Single‐ or Poly‐Crystalline Ni‐Rich Layered Cathode, Sulfide or Halide Solid Electrolyte: Which Will be the Winners for All‐Solid‐State Batteries?
Abstract
Two newly emerging materials for application in all‐solid‐state batteries, namely, single‐crystalline Ni‐rich layered oxide cathode and halide solid electrolyte (SE), are of utmost interest because of their superior properties (good microstructural integrity and excellent electrochemical oxidation stability, respectively) to conventional polycrystalline layered oxides and sulfide SEs. In this work, four electrodes employing single‐ or polycrystalline LiNi 0.88 Co 0.11 Al 0.01 O 2 (NCA) and Li 3 YCl 6 or Li 6 PS 5 Cl 0.5 Br 0.5 are rigorously characterized by complementary analyses. It is shown that the synergy of employing cracking‐free single‐crystalline NCA and oxidation‐tolerable Li 3 YCl 6 can be achieved by considering intercoupled engineering factors that are prone to overlook, such as size, lightness, and mixing of particles. Accordingly, the highest level of performances in terms of discharge capacity (199 mA h g−1 at 0.1C), initial Coulombic efficiency (89.6%), cycling performance (96.8% of capacity retention at the 200th cycle), and rate capability (130 mA h g−1 at 4C) are demonstrated at 30 °C. Severe side reactions occurring at the Li 6 PS 5 Cl 0.5 Br 0.5/NCA interfaces are also quantified and probed. Importantly, an overlooked but significant contribution of the side reaction of Li 6 PS 5 Cl 0.5 Br 0.5 to the detrimental electrochemo‐mechanical degradation of polycrystalline NCA is revealed for the first time by postmortem scanning electron microscopy and operando electrochemical pressiometry measurements.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Challenges for Rechargeable Li Batteries
Goodenough, J. B., & Kim, Y. (2010) · Chemistry of Materials · doi:10.1021/cm901452z · Cited by 10,943
Nonaqueous Liquid Electrolytes for Lithium-Based Rechargeable Batteries
Xu, K. (2004) · Chemical Reviews · doi:10.1021/cr030203g · Cited by 7,437
Toward Safe Lithium Metal Anode in Rechargeable Batteries: A Review
Cheng, X.-B., Zhang, R., Zhao, C.-Z., & Zhang, Q. (2017) · Chemical Reviews · doi:10.1021/acs.chemrev.7b00115 · Cited by 6,197
Promise and reality of post-lithium-ion batteries with high energy densities
Choi, J. W., & Aurbach, D. (2016) · Nature Reviews Materials · doi:10.1038/natrevmats.2016.13 · Cited by 5,110
High-power all-solid-state batteries using sulfide superionic conductors
Kato, Y., Hori, S., Saito, T., Suzuki, K., Hirayama, M., Mitsui, A., Yonemura, M., Iba, H., & Kanno, R. (2016) · Nature Energy · doi:10.1038/nenergy.2016.30 · Cited by 3,517
Negating interfacial impedance in garnet-based solid-state Li metal batteries
Han, X., Gong, Y., Fu, K., He, X., Hitz, G. T., Dai, J., Pearse, A., Liu, B., Wang, H., Rubloff, G., et al. (2017) · Nature Materials · doi:10.1038/nmat4821 · Cited by 2,025
Zhu, Y., He, X., & Mo, Y. (2015) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.5b07517 · Cited by 1,936
Albertus, P., Babinec, S., Litzelman, S., & Newman, A. (2017) · Nature Energy · doi:10.1038/s41560-017-0047-2 · Cited by 1,888
Lee, Y.-G., Fujiki, S., Jung, C., Suzuki, N., Yashiro, N., Omoda, R., Ko, D.-S., Shiratsuchi, T., Sugimoto, T., Ryu, S., et al. (2020) · Nature Energy · doi:10.1038/s41560-020-0575-z · Cited by 1,708
High electronic conductivity as the origin of lithium dendrite formation within solid electrolytes
Han, F., Westover, A. S., Yue, J., Fan, X., Wang, F., Chi, M., Leonard, D. N., Dudney, N. J., Wang, H., & Wang, C. (2019) · Nature Energy · doi:10.1038/s41560-018-0312-z · Cited by 1,695
Chen, R., Li, Q., Yu, X., Chen, L., & Li, H. (2020) · Chemical Reviews · doi:10.1021/acs.chemrev.9b00268 · Cited by 1,678
Interface Stability in Solid-State Batteries
Richards, W. D., Miara, L. J., Wang, Y., Kim, J. C., & Ceder, G. (2016) · Chemistry of Materials · doi:10.1021/acs.chemmater.5b04082 · Cited by 1,652
Materials for lithium-ion battery safety
Liu, K., Liu, Y., Lin, D., Pei, A., & Cui, Y. (2018) · Science Advances · doi:10.1126/sciadv.aas9820 · Cited by 1,625
Interfaces and Interphases in All-Solid-State Batteries with Inorganic Solid Electrolytes
Banerjee, A., Wang, X., Fang, C., Wu, E. A., & Meng, Y. S. (2020) · Chemical Reviews · doi:10.1021/acs.chemrev.0c00101 · Cited by 1,526
New horizons for inorganic solid state ion conductors
Zhang, Z., Shao, Y., Lotsch, B., Hu, Y.-S., Li, H., Janek, J., Nazar, L. F., Nan, C.-W., Maier, J., Armand, M., et al. (2018) · Energy & Environmental Science · doi:10.1039/c8ee01053f · Cited by 1,321
Asano, T., Sakai, A., Ouchi, S., Sakaida, M., Miyazaki, A., & Hasegawa, S. (2018) · Advanced Materials · doi:10.1002/adma.201803075 · Cited by 1,275
Koerver, R., Aygün, I., Leichtweiß, T., Dietrich, C., Zhang, W., Binder, J. O., Hartmann, P., Zeier, W. G., & Janek, J. (2017) · Chemistry of Materials · doi:10.1021/acs.chemmater.7b00931 · Cited by 1,020
Prospect and Reality of Ni‐Rich Cathode for Commercialization
Kim, J., Lee, H., Cha, H., Yoon, M., Park, M., & Cho, J. (2017) · Advanced Energy Materials · doi:10.1002/aenm.201702028 · Cited by 933
Ohta, N., Takada, K., Zhang, L., Ma, R., Osada, M., & Sasaki, T. (2006) · Advanced Materials · doi:10.1002/adma.200502604 · Cited by 899
Physicochemical Concepts of the Lithium Metal Anode in Solid-State Batteries
Krauskopf, T., Richter, F. H., Zeier, W. G., & Janek, J. (2020) · Chemical Reviews · doi:10.1021/acs.chemrev.0c00431 · Cited by 892
Reversible planar gliding and microcracking in a single-crystalline Ni-rich cathode
Bi, Y., Tao, J., Wu, Y., Li, L., Xu, Y., Hu, E., Wu, B., Hu, J., Wang, C., Zhang, J.-G., et al. (2020) · Science · doi:10.1126/science.abc3167 · Cited by 889
Koerver, R., Zhang, W., de Biasi, L., Schweidler, S., Kondrakov, A. O., Kolling, S., Brezesinski, T., Hartmann, P., Zeier, W. G., & Janek, J. (2018) · Energy & Environmental Science · doi:10.1039/c8ee00907d · Cited by 872
Structure and electrochemistry of Li1±yNiO2 and a new Li2NiO2 phase with the Ni (OH)2 structure
Dahn, J. (1990) · Solid State Ionics · doi:10.1016/0167-2738(90)90049-w · Cited by 806
Progress and perspectives on halide lithium conductors for all-solid-state lithium batteries
Li, X., Liang, J., Yang, X., Adair, K. R., Wang, C., Zhao, F., & Sun, X. (2020) · Energy & Environmental Science · doi:10.1039/c9ee03828k · Cited by 755
Air-stable Li3InCl6 electrolyte with high voltage compatibility for all-solid-state batteries
Li, X., Liang, J., Luo, J., Norouzi Banis, M., Wang, C., Li, W., Deng, S., Yu, C., Zhao, F., Hu, Y., et al. (2019) · Energy & Environmental Science · doi:10.1039/c9ee02311a · Cited by 753
Review—Practical Challenges Hindering the Development of Solid State Li Ion Batteries
Kerman, K., Luntz, A., Viswanathan, V., Chiang, Y.-M., & Chen, Z. (2017) · Journal of The Electrochemical Society · doi:10.1149/2.1571707jes · Cited by 712
Kondrakov, A. O., Schmidt, A., Xu, J., Geßwein, H., Mönig, R., Hartmann, P., Sommer, H., Brezesinski, T., & Janek, J. (2017) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.6b12885 · Cited by 701
Adeli, P., Bazak, D. J., Park, K. H., Kochetkov, I. R., Huq, A., Goward, G. R., & Nazar, L. F. (2019) · Angewandte Chemie International Edition · doi:10.1002/anie.201814222 · Cited by 671
There and Back Again—The Journey of LiNiO2 as a Cathode Active Material
Bianchini, M., Roca‐Ayats, M., Hartmann, P., Brezesinski, T., & Janek, J. (2019) · Angewandte Chemie International Edition · doi:10.1002/anie.201812472 · Cited by 670
Fan, X., Hu, G., Zhang, B., Ou, X., Zhang, J., Zhao, W., Jia, H., Zou, L., Li, P., & Yang, Y. (2020) · Nano Energy · doi:10.1016/j.nanoen.2020.104450 · Cited by 661
Auvergniot, J., Cassel, A., Ledeuil, J.-B., Viallet, V., Seznec, V., & Dedryvère, R. (2017) · Chemistry of Materials · doi:10.1021/acs.chemmater.6b04990 · Cited by 644
Park, K. H., Bai, Q., Kim, D. H., Oh, D. Y., Zhu, Y., Mo, Y., & Jung, Y. S. (2018) · Advanced Energy Materials · doi:10.1002/aenm.201800035 · Cited by 589
Self-citationStructural change of Li2S–P2S5 sulfide solid electrolytes in the atmosphere
Muramatsu, H., Hayashi, A., Ohtomo, T., Hama, S., & Tatsumisago, M. (2010) · Solid State Ionics · doi:10.1016/j.ssi.2010.10.013 · Cited by 568
Site-Occupation-Tuned Superionic LixScCl3+xHalide Solid Electrolytes for All-Solid-State Batteries
Liang, J., Li, X., Wang, S., Adair, K. R., Li, W., Zhao, Y., Wang, C., Hu, Y., Zhang, L., Zhao, S., et al. (2020) · Journal of the American Chemical Society · doi:10.1021/jacs.0c00134 · Cited by 567
Qian, G., Zhang, Y., Li, L., Zhang, R., Xu, J., Cheng, Z., Xie, S., Wang, H., Rao, Q., He, Y., et al. (2020) · Energy Storage Materials · doi:10.1016/j.ensm.2020.01.027 · Cited by 564
High-Voltage Superionic Halide Solid Electrolytes for All-Solid-State Li-Ion Batteries
Park, K.-H., Kaup, K., Assoud, A., Zhang, Q., Wu, X., & Nazar, L. F. (2020) · ACS Energy Letters · doi:10.1021/acsenergylett.9b02599 · Cited by 506
Li metal deposition and stripping in a solid-state battery via Coble creep
Chen, Y., Wang, Z., Li, X., Yao, X., Wang, C., Li, Y., Xue, W., Yu, D., Kim, S. Y., Yang, F., et al. (2020) · Nature · doi:10.1038/s41586-020-1972-y · Cited by 500
Hou, Q., Wu, Y., Zhou, S., Wei, Y., Caro, J., & Wang, H. (2019) · Angewandte Chemie International Edition · doi:10.1002/anie.201813331 · Cited by 461
Walther, F., Koerver, R., Fuchs, T., Ohno, S., Sann, J., Rohnke, M., Zeier, W. G., & Janek, J. (2019) · Chemistry of Materials · doi:10.1021/acs.chemmater.9b00770 · Cited by 433
Surface regulation enables high stability of single-crystal lithium-ion cathodes at high voltage
Zhang, F., Lou, S., Li, S., Yu, Z., Liu, Q., Dai, A., Cao, C., Toney, M. F., Ge, M., Xiao, X., et al. (2020) · Nature Communications · doi:10.1038/s41467-020-16824-2 · Cited by 431
The Detrimental Effects of Carbon Additives in Li10GeP2S12-Based Solid-State Batteries
Zhang, W., Leichtweiß, T., Culver, S. P., Koerver, R., Das, D., Weber, D. A., Zeier, W. G., & Janek, J. (2017) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.7b11530 · Cited by 392
Nam, Y. J., Oh, D. Y., Jung, S. H., & Jung, Y. S. (2018) · Journal of Power Sources · doi:10.1016/j.jpowsour.2017.11.031 · Cited by 390
Self-citationInterfacial Chemistry in Solid-State Batteries: Formation of Interphase and Its Consequences
Wang, S., Xu, H., Li, W., Dolocan, A., & Manthiram, A. (2018) · Journal of the American Chemical Society · doi:10.1021/jacs.7b09531 · Cited by 342
High Active Material Loading in All‐Solid‐State Battery Electrode via Particle Size Optimization
Shi, T., Tu, Q. H., Tian, Y., Xiao, Y., Miara, L. J., Kononova, O., & Ceder, G. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201902881 · Cited by 338
A new halospinel superionic conductor for high-voltage all solid state lithium batteries
Zhou, L., Kwok, C. Y., Shyamsunder, A., Zhang, Q., Wu, X., & Nazar, L. F. (2020) · Energy & Environmental Science · doi:10.1039/d0ee01017k · Cited by 335
Kwak, H., Han, D., Lyoo, J., Park, J., Jung, S. H., Han, Y., Kwon, G., Kim, H., Hong, S., Nam, K., et al. (2021) · Advanced Energy Materials · doi:10.1002/aenm.202003190 · Cited by 323
Self-citationSolution‐Processable Glass LiI‐Li4SnS4 Superionic Conductors for All‐Solid‐State Li‐Ion Batteries
Park, K. H., Oh, D. Y., Choi, Y. E., Nam, Y. J., Han, L., Kim, J., Xin, H. L., Lin, F., Oh, S. M., & Jung, Y. S. (2015) · Advanced Materials · doi:10.1002/adma.201505008 · Cited by 321
Self-citationThe nanoscale circuitry of battery electrodes
Zhu, C., Usiskin, R. E., Yu, Y., & Maier, J. (2017) · Science · doi:10.1126/science.aao2808 · Cited by 302
High-Throughput Screening of Solid-State Li-Ion Conductors Using Lattice-Dynamics Descriptors
Muy, S., Voss, J., Schlem, R., Koerver, R., Sedlmaier, S. J., Maglia, F., Lamp, P., Zeier, W. G., & Shao-Horn, Y. (2019) · iScience · doi:10.1016/j.isci.2019.05.036 · Cited by 262
Jung, S. H., Kim, U., Kim, J., Jun, S., Yoon, C. S., Jung, Y. S., & Sun, Y. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201903360 · Cited by 259
Self-citationMaterials Design Principles for Air‐Stable Lithium/Sodium Solid Electrolytes
Zhu, Y., & Mo, Y. (2020) · Angewandte Chemie International Edition · doi:10.1002/anie.202007621 · Cited by 248
Li3BO3–Li2CO3: Rationally Designed Buffering Phase for Sulfide All-Solid-State Li-Ion Batteries
Jung, S. H., Oh, K., Nam, Y. J., Oh, D. Y., Brüner, P., Kang, K., & Jung, Y. S. (2018) · Chemistry of Materials · doi:10.1021/acs.chemmater.8b03321 · Cited by 233
Self-citationBoosting Reaction Homogeneity in High‐Energy Lithium‐Ion Battery Cathode Materials
Cha, H., Kim, J., Lee, H., Kim, N., Hwang, J., Sung, J., Yoon, M., Kim, K., & Cho, J. (2020) · Advanced Materials · doi:10.1002/adma.202003040 · Cited by 231
Unexpected Improved Performance of ALD Coated LiCoO2/Graphite Li‐Ion Batteries
Jung, Y. S., Lu, P., Cavanagh, A. S., Ban, C., Kim, G., Lee, S., George, S. M., Harris, S. J., & Dillon, A. C. (2013) · Advanced Energy Materials · doi:10.1002/aenm.201200370 · Cited by 228
Self-citationWang, M. J., Carmona, E. A., Gupta, A., Albertus, P. S., & Sakamoto, J. S. (2020) · Nature Communications · doi:10.1038/s41467-020-19004-4 · Cited by 222
Liu, Z., Ma, S., Liu, J., Xiong, S., Ma, Y., & Chen, H. (2020) · ACS Energy Letters · doi:10.1021/acsenergylett.0c01690 · Cited by 218
Oh, D. Y., Nam, Y. J., Park, K. H., Jung, S. H., Kim, K. T., Ha, A. R., & Jung, Y. S. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201802927 · Cited by 217
Self-citationKim, D. H., Lee, Y.-H., Song, Y. B., Kwak, H., Lee, S.-Y., & Jung, Y. S. (2020) · ACS Energy Letters · doi:10.1021/acsenergylett.0c00251 · Cited by 215
Self-citationShin, B. R., Nam, Y. J., Oh, D. Y., Kim, D. H., Kim, J. W., & Jung, Y. S. (2014) · Electrochimica Acta · doi:10.1016/j.electacta.2014.08.139 · Cited by 214
Self-citationHakari, T., Deguchi, M., Mitsuhara, K., Ohta, T., Saito, K., Orikasa, Y., Uchimoto, Y., Kowada, Y., Hayashi, A., & Tatsumisago, M. (2017) · Chemistry of Materials · doi:10.1021/acs.chemmater.7b00551 · Cited by 205
Synthesis of Single Crystal LiNi0.88Co0.09Al0.03O2 with a Two-Step Lithiation Method
Li, H., Li, J., Zaker, N., Zhang, N., Botton, G. A., & Dahn, J. R. (2019) · Journal of The Electrochemical Society · doi:10.1149/2.0681910jes · Cited by 168
Ghanty, C., Markovsky, B., Erickson, E. M., Talianker, M., Haik, O., Tal‐Yossef, Y., Mor, A., Aurbach, D., Lampert, J., Volkov, A., et al. (2015) · ChemElectroChem · doi:10.1002/celc.201500160 · Cited by 163
Oh, D. Y., Kim, D. H., Jung, S. H., Han, J., Choi, N., & Jung, Y. S. (2017) · Journal of Materials Chemistry A · doi:10.1039/c7ta06873e · Cited by 154
Self-citationA stable 3 V all-solid-state sodium–ion battery based on a closo -borate electrolyte
Duchêne, L., Kühnel, R., Stilp, E., Cuervo‐Reyes, E., Remhof, A., Hagemann, H. R., & Battaglia, C. (2017) · Energy & Environmental Science · doi:10.1039/c7ee02420g · Cited by 154
Strauss, F., de Biasi, L., Kim, A., Hertle, J., Schweidler, S., Janek, J., Hartmann, P., & Brezesinski, T. (2019) · ACS Materials Letters · doi:10.1021/acsmaterialslett.9b00441 · Cited by 111
Nakamura, H., Kawaguchi, T., Masuyama, T., et al. (2019) · Journal of Power Sources · doi:10.1016/j.jpowsour.2019.227579 · Cited by 93
Jun, S., Nam, Y. J., Kwak, H., Kim, K. T., Oh, D. Y., & Jung, Y. S. (2020) · Advanced Functional Materials · doi:10.1002/adfm.202002535 · Cited by 86
Self-citationKim, K. T., Oh, D. Y., Jun, S., Song, Y. B., Kwon, T. Y., Han, Y., & Jung, Y. S. (2021) · Advanced Energy Materials · doi:10.1002/aenm.202003766 · Cited by 74
Self-citationDiagnosis of failure modes for all-solid-state Li-ion batteries enabled by three-electrode cells
Nam, Y. J., Park, K. H., Oh, D. Y., An, W. H., & Jung, Y. S. (2018) · Journal of Materials Chemistry A · doi:10.1039/c8ta03450h · Cited by 68
Self-citation
Cited by
Prospects of halide-based all-solid-state batteries: From material design to practical application
Wang, C., Liang, J., Kim, J. T., & Sun, X. (2022) · Science Advances · doi:10.1126/sciadv.adc9516 · Cited by 366
Kwak, H., Wang, S., Park, J., Liu, Y., Kim, K. T., Choi, Y., Mo, Y., & Jung, Y. S. (2022) · ACS Energy Letters · doi:10.1021/acsenergylett.2c00438 · Cited by 341
Self-citationDesigning Cathodes and Cathode Active Materials for Solid‐State Batteries
Minnmann, P., Strauss, F., Bielefeld, A., Ruess, R., Adelhelm, P., Burkhardt, S., Dreyer, S. L., Trevisanello, E., Ehrenberg, H., Brezesinski, T., et al. (2022) · Advanced Energy Materials · doi:10.1002/aenm.202201425 · Cited by 277
Liang, Y., Liu, H., Wang, G., Wang, C., Ni, Y., Nan, C., & Fan, L. (2022) · InfoMat · doi:10.1002/inf2.12292 · Cited by 273
Metadata
- Authors
- Han, Y., Jung, S. H., Kwak, H., Jun, S., Kwak, H. H., Lee, J. H., Hong, S., & Jung, Y. S.
- Venue
- Advanced Energy Materials
- Publisher
- Wiley
- Published
- 2021-04-17
- Volume
- 11
- Issue
- 21
- ISSN
- 1614-6832 (ISSN-L)
- 1614-6840
- OpenAlex
- W3153036406
- Cited by
- 312
- References
- 69
- FWCI
- 15.77
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.