The DOI matches its Crossref record; 6 of the 6 references it cites were found in a registry or an index.
Investigation on reducing distortion by preheating during manufacture of aluminum components using selective laser melting
Abstract
The additive manufacturing process selective laser melting (SLM) can be used to directly produce functional components made out of metal. During the construction process, however, thermally induced residual stress occurs due to the layered build-up and the local input of energy by means of a focused laser beam, which can lead to distortion of the component or sections of the component itself. Normally, distortion is prevented due to supporting structures between the component and the substrate plate. It is not always possible, however, to provide all the areas of a component with supporting structures or to remove them later, depending on how complex the geometry or how accessible the structures are. When the substrate plate is heated during the construction process, the distortion can be reduced or eliminated entirely. Nonetheless, a systematic investigation of the extent to which preheating influences distortion of aluminum components has not yet been conducted. This works aims at systematically investigating the effects of preheating during SLM of aluminum components and determining an appropriate preheating temperature at which distortion practically no longer occurs. A significant reduction in distortion compared to the distortion without preheating can be seen beginning at a preheating temperature of 150 °C. At a preheating temperature of 250 °C, distortion can no longer be detected within the scope of the measuring accuracy independent of the twin cantilever test geometry investigated. In addition to reducing distortion, the preheating avoids the stress-related cracks in the component, which can lead to tearing of the parts of the test geometry. With 90 HV 0.1 at a preheating temperature of 250 °C, the hardness is greater than the required minimum hardness according to DIN EN 1706 of die-cast parts from the material AlSi10Mg. From these results, it can be concluded that a preheating temperature of 250 °C is suitable for reliably manufacturing components made out of the material AlSi10Mg using SLM free of defects and for preventing distortion completely.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Thijs, L., Kempen, K., Kruth, J.-P., & Van Humbeeck, J. (2013) · Acta Materialia · doi:10.1016/j.actamat.2012.11.052 · Cited by 1,917
Selective laser melting of iron-based powder
Kruth, J. P., Froyen, L., Van Vaerenbergh, J., Mercelis, P., Rombouts, M., & Lauwers, B. (2004) · Journal of Materials Processing Technology · doi:10.1016/j.jmatprotec.2003.11.051 · Cited by 1,550
Investigations on residual stresses and deformations in selective laser melting
Zaeh, M. F., & Branner, G. (2010) · Production Engineering · doi:10.1007/s11740-009-0192-y · Cited by 666
Kruth, J.-P., Deckers, J., Yasa, E., & Wauthlé, R. (2012) · Proceedings of the Institution of Mechanical Engineers, Part B: Journal of Engineering Manufacture · doi:10.1177/0954405412437085 · Cited by 532
Vasinonta, A., Beuth, J., & Griffith, M. L. (2006) · Journal of Manufacturing Science and Engineering · doi:10.1115/1.2335852 · Cited by 188
Direktes selektives Laser-Sintern einkomponentiger metallischer Werkstoffe
Meiners, W., & Poprawe, R. (1999) · Cited by 145
Self-citation
Cited by
Additive manufacturing of metallic components – Process, structure and properties
DebRoy, T., Wei, H. L., Zuback, J. S., Mukherjee, T., Elmer, J. W., Milewski, J. O., Beese, A. M., Wilson-Heid, A., De, A., & Zhang, W. (2018) · Progress in Materials Science · doi:10.1016/j.pmatsci.2017.10.001 · Cited by 8,805
Material-structure-performance integrated laser-metal additive manufacturing
Gu, D., Shi, X., Poprawe, R., Bourell, D. L., Setchi, R., & Zhu, J. (2021) · Science · doi:10.1126/science.abg1487 · Cited by 1,703
Svetlizky, D., Das, M., Zheng, B., Vyatskikh, A. L., Bose, S., Bandyopadhyay, A., Schoenung, J. M., Lavernia, E. J., & Eliaz, N. (2021) · Materials Today · doi:10.1016/j.mattod.2021.03.020 · Cited by 1,371
Materials for additive manufacturing
Bourell, D., Kruth, J. P., Leu, M., Levy, G., Rosen, D., Beese, A. M., & Clare, A. (2017) · CIRP Annals · doi:10.1016/j.cirp.2017.05.009 · Cited by 1,034
Process defects and in situ monitoring methods in metal powder bed fusion: a review
Grasso, M., & Colosimo, B. M. (2017) · Measurement Science and Technology · doi:10.1088/1361-6501/aa5c4f · Cited by 833
Metadata
- Authors
- Buchbinder, D., Meiners, W., Pirch, N., Wissenbach, K., & Schrage, J.
- Venue
- Journal of Laser Applications
- Publisher
- Laser Institute of America
- Published
- 2013-11-06
- Volume
- 26
- Issue
- 1
- ISSN
- 1042-346X (ISSN-L)
- 1938-1387
- OpenAlex
- W2076034183
- Cited by
- 390
- References
- 6
- FWCI
- 10.19
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: Investigation on reducing distortion by preheating during manufacture of aluminum components using selective laser melting. https://app.cochat.ai/papers/10.2351/1.4828755
- The paper
- Buchbinder, D., Meiners, W., Pirch, N., Wissenbach, K., & Schrage, J. (2014). Investigation on reducing distortion by preheating during manufacture of aluminum components using selective laser melting. Journal of Laser Applications. https://doi.org/10.2351/1.4828755
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.