CoChat

Performance Evolution of Recycled Aggregate Concrete under the Coupled Effect of Freeze–Thaw Cycles and Sulfate Attack

Open access
Jia, Pu, Li, Lang, Zhou, Jin, Zhang, Di, Guan, Zhongwei, Dong, Jiangfeng, Wang, Qingyuan · 2022 · Applied Sciences

The DOI matches its Crossref record; 39 of the 40 references it cites were found in a registry or an index; none of the 32 sources its claims cite is checked for support yet.

Abstract

The high porosity of recycled coarse aggregate, which results in recycled aggregate concrete (RAC) more vulnerable to freeze–thaw (FT) damage and chemical attack, is a dominant factor that limits the industrialization of recycled aggregate concrete in civil engineering. This paper presents an experimental study on the combined effects of FT damage and sulfate attack on mechanical properties of high-performance RAC. The influence of the combined damage on the mass, solution-filled pore volume, dynamic elastic modulus, compressive strength, splitting tensile strength and fracture energy of RAC was studied. Results showed that the water-exposed FT cycles would result in more severe deterioration in the mass loss, elastic modulus and compressive strength, while for the sulfate-exposed FT cycles, the splitting tensile strength and fracture energy have more significant degradation. Moreover, compared with compressive strength, deterioration in splitting tensile strength is more severe. The maximum losses in compressive and splitting tensile strength were 28.7% and 35%, respectively. The fracture energy showed an increasing trend to 60 FT cycles, followed by an overall decrease to 180 FT cycles. The fracture energy exhibits a maximum increment of about 45% and 39% for water- and sulfate-exposed samples, respectively, after being subjected to 60 FT cycles. The analysis of failure modes of coarse aggregate has revealed that FT damage results in a significant deterioration in the binding force of mortar. After being subjected to 180 FT cycles, the area percentage of pulled-out failure was increased from 7.3% to larger than 17.3%.

Overview

CoChat Summary

TL;DR

This experimental study examines how coupled freeze–thaw (FT) cycles and sulfate attack affect high-performance recycled aggregate concrete (RAC). Water-exposed FT cycles caused greater mass, elastic modulus, and compressive strength loss, while sulfate-exposed FT cycles caused greater splitting tensile strength and fracture energy degradation.

Key findings

  • Water-exposed FT cycles produced more severe deterioration in mass loss, dynamic elastic modulus, and compressive strength; sulfate-exposed FT cycles produced more severe degradation in splitting tensile strength and fracture energy.
  • Maximum losses in compressive and splitting tensile strength were 28.7% and 35%, respectively. After 180 FT cycles, residual compressive strength was about 71% (water) and 78% (sulfate) of original, while residual splitting tensile strength was about 65% for both exposures.
  • Fracture energy increased up to 60 FT cycles, then decreased to 180 FT cycles. Maximum increments at 60 FT cycles were about 45% (water) and 39% (sulfate); at 180 FT cycles, fracture energy decreased about 16% for sulfate-exposed and 9% for water-exposed specimens.
  • After 180 FT cycles, the area percentage of pulled-out failure increased from 7.3% to larger than 17.3%; at 180 FT cycles it was 22.1% for sulfate-exposed and 17.3% for water-exposed specimens.

Methods

  • Experimental study on high-performance RAC made with recycled coarse aggregate from crushed and sieved waste pavement concrete (water absorption 8.5%), 20% fly ash replacement, polycarboxylic superplasticizer, w/c = 0.5, w/b = 0.4; specimens cured in water at 20 °C for 3 months.
  • Rapid FT tests followed GB/T 50082-2009, with internal temperature cycling between 5 ± 2 °C and −15 ± 2 °C over nearly 4 h per cycle. Specimens were exposed to water or 5% sodium sulfate solution and tested after 60, 90, 120, 150, and 180 FT cycles.
  • Beam specimens were 100 mm × 100 mm × 400 mm; notched beams had span-to-depth ratio 3 and notch-to-depth ratio 0.3. Measured mass, solution-filled pore volume, dynamic elastic modulus, compressive strength, splitting tensile strength, and fracture energy via three-point bending; XRD was performed on control and sulfate-exposed S150 specimens.

Limitations

  • The paper does not state a limitations section; no explicit limitations are given.
  • Evident from the text: the study uses a single RAC mixture and a single RCA source, and only water or 5% sodium sulfate exposure, so broader mixture and exposure variability is not captured.
  • Evident from the text: XRD analysis was performed only on sulfate-exposed specimens, not water-exposed specimens, and the text does not report replicate numbers or statistical uncertainty.

Model-written summary. Check it against the paper before relying on it.

Integrity signals

Registry

Crossref · 10.3390/app12146950

Cites

39 of 40 references verified0 citation errors · 1 not checkable

Statistics

Nothing to recompute.

Figures

Figure 1 The gradation curves for fly ash, fine aggregate, NCA and RCA. Figure 1. The gradation curves for fly ash, fine aggregate, NCA and RCA.
Figure 1 The gradation curves for fly ash, fine aggregate, NCA and RCA. Figure 1. The gradation curves for fly ash, fine aggregate, NCA and RCA.CC-BY · From the PDF
Figure 2 Schematic of the notched beam ( A ) and experimental apparatus of the notched beam ( B ) under quasi-static three-point bending test. Figure 2. Schematic of the notched beam ( A ) and experimental apparatus of the notched beam ( B ) under quasi-static three-point bending test. Figure 2. Schematic of the notched beam ( A ) and experimental apparatus of the notched beam ( B ) under quasi-static three-point bending test.
Figure 2 Schematic of the notched beam ( A ) and experimental apparatus of the notched beam ( B ) under quasi-static three-point bending test. Figure 2. Schematic of the notched beam ( A ) and experimental apparatus of the notched beam ( B ) under quasi-static three-point bending test. Figure 2. Schematic of the notched beam ( A ) and experimental apparatus of the notched beam ( B ) under quasi-static three-point bending test.CC-BY · From the PDF
Image 3
CC-BY · From the PDF
Figure 4 Saturated mass loss ( A ) and oven-dried mass loss ( B ) at different FT cycles of water saturated (W) and sulfate attack (S) RAC. Figure 4. Saturated mass loss ( A ) and oven-dried mass loss ( B ) at different FT cycles of water saturated (W) and sulfate attack (S) RAC.
Figure 4 Saturated mass loss ( A ) and oven-dried mass loss ( B ) at different FT cycles of water saturated (W) and sulfate attack (S) RAC. Figure 4. Saturated mass loss ( A ) and oven-dried mass loss ( B ) at different FT cycles of water saturated (W) and sulfate attack (S) RAC.CC-BY · From the PDF
Figure 5 Changes of solution-filled pore volume of water-exposed (W) and sulfate-exposed (S) RAC samples at different freeze-thaw cycles. Figure 5. Changes of solution-filled pore volume of water-exposed (W) and sulfate-exposed (S) RAC samples at different freeze-thaw cycles.
Figure 5 Changes of solution-filled pore volume of water-exposed (W) and sulfate-exposed (S) RAC samples at different freeze-thaw cycles. Figure 5. Changes of solution-filled pore volume of water-exposed (W) and sulfate-exposed (S) RAC samples at different freeze-thaw cycles.CC-BY · From the PDF
Figure 6 Evolutions of damage parameter of water-exposed (W) and sulfate-exposed (S) RAC samples at different freeze-thaw cycles. Figure 6. Evolutions of damage parameter of water-exposed (W) and sulfate-exposed (S) RAC samples at different freeze-thaw cycles. 9 of 14
Figure 6 Evolutions of damage parameter of water-exposed (W) and sulfate-exposed (S) RAC samples at different freeze-thaw cycles. Figure 6. Evolutions of damage parameter of water-exposed (W) and sulfate-exposed (S) RAC samples at different freeze-thaw cycles. 9 of 14CC-BY · From the PDF
Figure 7 Evolutions of residual strength ( A ) and interfacial transition zones ( B , C ) at different freeze-thaw cycles. Figure 7. Evolutions of residual strength ( A ) and interfacial transition zones ( B , C ) at different freeze-thaw cycles.
Figure 7 Evolutions of residual strength ( A ) and interfacial transition zones ( B , C ) at different freeze-thaw cycles. Figure 7. Evolutions of residual strength ( A ) and interfacial transition zones ( B , C ) at different freeze-thaw cycles.CC-BY · From the PDF
Image 8
CC-BY · From the PDF
Figure 9 The relationship between strength loss and damage parameter for water-exposed ( A ) and sulfate-exposed ( B ) RAC. Figure 9. The relationship between strength loss and damage parameter for water-exposed ( A ) and sulfate-exposed ( B ) RAC.
Figure 9 The relationship between strength loss and damage parameter for water-exposed ( A ) and sulfate-exposed ( B ) RAC. Figure 9. The relationship between strength loss and damage parameter for water-exposed ( A ) and sulfate-exposed ( B ) RAC.CC-BY · From the PDF
Figure 10 XRD patterns of RAC in control condition (S0) and subjected to sulfate-exposed FT cycles (S150). Figure 10. XRD patterns of RAC in control condition (S0) and subjected to sulfate-exposed FT cycles (S150).
Figure 10 XRD patterns of RAC in control condition (S0) and subjected to sulfate-exposed FT cycles (S150). Figure 10. XRD patterns of RAC in control condition (S0) and subjected to sulfate-exposed FT cycles (S150).CC-BY · From the PDF

Verification

Claims the paper makes

0 Valid · 0 Not valid · 27 Not checked · 73 Own results and interpretations

56 more claims

Create a free account to see all 100 claims and to verify the 32 references still open.

See all claims — free account
  • It may state two separate claims as one. 25
  • Probably not a substantial claim. 20

Create a free account to see these claims.

Claims other papers make about this one

Each is checked against this paper’s own text: does it say what the citing paper says it does?

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

1 of 1

Citations

Cites

Research works printed but not linked: 2

  1. Mehta, P.K.; Monteiro, P.J.M. Concrete: Microstructure, Properties and Materials; McGraw Hill: New York, NY, USA, 2006.
  2. Wan, X.S.; Lai, Y.M. Experimental study on freezing temperature and salt crystal precipitation of sodium sulphate soulotion and sodium sulphate saline soil. Chin. J. Geotech. Eng. 2013, 35, 7. (In Chinese)

Cited by

See all 24

Metadata

Authors
Jia, P., Li, L., Zhou, J., Zhang, D., Guan, Z., Dong, J., & Wang, Q.
Affiliations
  • Xi'an Jiaotong University (CN)
  • Sichuan University (CN)
  • University of Liverpool (GB)
Corresponding author
  • Dong, Jiangfeng
  • Wang, Qingyuan
Venue
Applied Sciences
Publisher
MDPI AG
Published
2022-07-08
Volume
12
Issue
14
Pages
6950
ISSN
2076-3417 (ISSN-L)
OpenAlex
W4284966813
Cited by
24
References
39
Citations by year
2026: 8 · 2025: 3 · 2024: 8 · 2023: 4 · 2022: 1
FWCI
1.55
Type
journal article
Language
en
Open access
Locations
  • Applied Sciences (publishedVersion, cc-by)
  • DOAJ (DOAJ: Directory of Open Access Journals) (submittedVersion)
Funders
  • Natural Science Basic Research Program of Shaanxi (2021JQ-004, FMEDP202114)
  • 2021 Open Project of Failure Mechanics and Engineering Disaster Prevention, Key Lab of Sichuan Province (2021JQ-004, FMEDP202114)
Topics
  • Physical Sciences › Engineering › Building and Construction › Recycled Aggregate Concrete Performance
  • Physical Sciences › Engineering › Civil and Structural Engineering › Concrete and Cement Materials Research
  • Physical Sciences › Engineering › Civil and Structural Engineering › Innovative concrete reinforcement materials
Keywords
recycled aggregate concrete, freeze-thaw cycles, sulfate attack, compressive strength, splitting tensile strength, fracture energy, elastic modulus, pore volume, failure modes, high-performance concrete

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

A language model drew the claims from the paper on 2026-11-27, under version 3 of the claim definition (model deepseek-v4.1-flash, prompt extract-v3).

A second model labelled each claim on 2026-11-27 (model jev-1.13-20260917, definition revision gold-guideline-v0.2).

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.