CoChat

High-Temperature Corrosion Mechanisms for Selected Iron and Nickel-Based Alloys Exposed to Sulfur and Chlorine-Containing Environments

Kung, Steven C. · 2015 · Corrosion

The DOI matches its Crossref record; 15 of the 17 references it cites were found in a registry or an index.

Abstract

A comprehensive research project consisting of pilot-scale combustion testing and long-term laboratory corrosion study has been performed. A pilot-scale combustion facility was modified to enable burning of pulverized coals under the conditions typical for coal-fired utility boilers. Eight United States (U.S.) coals were selected for this investigation, with the test conditions for all coals set to have the same heat input to the combustor. In addition, the air/fuel ratio was controlled so that approximately 3% excess oxygen was attained in the combustion gas at the furnace outlet, a location equivalent to the furnace exit of commercial boilers. During each pilot-scale combustion test, extensive online measurements of the flue gas compositions were performed. In addition, deposit samples were collected at the same location for chemical analyses. This information characterized well the combustion environments adjacent to the superheaters and reheaters of utility boilers burning different U.S. coals. The gas and deposit compositions were then simulated in a series of 1,000-h laboratory corrosion tests in which the corrosion performances of different alloys were evaluated at 704°C (1,300°F). Results of this laboratory study led to better understanding of the corrosion mechanisms operating on superheaters and reheaters in coal-fired boilers due to the coexistence of sulfur and chlorine in coal. A new corrosion mechanism, i.e., “active sulfide-to-oxide corrosion mechanism,” accounts for the rapid corrosion attack on low-alloy ferritic steels and lower-grade stainless steels resulting from the formation of iron chloride (FeCl2) vapor and associated cycling reactions. For higher alloys containing sufficient chromium, the attack is dominated by “hot corrosion” in the presence of a fused salt. In addition, two stages of the hot corrosion mechanism have been elucidated here in detail. The initiation of hot corrosion attack induced by molten sulfate may involve Stage 1 “acidic” fluxing and re-precipitation of the protective scale formed initially on the deposit-covered alloy surfaces, followed by Stage 2 Hot Corrosion dominated by “basic” fluxing and re-precipitation after the scale is locally penetrated by the fused salt.

Overview

Integrity signals

Registry

Crossref · 10.5006/1409

Cites

15 of 15 references verified0 citation errors · 0 not checkable

Statistics

Recomputing p-values needs the paper’s full text.

Verification

Claims the paper makes

This paper’s full text isn’t openly available, so its claims and self-check weren’t run. The registry and citation checks still apply.

Citations

Cites

Research works printed but not linked: 5

  1. Rapp, 1994, J. Met, 46, 47
  2. Daniel, 1991, “The Effect of Coal Chlorides on Furnace Wall Corrosion,”, Coal Science and Technology 17 Chlorine in Coal, 207
  3. Kaminskii, 1996, Therm. Eng, 43, 505
  4. Grabke, 1998, Molten Salt Forum, 5–6, 405
  5. Rapp, 2009, Electrochem. Trans, 16, 271

Cited by

See all 13

Metadata

Authors
Kung, S. C.
Corresponding author
Kung, Steven C.
Venue
Corrosion
Published
2014-11-07
Volume
71
Issue
4
Pages
483-501
ISSN
  • 0010-9312 (ISSN-L)
  • 1938-159X
OpenAlex
W1985426096
Cited by
13
References
17
Citations by year
2026: 1 · 2025: 1 · 2024: 1 · 2022: 1 · 2021: 3 · 2018: 2 · 2017: 1 · 2016: 3
FWCI
1.97
Type
journal article
Language
en
Open access
closed
Locations
CORROSION (publishedVersion)
Topics
  • Physical Sciences › Materials Science › Surfaces, Coatings and Films › High-Temperature Coating Behaviors
  • Physical Sciences › Engineering › Mechanical Engineering › High Temperature Alloys and Creep
  • Physical Sciences › Materials Science › Materials Chemistry › Corrosion Behavior and Inhibition
Keywords
high-temperature corrosion, iron alloys, nickel-based alloys, coal-fired boilers, superheater, reheater, hot corrosion, molten sulfates, molten salts, low alloy ferritic steel, stainless steel, coal deposits, flue gas composition, corrosion mechanism

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.