Review of Wood Modification and Wood Functionalization Technologies
Open accessThe DOI matches its Crossref record; 144 of the 144 references it cites were found in a registry or an index.
Abstract
Wood modifications are becoming popular as a way to enhance the performance of wood, either to make it more durable, improve the performance of wood, or give it new functionality as a multifunctional or smart material. While wood modifications have been examined since the early 1900s, the topic has become a dominant area of study in wood science over the past decade. This review summarizes recent advances and provides future perspective on a selection of wood modifications, i.e., the methods that are currently commercialized (acetylation, furfurylation, and thermal modification), a rediscovered ancient practice (charring), a family of polymerization modifications that have so far made it to the pilot scale, and examples of novel wood-based functional materials explored at laboratory scale.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Handbook of Wood Chemistry and Wood Composites
(2005) · CRC Press eBooks · doi:10.1201/9780203492437 · Cited by 1,480
Structure–property–function relationships of natural and engineered wood
Chen, C., Kuang, Y., Zhu, S., Burgert, I., Keplinger, T., Gong, A., Li, T., Berglund, L., Eichhorn, S. J., & Hu, L. (2020) · Nature Reviews Materials · doi:10.1038/s41578-020-0195-z · Cited by 1,295 · cited 2×
“Considering the multi-hierarchical structure of wood based on aligned microchannels it is obvious that wood represents a promising material for different types of membraneand flow through applications, such as filtration of catalytic processes [311].”
BackgroundSelf-citationWood modification by heat treatment: A review
Esteves, B. M., & Pereira, H. M. (2008) · BioResources · doi:10.15376/biores.4.1.370-404 · Cited by 1,270 · cited 1×
“Technical details of some commercial processes are discussed by Esteves and Pereira [143], Militz and Altgen [144], and Sandberg and Kutnar [145].”
MethodSiau, J. F. (1984) · Springer series in wood science · doi:10.1007/978-3-642-69213-0 · Cited by 1,190 · cited 1×
“(The rule of thumb exists because the bordered pits connecting tracheids in the latewood xylem do not as easily close during drying as those between tracheids in the earlywood [133]).”
BackgroundWood Modification: Chemical, Thermal and Other Processes
Hill, C. A. S. (2006) · Wiley eBooks · doi:10.1002/0470021748 · Cited by 1,138
Hydrothermal processing of lignocellulosic materials
Garrote, G., Domínguez, H., & Parajó, J. C. (1999) · Holz als Roh- und Werkstoff · doi:10.1007/s001070050039 · Cited by 880 · cited 1×
“Furfural and hydroxymethylfurfural are the dehydration products of pentoses and hexoses, respectively, and they can undergo further degradation or react with lignin and other degradation products [148–150].”
BackgroundHighly Anisotropic, Highly Transparent Wood Composites
Zhu, M., Song, J., Li, T., Gong, A., Wang, Y., Dai, J., Yao, Y., Luo, W., Henderson, D., & Hu, L. (2016) · Advanced Materials · doi:10.1002/adma.201600427 · Cited by 744 · cited 3×
“Since these reports by Bing and Berglund et al. [315,318] considerable progress has been made regarding the material.”
BackgroundResultRole of forest regrowth in global carbon sink dynamics
Pugh, T. A. M., Lindeskog, M., Smith, B., Poulter, B., Arneth, A., Haverd, V., & Calle, L. (2019) · Proceedings of the National Academy of Sciences · doi:10.1073/pnas.1810512116 · Cited by 731 · cited 1×
“While wood has a long history as a construction material and with numerous environmental benefits [5], the use of wood as a building material is made difficult by its interaction with water.”
BackgroundCharacterisation of thermally modified wood: molecular reasons for wood performance improvement
Tjeerdsma, B. F., Boonstra, M., Pizzi, A., Tekely, P., & Militz, H. (1998) · Holz als Roh- und Werkstoff · doi:10.1007/s001070050287 · Cited by 672 · cited 1×
“Furfural and hydroxymethylfurfural are the dehydration products of pentoses and hexoses, respectively, and they can undergo further degradation or react with lignin and other degradation products [148–150].”
BackgroundBornehag, C.-G., Blomquist, G., Gyntelberg, F., Järvholm, B., Malmberg, P., Nordvall, L., Nielsen, A., Pershagen, G., & Sundell, J. (2001) · Indoor Air · doi:10.1034/j.1600-0668.2001.110202.x · Cited by 659 · cited 1×
“While mold fungi do not affect the strength of wood [9], and molds may grow on many surfaces in addition to wood, molds discolor wood and may present a health hazard in the indoor environment [10].”
BackgroundChemical Finishing of Textiles
Schindler, W., Hauser, P., & Hauser, P. (2004) · CRC Press eBooks · doi:10.1201/9781439823477 · Cited by 591
Durability of heat-treated wood
Kamdem, D. P., Pizzi, A., & Jermannaud, A. (2002) · Holz als Roh- und Werkstoff · doi:10.1007/s00107-001-0261-1 · Cited by 574 · cited 1×
“However, thermal modification is less effective in improving the biological durability in ground-contact, which has been shown under laboratory conditions [181,187] and in field tests [182].”
BackgroundLi, Y., Fu, Q., Yu, S., Yan, M., & Berglund, L. (2016) · Biomacromolecules · doi:10.1021/acs.biomac.6b00145 · Cited by 570 · cited 2×
“Since these reports by Bing and Berglund et al. [315,318] considerable progress has been made regarding the material.”
BackgroundResultBioinspired wood nanotechnology for functional materials
Berglund, L. A., & Burgert, I. (2018) · Advanced Materials · doi:10.1002/adma.201704285 · Cited by 518 · cited 5×
“It is beyond the scope of this section to provide a complete overview of this vastly growing research field and the reader is referred to detailed recent reviews [310–313].”
BackgroundInfluentialWood modification technologies - a review
Sandberg, D., Kutnar, A., & Mantanis, G. (2017) · iForest - Biogeosciences and Forestry · doi:10.3832/ifor2380-010 · Cited by 486
Melamine formaldehyde: curing studies and reaction mechanism
Merline, D. J., Vukusic, S., & Abdala, A. A. (2012) · Polymer Journal · doi:10.1038/pj.2012.162 · Cited by 479 · cited 1×
“Basically, the morphology of polymerized resin and the curing reaction depend on distinct factors, including the reactive functional groups, molar ratios of the reactants, the temperature and moisture conditions during the reaction, and the pH [261,262,265,283–285].”
BackgroundMechanical and chemical behavior of spruce wood modified by heat
Yildiz, S., Gezer, E. D., & Yildiz, U. C. (2006) · Building and Environment · doi:10.1016/j.buildenv.2005.07.017 · Cited by 456 · cited 1×
“For example, the tensile strength parallel to the grain decreases strongly after thermal modification [188,189], while the compression strength shows a moderate decrease [190] or even increases [188].”
BackgroundInvestigation of wood wettability changes during heat treatment on the basis of chemical analysis
Hakkou, M., Pétrissans, M., Zoulalian, A., & Gérardin, P. (2005) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2004.10.017 · Cited by 388 · cited 1×
“Hakkou et al. [167,197] showed that an exposure of wood to elevated temperatures reduces its wettability by water before mass loss and hemicellulose degradation take place.”
BackgroundThermal modification of wood—a review: chemical changes and hygroscopicity
Hill, C., Altgen, M., & Rautkari, L. (2021) · Journal of Materials Science · doi:10.1007/s10853-020-05722-z · Cited by 378 · cited 5×
“As reviewed by Hill et al. [25] several explanations for the behavior of thermally modified wood other than the removal of hemicelluloses have been provided in the literature, such as the formation of covalent cross-links, permanently aggregated structures after drying at elevated temperatures, or…”
BackgroundMethodInfluentialSelf-citationBoonstra, M. J., Van Acker, J., Tjeerdsma, B. F., & Kegel, E. V. (2007) · Annals of Forest Science · doi:10.1051/forest:2007048 · Cited by 367 · cited 2×
“The strength loss is dependent on the direction of load [188].”
BackgroundInvestigations of the reasons for fungal durability of heat-treated beech wood
Hakkou, M., Pétrissans, M., Gérardin, P., & Zoulalian, A. (2006) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2005.04.042 · Cited by 346 · cited 2×
“Hemicellu-lose degradation interferes with the load-sharing capabilities of the cell wall to decrease the strength and toughness of the wood [153,194], reduces the number of sorption sites for water [175,195] and removes easily accessible nutrients for decay fungi [180].”
BackgroundChemistry of Weathering and Protection
FEIST, W. C., & HON, D. N.-S. (1984) · Advances in Chemistry · doi:10.1021/ba-1984-0207.ch011 · Cited by 341 · cited 2×
“Visible light only penetrates the surface down to about 200 (cid:22) m [238] and degraded components take time to wash off.”
BackgroundEsteves, B., Marques, A. V., Domingos, I., & Pereira, H. (2007) · Wood Science and Technology · doi:10.1007/s00226-006-0099-0 · Cited by 304 · cited 2×
“Consequently, wood property changes often correlate with the wood mass loss during the thermal modification, which is primarily caused by hemicellulose degradation [159,196].”
BackgroundInfluentialPhotodegradation and photostabilisation of wood – the state of the art
George, B., Suttie, E., Merlin, A., & Deglise, X. (2005) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2004.10.018 · Cited by 303 · cited 1×
“The most important component to consider in the context of weathering is lignin, which is the only structural polymer to absorb UV radiation [236–238].”
BackgroundMagnetic Resonance Studies of Thermally Modified Wood
Sivonen, H., Maunu, S. L., Sundholm, F., Jämsä, S., & Viitaniemi, P. (2002) · Holzforschung · doi:10.1515/hf.2002.098 · Cited by 300
Lignin‐Retaining Transparent Wood
Li, Y., Fu, Q., Rojas, R., Yan, M., Lawoko, M., & Berglund, L. (2017) · ChemSusChem · doi:10.1002/cssc.201701089 · Cited by 298 · cited 1×
“For example, lignin-retaining wood was developed, bio-based polymeric systems were introduced for refractive index matching and targeted interface modifications between cellulose matrix and the cellulose scaffold improved the overall transparency [319–321].”
BackgroundBiotechnology and microbiology of coal degradation
Fakoussa, R. M., & Hofrichter, M. (1999) · Applied Microbiology and Biotechnology · doi:10.1007/s002530051483 · Cited by 274 · cited 1×
“Everything considered, there are degrading organisms even for lignite and hard coal [235], so complete protection of wood may be impossible without biocides.”
BackgroundDominguez- Rodrigo, M., Serrallonga, J., Juan-Tresserras, J., Alcala, L., & Luque, L. (2001) · Journal of Human Evolution · doi:10.1006/jhev.2000.0466 · Cited by 264 · cited 1×
“Evidence of the use of wood by ancient cultures dates back at least 1.5 million years [1].”
BackgroundInfluentialThermal Modifications in Softwood Studied by FT‐IR and UV Resonance Raman Spectroscopies
Nuopponen, M., Vuorinen, T., Jämsä, S., & Viitaniemi, P. (2005) · Journal of Wood Chemistry and Technology · doi:10.1081/wct-120035941 · Cited by 263
Sun, J., Guo, H., Ribera, J., Wu, C., Tu, K., Binelli, M., Panzarasa, G., Schwarze, F. W. M. R., Wang, Z. L., & Burgert, I. (2020) · ACS Nano · doi:10.1021/acsnano.0c05493 · Cited by 248 · cited 2×
“Recently, Sun et al. [325] tackled these shortcomings by simple delignification approaches to enhance the electrical output.”
BackgroundControl of wood thermal treatment and its effects on decay resistance: a review
Candelier, K., Thevenon, M.-F., Petrissans, A., Dumarcay, S., Gerardin, P., & Petrissans, M. (2016) · Annals of Forest Science · doi:10.1007/s13595-016-0541-x · Cited by 247 · cited 1×
“Contact charring has been proposed [205–207 , 245 ] as a viable modification method to facilitate a longer modification time and a careful control of temperature.”
MethodTransparent Wood for Thermal Energy Storage and Reversible Optical Transmittance
Montanari, C., Li, Y., Chen, H., Yan, M., & Berglund, L. A. (2019) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.9b05525 · Cited by 236 · cited 1×
“In addition, transparent wood possesses lower thermal conductivity compared to glass, high impact strength, and low density [310,322,323].”
Nanostructured Wood Hybrids for Fire-Retardancy Prepared by Clay Impregnation into the Cell Wall
Fu, Q., Medina, L., Li, Y., Carosio, F., Hajian, A., & Berglund, L. A. (2017) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.7b10008 · Cited by 235 · cited 1×
“These include a variety of bio-inspired mineralization on the nano-and submicron scale [333–335], co-reaction with modifications for improving decay resistance [336], formation of zinc oxide nano-rods [337], and clay impregnation of cell walls [338].”
BackgroundWettability of Heat-Treated Wood
Pétrissans, M., Gérardin, P., bakali, I. E., & Serraj, M. (2003) · Holzforschung · doi:10.1515/hf.2003.045 · Cited by 226
Rowell, R. M., Ibach, R. E., McSweeny, J., & Nilsson, T. (2009) · Wood Material Science and Engineering · doi:10.1080/17480270903261339 · Cited by 212 · cited 2×
“The first hypotheses, that the acetylation makes the wood polymers unrecognizable to enzymes produced by the decay fungus or unavailable as fungal nutrients have been mentioned in reviews by Rowell [58,59] and Hill [60].”
BackgroundTransparent Wood – A New Approach in the Functional Study of Wood Structure
Fink, S. (1992) · Holzforschung · doi:10.1515/hfsg.1992.46.5.403 · Cited by 206 · cited 1×
“The basic idea of transparent wood goes back to initial works by Fink et al. in 1992 [317].”
Fungal Degradation of Wood: Emerging Data, New Insights and Changing Perceptions
Goodell, B., Winandy, J. E., & Morrell, J. J. (2020) · Coatings · doi:10.3390/coatings10121210 · Cited by 199 · cited 1×
“Brown rot fungi are believed to degrade wood using a two-step approach, with an oxidative phase followed by a hydrolytic phase [129,130].”
Metsä-Kortelainen, S., Antikainen, T., & Viitaniemi, P. (2006) · Holz als Roh- und Werkstoff · doi:10.1007/s00107-005-0063-y · Cited by 194
Wood-water relationships and their role for wood susceptibility to fungal decay
Brischke, C., & Alfredsen, G. (2020) · Applied Microbiology and Biotechnology · doi:10.1007/s00253-020-10479-1 · Cited by 192 · cited 1×
“In other words, furfurylation reduces the space available for water within the cell wall, which in itself is known to slow down or even hinder fungal decomposition [43,128], as discussed above regarding acetylation.”
BackgroundMantanis, G. I. (2017) · BioResources · doi:10.15376/biores.12.2.mantanis · Cited by 179 · cited 1×
“The reaction between acetic anhydride and wood is a single displacement reaction; that is there is a 1:1 substitution of acetyl groups for hydroxyl groups and no further reactions or polymerizations occur [35].”
BackgroundMerk, V., Chanana, M., Keplinger, T., Gaan, S., & Burgert, I. (2015) · Green Chemistry · doi:10.1039/c4gc01862a · Cited by 177
Self-citationBurning rate of solid wood measured in a heat release rate calorimeter
Tran, H. C., & White, R. H. (1992) · Fire and Materials · doi:10.1002/fam.810160406 · Cited by 174 · cited 1×
“Tran and White [243] quote several studies placing the char formation temperature between 280 and 350 ◦ C.”
BackgroundThygesen, L. G., Thybring, E. E., & Hoffmeyer, P. (2010) · Holzforschung · doi:10.1515/hf.2010.044 · Cited by 173 · cited 1×
“In a desorption study carried out for the upper part of the hygroscopic range [110], the reduction compared to untreated wood was more modest than these values, most likely because the EMC calculation was based on the dry weight of the unmodified wood, not the modified wood.”
BackgroundSelf-citationStudy on the deacetylation of hemicelluloses during the hydrothermal processing of Eucalyptus wood
Garrote, G., Domínguez, H., & Parajó, J. C. (2001) · Holz als Roh- und Werkstoff · doi:10.1007/s001070050473 · Cited by 171 · cited 1×
“Their degradation typically starts with the cleavage of acetyl groups from the side groups of hemicelluloses, i.e., xylans, which results in the formation of acetic acid that catalyzes further degradation [147].”
BackgroundRepellin, V., & Guyonnet, R. (2004) · Holzforschung · doi:10.1515/hf.2005.005 · Cited by 170 · cited 2×
“Based on results from differential scanning calorimetry and chemical composition analyses, Repellin and Guyonnet [198] concluded that the reduction in swelling and fiber saturation point of thermally modified wood cannot be attributed to hemicellulose degradation.”
ResultOn the effect of heat on the chemical composition and dimensions of thermally-modified wood
González-Peña, M. M., Curling, S. F., & Hale, M. D. C. (2009) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2009.09.003 · Cited by 168 · cited 1×
“In drying and re-wetting cycles, thermally modified wood not only shows a reduced water-saturated wood volume [175,176], but the removal of cell wall constituents also reduces the dry wood volume compared to untreated wood [177].”
BackgroundOptimisation of a two-stage heat treatment process: durability aspects
Boonstra, M. J., van Acker, J., Kegel, E., & Stevens, M. (2007) · Wood Science and Technology · doi:10.1007/s00226-006-0087-4 · Cited by 168 · cited 1×
“In laboratory tests with basidiomycetes on an agar malt-medium, an improved resistance has been found for a number of wood decaying basidiomycetes, including white-and brown-rot fungi [179–182].”
BackgroundHigh Performance, Fully Bio‐Based, and Optically Transparent Wood Biocomposites
Montanari, C., Ogawa, Y., Olsén, P., & Berglund, L. A. (2021) · Advanced Science · doi:10.1002/advs.202100559 · Cited by 166 · cited 1×
“For example, lignin-retaining wood was developed, bio-based polymeric systems were introduced for refractive index matching and targeted interface modifications between cellulose matrix and the cellulose scaffold improved the overall transparency [319–321].”
BackgroundHill, C. A. S., Forster, S. C., Farahani, M. R. M., Hale, M. D. C., Ormondroyd, G. A., & Williams, G. R. (2004) · International Biodeterioration & Biodegradation · doi:10.1016/j.ibiod.2004.07.003 · Cited by 166 · cited 3×
“Although it is often claimed that acetylated wood with a high mass gain (above R mod ~0.15–0.20 g g − 1 ) is decay resistant [66–74], many recent papers have shown that acetylation does not prevent decay but rather greatly reduces the decay kinetics [57,60,62,63].”
BackgroundInfluentialInvestigation of the chemical modifications of beech wood lignin during heat treatment
Brosse, N., El Hage, R., Chaouch, M., Pétrissans, M., Dumarçay, S., & Gérardin, P. (2010) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2010.05.018 · Cited by 164 · cited 1×
“However, although the lignin content increases, lignin still undergoes chemical changes during thermal modification involving both depolymerization and repolymerization [154,156].”
BackgroundStaybwood—Heat-Stabilized Wood
Stamm, A. J., Burr, H. K., & Kline, A. A. (1946) · Industrial & Engineering Chemistry · doi:10.1021/ie50438a027 · Cited by 162 · cited 1×
“After early attempts at a commercialization in the USA [139] and in Germany [140,141], the industrial production of thermally modified wood began in earnest in the 1990s in Finland, France, Germany, and the Netherlands.”
BackgroundLang, A. W., Li, Y., De Keersmaecker, M., Shen, D. E., Österholm, A. M., Berglund, L., & Reynolds, J. R. (2018) · ChemSusChem · doi:10.1002/cssc.201702026 · Cited by 160
Piezoelectricity as a fundamental property of wood
Fukada, E. (1968) · Wood Science and Technology · doi:10.1007/bf00350276 · Cited by 157 · cited 1×
“Initial studies on “electromechanical coupling” of wood and wood materials dates to the 1940s and the reported piezoelectrical effects were small, around 1/20 of that of a quartz crystal [324].”
BackgroundCell-wall hardness and Young's modulus of melamine-modified spruce wood by nano-indentation
Gindl‐Altmutter, W., & Gupta, H. S. (2002) · Composites Part A Applied Science and Manufacturing · doi:10.1016/s1359-835x(02)00080-5 · Cited by 152
Functionalized wood with tunable tribopolarity for efficient triboelectric nanogenerators
Sun, J., Tu, K., Büchele, S., Koch, S. M., Ding, Y., Ramakrishna, S. N., Stucki, S., Guo, H., Wu, C., Keplinger, T., et al. (2021) · Matter · doi:10.1016/j.matt.2021.07.022 · Cited by 149 · cited 1×
“This functionalized wood possess potential for the design of the next generation of sustainable power supplies in smart buildings [327].”
BackgroundSelf-citationProperties of furfurylated wood (Pinus pinaster)
Esteves, B., Nunes, L., & Pereira, H. (2010) · European Journal of Wood and Wood Products · doi:10.1007/s00107-010-0480-4 · Cited by 147 · cited 3×
“For a furfurylation mass gain of around 0.38 g g − 1 , Esteves et al. [109] obtained ASE values in the range from 29–45% depending on the RH interval tested.”
BackgroundInfluentialBio-inspired functional wood-based materials – hybrids and replicates
Burgert, I., Cabane, É., Zollfrank, C., & Berglund, L. A. (2015) · International Materials Reviews · doi:10.1179/1743280415y.0000000009 · Cited by 140 · cited 1×
“For example, in the case of transparent wood, low density species are the wood of choice whereas for membrane application wood species with large vessels should be applied [310,314].”
BackgroundMineralization of wood by calcium carbonate insertion for improved flame retardancy
Merk, V. M., Chanana, M., Gaan, S., & Burgert, I. (2016) · Holzforschung · doi:10.1515/hf-2015-0228 · Cited by 135 · cited 1×
“These include a variety of bio-inspired mineralization on the nano-and submicron scale [333–335], co-reaction with modifications for improving decay resistance [336], formation of zinc oxide nano-rods [337], and clay impregnation of cell walls [338].”
BackgroundThermal Decomposition of Cellulose Crystallites in Wood
Kim, D., Nishiyama, Y., Wada, M., Kuga, S., & Okano, T. (2001) · Holzforschung · doi:10.1515/hf.2001.084 · Cited by 133 · cited 1×
“Crystalline cellulose is presumably unaffected by temperatures below 300 ◦ C [155].”
BackgroundImpregnation of softwood cell walls with melamine-formaldehyde resin
Gindl‐Altmutter, W. (2002) · Bioresource Technology · doi:10.1016/s0960-8524(02)00233-x · Cited by 131
Luminescent and Hydrophobic Wood Films as Optical Lighting Materials
Fu, Q., Tu, K., Goldhahn, C., Keplinger, T., Adobes‐Vidal, M., Sorieul, M., & Burgert, I. (2020) · ACS Nano · doi:10.1021/acsnano.0c06110 · Cited by 127
Self-citationEnvironmentally Benign Wood Modifications: A Review
Dong, Y., Wang, K., Li, J., Zhang, S., & Shi, S. Q. (2020) · ACS Sustainable Chemistry & Engineering · doi:10.1021/acssuschemeng.0c00342 · Cited by 126
Mode of action of brown rot decay resistance in modified wood: a review
Ringman, R., Pilgård, A., Brischke, C., & Richter, K. (2013) · Holzforschung · doi:10.1515/hf-2013-0057 · Cited by 126 · cited 4×
“Recent reviews on the mechanism of wood protection in acetylated wood by Ringman et al. [55–57] have summarized five major competing theories: (1) acetylation renders the wood polymers unrecognizable to fungal enzymes, (2) acetylation blocks the availability of nutrients to the fungus, (3)…”
BackgroundInfluentialJakes, J. E., Hunt, C. G., Zelinka, S. L., Ciesielski, P. N., & Plaza, N. Z. (2019) · Forests · doi:10.3390/f10121084 · Cited by 119 · cited 7×
“The polymer science models for diffusion in wood developed by Jakes [75,82] give important clues to how acetylation may greatly reduce the diffusion kinetics, and thus retard fungal growth in acetylated wood.”
BackgroundInfluentialSelf-citationDeterioration and Protection of Sustainable Biomaterials
Schultz, T. P., Goodell, B. S., & Nicholas, D. D. (2014) · ACS symposium series · doi:10.1021/bk-2014-1158 · Cited by 118
Wood Modification as a Tool to Understand Moisture in Wood
Thybring, E. E., & Fredriksson, M. (2021) · Forests · doi:10.3390/f12030372 · Cited by 117
Self-citationFirst chemical events in pyrolysis of wood
DeGroot, W. F., Pan, W., Rahman, M., & Richards, G. N. (1988) · Journal of Analytical and Applied Pyrolysis · doi:10.1016/0165-2370(88)80024-x · Cited by 116 · cited 1×
“Thermal degradation leads to a loss in wood mass, mainly due to the emission of water, carbon dioxide, methanol, acetic acid and formic acid from degraded cell wall polysaccharides [146].”
BackgroundWelzbacher, C., Brischke, C., & Rapp, A. O. (2007) · Wood Material Science and Engineering · doi:10.1080/17480270701770606 · Cited by 115 · cited 2×
“A more common approach is to investigate how the structure-property relationship of wood is affected by variation of the process conditions, such as the temperature and duration [196], the shielding atmosphere [206], the pressure and the relative humidity [163,206] or the wood moisture content during the process [201].”
BackgroundReview of Functional Treatments for Modified Wood
Spear, M. J., Curling, S., Dimitriou, A., & Ormondroyd, G. A. (2021) · Coatings · doi:10.3390/coatings11030327 · Cited by 110 · cited 1×
“However, within the last ten years there has been a fascinating increase in projects, works, efforts and publications dealing with the development of novel wood-based functional materials [25,309].”
BackgroundAging of wood: Analysis of color changes during natural aging and heat treatment
Matsuo, M., Yokoyama, M., Umemura, K., Sugiyama, J., Kawai, S., Gril, J., Kubodera, S., Mitsutani, T., Ozaki, H., Sakamoto, M., et al. (2011) · Holzforschung · doi:10.1515/hf.2011.040 · Cited by 108
Nanofibrillated cellulose composites and wood derived scaffolds for functional materials
Keplinger, T., Wang, X., & Burgert, I. (2019) · Journal of Materials Chemistry A · doi:10.1039/c8ta10711d · Cited by 108
Self-citationRiedl, B., & He, G. (2004) · Wood Science and Technology · doi:10.1007/s00226-003-0221-5 · Cited by 107 · cited 3×
“Nevertheless, recent studies found indications but no evidence for covalent bonds between DMDHEU monomers and accessibly hydroxyl groups (co-condensation) of the cell wall polymers [265,266,280].”
BackgroundWater Filtration Using Plant Xylem
Boutilier, M. S. H., Lee, J., Chambers, V., Venkatesh, V., & Karnik, R. (2014) · PLoS ONE · doi:10.1371/journal.pone.0089934 · Cited by 106 · cited 2×
“Upon drying the pits close and the fluid pathways are blocked [328,329].”
BackgroundInfluentialHill, C. A. S. (2011) · BioResources · doi:10.15376/biores.6.2.918-919 · Cited by 105 · cited 1×
“early as the beginning of the 20th century [23], it has become an active area of research with over seven thousand papers published on the topic since 2000 according to Google Scholar.”
BackgroundBioinspired Struvite Mineralization for Fire-Resistant Wood
Guo, H., Luković, M., Mendoza, M., Schlepütz, C. M., Griffa, M., Xu, B., Gaan, S., Herrmann, H. J., & Burgert, I. (2019) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.8b19967 · Cited by 105 · cited 1×
“These include a variety of bio-inspired mineralization on the nano-and submicron scale [333–335], co-reaction with modifications for improving decay resistance [336], formation of zinc oxide nano-rods [337], and clay impregnation of cell walls [338].”
BackgroundMilitz, H. (1993) · Wood Science and Technology · doi:10.1007/bf00192221 · Cited by 104 · cited 1×
“As a key objective of chemical modification technologies, moisture-induced dimensional changes of the cell wall may be reduced up to 70% by resin treatments [34,251,255,262,268,304,305].”
BackgroundPyrolysis of a wood-derived material. Effects of moisture and ash content
Gray, M. R., Corcoran, W. H., & Gavalas, G. R. (1985) · Industrial & Engineering Chemistry Process Design and Development · doi:10.1021/i200030a020 · Cited by 102 · cited 2×
“Gray et al. [218] reported that increased MC improves the porosity, and char yield by about 5% (0.16 g g − 1 vs. 0 g g − 1 moisture content), but in surface charring the quantitative relevance may not be crucial, considering the charred layer is relatively thin.”
BackgroundInfluentialPast, Present, and Future of the Wood Preservation Industry
Freeman, M. H., Shupe, T. F., & Vlosky, R. P. (2003) · Civil War Book Review · Cited by 100
Altgen, M., Hofmann, T., & Militz, H. (2016) · Wood Science and Technology · doi:10.1007/s00226-016-0845-x · Cited by 99 · cited 2×
“Furthermore, elevated wood moisture contents during the thermal modification facilitate the removal of hemicelluloses, but do not result in a further reduction of the EMC or swelling of the final product [199–201].”
BackgroundSelf-citationCandelier, K., Dumarçay, S., Pétrissans, A., Desharnais, L., Gérardin, P., & Pétrissans, M. (2012) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2012.10.022 · Cited by 99 · cited 2×
“Unfortunately, the thermal behavior of isolated polysaccharides may be different from the behavior of polysaccharides within the cell wall in presence of lignin [204,205].”
BackgroundMethodEffect of severe thermal treatment on spruce and beech wood lignins
Rousset, P. L. A., Lapierre, C., Pollet, B., Quirino, W. F., & Perré, P. (2009) · Annals of Forest Science · doi:10.1051/forest/2008078 · Cited by 98 · cited 1×
“temperatures (below 300 ◦C), increasing the oxygen concentration from 2 to 21% had no significance, but temperature was the main contributor [246].”
BackgroundBehaviour of lignin during thermal treatments of wood
Windeisen, E., & Wegener, G. (2007) · Industrial Crops and Products · doi:10.1016/j.indcrop.2007.07.015 · Cited by 97 · cited 1×
“Lignin pyrolysis forms aromatic products and reduction and condensation of structural units occur [239].”
BackgroundKong, L., Tu, K., Guan, H., & Wang, X. (2017) · Applied Surface Science · doi:10.1016/j.apsusc.2017.02.252 · Cited by 95 · cited 1×
“These include a variety of bio-inspired mineralization on the nano-and submicron scale [333–335], co-reaction with modifications for improving decay resistance [336], formation of zinc oxide nano-rods [337], and clay impregnation of cell walls [338].”
BackgroundEnhanced mechanical energy conversion with selectively decayed wood
Sun, J., Guo, H., Schädli, G. N., Tu, K., Schär, S., Schwarze, F. W. M. R., Panzarasa, G., Ribera, J., & Burgert, I. (2021) · Science Advances · doi:10.1126/sciadv.abd9138 · Cited by 94
Wood Modification in Europe: A state-of-the-art about processes, products and applications
Edited by: Dennis Jones, D. S., Jones, D., Sandberg, D., Goli, G., & Todaro, L. (2020) · Proceedings e report · doi:10.36253/978-88-6453-970-6 · Cited by 94
Interface tailoring by a versatile functionalization platform for nanostructured wood biocomposites
Montanari, C., Olsén, P., & Berglund, L. A. (2020) · Green Chemistry · doi:10.1039/d0gc02768e · Cited by 88
Humin based resin for wood modification and property improvement
Sangregorio, A., Muralidhara, A., Guigo, N., Thygesen, L. G., Marlair, G., Angelici, C., de Jong, E., & Sbirrazzuoli, N. (2020) · Green Chemistry · doi:10.1039/c9gc03620b · Cited by 87 · cited 2×
“To perhaps produce similar modified wood by valorizing a side-stream product, it was recently suggested to use humins instead of furfuryl alcohol [134].”
BackgroundSelf-citationRapp, A. O., Bestgen, H., Adam, W. J., & Peek, R. D. (1999) · Holzforschung · doi:10.1515/hf.1999.018 · Cited by 86
Effect of moisture on the bending properties of thermally modified beech and spruce
Arnold, M. (2010) · Journal of Materials Science · doi:10.1007/s10853-009-3984-8 · Cited by 84 · cited 1×
“The impact of thermal modification is often evaluated in static bending tests, which show only a small impact on the stiffness, a loss in strength, but most significantly, a brittle behavior with little plastic deformation and a strong reduction in toughness [157,191,192].”
BackgroundEvidence of char formation during wood heat treatment by mild pyrolysis
Inari, G. N., Mounguengui, S., Dumarçay, S., Pétrissans, M., & Gérardin, P. (2007) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2007.03.003 · Cited by 77 · cited 1×
“Some hemicellulose degradation products, such as furfural or hydroxymethylfurfural, can also react with the lignin and they may contribute to the increased lignin content that is determined by sulfuric acid digestion [156–158].”
BackgroundAltgen, M., Willems, W., Hosseinpourpia, R., & Rautkari, L. (2018) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2018.05.005 · Cited by 76 · cited 3×
“Hemicellu-lose degradation interferes with the load-sharing capabilities of the cell wall to decrease the strength and toughness of the wood [153,194], reduces the number of sorption sites for water [175,195] and removes easily accessible nutrients for decay fungi [180].”
BackgroundSelf-citationHow does delignification influence the furfurylation of wood?
Yang, T., Cao, J., & Ma, E. (2019) · Industrial Crops and Products · doi:10.1016/j.indcrop.2019.04.019 · Cited by 73
Microstructure of wood charcoal prepared by flash heating
Kurosaki, F., Ishimaru, K., Hata, T., Bronsveld, P. M., Kobayashi, E., & Imamura, Y. (2003) · Carbon · doi:10.1016/s0008-6223(03)00434-2 · Cited by 71 · cited 1×
“Therefore, the microstructure and surface chemical structure differ from char formed by slow heating [226,227].”
BackgroundBeck, G., Thybring, E. E., Thygesen, L. G., & Hill, C. A. S. (2017) · Holzforschung · doi:10.1515/hf-2017-0072 · Cited by 71
Self-citationThermally modified timber : Recent developments in Europe and North America
Sandberg, D., & Kutnar, A. (2016) · Wood and Fiber Science (Society of Wood Science and Technology) · Cited by 68
Not Just Lumber—Using Wood in the Sustainable Future of Materials, Chemicals, and Fuels
Jakes, J. E., Arzola-Villegas, X., Bergman, R. D., Ciesielski, P. N., Hunt, C. G., Rahbar, N., Tshabalala, M. A., Wiedenhoeft, A. C., & Zelinka, S. L. (2016) · JOM · doi:10.1007/s11837-016-2026-7 · Cited by 66 · cited 1×
“While wood is a commercially important construction material, its potential uses extend beyond lumber [30].”
BackgroundSelf-citationAltgen, M., Awais, M., Altgen, D., Klüppel, A., Mäkelä, M., & Rautkari, L. (2020) · Scientific Reports · doi:10.1038/s41598-020-60418-3 · Cited by 64 · cited 5×
“For this, and to minimize undesired formaldehyde emissions from treated wood blocks, curing process conditions (temperature, duration), especially moisture conditions [251,261], appear crucial for the polymerization and fixation of resin molecules [248,262,267].”
BackgroundInfluentialSelf-citationA Decade of Improved Lumber Drying Technology
Bond, B., & Espinoza, O. (2016) · Current Forestry Reports · doi:10.1007/s40725-016-0034-z · Cited by 64 · cited 1×
“The kiln drying process is a major consumer of energy in the production of lumber and negates some of the carbon benefits of using wood as a building material [6].”
BackgroundA Percolation Model for Electrical Conduction in Wood with Implications for Wood-Water Relations
Zelinka, S. L., Glass, S. V., & Stone, D. S. (2008) · Wood and Fiber Science · Cited by 63
Self-citationStructure of carbon black continuously produced from biomass pyrolysis oil
Tóth, P., Vikström, T., Molinder, R., & Wiinikka, H. (2018) · Green Chemistry · doi:10.1039/c8gc01539b · Cited by 61 · cited 1×
“Additives, such as carbon black, could also be used, but the renewability of the source material should be considered; for example, carbon black was recently reported to have been produced from biomass pyrolysis oil [247].”
BackgroundEffect of relative humidity on thermal degradation of Norway spruce (Picea abies) wood
Borrega, M., & Kärenlampi, P. P. (2008) · Journal of Wood Science · doi:10.1007/s10086-008-0953-9 · Cited by 58 · cited 1×
“…is to investigate how the structure-property relationship of wood is affected by variation of the process conditions, such as the temperature and duration [196], the shielding atmosphere [206], the pressure and the relative humidity [163,206] or the wood moisture content during the process [201].”
BackgroundHughes, M., Hill, C. A. S., & Pfriem, A. (2015) · Holzforschung · doi:10.1515/hf-2014-0184 · Cited by 56 · cited 1×
“Hemicellulose degradation interferes with the load-sharing capabilities of the cell wall to decrease the strength and toughness of the wood [153,194], reduces the number of sorption sites for water [175,195] and removes easily accessible nutrients for decay fungi [180].”
BackgroundOpening Furan for Tailoring Properties of Bio‐based Poly(Furfuryl Alcohol) Thermoset
Falco, G., Guigo, N., Vincent, L., & Sbirrazzuoli, N. (2018) · ChemSusChem · doi:10.1002/cssc.201800620 · Cited by 54
Self-citationWood carbonization as a protective treatment on resistance to wood destroying fungi
Wang, Y., Zhang, Z., Fan, H., & Wang, J. (2018) · International Biodeterioration & Biodegradation · doi:10.1016/j.ibiod.2018.01.003 · Cited by 54 · cited 1×
“Although the wood can still be degraded by fungi, thermal modification prolongs the time until decay starts and decreases the rate at which mass loss proceeds during the incubation with decay fungi [183,184].”
BackgroundBrown-rot fungal degradation and de-acetylation of acetylated wood
Beck, G., Thybring, E. E., & Thygesen, L. G. (2018) · International Biodeterioration & Biodegradation · doi:10.1016/j.ibiod.2018.09.009 · Cited by 54 · cited 1×
“[64] have measured the acetyl content of modified wood during decay and found that the acetyl content of the wood dropped as the wood was decayed.”
BackgroundSelf-citationWillems, W., Lykidis, C., Altgen, M., & Clauder, L. (2015) · Holzforschung · doi:10.1515/hf-2014-0185 · Cited by 53 · cited 1×
“However, it seems impossible to define characteristic attributes to describe the entire range of thermally modified wood products [207].”
BackgroundSelf-citationWater relations in untreated and modified wood under brown-rot and white-rot decay
Thybring, E. E. (2017) · International Biodeterioration & Biodegradation · doi:10.1016/j.ibiod.2017.01.034 · Cited by 52 · cited 1×
“Thybring [84] reviewed the literature and developed a model for correlating the moisture content at the end of a decay test to the amount of mass loss for modified and unmodified wood.”
BackgroundSelf-citationSurface modification of solid wood by charring
Kymäläinen, M., Hautamäki, S., Lillqvist, K., et al. (2017) · Journal of Materials Science · doi:10.1007/s10853-017-0850-y · Cited by 51 · cited 4×
“Several papers have been published on surface modification with a hot plate [213–216].”
BackgroundInfluentialSelf-citationOrganic chemical structure and structural shrinkage of chars prepared from rockrose
Pastor-Villegas, J., Duran-Valle, C. J., Valenzuela-Calahorro, C., & Gómez-Serrano, V. (1998) · Carbon · doi:10.1016/s0008-6223(97)00200-5 · Cited by 51 · cited 1×
“The char line is therefore usually considered to be located at the 300 ◦C isotherm [221], and the carbonization is almost (80%) complete between 400 ◦C to 600 ◦C [244].”
BackgroundLiu, M., Lyu, S., Peng, L., Cai, L., Huang, Z., & Lyu, J. (2021) · ACS Sustainable Chemistry & Engineering · doi:10.1021/acssuschemeng.1c01358 · Cited by 50 · cited 1×
“A recent study [137] tested impregnation of wood with a mixture of furfuryl alcohol and epoxidized soybean oil, followed by heat curing.”
Targeted acetylation of wood: a tool for tuning wood-water interactions
Digaitis, R., Thybring, E. E., Thygesen, L. G., & Fredriksson, M. (2021) · Cellulose · doi:10.1007/s10570-021-04033-z · Cited by 50 · cited 1×
“One exciting development on this front was recently presented by Digaitis et al. [86] who developed a method for targeting acetylation so that it only modified areas of the cell wall near the cell lumina.”
MethodSelf-citationAssessment of Eurocode 5 Charring Rate Calculation Methods
Cachim, P. B., & Franssen, J. (2009) · Fire Technology · doi:10.1007/s10694-009-0092-x · Cited by 49
Biziks, V., Andersons, B., Sansonetti, E., Andersone, I., Militz, H., & Grīniņš, J. (2014) · Holzforschung · doi:10.1515/hf-2014-0083 · Cited by 46 · cited 1×
“Leaching of such soluble degradation products during wetting and re-drying cycles causes a further decrease in wood dry volume, which reduces the ASE [161,178].”
BackgroundMetsä-Kortelainen, S., & Viitanen, H. A. (2009) · Wood Material Science and Engineering · doi:10.1080/17480270903326140 · Cited by 45 · cited 2×
“Similar to the reduction in hygroscopicity, the effect on the decay resistance is dependent on the process conditions; hence, higher temperatures and longer treatment durations cause an increase in the decay resistance [180,181].”
BackgroundOne-sided surface charring of beech wood
Čermák, P., Dejmal, A., Paschová, Z., Kymäläinen, M., Dömény, J., Brabec, M., Hess, D., & Rautkari, L. (2019) · Journal of Materials Science · doi:10.1007/s10853-019-03589-3 · Cited by 45 · cited 1×
“Naturally, the grain direction has an effect on thermal conduction, but the only peer-reviewed paper on the subject did not report significant differences between radial and tangential surfaces [215].”
BackgroundSelf-citationHumins from Biorefineries as Thermoreactive Macromolecular Systems
Sangregorio, A., Guigo, N., van der Waal, J. C., & Sbirrazzuoli, N. (2018) · ChemSusChem · doi:10.1002/cssc.201802066 · Cited by 43
Self-citationAltgen, M., Uimonen, T., & Rautkari, L. (2017) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2017.12.007 · Cited by 43 · cited 1×
“The impact of thermal modification is often evaluated in static bending tests, which show only a small impact on the stiffness, a loss in strength, but most significantly, a brittle behavior with little plastic deformation and a strong reduction in toughness [157,191,192].”
BackgroundSelf-citationSorption-Related Characteristics of Surface Charred Spruce Wood
Kymäläinen, M., Turunen, H., Čermák, P., Hautamäki, S., & Rautkari, L. (2018) · Materials · doi:10.3390/ma11112083 · Cited by 42 · cited 2×
“Because char is rather inert both chemically and biologically, it is presumed that the overall performance is determined by the thickness of the carbonized layer [211,214,229].”
BackgroundSelf-citationHighly Stable Wood Material with Low Resin Consumption via Vapor Phase Furfurylation in Cell Walls
Liu, M., Guo, F. Y., Wang, H., Ren, W., Cao, M., & Yu, Y. (2020) · ACS Sustainable Chemistry & Engineering · doi:10.1021/acssuschemeng.0c03172 · Cited by 42 · cited 1×
“A process relying on gas phase furfurylation [136] is another recent suggestion that could cut costs by reducing the consumption of furfuryl alcohol.”
BackgroundMechanism for Diffusion through Secondary Cell Walls in Lignocellulosic Biomass
Jakes, J. E. (2019) · The Journal of Physical Chemistry B · doi:10.1021/acs.jpcb.9b01430 · Cited by 41 · cited 2×
“Jakes [82] used nanoindentation to measure the mechanical damping as a function of moisture content.”
BackgroundMethodSorption behaviour of torrefied wood and charcoal determined by dynamic vapour sorption
Kymäläinen, M., Rautkari, L., & Hill, C. A. S. (2015) · Journal of Materials Science · doi:10.1007/s10853-015-9332-2 · Cited by 41 · cited 1×
“The surface is prone to liquid water absorption, but adsorption/absorption of water vapor is reduced due to compositional modifications, namely lignin cross-linking, increased crystallinity, and reduced number/accessibility of hydroxyl groups [214,231].”
BackgroundSelf-citationThermal behavior of extracted and delignified pine wood flour
Chen, Y., Tshabalala, M. A., Gao, J., Stark, N. M., Fan, Y., & Ibach, R. E. (2014) · Thermochimica Acta · doi:10.1016/j.tca.2014.06.012 · Cited by 40 · cited 1×
“Unfortunately, the thermal behavior of isolated polysaccharides may be different from the behavior of polysaccharides within the cell wall in presence of lignin [204,205].”
BackgroundSurface Characteristics of One-Sided Charred Beech Wood
Machová, D., Oberle, A., Zárybnická, L., Dohnal, J., Šeda, V., Dömény, J., Vacenovská, V., Kloiber, M., Pěnčík, J., Tippner, J., et al. (2021) · Polymers · doi:10.3390/polym13101551 · Cited by 39 · cited 4×
“Several papers have been published on surface modification with a hot plate [213–216].”
BackgroundInfluentialLiao, R., Jiang, J., Li, Y., Gan, Z., Su, S., Ding, S., Li, Z., & Hou, L. (2020) · Environmental Science Processes & Impacts · doi:10.1039/d0em00106f · Cited by 38 · cited 1×
“Conventional halogen and boron-based fire retardants have potential health risks, may produce toxic gases, and accumulate in the environment because of their stability [332].”
BackgroundBiological degradation of torrefied wood and charcoal
Kymäläinen, M., Havimo, M., Keriö, S., Kemell, M., & Solio, J. (2014) · Biomass and Bioenergy · doi:10.1016/j.biombioe.2014.10.009 · Cited by 35 · cited 1×
“Similar results were reported by Kymäläinen et al. [233] after torrefied wood and charcoal field storage experiments, where naturally occurring fungi were reported to colonize the material, despite soluble sugars mostly being depleted in the manufacturing process.”
ResultSelf-citationPlant-based torsional actuator with memory
Plaza, N. Z., Zelinka, S. L., Stone, D. S., & Jakes, J. E. (2013) · Smart Materials and Structures · doi:10.1088/0964-1726/22/7/072001 · Cited by 34 · cited 1×
“Wood has been used as a bioinspiring smart material with shape memory properties [31].”
MethodSelf-citationNatural Wood-Based Catalytic Membrane Microreactors for Continuous Hydrogen Generation
Tu, K., Büchele, S., Mitchell, S. J., Stricker, L., Liu, C., Goldhahn, C., Allaz, J. M., Ding, Y., Günther, R., Zhang, Z., et al. (2022) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.1c22850 · Cited by 34 · cited 2×
“Tu et al. [331] recently reported the fabrication of a structured bimetallic silver-palladium catalytic native wood microreactor for continuous hydrogen generation (Figure 11).”
BackgroundSelf-citationDurability and Fire Performance of Charred Wood Siding (Shou Sugi Ban)
Hasburgh, L. E., Zelinka, S. L., Bishell, A. B., et al. (2021) · Forests · doi:10.3390/f12091262 · Cited by 32
Self-citationEbner, D. H., Barbu, M. C., Klaushofer, J., & Čermák, P. (2021) · Polymers · doi:10.3390/polym13101662 · Cited by 31 · cited 6×
“Dimensional stability of surface charred wood has not been thoroughly reported in literature but cupping towards the charred side is normal due to a strong temperature gradient [212].”
BackgroundMethodInfluentialFleckenstein, M., Biziks, V., Mai, C., & Militz, H. (2017) · European Journal of Wood and Wood Products · doi:10.1007/s00107-017-1275-7 · Cited by 27
Rabe, S., Klack, P., Bahr, H., & Schartel, B. (2020) · Fire and Materials · doi:10.1002/fam.2809 · Cited by 27 · cited 1×
“However, certain wood species can form a compact char later with little cracking depending on the density and lignin content [230].”
BackgroundSkrede, I., Solbakken, M. H., Hess, J., Fossdal, C. G., Hegnar, O. A., & Alfredsen, G. (2019) · Applied and Environmental Microbiology · doi:10.1128/aem.00338-19 · Cited by 27 · cited 2×
“Mapping of gene expression of the system just mentioned showed that the oxidative phase was maintained or extended for furfurylated wood [62,113].”
BackgroundRamchander, K., Hegde, M., Antony, A. P., Wang, L., Leith, K., Smith, A. E., & Karnik, R. (2021) · Nature Communications · doi:10.1038/s41467-021-22055-w · Cited by 24
Effect of Weathering on Surface Functional Groups of Charred Norway Spruce Cladding Panels
Kymäläinen, M., Turunen, H., & Rautkari, L. (2020) · Forests · doi:10.3390/f11121373 · Cited by 23 · cited 1×
“Kymäläinen et al. [240] analyzed contact charred spruce panels after two years of natural weathering and reported degradation of lignin by the use of FTIR.”
MethodSelf-citationWinandy, J. E. (2017) · Wood and Fiber Science · Cited by 22
Status and Trends for the U.S. Forest Products Sector
Brandeis, C., Taylor, M. E., Abt, K. L., Alderman, D. R., & Buehlmann, U. (2020) · doi:10.2737/srs-gtr-258 · Cited by 21 · cited 1×
“In the United States, approximately 70% of the lumber produced is used in the construction of buildings and 44% of the construction material is used in the construction of new, single family homes [4].”
BackgroundAntonetti, C., Licursi, D., & Galletti, A. M. R. (2020) · Catalysts · doi:10.3390/catal10090961 · Cited by 21 · cited 1×
“This furanic compound enjoys industrial production worldwide and should reach a growing market share of €634 M in 2024 [87].”
BackgroundZimmer, K., Høibø, O. A., Vestøl, G. I., & Larnøy, E. (2014) · Wood Science and Technology · doi:10.1007/s00226-014-0660-1 · Cited by 21 · cited 1×
“Regarding impregnation of P. sylvestris sapwood with an aqueous solution of FA and initiators, it has been found that in general sapwood from fast grown individuals is easier to impregnate [132].”
MethodDesigning functional wood materials for novel engineering applications
Panzarasa, G., & Burgert, I. (2021) · Holzforschung · doi:10.1515/hf-2021-0125 · Cited by 20 · cited 1×
“Wood possesses a unique anisotropic hierarchical porous structure from the nano-to the macroscale that can be extremely valuable for the development of functional materials when equipped with materials including polymers, nanoparticles, metal-organic frameworks, or metals [310–312].”
BackgroundRingman, R., Pilgård, A., Brischke, C., Windeisen, E., & Richter, K. (2017) · International Wood Products Journal · doi:10.1080/20426445.2017.1344382 · Cited by 20 · cited 1×
“However, many researchers have shown that acetylation also retards the chelator-mediated-Fenton (CMF) reaction chemistry that precedes enzymatic degradation in brown rot decay [55–57 , 61– 63 ].”
BackgroundThe Shigir idol in the context of early art in Eurasia
Terberger, T., Zhilin, M., & Savchenko, S. (2020) · Quaternary International · doi:10.1016/j.quaint.2020.10.025 · Cited by 16 · cited 1×
“Wooden artifacts that have been kept dry such as the sarcophagus of Tutankhamun and the Shigir Idol have remained intact for thousands of years [12–14].”
BackgroundA note on artificial weathering of spruce ( Picea abies ) with a carbonised layer
Kampe, A., & Pfriem, A. (2018) · International Wood Products Journal · doi:10.1080/20426445.2018.1493841 · Cited by 13 · cited 2×
“Because char is rather inert both chemically and biologically, it is presumed that the overall performance is determined by the thickness of the carbonized layer [211,214,229].”
BackgroundRejection of micron-sized particles using beech wood xylem
Vitas, S., Beckmann, P., Skibinski, B., Goldhahn, C., Muff, L. F., & Cabane, É. (2019) · Environmental Science Water Research & Technology · doi:10.1039/c8ew00774h · Cited by 13 · cited 2×
“[328,329] utilized pine sapwood membranes (thickness ca.”
BackgroundAltgen, M., Awais, M., Altgen, D., Kyyrö, S., Seppäläinen, H., & Rautkari, L. (2020) · Journal of Materials Science · doi:10.1007/s10853-020-04943-6 · Cited by 11 · cited 1×
“For example, the tensile strength parallel to the grain decreases strongly after thermal modification [188,189], while the compression strength shows a moderate decrease [190] or even increases [188].”
BackgroundSelf-citation
Metadata
- Authors
- Zelinka, S. L., Altgen, M., Emmerich, L., Guigo, N., Keplinger, T., Kymäläinen, M., Thybring, E. E., & Thygesen, L. G.
- Venue
- Forests
- Publisher
- MDPI AG
- Published
- 2022-06-26
- Volume
- 13
- Issue
- 7
- Pages
- 1004
- ISSN
- 1999-4907 (ISSN-L)
- OpenAlex
- W4283521276
- Cited by
- 182
- References
- 144
- FWCI
- 15.32
- Type
- journal article
- Language
- en
- Open access
- gold
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.