Two-body wear of monolithic, veneered and glazed zirconia and their corresponding enamel antagonists
Open accessThe DOI matches its Crossref record; 1 of the 1 references it cites were found in a registry or an index.
Abstract
OBJECTIVE: This study tested whether the two-body wear of monolithic zirconia and their corresponding enamel antagonists was higher compared to monolithic alloy and veneered zirconia. MATERIALS AND METHODS: Cylindrical specimens (N = 36, n = 6) were prepared out of (A) veneered zirconia (VZ), (B) glazed zirconia using a glaze ceramic (GZC), (C) glazed zirconia using a glaze spray (GZS), (D) manually polished monolithic zirconia (MAZ), (E) mechanically polished monolithic zirconia (MEZ) and (F) monolithic base alloy (control group, MA). Wear tests were performed in a chewing simulator (49 N, 1.7 Hz, 5°C/50°C) with enamel antagonists. The wear analysis was performed using a 3D profilometer before and after 120,000, 240,000, 640,000 and 1,200,000 masticatory cycles. SEM images were used for evaluating wear qualitatively. The longitudinal results were analysed using linear mixed models (α = 0.05). RESULTS: Materials (p < 0.001) and number of masticatory cycles (p < 0.001) had a significant effect on the wear level. The least enamel antagonist wear was observed for MAZ and MEZ (27.3 ± 15.2, 28 ± 11.1 μm, respectively). GZC (118 ± 30.9 μm) showed the highest wear of enamel antagonists. The highest wear rate in the material was observed in GZS (91.3 ± 38.6 μm). While in the groups of MA, VZ, GZC and GZS 50% of the specimens developed cracks in enamel, it was 100% in MAZ and MEZ groups. CONCLUSION: Polished monolithic zirconia showed lower wear rate on enamel antagonists as well as within the material itself but developed higher rates of enamel cracks.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Clinical trials in zirconia: a systematic review
AL-AMLEH, B., LYONS, K., & SWAIN, M. (2010) · Journal of Oral Rehabilitation · doi:10.1111/j.1365-2842.2010.02094.x · Cited by 587
Cited by
Emerging Ceramic-based Materials for Dentistry
Denry, I., & Kelly, J. R. (2014) · Journal of Dental Research · doi:10.1177/0022034514553627 · Cited by 464
Mörmann, W. H., Stawarczyk, B., Ender, A., Sener, B., Attin, T., & Mehl, A. (2013) · Journal of the Mechanical Behavior of Biomedical Materials · doi:10.1016/j.jmbbm.2013.01.003 · Cited by 342
Self-citationHarada, K., Raigrodski, A. J., Chung, K.-H., Flinn, B. D., Dogan, S., & Mancl, L. A. (2016) · The Journal of Prosthetic Dentistry · doi:10.1016/j.prosdent.2015.11.019 · Cited by 243
“In addition, in some in vitro studies polished zirconia showed a similar wear rate of the opposing enamel compared with Co-Cr alloy and less wear than lithium disilicate glass ceramic.(13,14) To enhance the translucency of zirconia, residual pores and impurities which create volumes of differing refractive indexes and…”
Mundhe, K., Jain, V., Pruthi, G., & Shah, N. (2015) · The Journal of Prosthetic Dentistry · doi:10.1016/j.prosdent.2015.03.001 · Cited by 196
“However, various authors have recommended the use of polished zirconia as it causes less wear of the antagonist enamel under in vitro conditions.(9,10,12,13)”
BackgroundEnamel wear caused by monolithic zirconia crowns after 6 months of clinical use
Stober, T., Bermejo, J. L., Rammelsberg, P., & Schmitter, M. (2014) · Journal of Oral Rehabilitation · doi:10.1111/joor.12139 · Cited by 174
Revolution of Current Dental Zirconia: A Comprehensive Review
Alqutaibi, A. Y., Ghulam, O., Krsoum, M., Binmahmoud, S., Taher, H., Elmalky, W., & Zafar, M. S. (2022) · Molecules · doi:10.3390/molecules27051699 · Cited by 142
“In a clinical study, monolithic translucent Zir (Zenostar Zir Translucent) crowns produced more occlusal wear than natural enamel but generated less wear in enamel than other ceramic restorative materials [84,85].”
Background
Metadata
- Authors
- Stawarczyk, B., Özcan, M., Schmutz, F., Trottmann, A., Roos, M., & Hämmerle, C. H. F.
- Venue
- Acta Odontologica Scandinavica
- Published
- 2012-02-27
- Volume
- 71
- Issue
- 1
- Pages
- 102-112
- ISSN
- 0001-6357 (ISSN-L)
- 1502-3850
- OpenAlex
- W2005296761
- Cited by
- 182
- References
- 1
- FWCI
- 15.30
- Type
- journal article
- Language
- en
- Open access
- diamond
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.