Al2O3/ZrO2 Nanolaminates as Ultrahigh Gas‐Diffusion Barriers—A Strategy for Reliable Encapsulation of Organic Electronics
Abstract
Adv. Mater. 2009, 21, 1845–1849 2009 WILEY-VCH Verlag G Gas-diffusion barriers play an important role in many applications today, such as flat-panel displays or solar cells grown on plastic substrates. In particular, organic light-emitting diodes (OLEDs) need efficient encapsulation because of the high sensitivity of many organic or electrode materials to moisture and oxygen, which has been demonstrated to cause device degradation and limited lifetime. Maximum allowable permeation rates for a viable encapsulant to be used in organic optoelectronics are still under debate, but it is common sense that the requirements are far more demanding than those for typical barrier films used in food or pharmacy packaging. A very commonly quoted figure for the upper limit of the water-vaportransmission rate (WVTR) in order to reach a minimum OLED lifetime of 10000 h is 10 6 gm 2 day . This value originated from an estimate of the amount of water needed to degrade the reactive cathode material. For the oxygen-transmission rate (OTR), maximum values for similar OLED lifetimes have been reported in the region of 10 –10 3 cmm 2 day . Nowadays, a very common technique is the encapsulation of organic devices with a glass or metal lid, which is applied under nitrogen atmosphere using, for example, an epoxy resin as glue. In addition, the residual moisture in the cavity between the organic device and lid is further minimized by an opaque getter material. For large-area, flexible, or transparent applications, glass-lid encapsulation is not suitable. A promising alternative is thin-film barriers of metal oxides or nitrides, such as Al2O3, SiO2, TiO2, or SiN. These materials can be deposited by several techniques. Plasma-assisted processes, such as sputtering or plasma-enhanced chemical vapor deposition (PECVD), provide high quality films, but their typically reported OTR and WVTR values of about 0.5 cmm 2 day 1 and 0.3 gm 2 day , respectively, limited by imperfections in the films, are not sufficient for OLED applications. Moreover, efficient step coverage and conformal coating are not straightforward with these techniques. As a workaround, hybrid organic/inorganic multilayer structures have been introduced. In these, the polymeric intermediate layer levels the inorganic layer so that diffusion pathways through the entire stack of the barrier can be reduced. However, the combination of alternating nonvacuum-based polymer deposition processes and vacuum-based deposition processes is timeconsuming and costly, and therefore not really practical for production. An alternative technique that promises highly uniform thin-film coatings is atomic-layer deposition (ALD). ALD relies on the sequential exposure of the surface to be coated to a metal–organic precursor and a reactant (H2O, O3, NH3, etc.). The sequential dosing of precursors leads to a self-limiting process with concomitant precise control over thickness and homogeneity. The technique is well-established in the processing of insulating films for gate dielectrics and capacitors. ALD has the advantage of allowing the deposition of very dense films at low temperatures (<100 8C), and thus appears to be a promising technique suitable for preparing encapsulation layers on top of organic electronic devices. There are a few reports dealing with ALD-grown thin films for OLED encapsulation. Very-low permeation rates of 6.5 10 5 gm 2 day 1 at 60 8C have been reported for Al2O3 films that were grown at 120 8C. [13] However, deposition temperatures above 100 8C might be critical, because glass-transition temperatures for many functional OLED materials have been reported in this very temperature range. In this Communication, we report on thin encapsulation layers prepared by ALD at a temperature of 80 8C. Specifically, we study neat Al2O3 films as a reference, and introduce novel highly efficient permeation barriers based on so-called nanolaminate structures. A nanolaminate, in this case, is a composite film consisting of repetitively deposited ultrathin (a few nanometers thick) alternating layers of Al2O3 and ZrO2. The alternating nanolayer structure suppresses the formation of both microscopic voids and nanocrystals. As a result, the probability of the occurrence of statistical defects in the barrier structure related to permeation paths along connected voids or grain boundaries is significantly reduced.We demonstrate that nanolaminates render pinhole-free thin-film encapsulation layers suitable for large-area organic devices possible. First, the quantitative assessment of permeation rates on the order of 10 6 gm 2 day 1 for water and 10 3 cmm 2 day 1 for oxygen is very challenging and, as yet, no commercially available method can be applied in this range. Therefore, we used a very sensitive permeation-measurement technique that was introduced by Paetzold et al. The method allows the measurement
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Charge Carrier Transporting Molecular Materials and Their Applications in Devices
Shirota, Y., & Kageyama, H. (2007) · Chemical Reviews · doi:10.1021/cr050143+ · Cited by 1,756
Low-Temperature Al2O3 Atomic Layer Deposition
Groner, M. D., Fabreguette, F. H., Elam, J. W., & George, S. M. (2004) · Chemistry of Materials · doi:10.1021/cm0304546 · Cited by 1,403
Atomic Layer Deposition of Hafnium and Zirconium Oxides Using Metal Amide Precursors
Hausmann, D. M., Kim, E., Becker, J., & Gordon, R. G. (2002) · Chemistry of Materials · doi:10.1021/cm020357x · Cited by 542
Al3O3 thin film growth on Si(100) using binary reaction sequence chemistry
Ott, A. W., Klaus, J. W., Johnson, J. M., & George, S. M. (1997) · Thin Solid Films · doi:10.1016/s0040-6090(96)08934-1 · Cited by 517
Surface chemistry of Al2O3 deposition using Al(CH3)3 and H2O in a binary reaction sequence
Dillon, A. C., Ott, A. W., Way, J. D., & George, S. M. (1995) · Surface Science · doi:10.1016/0039-6028(95)90033-0 · Cited by 462
Ca test of Al2O3 gas diffusion barriers grown by atomic layer deposition on polymers
Carcia, P. F., McLean, R. S., Reilly, M. H., Groner, M. D., & George, S. M. (2006) · Applied Physics Letters · doi:10.1063/1.2221912 · Cited by 436
Graff, G. L., Williford, R. E., & Burrows, P. E. (2004) · Journal of Applied Physics · doi:10.1063/1.1768610 · Cited by 414
Oxygen diffusion barrier properties of transparent oxide coatings on polymeric substrates
Chatham, H. (1996) · Surface and Coatings Technology · doi:10.1016/0257-8972(95)02420-4 · Cited by 362
Thin film atomic layer deposition equipment for semiconductor processing
Sneh, O., Clark-Phelps, R. B., Londergan, A. R., Winkler, J., & Seidel, T. E. (2002) · Thin Solid Films · doi:10.1016/s0040-6090(01)01678-9 · Cited by 294
Thin-film encapsulation of organic light-emitting devices
Ghosh, A. P., Gerenser, L. J., Jarman, C. M., & Fornalik, J. E. (2005) · Applied Physics Letters · doi:10.1063/1.1929867 · Cited by 263
Cited by
Atomic Layer Deposition: An Overview
George, S. M. (2010) · Chemical Reviews · doi:10.1021/cr900056b · Cited by 5,814
Crystallinity of inorganic films grown by atomic layer deposition: Overview and general trends
Miikkulainen, V., Leskelä, M., Ritala, M., & Puurunen, R. L. (2013) · Journal of Applied Physics · doi:10.1063/1.4757907 · Cited by 1,413
Materials for flexible bioelectronic systems as chronic neural interfaces
Song, E., Li, J., Won, S. M., Bai, W., & Rogers, J. A. (2020) · Nature Materials · doi:10.1038/s41563-020-0679-7 · Cited by 498
Wafer-scale single-crystal hexagonal boron nitride film via self-collimated grain formation
Lee, J. S., Choi, S. H., Yun, S. J., Kim, Y. I., Boandoh, S., Park, J.-H., Shin, B. G., Ko, H., Lee, S. H., Kim, Y.-M., et al. (2018) · Science · doi:10.1126/science.aau2132 · Cited by 476
Thin film encapsulation for flexible AM-OLED: a review
Park, J.-S., Chae, H., Chung, H. K., & Lee, S. I. (2011) · Semiconductor Science and Technology · doi:10.1088/0268-1242/26/3/034001 · Cited by 464
Approaches for Long Lifetime Organic Light Emitting Diodes
Sudheendran Swayamprabha, S., Dubey, D. K., Shahnawaz, Yadav, R. A. K., Nagar, M. R., Sharma, A., Tung, F., & Jou, J. (2021) · Advanced Science · doi:10.1002/advs.202002254 · Cited by 318
Recent advances in flexible organic light-emitting diodes
Xu, R.-P., Li, Y.-Q., & Tang, J.-X. (2016) · Journal of Materials Chemistry C · doi:10.1039/c6tc03230c · Cited by 307
Recent progress on thin-film encapsulation technologies for organic electronic devices
Yu, D., Yang, Y.-Q., Chen, Z., Tao, Y., & Liu, Y.-F. (2016) · Optics Communications · doi:10.1016/j.optcom.2015.08.021 · Cited by 274
Dissolution Behaviors and Applications of Silicon Oxides and Nitrides in Transient Electronics
Kang, S., Hwang, S., Cheng, H., Yu, S., Kim, B. H., Kim, J., Huang, Y., & Rogers, J. A. (2014) · Advanced Functional Materials · doi:10.1002/adfm.201304293 · Cited by 258
Metadata
- Authors
- Meyer, J., Görrn, P., Bertram, F., Hamwi, S., Winkler, T., Johannes, H., Weimann, T., Hinze, P., Riedl, T., & Kowalsky, W.
- Venue
- Advanced Materials
- Publisher
- Wiley
- Published
- 2009-05-04
- Volume
- 21
- Issue
- 18
- Pages
- 1845-1849
- ISSN
- 0935-9648 (ISSN-L)
- 1521-4095
- OpenAlex
- W2136013851
- Cited by
- 317
- References
- 12
- FWCI
- 10.30
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.