The DOI matches its Crossref record; 6 of the 6 references it cites were found in a registry or an index.
Investigation on reducing distortion by preheating during manufacture of aluminum components using selective laser melting
Abstract
The additive manufacturing process selective laser melting (SLM) can be used to directly produce functional components made out of metal. During the construction process, however, thermally induced residual stress occurs due to the layered build-up and the local input of energy by means of a focused laser beam, which can lead to distortion of the component or sections of the component itself. Normally, distortion is prevented due to supporting structures between the component and the substrate plate. It is not always possible, however, to provide all the areas of a component with supporting structures or to remove them later, depending on how complex the geometry or how accessible the structures are. When the substrate plate is heated during the construction process, the distortion can be reduced or eliminated entirely. Nonetheless, a systematic investigation of the extent to which preheating influences distortion of aluminum components has not yet been conducted. This works aims at systematically investigating the effects of preheating during SLM of aluminum components and determining an appropriate preheating temperature at which distortion practically no longer occurs. A significant reduction in distortion compared to the distortion without preheating can be seen beginning at a preheating temperature of 150 °C. At a preheating temperature of 250 °C, distortion can no longer be detected within the scope of the measuring accuracy independent of the twin cantilever test geometry investigated. In addition to reducing distortion, the preheating avoids the stress-related cracks in the component, which can lead to tearing of the parts of the test geometry. With 90 HV 0.1 at a preheating temperature of 250 °C, the hardness is greater than the required minimum hardness according to DIN EN 1706 of die-cast parts from the material AlSi10Mg. From these results, it can be concluded that a preheating temperature of 250 °C is suitable for reliably manufacturing components made out of the material AlSi10Mg using SLM free of defects and for preventing distortion completely.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Thijs, L., Kempen, K., Kruth, J.-P., & Van Humbeeck, J. (2013) · Acta Materialia · doi:10.1016/j.actamat.2012.11.052 · Cited by 1,917
Selective laser melting of iron-based powder
Kruth, J. P., Froyen, L., Van Vaerenbergh, J., Mercelis, P., Rombouts, M., & Lauwers, B. (2004) · Journal of Materials Processing Technology · doi:10.1016/j.jmatprotec.2003.11.051 · Cited by 1,550
Investigations on residual stresses and deformations in selective laser melting
Zaeh, M. F., & Branner, G. (2010) · Production Engineering · doi:10.1007/s11740-009-0192-y · Cited by 666
Kruth, J.-P., Deckers, J., Yasa, E., & Wauthlé, R. (2012) · Proceedings of the Institution of Mechanical Engineers, Part B: Journal of Engineering Manufacture · doi:10.1177/0954405412437085 · Cited by 532
Vasinonta, A., Beuth, J., & Griffith, M. L. (2006) · Journal of Manufacturing Science and Engineering · doi:10.1115/1.2335852 · Cited by 209
Direktes selektives Laser-Sintern einkomponentiger metallischer Werkstoffe
Meiners, W., & Poprawe, R. (1999) · Cited by 145
Self-citation
Cited by
Additive manufacturing of metallic components – Process, structure and properties
DebRoy, T., Wei, H. L., Zuback, J. S., Mukherjee, T., Elmer, J. W., Milewski, J. O., Beese, A. M., Wilson-Heid, A., De, A., & Zhang, W. (2018) · Progress in Materials Science · doi:10.1016/j.pmatsci.2017.10.001 · Cited by 8,805
Material-structure-performance integrated laser-metal additive manufacturing
Gu, D., Shi, X., Poprawe, R., Bourell, D. L., Setchi, R., & Zhu, J. (2021) · Science · doi:10.1126/science.abg1487 · Cited by 1,703
Aboulkhair, N. T., Simonelli, M., Parry, L., Ashcroft, I., Tuck, C., & Hague, R. (2019) · Progress in Materials Science · doi:10.1016/j.pmatsci.2019.100578 · Cited by 1,552
Svetlizky, D., Das, M., Zheng, B., Vyatskikh, A. L., Bose, S., Bandyopadhyay, A., Schoenung, J. M., Lavernia, E. J., & Eliaz, N. (2021) · Materials Today · doi:10.1016/j.mattod.2021.03.020 · Cited by 1,371
Materials for additive manufacturing
Bourell, D., Kruth, J. P., Leu, M., Levy, G., Rosen, D., Beese, A. M., & Clare, A. (2017) · CIRP Annals · doi:10.1016/j.cirp.2017.05.009 · Cited by 1,034
Process defects and in situ monitoring methods in metal powder bed fusion: a review
Grasso, M., & Colosimo, B. M. (2017) · Measurement Science and Technology · doi:10.1088/1361-6501/aa5c4f · Cited by 833
“The choice of improper pre-heating settings is a possible cause of residual stress development (Leuders et al., 2013; Edwards et al., 201; Chlebus et al., 2011; Buchbinder et al., 2014).”
Parry, L., Ashcroft, I. A., & Wildman, R. D. (2016) · Additive Manufacturing · doi:10.1016/j.addma.2016.05.014 · Cited by 739
Residual Stress in Metal Additive Manufacturing
Li, C., Liu, Z. Y., Fang, X. Y., & Guo, Y. B. (2018) · Procedia CIRP · doi:10.1016/j.procir.2018.05.039 · Cited by 708
An overview of residual stresses in metal powder bed fusion
Bartlett, J. L., & Li, X. (2019) · Additive Manufacturing · doi:10.1016/j.addma.2019.02.020 · Cited by 616
Defects and anomalies in powder bed fusion metal additive manufacturing
Mostafaei, A., Zhao, C., He, Y., Reza Ghiaasiaan, S., Shi, B., Shao, S., Shamsaei, N., Wu, Z., Kouraytem, N., Sun, T., et al. (2022) · Current Opinion in Solid State and Materials Science · doi:10.1016/j.cossms.2021.100974 · Cited by 491
Song, B., Zhao, X., Li, S., Han, C., Wei, Q., Wen, S., Liu, J., & Shi, Y. (2015) · Frontiers of Mechanical Engineering · doi:10.1007/s11465-015-0341-2 · Cited by 427
Multi-scale defects in powder-based additively manufactured metals and alloys
Fu, J., Li, H., Song, X., & Fu, M. W. (2022) · Journal of Materials Science & Technology · doi:10.1016/j.jmst.2022.02.015 · Cited by 391
Rao, H., Giet, S., Yang, K., Wu, X., & Davies, C. H. J. (2016) · Materials & Design · doi:10.1016/j.matdes.2016.07.009 · Cited by 331
Main defects observed in aluminum alloy parts produced by SLM: From causes to consequences
Galy, C., Le Guen, E., Lacoste, E., & Arvieu, C. (2018) · Additive Manufacturing · doi:10.1016/j.addma.2018.05.005 · Cited by 318
Zhao, L., Song, L., Santos Macías, J. G., Zhu, Y., Huang, M., Simar, A., & Li, Z. (2022) · Additive Manufacturing · doi:10.1016/j.addma.2022.102914 · Cited by 292
Textures formed in a CoCrMo alloy by selective laser melting
Zhou, X., Li, K., Zhang, D., Liu, X., Ma, J., Liu, W., & Shen, Z. (2015) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2015.01.096 · Cited by 291
Geometrical metrology for metal additive manufacturing
Leach, R. K., Bourell, D., Carmignato, S., Donmez, A., Senin, N., & Dewulf, W. (2019) · CIRP Annals · doi:10.1016/j.cirp.2019.05.004 · Cited by 289
Metadata
- Authors
- Buchbinder, D., Meiners, W., Pirch, N., Wissenbach, K., & Schrage, J.
- Venue
- Journal of Laser Applications
- Publisher
- Laser Institute of America
- Published
- 2013-11-06
- Volume
- 26
- Issue
- 1
- ISSN
- 1042-346X (ISSN-L)
- 1938-1387
- OpenAlex
- W2076034183
- Cited by
- 390
- References
- 6
- FWCI
- 10.19
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.