A Review of Green Scale Inhibitors: Process, Types, Mechanism and Properties
Open accessThe DOI matches its Crossref record; 49 of the 49 references it cites were found in a registry or an index.
Abstract
In the present time, more often, it has been seen that scaling has grown as widely and caused problems in the oilfield industry. Scaling is the deposition of various salts of inorganic/organic materials due to the supersaturation of salt-water mixtures. Many works have been proposed by researchers using different methods to solve the problem, of which scale inhibition is one of them. The scale inhibitors, particularly for antiscaling, have derived from natural and synthetic polymers. Among different polymers, inorganic and organic compounds (polyphosphates, carboxylic acid, ethylenediaminetetraacetic acid (EDTA), etc.) can effectively manage the oilfield scales of which many are toxic and expansive. Scale inhibitors of alkaline earth metal carbonate and sulfates and transition metal sulfide are commonly used in oilfield applications. Scale inhibition of metallic surfaces is an essential activity in technical, environmental, economic, and safety purposes. Scale inhibitors containing phosphorus appear to have significant achievements in the inhibition process despite its toxicity. However, phosphorus-based inhibitors can serve as supplements prompting eutrification difficulties. Besides these increasing environmental concerns, green scale inhibitors are renewable, biodegradable, and ecologically acceptable that has been used to prevent, control, and retard the formation of scale. Considering the facts, this review article summarized the concept of scale, various green scale inhibitors, types, mechanisms, comparative performance, significance, and future aspects of green scale inhibitors, which will shed light and be helpful for the professionals working in the oil and gas industries.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Environmental impact and impact assessment of seawater desalination
Lattemann, S., & Höpner, T. (2008) · Desalination · doi:10.1016/j.desal.2007.03.009 · Cited by 1,044 · cited 1×
“There is a particular concern about the phosphorus-based inhibitors, which can fill in as supplements prompting eutrification difficulties [149].”
BackgroundProduction Chemicals for the Oil and Gas Industry
Kelland, M. A. (2016) · CRC Press eBooks · doi:10.1201/9781420092974 · Cited by 454
State of the Art of Friendly “Green” Scale Control Inhibitors: A Review Article
Hasson, D., Shemer, H., & Sher, A. (2011) · Industrial & Engineering Chemistry Research · doi:10.1021/ie200370v · Cited by 402 · cited 1×
“They are steady at high working temperatures and stringent chemical and biological environments [148].”
Background⌈Pectin, Pectinase, and Protopectinase: Production,⌈ Properties, and Applications
Sakai, T., Sakamoto, T., Hallaert, J., & Vandamme, E. J. (1993) · Advances in Applied Microbiology · doi:10.1016/s0065-2164(08)70597-5 · Cited by 399
State of art of natural inhibitors of calcium carbonate scaling. A review article
Chaussemier, M., Pourmohtasham, E., Gelus, D., Pécoul, N., Perrot, H., Lédion, J., Cheap-Charpentier, H., & Horner, O. (2015) · Desalination · doi:10.1016/j.desal.2014.10.014 · Cited by 350 · cited 2×
“The active ingredients in commercially available antiscalants are mostly proprietary mixtures of various polycarboxylates and polyacrylates, condensed polyphosphates, and organophosphonates [129,146].”
BackgroundMethodA review of oilfield scale management technology for oil and gas production
Olajire, A. A. (2015) · Journal of Petroleum Science and Engineering · doi:10.1016/j.petrol.2015.09.011 · Cited by 321 · cited 1×
“On a large scale, the chemicals are needed for the successful prevention of scales as they are functioning in a stoichiometric fashion [5,77].”
BackgroundLi, X., Chen, G., & Zhu, H. (2016) · Process Safety and Environmental Protection · doi:10.1016/j.psep.2016.06.006 · Cited by 298
Lee, O.-H., Lee, B.-Y., Lee, J., Lee, H.-B., Son, J.-Y., Park, C.-S., Shetty, K., & Kim, Y.-C. (2009) · Bioresource Technology · doi:10.1016/j.biortech.2009.06.059 · Cited by 231
Corrosion induced failure analysis of subsea pipelines
Yang, Y., Khan, F. I., Thodi, P., & Abbassi, R. (2016) · Reliability Engineering & System Safety · doi:10.1016/j.ress.2016.11.014 · Cited by 220 · cited 1×
“The most environmentally acceptable materials gradually terminate them [23].”
BackgroundCalcite Crystal Growth Rate Inhibition by Polycarboxylic Acids
Reddy, M. M., & Hoch, A. R. (2001) · Journal of Colloid and Interface Science · doi:10.1006/jcis.2000.7378 · Cited by 204 · cited 2×
“CG 15 91 - [158] Poly(carboxylic acid) 1 80 - [97]”
MethodBonoli, M., Bendini, A., Cerretani, L., Lercker, G., & Toschi, T. G. (2004) · Journal of Agricultural and Food Chemistry · doi:10.1021/jf048868m · Cited by 176
Liu, D., Dong, W., Li, F., Hui, F., & Lédion, J. (2012) · Desalination · doi:10.1016/j.desal.2012.07.032 · Cited by 176 · cited 14×
“to show the effect of PASP on the efficiency of scale inhibition at 80 °C under static test conditions in mineral water containing Ca2+ ion concentrations of 253 mg L−1, and they found the efficiency ≈ 80%, which confirms the better inhibition activity of PASP [114].”
BackgroundInfluentialA natural extract as scale and corrosion inhibitor for steel surface in brine solution
Abdel-Gaber, A. M., Abd-El-Nabey, B. A., Khamis, E., & Abd-El-Khalek, D. E. (2011) · Desalination · doi:10.1016/j.desal.2011.05.048 · Cited by 167
Synthesis and Biodegradability of Polyaspartic Acid: A Critical Review
Thombre, S. M., & Sarwade, B. D. (2005) · Journal of Macromolecular Science, Part A · doi:10.1080/10601320500189604 · Cited by 164
Antimicrobial Properties of a Chitosan Dextran-Based Hydrogel for Surgical Use
Aziz, M. A., Cabral, J. D., Brooks, H. J. L., Moratti, S. C., & Hanton, L. R. (2011) · Antimicrobial Agents and Chemotherapy · doi:10.1128/aac.05463-11 · Cited by 156
Developments in oilfield scale handling towards green technology-A review
Kumar, S. S., Naiya, T. K., & Kumar, T. (2018) · Journal of Petroleum Science and Engineering · doi:10.1016/j.petrol.2018.05.068 · Cited by 154 · cited 4×
“to show the performance of scale inhibition and they reported that a 100% scale inhibition was obtained through jar tests with the concentration of PGLU about 120 mg L−1 at 70 °C [77].”
BackgroundInfluentialScale formation and control in oil and gas fields: A review
Li, J., Tang, M., Ye, Z., Chen, L., & Zhou, Y. (2016) · Journal of Dispersion Science and Technology · doi:10.1080/01932691.2016.1185953 · Cited by 151 · cited 4×
“More studies have also been conducted using naturally occurring organic molecules to inhibit scale [14,15,95].”
BackgroundInfluentialThe mechanisms of crystal growth inhibition by organic and inorganic inhibitors
Dobberschütz, S., Nielsen, M., Sand, K. K. S., Civioc, R., Bovet, N., Stipp, S. L. S., & Andersson, M. (2018) · Nature Communications · doi:10.1038/s41467-018-04022-0 · Cited by 130 · cited 1×
“The insoluble particles do not stockpile yet remains as small strong particles dispersed in the fluid phase, and develop without noticeable sorption of bisphosphonate on the crystal edges or some other crystal development centers; subsequently, obstruct the CaSO4 crystals dynamic development sites, and retard the form…”
BackgroundGao, Y., Fan, L., Ward, L. P., & Liu, Z. (2015) · Desalination · doi:10.1016/j.desal.2015.03.006 · Cited by 127
Peng, R., Chen, G., Zhou, F., Man, R., & Huang, J. (2019) · Chemical Engineering Journal · doi:10.1016/j.cej.2019.04.063 · Cited by 127
Prospects for high water recovery membrane desalination
Turek, M., Mitko, K., Piotrowski, K., et al. (2016) · Desalination · doi:10.1016/j.desal.2016.07.047 · Cited by 122 · cited 1×
“The active ingredients in commercially available antiscalants are mostly proprietary mixtures of various polycarboxylates and polyacrylates, condensed polyphosphates, and organophosphonates [129,146].”
BackgroundNovel and efficient curcumin based fluorescent polymer for scale and corrosion inhibition
Yuan, X., Dong, S., Zheng, Q., Yang, W., & Huang, T. (2020) · Chemical Engineering Journal · doi:10.1016/j.cej.2020.124296 · Cited by 117
Yu, W., Wang, Y., Li, A., & Yang, H. (2018) · Water Research · doi:10.1016/j.watres.2018.04.021 · Cited by 116
Yang, L., Yang, W., Xu, B., Yin, X., Chen, Y., Liu, Y., Ji, Y. J., & Huan, Y. (2017) · Desalination · doi:10.1016/j.desal.2017.05.010 · Cited by 107 · cited 1×
“Several researchers have reported an additional source of iron in the well by introducing proppant during hydraulic fracturing processes [55,56].”
BackgroundChung, Y., Yeh, J., & Tsai, C. (2011) · Molecules · doi:10.3390/molecules16108504 · Cited by 102 · cited 1×
“Besides this, the scale inhibition performance and structural properties of chitosan were studied by quantum chemical calculations [118].”
BackgroundInhibition of adhesion and precipitation of CaCO3 by aminopolyphosphonate
Abdel-Aal, N., & Sawada, K. (2003) · Journal of Crystal Growth · doi:10.1016/s0022-0248(03)01354-x · Cited by 99 · cited 1×
“This type of mechanism is defined by adding a substoichiometric quantity of inhibitors that intermingles with growing crystals and delays crystal growth [78,79].”
BackgroundDavies, M. C., Dawkins, J. V., & Hourston, D. J. (2005) · Polymer · doi:10.1016/j.polymer.2004.12.037 · Cited by 96
Kelland, M. A. (2011) · Industrial & Engineering Chemistry Research · doi:10.1021/ie2003494 · Cited by 95
Phosphorus in Water Quality and Waste Management
Kroiß, H., Rechberger, H., & Egle, L. (2011) · InTech eBooks · doi:10.5772/18482 · Cited by 79
Inhibition of calcium carbonate precipitation by aqueous extract of Paronychia argentea
Belarbi, Z., Gamby, J., Makhloufi, L., Sotta, B., & Tribollet, B. (2013) · Journal of Crystal Growth · doi:10.1016/j.jcrysgro.2013.09.048 · Cited by 63 · cited 1×
“Many researchers have revealed via experimental investigations that two morphological structures of gypsum, needles and platelets with monoclinic and prismatic structures, are available [127,136].”
BackgroundPredicting Carbonate Scale in Oil Producers From High-Temperature Reservoirs
Ramstad, K., Tydal, T., Askvik, K. M., & Fotland, P. (2005) · SPE Journal · doi:10.2118/87430-pa · Cited by 60
Ling, L., Zhou, Y., Huang, J., Yao, Q., Liu, G., Zhang, P., Sun, W., & Wu, W. (2012) · Desalination · doi:10.1016/j.desal.2012.07.014 · Cited by 58
The influence of xanthan on the crystallization of calcium carbonate
Yang, X., & Xu, G. (2010) · Journal of Crystal Growth · doi:10.1016/j.jcrysgro.2010.11.158 · Cited by 54 · cited 2×
“More studies have also been conducted using naturally occurring organic molecules to inhibit scale [14,15,95].”
BackgroundGabriel, J. D. S., Tiera, M. J., & Tiera, V. A. D. O. (2015) · Journal of Agricultural and Food Chemistry · doi:10.1021/acs.jafc.5b00278 · Cited by 49
New Insights into the Removal of Calcium Sulfate Scale
Al-Khaldi, M. H., Al-Juhani, A. M., Al-Mutairi, S. H., & Gürmen, M. N. (2011) · SPE European Formation Damage Conference · doi:10.2118/144158-ms · Cited by 47 · cited 1×
“confirms that CaSO4 may cause considerable change in injector and producer reservoirs [67].”
BackgroundGreen Anti-scalent for Cooling Water Systems
Abdel‐Gaber, A. M., Abd-El-Nabey, B. A., Khamis, E., Abd-El-Rhmann, H., & Aglan, H. (2012) · International Journal of Electrochemical Science · doi:10.1016/s1452-3981(23)16515-1 · Cited by 44
Zhang, Z., Lu, M.-L., Liu, J., Chen, H., Chen, Q., & Wang, B. (2020) · Materials Today Communications · doi:10.1016/j.mtcomm.2020.101359 · Cited by 43
The effect of sodium alginate on the crystal growth of calcium carbonate
Manoli, F., & Dalas, E. (2002) · Journal of Materials Science Materials in Medicine · doi:10.1023/a:1013825912150 · Cited by 41 · cited 1×
“02 94 - [160] PAA/APEG-PGCOOH 14 82 - [153]”
Li, J., Zhou, Y., Yao, Q., Wang, T., Zhang, A., Chen, Y., Wu, W., & Sun, W. (2017) · Industrial & Engineering Chemistry Research · doi:10.1021/acs.iecr.6b04427 · Cited by 41
Jain, T., Sanchez, E., Owens‐Bennett, E., Trussell, R. R., Walker, S. L., & Liu, H. (2019) · Environmental Science Water Research & Technology · doi:10.1039/c9ew00351g · Cited by 40 · cited 1×
“Most studied metal ions of Ca, and Fe bear the formation of scales that originate from hard water, biological activities, corrosion, and chemicals used for the purification of ferric water [40,41].”
BackgroundThe effect of leucine on the crystal growth of calcium carbonate
Malkaj, P., Kanakis, I., & Dalas, E. (2004) · Journal of Crystal Growth · doi:10.1016/j.jcrysgro.2004.02.114 · Cited by 36
Application of ionic liquid polymeric microsphere in oil field scale control process
Lakshmi, D. S., Senthilmurugan, B., Drioli, E., & Figoli, A. (2013) · Journal of Petroleum Science and Engineering · doi:10.1016/j.petrol.2013.09.011 · Cited by 36
Oshchepkov, M., Golovesov, V. A., Ryabova, A. V., Tkachenko, S., Redchuk, A., Rönkkömäki, H., Rudakova, G. Y., Pervov, A. G., & Popov, K. (2020) · Separation and Purification Technology · doi:10.1016/j.seppur.2020.117382 · Cited by 35 · cited 1×
“A similar outcome was acquired for PAA-F1 that was realized in the presence of HEDP-F for CaSO4 RO desalination process [88], batch static tests with CaSO4 [84] and barite [89], and supports the proposed mechanism.”
ResultFeng, Y., Lin, X., Li, H., He, L., Sridhar, T., Suresh, A. K., Bellare, J. R., & Wang, H. (2014) · Industrial & Engineering Chemistry Research · doi:10.1021/ie502599p · Cited by 34
Oshchepkov, M., Golovesov, V. A., Ryabova, A. V., Redchuk, A., Tkachenko, S., Pervov, A. G., & Popov, K. (2020) · Crystals · doi:10.3390/cryst10040309 · Cited by 27 · cited 3×
“A similar outcome was acquired for PAA-F1 that was realized in the presence of HEDP-F for CaSO4 RO desalination process [88], batch static tests with CaSO4 [84] and barite [89], and supports the proposed mechanism.”
BackgroundMethodThe inhibition of calcium carbonate crystal growth by the cysteine-rich Mdm2 peptide
Dalas, E., Chalias, A., Gatos, D., & Barlos, K. K. (2006) · Journal of Colloid and Interface Science · doi:10.1016/j.jcis.2006.04.003 · Cited by 24 · cited 1×
“studied the crystal growth of calcite in the presence of cysteine-rich Mdm2 peptide, which has also been performed using the constant composition technique [99].”
MethodNtourou, K., DeFranco, E. O., Conture, E. G., Walden, T. A., & Mushtaq, N. (2020) · Journal of Fluency Disorders · doi:10.1016/j.jfludis.2020.105748 · Cited by 22
pH-mediated interfacial chemistry and particle interactions in aqueous chlorite dispersions
Tan, H., Skinner, W. M., & Addai‐Mensah, J. (2012) · Chemical Engineering Research and Design · doi:10.1016/j.cherd.2012.08.011 · Cited by 22 · cited 1×
“For example, the NaCl scale shows solubility in the water, while CaCO3, FeS, FeO are soluble in acid [52,53].”
BackgroundHydrophobically modified pectates as novel functional polymers in food and non-food applications
Hromàdková, Z., Malovíková, A., Mozeš, Š., Sroková, I., & Ebringerová, A. (2007) · BioResources · doi:10.15376/biores.3.1.71-78 · Cited by 6 · cited 1×
“[123] have investigated the synthesis of a few pectates from citrus pectin through alkyl amidation followed by alkaline hydrolysis.”
Background
Cited by
Inorganic Scaling in Membrane Desalination: Models, Mechanisms, and Characterization Methods
Rolf, J., Cao, T., Huang, X., Boo, C., Li, Q., & Elimelech, M. (2022) · Environmental Science & Technology · doi:10.1021/acs.est.2c01858 · Cited by 237
Ahmed, M. A., Amin, S., & Mohamed, A. A. (2023) · Heliyon · doi:10.1016/j.heliyon.2023.e14908 · Cited by 234
Metadata
- Authors
- Jafar Mazumder, M. A.
- Venue
- Coatings
- Publisher
- MDPI AG
- Published
- 2020-09-28
- Volume
- 10
- Issue
- 10
- Pages
- 928
- ISSN
- 2079-6412 (ISSN-L)
- OpenAlex
- W3088847534
- Cited by
- 172
- References
- 49
- FWCI
- 4.13
- Type
- journal article
- Language
- en
- Open access
- gold
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.