Temperature‐Dependent Nucleation and Growth of Dendrite‐Free Lithium Metal Anodes
Abstract
It is essential to develop a facile and effective method to enhance the electrochemical performance of lithium metal anodes for building high‐energy‐density Li‐metal based batteries. Herein, we explored the temperature‐dependent Li nucleation and growth behavior and constructed a dendrite‐free Li metal anode by elevating temperature from room temperature (20 °C) to 60 °C. A series of ex situ and in situ microscopy investigations demonstrate that increasing Li deposition temperature results in large nuclei size, low nucleation density, and compact growth of Li metal. We reveal that the enhanced lithiophilicity and the increased Li‐ion diffusion coefficient in aprotic electrolytes at high temperature are essential factors contributing to the dendrite‐free Li growth behavior. As anodes in both half cells and full cells, the compact deposited Li with minimized specific surface area delivered high Coulombic efficiencies and long cycling stability at 60 °C.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Reviving the lithium metal anode for high-energy batteries
Lin, D., Liu, Y., & Cui, Y. (2017) · Nature Nanotechnology · doi:10.1038/nnano.2017.16 · Cited by 6,763
A highly ordered nanostructured carbon–sulphur cathode for lithium–sulphur batteries
Ji, X., Lee, K. T., & Nazar, L. F. (2009) · Nature Materials · doi:10.1038/nmat2460 · Cited by 5,988
Lithium metal anodes for rechargeable batteries
Xu, W., Wang, J., Ding, F., Chen, X., Nasybulin, E., Zhang, Y., & Zhang, J.-G. (2014) · Energy Environ. Sci. · doi:10.1039/c3ee40795k · Cited by 4,704
Self-citationPathways for practical high-energy long-cycling lithium metal batteries
Liu, J., Bao, Z., Cui, Y., Dufek, E. J., Goodenough, J. B., Khalifah, P., Li, Q., Liaw, B. Y., Liu, P., Manthiram, A., et al. (2019) · Nature Energy · doi:10.1038/s41560-019-0338-x · Cited by 3,412
Self-citationSelective deposition and stable encapsulation of lithium through heterogeneous seeded growth
Yan, K., Lu, Z., Lee, H.-W., Xiong, F., Hsu, P.-C., Li, Y., Zhao, J., Chu, S., & Cui, Y. (2016) · Nature Energy · doi:10.1038/nenergy.2016.10 · Cited by 2,116
Self-citationNanoscale Nucleation and Growth of Electrodeposited Lithium Metal
Pei, A., Zheng, G., Shi, F., Li, Y., & Cui, Y. (2017) · Nano Letters · doi:10.1021/acs.nanolett.6b04755 · Cited by 1,726
Self-citationAn Artificial Solid Electrolyte Interphase Layer for Stable Lithium Metal Anodes
Li, N., Yin, Y., Yang, C., & Guo, Y. (2016) · Advanced Materials · doi:10.1002/adma.201504526 · Cited by 1,577
A Graphene–Pure‐Sulfur Sandwich Structure for Ultrafast, Long‐Life Lithium–Sulfur Batteries
Zhou, G., Pei, S., Li, L., Wang, D., Wang, S., Huang, K., Yin, L., Li, F., & Cheng, H. (2014) · Advanced Materials · doi:10.1002/adma.201302877 · Cited by 997
Lithium-coated polymeric matrix as a minimum volume-change and dendrite-free lithium metal anode
Liu, Y., Lin, D., Liang, Z., Zhao, J., Yan, K., & Cui, Y. (2016) · Nature Communications · doi:10.1038/ncomms10992 · Cited by 902
Self-citationLithium-ion battery structure that self-heats at low temperatures
Wang, C.-Y., Zhang, G., Ge, S., Xu, T., Ji, Y., Yang, X.-G., & Leng, Y. (2016) · Nature · doi:10.1038/nature16502 · Cited by 878
Cited by
A Growing Appreciation for the Role of LiF in the Solid Electrolyte Interphase
Tan, J., Matz, J., Dong, P., Shen, J., & Ye, M. (2021) · Advanced Energy Materials · doi:10.1002/aenm.202100046 · Cited by 1,019
Liu, W., Liu, P., & Mitlin, D. (2020) · Advanced Energy Materials · doi:10.1002/aenm.202002297 · Cited by 687
Zinc Anode for Mild Aqueous Zinc-Ion Batteries: Challenges, Strategies, and Perspectives
Yang, J., Yin, B., Sun, Y., Pan, H., Sun, W., Jia, B., Zhang, S., & Ma, T. (2022) · Nano-Micro Letters · doi:10.1007/s40820-021-00782-5 · Cited by 584
Thermodynamic Understanding of Li-Dendrite Formation
Gao, X., Zhou, Y.-N., Han, D., Zhou, J., Zhou, D., Tang, W., & Goodenough, J. B. (2020) · Joule · doi:10.1016/j.joule.2020.06.016 · Cited by 537
Self-citationLiu, D.-H., Bai, Z., Li, M., Yu, A., Luo, D., Liu, W., Yang, L., Lu, J., Amine, K., & Chen, Z. (2020) · Chemical Society Reviews · doi:10.1039/c9cs00636b · Cited by 483
Review on Li Deposition in Working Batteries: From Nucleation to Early Growth
Chen, X., Zhao, B., Yan, C., & Zhang, Q. (2021) · Advanced Materials · doi:10.1002/adma.202004128 · Cited by 456
Lai, X., Jin, C., Yi, W., Han, X., Feng, X., Zheng, Y., & Ouyang, M. (2021) · Energy Storage Materials · doi:10.1016/j.ensm.2020.11.026 · Cited by 438
Zinc dendrite growth and inhibition strategies
Zuo, Y., Wang, K., Pei, P., Wei, M., Liu, X., Xiao, Y., & Zhang, P. (2021) · Materials Today Energy · doi:10.1016/j.mtener.2021.100692 · Cited by 409
A Review of Solid Electrolyte Interphase (SEI) and Dendrite Formation in Lithium Batteries
Li, B., Chao, Y., Li, M., Xiao, Y., Li, R., Yang, K., Cui, X., Xu, G., Li, L., Yang, C., et al. (2023) · Electrochemical Energy Reviews · doi:10.1007/s41918-022-00147-5 · Cited by 406
Wu, K.-J., Tse, E. C. M., Shang, C., & Guo, Z. (2022) · Progress in Materials Science · doi:10.1016/j.pmatsci.2021.100821 · Cited by 400
The passivity of lithium electrodes in liquid electrolytes for secondary batteries
He, X., Bresser, D., Passerini, S., Baakes, F., Krewer, U., Lopez, J., Mallia, C. T., Shao-Horn, Y., Cekic-Laskovic, I., Wiemers-Meyer, S., et al. (2021) · Nature Reviews Materials · doi:10.1038/s41578-021-00345-5 · Cited by 393
Chen, S., Dai, F., & Cai, M. (2020) · ACS Energy Letters · doi:10.1021/acsenergylett.0c01545 · Cited by 362
Ding, J., Xu, R., Yao, N., Chen, X., Xiao, Y., Yao, Y., Yan, C., Xie, J., & Huang, J. (2021) · Angewandte Chemie International Edition · doi:10.1002/anie.202101627 · Cited by 337
Advances in Composite Polymer Electrolytes for Lithium Batteries and Beyond
Tang, S., Guo, W., & Fu, Y. (2021) · Advanced Energy Materials · doi:10.1002/aenm.202000802 · Cited by 335
Gel polymer electrolytes for rechargeable batteries toward wide-temperature applications
Zhou, X., Zhou, Y., Yu, L., Qi, L., Oh, K.-S., Hu, P., Lee, S.-Y., & Chen, C. (2024) · Chemical Society Reviews · doi:10.1039/d3cs00551h · Cited by 333
Hao, H., Hutter, T., Boyce, B. L., Watt, J., Liu, P., & Mitlin, D. (2022) · Chemical Reviews · doi:10.1021/acs.chemrev.1c00838 · Cited by 314
A review on the failure and regulation of solid electrolyte interphase in lithium batteries
Ding, J.-F., Xu, R., Yan, C., Li, B.-Q., Yuan, H., & Huang, J.-Q. (2021) · Journal of Energy Chemistry · doi:10.1016/j.jechem.2020.11.016 · Cited by 313
How to avoid dendrite formation in metal batteries: Innovative strategies for dendrite suppression
Aslam, M. K., Niu, Y., Hussain, T., Tabassum, H., Tang, W., Xu, M., & Ahuja, R. (2021) · Nano Energy · doi:10.1016/j.nanoen.2021.106142 · Cited by 308
Surface engineering toward stable lithium metal anodes
Lu, G., Nai, J., Luan, D., Tao, X., & Lou, X. W. (. (2023) · Science Advances · doi:10.1126/sciadv.adf1550 · Cited by 289
Guo, W., Zhang, W., Si, Y., Wang, D., Fu, Y., & Manthiram, A. (2021) · Nature Communications · doi:10.1038/s41467-021-23155-3 · Cited by 268
Plating/Stripping Behavior of Actual Lithium Metal Anode
Liu, H., Cheng, X., Xu, R., Zhang, X., Yan, C., Huang, J., & Zhang, Q. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201902254 · Cited by 260
An electron-deficient carbon current collector for anode-free Li-metal batteries
Kwon, H., Lee, J.-H., Roh, Y., Baek, J., Shin, D. J., Yoon, J. K., Ha, H. J., Kim, J. Y., & Kim, H.-T. (2021) · Nature Communications · doi:10.1038/s41467-021-25848-1 · Cited by 257
Metadata
- Authors
- Yan, K., Wang, J., Zhao, S., Zhou, D., Sun, B., Cui, Y., & Wang, G.
- Venue
- Angewandte Chemie International Edition
- Publisher
- Wiley
- Published
- 2019-07-08
- Volume
- 58
- Issue
- 33
- Pages
- 11364-11368
- ISSN
- 1433-7851 (ISSN-L)
- 1521-3773
- OpenAlex
- W2946861946
- Cited by
- 273
- References
- 20
- FWCI
- 12.69
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.