Abstract
Highly efficient electric power generation from biomass/waste fuels becomes an important worldwide issue to prevent global warming. In these plants, severe high-temperature corrosion and erosion-corrosion damage occur in boiler tubes influenced by HCl, SOx gases, and chlorides as contaminants in fuels. Coating technologies become important as a countermeasure for such damage, because of the easy maintenance, cost performance, and ease of application on various materials. In severe corrosive conditions of boilers, formation of dense, homogenous, and tough coating layers, as well as protective oxide layers of corrosion-resistant materials, are important. In the last 30 years, materials and coating processes applied in shop and on site have progressed based on many field observations and the consideration of deterioration mechanisms in order to maintain long lifetimes in the plants. Furthermore, new innovative coatings are now being developed by using advanced precise control, nanotechnologies, etc. This paper introduces recent trends of advanced coating developments and applications, such as weld-overlay, cladding, thermal spray coating, and slurry coating for biomass/waste boilers. Furthermore, the evaluation results of deterioration mechanisms and lifetime of coatings, and the future issue for innovative coatings, are presented.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Practical estimation of erosion damage caused by solid particle impact
Oka, Y. I., Okamura, K., & Yoshida, T. (2005) · Wear · doi:10.1016/j.wear.2005.01.039 · Cited by 900 · cited 3×
“Impact angle dependence of erosion rates relating erosion mechanisms in materials having various hardness and toughness [34].”
BackgroundInfluentialKawahara, Y. (2002) · Corrosion Science · doi:10.1016/s0010-938x(01)00058-0 · Cited by 184 · cited 3×
“The addition of alloying elements such as Mo, Nb(Cb), Si to Ni–Cr–Fe alloys is considered to be effective in reducing the corrosion rate, as based on field corrosion tests [22].”
BackgroundInfluentialSelf-citationZahs, A., Spiegel, M., & Grabke, H. (1999) · Materials and Corrosion · doi:10.1002/(sici)1521-4176(199910)50:10<561::aid-maco561>3.0.co;2-l · Cited by 131 · cited 2×
“This type of corrosion is referred to as “molten salt induced corrosion,” because the gaseous corrosion reaction becomes active, when the amount of deposits increases and a part of the deposits melts [32].”
BackgroundKawahara, Y. (2007) · Journal of Thermal Spray Technology · doi:10.1007/s11666-006-9012-5 · Cited by 102 · cited 5×
“Deterioration mechanisms of thermal spray coating layer in severe corrosive environment [6].”
BackgroundMethodInfluentialSelf-citationThe role of combustion synthesis in the formation of slurry aluminization
Galetz, M. C., Montero, X., Mollard, M., Günthner, M., Pedraza, F., & Schütze, M. (2013) · Intermetallics · doi:10.1016/j.intermet.2013.08.002 · Cited by 79 · cited 1×
“The good results have been reported [17].”
Kawahara, Y., & Kira, M. (1997) · CORROSION · doi:10.5006/1.3280466 · Cited by 46
Self-citationKawahara, Y. (2006) · Materials and Corrosion · doi:10.1002/maco.200503895 · Cited by 39 · cited 4×
“Schematic illustration of corrosion mechanisms in Ni–Cr–Mo–(Nb, Fe) alloy [33].”
BackgroundMethodInfluentialSelf-citationProduction of Nanocrystalline Ni-20Cr Coatings for High-Temperature Applications
Kumar, M., Singh, H., & Singh, N. (2014) · Journal of Thermal Spray Technology · doi:10.1007/s11666-014-0055-8 · Cited by 31
Advanced Coatings on Furnace Wall Tubes
MATSUBARA, Y., Sochi, Y., Tanabe, M., & TAKEYA, A. (2007) · Journal of Thermal Spray Technology · doi:10.1007/s11666-007-9030-y · Cited by 27
Evaluation of New Corrosion-Resistant Superheater Tubing in High-Efficiency Waste-to-Energy Plants
Kawahara, Y., Nakamura, M., Tsuboi, H., & Yukawa, K.-I. (1998) · CORROSION · doi:10.5006/1.3284886 · Cited by 27 · cited 2×
“9 MPa boilers for corrosion resistance and cost performance, because the corrosion resistance between Ni–Cr–Fe alloys and Ni base alloys is not so different under the steam conditions below 450 °C, as shown in Figure 13 [23].”
BackgroundSelf-citation
Research works printed but not linked: 7
- Formation and Break-down of Protective Oxides Layer in High Temperature Corrosion Resistant Materials Used in Environmental and Energy Equipment. Y Kawahara, Semin. Text Jpn. Inst. Met. 992006
- Performance of corrosion-resistant weld overlays in power boilers & kraft recovery boilers. G Lai, P Hulsizer, Proceedings of the Stainless Steel World/99 Conference. the Stainless Steel World/99 ConferenceDen Haag, The NetherlandsNovember 1999
- Composite Tubes in Waste Incineration Boilers. A Wilson, U Forsberg, M Lunderg, L Nylöf, Proceedings of the Stainless Steel World/99, Den Haag. the Stainless Steel World/99, Den HaagThe NetherlandsNovember 1999
- Improvement of Durability and Evaluation Technologies for Refractories in Waste Incinerator and Industrial Boiler. Y Kawahara, 200961
- The oxidation of silicon-carbide refractory materials. A C Lea, J. Soc. Glass Technol. 331949
- Refractory materials for refuse incinerator. I Iemura, Shinagawa Giho. 23731979
- Ohoba, 2008, Application and Life-time Evaluation of Metal Spray Coatings for Fire-Side Corrosion of Boiler Waterwall, J. Jpn. Boiler Assoc., 348, 14
Cited by
Sadeghi, E., Markocsan, N., & Joshi, S. V. (2019) · Journal of Thermal Spray Technology · doi:10.1007/s11666-019-00938-1 · Cited by 165
Errington, E., Guo, M., & Heng, J. Y. Y. (2023) · Green Chemistry · doi:10.1039/d2gc01433e · Cited by 46
Wang, G., Liu, H., Chen, T., Zhang, X., Li, H., Yu, Y., & Yao, H. (2021) · Corrosion Science · doi:10.1016/j.corsci.2021.109592 · Cited by 36
High Temperature Corrosion Resistant and Anti-slagging Coatings for Boilers: A Review
Khantisopon, K., Singh, S., Jitputti, J., Berndt, C. C., & Ang, A. S. M. (2024) · High Temperature Corrosion of Materials · doi:10.1007/s11085-024-10251-0 · Cited by 30
Qu, Z., & Tian, X. (2024) · Coatings · doi:10.3390/coatings14111391 · Cited by 24
Akhil, U. V., Radhika, N., Rajeshkumar, L., & Sivaswamy, G. (2023) · Journal of Bio- and Tribo-Corrosion · doi:10.1007/s40735-023-00765-6 · Cited by 23
Adoption of strategies for clean combustion of biomass in boilers
Sharma, S., Sharma, M., Mudgal, D., & Bhowmick, H. (2021) · Corrosion Reviews · doi:10.1515/corrrev-2020-0095 · Cited by 23
Wear Transition of CrN Coated M50 Steel under High Temperature and Heavy Load
Zhang, C., Gu, L., Tang, G., & Mao, Y. (2017) · Coatings · doi:10.3390/coatings7110202 · Cited by 23
Recent Development of Corrosion Factors and Coating Applications in Biomass Firing Plants
Wu, D., Yuan, Z., Liu, S., Zheng, J., Wei, X., & Zhang, C. (2020) · Coatings · doi:10.3390/coatings10101001 · Cited by 22
Li, H., Liu, H., Bai, M., Zhang, X., Chi, H., Chen, T., Yu, Y., & Yao, H. (2023) · Corrosion Science · doi:10.1016/j.corsci.2023.111085 · Cited by 21
Hot corrosion behavior of wire-arc sprayed NiCrB coatings
Wang, X., He, D., Guo, X., Zhou, Z., Wang, G., & Guo, F. (2019) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2019.03.058 · Cited by 19
Mele, C., Lionetto, F., & Bozzini, B. (2020) · Coatings · doi:10.3390/coatings10020092 · Cited by 18
Pokwitidkul, S., Chaleawlert‐umpon, S., Treewiriyakitja, P., Kamonsuangkasem, K., Wannapaiboon, S., & Tungtrongpairoj, J. (2024) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2024.130519 · Cited by 17
Wang, Y., Wang, X., Wang, M., & Tan, H. (2020) · Energy & Fuels · doi:10.1021/acs.energyfuels.0c02634 · Cited by 17
Kawase, M., Ido, A., & Morinaga, M. (2019) · Applied Thermal Engineering · doi:10.1016/j.applthermaleng.2019.02.123 · Cited by 16
Wu, X., Li, B., Wang, W., Qi, S., Wu, Y., & Wang, Z. (2024) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2024.131291 · Cited by 15
Zhao, Z., Yao, X., Xu, K., & Li, J. (2025) · Journal of the Energy Institute · doi:10.1016/j.joei.2025.102227 · Cited by 14
Ramandhany, S., Triyono, D., Sugiarti, E., Wismogroho, A. S., Izzuddin, H., Afandi, A. M., Widayatno, W. B., Desiati, R. D., & Sundawa, R. Y. (2024) · Journal of Thermal Spray Technology · doi:10.1007/s11666-024-01720-8 · Cited by 13
“Numerous studies have been conducted to investigate the impact of sulfate or chloride environments on the hot corrosion and erosion of various coating materials (Ref 4, 5, 19-21).”
Kaddoura, M., Majeau‐Bettez, G., Amor, B., Moreau, C., & Margni, M. D. (2022) · Sustainable materials and technologies · doi:10.1016/j.susmat.2022.e00425 · Cited by 12
“Corrosion resistance coatings for critical components in biomass and waste-to-energy facilities have been recently developed to extend plant lifetimes [18].”
Mušálek, R., Tesař, T., Medřický, J., Lukáč, F., Chráska, T., & Gupta, M. (2020) · Journal of Thermal Spray Technology · doi:10.1007/s11666-020-00990-2 · Cited by 12
Corrosion Mechanisms and Anti‐Corrosive Coatings for Mild Steel in Industrial Environments
Karthick, S., Sonwani, R. K., Sinha, T., Gope, S., Chawla, R., & Pal, D. (2025) · ChemBioEng Reviews · doi:10.1002/cben.70036 · Cited by 8
Gutiérrez, M., Illana, A., Bahillo, A., Benito, M. J., García-Martín, G., Pérez, F. J., & Agüero, A. (2022) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2022.128982 · Cited by 8
Torrefaction as a Way to Remove Chlorine and Improve the Energy Properties of Plant Biomass
Bajcar, M., Zardzewiały, M., Saletnik, B. A., Zaguła, G., Puchalski, C., & Gorzelany, J. (2023) · Energies · doi:10.3390/en16217365 · Cited by 8
Wei, Z., Wang, L., Liang, X., Sharma, D., Zhu, H., Yuan, Z., & Wu, L. (2026) · Applied Energy · doi:10.1016/j.apenergy.2026.128092 · Cited by 7
Lindmark, H., Faust, R. L., Sand, T., Johansson, L.-G., Knutsson, P., & Liske, J. (2024) · Fuel · doi:10.1016/j.fuel.2024.133178 · Cited by 7
Prashar, G., & Vasudev, H. (2020) · Advances in chemical and materials engineering book series · doi:10.4018/978-1-7998-4870-7.ch005 · Cited by 7
Factors influencing the aqueous electrochemical response of TiC–Ni3Al cermets
Memarrashidi, Z., & Plucknett, K. P. (2017) · Journal of materials research/Pratt's guide to venture capital sources · doi:10.1557/jmr.2017.178 · Cited by 6
Issues of Corrosion and Degradation under Dusty Deposits of Energy Biomass
Bojanowska, M., Chmiel, J., Sozańska, M., Chmiela, B., Grudzień, J., & Halska, J. (2021) · Energies · doi:10.3390/en14030534 · Cited by 6
Hot Corrosion Behavior of Arc-Sprayed NiCrB and NiCrTi Coatings with Different Oxide Contents
Wang, X., He, D., Zhou, Z., Shao, W., Guo, X., & Wang, G. (2022) · Coatings · doi:10.3390/coatings12040497 · Cited by 5
Kumari, A., Sati, P., & Kumar, S. (2023) · Engineering materials · doi:10.1007/978-3-031-45534-6_2 · Cited by 5
Failure analysis of grate in a municipal solid waste incineration plant
Kochmańska, A. E., & Kochmański, P. (2024) · Engineering Failure Analysis · doi:10.1016/j.engfailanal.2024.108823 · Cited by 4
Pérez-Muñoz, D., Galeano-Jaramillo, Y., Arévalo, J. L. M., Tristancho-Reyes, J. L., Ríos‒Reyes, C. A., & Villarreal‒Jaimes, C. A. (2024) · Results in Surfaces and Interfaces · doi:10.1016/j.rsurfi.2024.100283 · Cited by 4
Hot corrosion of high-entropy alloys induced by KCl-55 %ZnCl2 molten salt films in air
Zhang, H., Wu, J., Wang, Q., & Zeng, C. (2025) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2025.184181 · Cited by 4
Development of CNT mixed HVOF coating for water tube boiler material to improve the degradations
Kumari, J., & Jegadeeswaran, N. (2021) · Materials Today Proceedings · doi:10.1016/j.matpr.2021.10.177 · Cited by 4
Qu, Z., & Josue, N. O. (2021) · Graphene · doi:10.4236/graphene.2021.102002 · Cited by 4
“Impurities which influence corrosion-erosion damage of boiler combustion gas environment in WTE plant [4].”
BackgroundInfluence of WS2 Nanoparticles Lubricants on Physical Characteristics of Wrought Aluminium Alloys
Al-Samarai, R. A., Mahmood, A. S., & Ahmed, O. M. (2019) · Iraqi Journal of Science · doi:10.24996/ijs.2019.60.6.7 · Cited by 4
Environmental Impacts of Rice Husk-Derived Silica under Uncertainty: Is “Bio” better?
Errington, E., Guo, M., & Heng, J. Y. Y. (2022) · Computer-aided chemical engineering/Computer aided chemical engineering · doi:10.1016/b978-0-323-95879-0.50270-8 · Cited by 4
Chen, T., Liang, Y., Hua, C., Cao, W., Su, C., Yang, Y., Yang, Z., Huang, T., Liu, G., & Song, P. Y. (2026) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2026.188311 · Cited by 3
Nanoindentation Evaluation of Suspension Thermal Sprayed Nanocomposite WC-Co Coatings
Ali, O., Ahmed, R., Faisal, N. H., Alanazi, N. M., Elakwah, Y. O., & Goosen, M. F. A. (2017) · Key engineering materials · doi:10.4028/www.scientific.net/kem.735.225 · Cited by 3
Surface Engineering Towards Better Material Performance
Wang, Y., Pang, Z., & He, J. (2022) · Royal Society of Chemistry eBooks · doi:10.1039/9781788019613-00106 · Cited by 3
Ash deposition mechanisms in Waste-to-Energy plants
NAGANUMA, H., Mori, T., Watanabe, S., SAWADA, A., Taeko, G. O. T. O., Ueki, Y., Yoshiie, R., & Naruse, I. (2022) · Mechanical Engineering Journal · doi:10.1299/mej.21-00435 · Cited by 3
Hot corrosion of Inconel 625 and NiCrMoAl alloys induced by KCl–55 %ZnCl2 molten salt films in air
Zhang, H., Wu, J., Wang, Q., & Zeng, C. (2025) · Journal of Materials Research and Technology · doi:10.1016/j.jmrt.2025.08.179 · Cited by 2
Zhang, H., Wu, J., Liu, H. J., Yang, L., Wang, Q., Zhang, D., & Zeng, C. (2026) · Corrosion Communications · doi:10.1016/j.corcom.2026.03.014 · Cited by 2
High‐Temperature Corrosion‐Resistant Coatings for the Energy Sector
Kumari, A., Sati, P., Kumar, S., & Singh, R. P. (2024) · Wiley eBooks · doi:10.1002/9781394263172.ch14 · Cited by 2
High Temperature Corrosion Study on NiCr Coated Low Alloy and Mild Steel
Technology, B. I. O. E. A., Kumar, J., Kushwaha, A., Technology, B. I. O. E. A., Rajput, S. K., Technology, B. I. O. E. A., Soota, T., & Technology, B. I. O. E. A. (2024) · International Journal of Integrated Engineering · doi:10.30880/ijie.2024.16.06.001 · Cited by 1
Zhang, H., & Wu, J. (2025) · Journal of Materials Engineering and Performance · doi:10.1007/s11665-025-12572-w · Cited by 1
Yang, Z., Jian, Y., Qi, H., Chen, Z., Zhang, J., & Huang, Z. (2026) · Corrosion Communications · doi:10.1016/j.corcom.2026.06.009 · Cited by 1
EFFECT OF MO DURING THE OXIDATION OF NI20CR-XMO ALLOYS AT 570°C
Izzuddin, H. (2022) · Metalurgi · doi:10.14203/metalurgi.v36i3.610 · Cited by 1
Case Studies from Boiler Tube Failures in the Electric Power Generating Industry
Gavras, A. G., & Winn, P. (2022) · Elsevier eBooks · doi:10.1016/b978-0-12-822944-6.00040-2 · Cited by 1
Bourtsalas, A. C., & Yan, D. (2023) · Technical Annals · doi:10.12681/ta.36792 · Cited by 1
Szajna, E., Moskal, G., Lewtak, R., Jagiełło, K., Tomaszewska, A., TUPAJ, M., Dudek, A., Szymański, K., Trzcionka-Szajna, A., & Wrona, A. (2025) · Journal of Pressure Vessel Technology · doi:10.1115/1.4069409 · Cited by 1
Short overview on the mitigation of corrosion in coal gasification plant
Agboola, O., Fayomi, O. S. I., Adegbola, T. A., Moropeng, L., & Sani., S. E. (2022) · AIP conference proceedings · doi:10.1063/5.0092508
Ash deposition and corrosion mechanisms of tubes in Waste-to-Energy plants
NAGANUMA, H., Mori, T., Watanabe, S., SAWADA, A., Taeko, G. O. T. O., Ueki, Y., Yoshiie, R., & Naruse, I. (2024) · Mechanical Engineering Journal · doi:10.1299/mej.23-00486
Pokwitidkul, S., Chaleawlert‐umpon, S., Thongyoug, P., Kamonsuangkasem, K., Wannapaiboon, S., & Tungtrongpairoj, J. (2024) · Materials science forum · doi:10.4028/p-h0zwte
Shetty, R. K., & Hebbale, A. M. (2025) · High Temperature Material Processes An International Quarterly of High-Technology Plasma Processes · doi:10.1615/hightempmatproc.2025060458
Modified high hardness steel coating for biomass corrosion protection
Agüero, A., Gutiérrez, M., Audigié, P., Rodríguez, S., & Pascual, J. (2025) · Materials for Renewable and Sustainable Energy · doi:10.1007/s40243-025-00330-w
“Coatings such as Ni-based alloy 625 applied via overlay welding or laser cladding, as well as thermal spray coatings, are currently employed for corrosion protection in biomass boilers [ 8 ].”
The Impacts of Surface Engineering on the Environment and the Material Flows
Kaddoura, M. (2024) · PolyPublie (École Polytechnique de Montréal)
Corrosion protection effect of polypyrrole on acrylic and powder coated sheet
Topaloğlu, K. (2023) · Hitit University Institutional Repository
Online monitoring of deposit-induced corrosion in a Waste-to-Energy boiler
Liu, W., Wang, Y., Wang, Y., Liu, Y., Du, A., Ren, Q., Zheng, X., Chen, X., Zhou, M., Wang, Y., et al. (2026) · Waste Management · doi:10.1016/j.wasman.2026.115507
Hot Corrosion Resistance of a NiCrMoAlSi Cladding Layers Under K2SO4-ZnCl2 Molten Salt Film in Air
Zhang, H., & Wu, J. (2026) · CORROSION · doi:10.5006/4846
Hot corrosion performance of Mo-containing nickel-based CMT cladding layers
Chu, Q., Liu, R., Song, H., Du, Y., Wang, Z., Wang, J., Liu, J., Bai, J., & Yang, D. (2026) · International Journal of Pressure Vessels and Piping · doi:10.1016/j.ijpvp.2026.105908
Yu, D., Wang, K., Cheng, J., Chen, X., Tan, B., Jiang, Y., & Dai, Q. (2026) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2026.189550
Nurhidayat, R. F. (2026) · Universitas Pasundan institutional repositories & scientific journals (Universitas Pasundan)
Gao, Y., Xie, S., Chen, M., Chen, Z., Li, Y., & Huang, D. (2026) · Coatings · doi:10.3390/coatings16091078
Maj, I., & Łój, P. (2026) · Energies · doi:10.3390/en19194668
Trivedi, J. K., Nikitin, Y., & Castaldi, M. J. (2026) · Materials and Corrosion · doi:10.1002/maco.70270
Metadata
- Authors
- Kawahara, Y.
- Affiliations
- DAI-ICHI HIGH Frequency Co., Ltd. (Japan) (JP)
- Corresponding author
- Kawahara, Yuuzou
- ORCID
- Kawahara, Yuuzou
- Venue
- Coatings
- Publisher
- MDPI AG
- Published
- 2016-08-05
- Volume
- 6
- Issue
- 3
- Pages
- 34
- ISSN
- 2079-6412 (ISSN-L)
- OpenAlex
- W2476770397
- Cited by
- 62
- References
- 20
- Citations by year
- 2026: 12 · 2025: 8 · 2024: 11 · 2023: 5 · 2022: 10 · 2021: 5 · 2020: 5 · 2019: 3 · 2017: 3
- FWCI
- 2.44
- Type
- journal article
- Language
- en
- Open access
- gold
- doi.org
- Licence
- Locations
- Coatings (publishedVersion, cc-by)
- Topics
- Physical Sciences › Materials Science › Surfaces, Coatings and Films › High-Temperature Coating Behaviors
- Physical Sciences › Engineering › Mechanical Engineering › Surface Treatment and Coatings
- Physical Sciences › Materials Science › Materials Chemistry › Corrosion Behavior and Inhibition
- Keywords
- corrosion protection coatings, biomass boiler, waste-to-energy plants, high-temperature corrosion, erosion-corrosion, boiler tubes, overlay welding, cladding, thermal spray coatings, slurry coating, coating lifetime
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.