 · Cited by 1,010
Deformation and stress in electrode materials for Li-ion batteries
Mukhopadhyay, A., & Sheldon, B. W. (2014) · Progress in Materials Science · doi:10.1016/j.pmatsci.2014.02.001 · Cited by 724
Silicon-based materials as high capacity anodes for next generation lithium ion batteries
Liang, B., Liu, Y., & Xu, Y. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2014.05.096 · Cited by 624
Qian, G., Zhang, Y., Li, L., Zhang, R., Xu, J., Cheng, Z., Xie, S., Wang, H., Rao, Q., He, Y., et al. (2020) · Energy Storage Materials · doi:10.1016/j.ensm.2020.01.027 · Cited by 564
A review on modeling of electro-chemo-mechanics in lithium-ion batteries
Zhao, Y., Stein, P., Bai, Y., Al-Siraj, M., Yang, Y., & Xu, B.-X. (2019) · Journal of Power Sources · doi:10.1016/j.jpowsour.2018.12.011 · Cited by 431
Fracture of electrodes in lithium-ion batteries caused by fast charging
Zhao, K., Pharr, M., Vlassak, J. J., & Suo, Z. (2010) · Journal of Applied Physics · doi:10.1063/1.3492617 · Cited by 428
Self-citationZhao, K., Wang, W. L., Gregoire, J., Pharr, M., Suo, Z., Vlassak, J. J., & Kaxiras, E. (2011) · Nano Letters · doi:10.1021/nl201501s · Cited by 342
Self-citationMechanical properties of cathode materials for lithium-ion batteries
Stallard, J. C., Wheatcroft, L., Booth, S. G., Boston, R., Corr, S. A., De Volder, M. F. L., Inkson, B. J., & Fleck, N. A. (2022) · Joule · doi:10.1016/j.joule.2022.04.001 · Cited by 336
“Electrochemical Shock” of Intercalation Electrodes: A Fracture Mechanics Analysis
Woodford, W. H., Chiang, Y.-M., & Carter, W. C. (2010) · Journal of The Electrochemical Society · doi:10.1149/1.3464773 · Cited by 323
Large Plastic Deformation in High‐Capacity Lithium‐Ion Batteries Caused by Charge and Discharge
Zhao, K., Pharr, M., Cai, S., Vlassak, J. J., & Suo, Z. (2011) · Journal of the American Ceramic Society · doi:10.1111/j.1551-2916.2011.04432.x · Cited by 322
Self-citation
Metadata
- Authors
- Hu, Y., Zhao, X., & Suo, Z.
- Venue
- Journal of Materials Research
- Published
- 2010-06
- Volume
- 25
- Issue
- 6
- Pages
- 1007-1010
- ISSN
- 0884-1616 (ISSN-L)
- 0884-2914
- 2044-5326
- OpenAlex
- W2118452293
- Cited by
- 182
- References
- 2
- FWCI
- 9.72
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.