High‐Voltage Charging‐Induced Strain, Heterogeneity, and Micro‐Cracks in Secondary Particles of a Nickel‐Rich Layered Cathode Material

Open access
Mao, Yuwei, Wang, Xuelong, Xia, Sihao, Zhang, Kai, Wei, Chenxi, Bak, Seongmin, Shadike, Zulipiya, Liu, Xuejun, Yang, Yang, Xu, Rong, Pianetta, Piero, Ermon, Stefano, Stavitski, Eli, Zhao, Kejie, Xu, Zhengrui, Lin, Feng, Yang, Xiao‐Qing, Hu, Enyuan, Liu, Yijin·2019·Advanced Functional Materials

Abstract

Nickel‐rich layered materials LiNi 1‐x‐y Mn x Co y O 2 are promising candidates for high‐energy‐density lithium‐ion battery cathodes. Unfortunately, they suffer from capacity fading upon cycling, especially with high‐voltage charging. It is critical to have a mechanistic understanding of such fade. Herein, synchrotron‐based techniques (including scattering, spectroscopy, and microcopy) and finite element analysis are utilized to understand the LiNi 0.6 Mn 0.2 Co 0.2 O 2 material from structural, chemical, morphological, and mechanical points of view. The lattice structural changes are shown to be relatively reversible during cycling, even when 4.9 V charging is applied. However, local disorder and strain are induced by high‐voltage charging. Nano‐resolution 3D transmission X‐ray microscopy data analyzed by machine learning methodology reveal that high‐voltage charging induced significant oxidation state inhomogeneities in the cycled particles. Regions at the surface have a rock salt–type structure with lower oxidation state and build up the impedance, while regions with higher oxidization state are scattered in the bulk and are likely deactivated during cycling. In addition, the development of micro‐cracks is highly dependent on the pristine state morphology and cycling conditions. Hollow particles seem to be more robust against stress‐induced cracks than the solid ones, suggesting that morphology engineering can be effective in mitigating the crack problem in these materials.

Overview

The claims and statistics of this paper haven’t been checked yet.

Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1002/adfm.201900247

Cites

42 of 42 references verified0 citation errors · 0 not checkable

Statistics

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.

A few free checks a day · papers already verified open instantly · results are public

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Show all 42 references

Cited by

See all 339

Metadata

Authors
Mao, Y., Wang, X., Xia, S., Zhang, K., Wei, C., Bak, S., Shadike, Z., Liu, X., Yang, Y., Xu, R., Pianetta, P., Ermon, S., Stavitski, E., Zhao, K., Xu, Z., Lin, F., Yang, X., Hu, E., & Liu, Y.
Venue
Advanced Functional Materials
Publisher
Wiley
Published
2019-03-07
Volume
29
Issue
18
ISSN
  • 1616-301X (ISSN-L)
  • 1616-3028
OpenAlex
W2921742660
Cited by
339
References
42
FWCI
14.45
Type
journal article
Language
en
Open access
green

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

How to cite

Cite CoChat for the checks on this page, and the paper for its own findings.

This page
CoChat. (2026). Citation check: High‐Voltage Charging‐Induced Strain, Heterogeneity, and Micro‐Cracks in Secondary Particles of a Nickel‐Rich Layered Cathode Material. https://app.cochat.ai/papers/10.1002/adfm.201900247
The paper
Mao, Y., Wang, X., Xia, S., Zhang, K., Wei, C., Bak, S., Shadike, Z., Liu, X., Yang, Y., Xu, R., Pianetta, P., Ermon, S., Stavitski, E., Zhao, K., Xu, Z., Lin, F., Yang, X., Hu, E., & Liu, Y. (2019). High‐Voltage Charging‐Induced Strain, Heterogeneity, and Micro‐Cracks in Secondary Particles of a Nickel‐Rich Layered Cathode Material. Advanced Functional Materials. https://doi.org/10.1002/adfm.201900247

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.