Abstract

Alginate addition did not change the HAp-Zn structure and phase; the uppermost ultimate compressive strength and modulus of elasticity were 2.05 ± 0.06 MPa and 0.037 ± 0.001 GPa at 6% alginate.

Checked 2026-11-23 · 1 reference not checked yet

Overview

CoChat Summary

TL;DR

HAp-Zn/SA composite scaffolds with 0–6% sodium alginate were prepared and characterized. Alginate did not alter the HAp-Zn phase but reduced crystallinity and crystallite size, produced interconnected pores, and increased compressive strength, peaking at 2.05 ± 0.06 MPa for 6% SA.

Key findings

  • XRD showed hexagonal HAp and parascholzite (CaZn₂(PO₄)₂H₂O), indicating Zn incorporation; alginate addition did not change the HAp-Zn phase/structure. Crystallinity decreased from 77.63% to 74.14%, 72.92%, and 70.21%, and crystallite size decreased from 11.77 nm to 9.56 nm, 8.54 nm, and 7.2 nm with increasing alginate.
  • FTIR confirmed phosphate groups and alginate COO⁻ peaks at 1434 cm⁻¹ and 1640–1641 cm⁻¹; OH stretching appeared at 3465–3434 cm⁻¹, and a C-Cl group at 633–631 cm⁻¹ was attributed to PBS. Peak intensities increased with alginate addition.
  • SEM showed 0% SA samples as powders with low interconnection, while alginate-containing samples had pores of 50–200 µm with good interconnectivity, suitable for cell attachment and growth (100–300 µm).
  • Compressive strength increased with alginate concentration; HAp-Zn/SA6% reached 2.05 ± 0.06 MPa compressive strength and 0.037 ± 0.001 GPa modulus of elasticity. This was still below an earlier study’s 3.3–9.01 MPa, possibly due to decreased crystallinity, but all samples were considered potentially applicable for pelvis head spongy parts requiring 1–15 MPa.

Methods

  • Zn-doped HAp powder was synthesized by sol-gel with microwave support: CaO dissolved in 2 M HNO₃, reacted with 0.18 M (NH₄)₂HPO₄, ZnCl₂ (15% w/v) added at pH 10, microwave radiation for 10 min, aging 24 h, washing to pH 7, drying, and sintering at 600°C for 2 h.
  • HAp-Zn/SA scaffolds were prepared with PBS:sample ratio 1:1, sodium alginate at 0%, 2%, 4%, and 6% in 0.65 M PBS, mixed with HAp-Zn powder, crosslinked with 1.08 M CaCl₂, stirred at 50°C, aged 24 h, poured into cylindrical molds, and freeze-dried at −30°C for 24 h.
  • Characterization included XRD (Bruker D8 Advance, 2θ = 10°–90°, Cu-Kα), crystallinity and Scherrer crystallite-size analysis, FTIR (4000–400 cm⁻¹, 4 cm⁻¹ resolution), SEM (Hitachi S3000N, 10 kV, gold-coated), and compressive testing (Universal Tensile Machine, 13 mm diameter × 25 mm height, ASTM E9-89a, 5 N load, 1.0 mm/min, three measurements per group).

Limitations

  • Stated: The paper notes limited prior studies on HAp-Zn/SA and that the maximum compressive strength remained below an earlier study’s 3.3–9.01 MPa, possibly due to decreased crystallinity.
  • Stated: No dedicated limitations section is included in the paper.
  • Evident from the text: Only physicochemical and mechanical characterization is reported; no in vitro/in vivo biocompatibility, degradation, or antibacterial testing appears in the provided text.

Model-written summary. Check it against the paper before relying on it.

Integrity signals

Registry

Crossref · 10.4028/p-86zw7g

Cites

12 of 13 references verified0 citation errors · 0 not checkable

Statistics

Nothing to recompute.

Verification

Claims the paper makes

0 Valid · 0 Not valid · 27 Not checked · 24 Own results and interpretations

29 more claims

Create a free account to see all 51 claims and to verify the 35 references still open.

See all claims — free account
  • It may state two separate claims as one. 10
  • Probably not a substantial claim. 8

Create a free account to see these claims.

Citations

Cites

Research works printed but not linked: 4

  1. A A Maharani, A Husni, N Ekantari, Karakteristik Natrium Alginat Rumput Laut Cokelat Sargassum Fluitans dengan Metode Ekstraksi yang Berbeda, Jphpi. 20A. A. Maharani, A. Husni, and N. Ekantari, Karakteristik Natrium Alginat Rumput Laut Cokelat Sargassum Fluitans dengan Metode Ekstraksi yang Berbeda, Jphpi, vol. 20, no. 3, (2017) 478-487.
  2. Perancah Berpori Hidroksiapatit dan β-Tricalcium Phosphate dari Limbah Cangkang Telur Ayam dengan Porogen Alginat Fitri Afriani. F Afriani, F. Afriani, Perancah Berpori Hidroksiapatit dan β-Tricalcium Phosphate dari Limbah Cangkang Telur Ayam dengan Porogen Alginat Fitri Afriani, (2015). · DOI
  3. Sintesis dan Karakterisasi Biokomposit Hidroksiapatit-Alginat-Zinc Sebagai Bone Graft untuk Penanganan Bone Defect. J N Setiadiputri, J. Chem. Inf. Model. 539J. N. Setiadiputri, Sintesis dan Karakterisasi Biokomposit Hidroksiapatit-Alginat-Zinc Sebagai Bone Graft untuk Penanganan Bone Defect, J. Chem. Inf. Model., vol. 53, no. 9 (2018) 1-102.
  4. Sintesis Scaffold Alginat-Kitosan-Karbonat Apatit Sebagai Bone Graft Menggunakan Metode. M R Aufan, A H Daulay, D Indriani, A Nuruddin, J. Biofisika. 81M. R. Aufan, A. H. Daulay, D. Indriani, and A. Nuruddin, Sintesis Scaffold Alginat-Kitosan- Karbonat Apatit Sebagai Bone Graft Menggunakan Metode, J. Biofisika, vol. 8, no. 1, (2012) 16-24.

Metadata

Authors
Ramadhani, J., Tajalla, G. U. N., Yusariarta, A. W., Rachmantyo, R., & Wibowo, A.
Affiliations
  • Institut Teknologi Kalimantan (ID)
  • Institut Teknologi Kalimantan
  • Bandung Institute of Technology (ID)
Corresponding author
Ramadhani, Jane
Venue
Advances in Science and Technology
Published
2023-03-01
Volume
125
Pages
3-9
ISSN
  • 1661-819X (ISSN-L)
  • 1662-0356
OpenAlex
W4322741193
Cited by
0
References
12
FWCI
0.00
Type
conference paper
Language
en
Open access
Licence
Locations
Advances in science and technology (publishedVersion, cc-by)
Topics
  • Physical Sciences › Engineering › Biomedical Engineering › Bone Tissue Engineering Materials
  • Physical Sciences › Engineering › Biomedical Engineering › 3D Printing in Biomedical Research
  • Physical Sciences › Engineering › Mechanical Engineering › Surface Treatment and Coatings
Keywords
alginate, bone scaffolds, porous scaffolds, low-temperature processing, alginate concentration, crystallinity, compressive strength, elastic modulus, intermolecular interactions, bone regeneration

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

A language model drew the claims from the paper on 2026-11-23, under version 3 of the claim definition (model deepseek-v4.1-flash, prompt extract-v3).

A second model labelled each claim on 2026-11-23 (model jev-1.13-20260917, definition revision gold-guideline-v0.2).

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.