Photooxidative effects on properties and structure of high-density polyethylene
The DOI matches its Crossref record; 19 of the 19 references it cites were found in a registry or an index.
Abstract
The environmental degradation of high‐density polyethylene (HDPE) has been studied, in addition to that of HDPE blends, containing various concentrations of ethylene carbon monoxide copolymer. Extruded sheets of each material were exposed to natural Arizona sunlight for times up to 6 months. Exposed samples were then analyzed with respect to molecular weight, density, thermal behavior, mechanical properties, and infrared absorption. Additional samples were exposed to laboratory weathering conditions, evaluated in terms of property changes, melted, reformed, and then reevaluated without further weathering exposure. Results indicate that sunlight exposure causes decreased elongation to break, increased embrittlement, decreased molecular weight, and increased crystallinity. Environmental oxidative degradation is elucidated by the measurement of specific infrared bands, sensitive to the formation of carbonyl and vinyl end groups. As environmental degradation causes reductions of molecular weight, polymer chain mobility increases, leading to a higher degree of crystallinity. This increased crystallinity, along with the decreased molecular weight, accounts for the loss of ductility, indicated by a sharp decrease in ultimate elongation. The presence of carbon monoxide copolymer in the blended samples accelerates the process of environmental degradation, however, the degradation mechanisms appear to be similar to those observed for nonblended HDPE. © 1994 John Wiley & Sons, Inc.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“Structural modifications and brittleness, although a usual observation, do not always correspond to mechanical strength and molecular weight changes (Andrady, 1990;Jabarin and Lofgren, 1994;Tidjani, 2000;Carrasco et al., 2001).”
From Microplastics Generation: Onset of Fragmentation of Polyethylene Films in Marine Environment Mesocosms (2017) · cites this paper as Jabarin and Lofgren, 1994
In the citing paper
“Essentially, at this degree of weathering no measurement is possible due to sample breakage (Andrady et al., 1993;Jabarin and Lofgren, 1994;Tidjani, 2000).”
From Microplastics Generation: Onset of Fragmentation of Polyethylene Films in Marine Environment Mesocosms (2017) · cites this paper as Jabarin and Lofgren, 1994
In the citing paper
“Jabarin and Lofgren (1994), using FTIR to measure crystallinity were able to deduce that absorbance bands tended to be wider with higher peaks with exposure time, in a similar manner to Tidjani (2000).”
From Microplastics Generation: Onset of Fragmentation of Polyethylene Films in Marine Environment Mesocosms (2017) · cites this paper as Jabarin and Lofgren, 1994
In the citing paper
“Jabarin and Lofgren (1994) reported that the molecular weight of HDPE decreased from 147,000 in the original sample to 34,100 after 6 months of exposure to artificial UV light.”
From Microplastics Generation: Onset of Fragmentation of Polyethylene Films in Marine Environment Mesocosms (2017) · cites this paper as Jabarin and Lofgren, 1994
Citations
Cites
Experiments in Polymer Science
Collins, E. A., Bareš, J., & Billmeyer, F. W. (1973) · Medical Entomology and Zoology · Cited by 408
Photochemistry of Ketone Polymers. I. Studies of Ethylene-Carbon Monoxide Copolymers
Hartley, G. H., & Guillet, J. E. (1968) · Macromolecules · doi:10.1021/ma60002a012 · Cited by 227
International symposium on macromolecular chemistry
(1978) · Fibre Chemistry · doi:10.1007/bf00546430 · Cited by 189
The effect of processing conditions on the u.v. stability of polyolefins
Mellor, D. C., Moir, A. B., & SCOTT, G. (1973) · European Polymer Journal · doi:10.1016/0014-3057(73)90129-8 · Cited by 118
Blais, P., Carlsson, D. J., & Wiles, D. M. (1972) · Journal of Polymer Science Part A-1 Polymer Chemistry · doi:10.1002/pol.1972.150100412 · Cited by 114
Mechanism of the photo-initiation process in polyethylene
Amin, M. U., Scott, G., & Tillekeratne, L. M. (1975) · European Polymer Journal · doi:10.1016/0014-3057(75)90179-2 · Cited by 108
Okada, T., & Mandelkern, L. (1967) · Journal of Polymer Science Part A-2 Polymer Physics · doi:10.1002/pol.1967.160050201 · Cited by 104
Chakraborty, K. B., & SCOTT, G. (1977) · European Polymer Journal · doi:10.1016/0014-3057(77)90074-x · Cited by 87
Photodegradation and stabilization of commercial polyolefins
Allen, N. S., & McKellar, J. F. (1975) · Chemical Society Reviews · doi:10.1039/cs9750400533 · Cited by 66
Autoxidation of semicrystalline polyethylene
Winslow, F. H., Hellman, M. Y., Matreyek, W., & Stills, S. M. (1966) · Polymer Engineering & Science · doi:10.1002/pen.760060317 · Cited by 65
Research works printed but not linked: 3
- Heaps J. M., 1966, Weathering and Degradation of Plastics
- Omichi H., 1983, Degradation and Stabilization of Polyolefins
- Wunderlich B., 1973, Macromolecular Physics: Volume 1 Crystal Structure, Morphology, Defects
Cited by
Items 101–151 of 151
Chiapasco, M., Valsecchi, M., Hill, G., Wallis, C., Porter, A. E., & Giuliani, F. (2024) · Nano Select · doi:10.1002/nano.202300082 · Cited by 6
“An increase in crystallinity and a decrease in crystallite dimensions has also been reported in studies on aged polymers using differential scanning calorimetry (DSC) [14, 15, 22, 23].”
Aboamer, M. A., Aboamer, A. A., Elgohary, D. H., Alqahtani, T. M., Abdel-Hadi, A., Al-Mutairi, S. M., EL-Bagory, T. M. A. A., Alshareef, K. M., & Mohamed, N. A. R. (2022) · Journal of Mechanical Science and Technology · doi:10.1007/s12206-022-1114-6 · Cited by 6
“Owing to its cheap production costs, HDPE has become one of the most extensively used polymers in daily life [37].”
BackgroundProcessing and Characterization of UV Irradiated HDPE/POSS Fibers
Biçer, E., Kodal, M., & Özkoç, G. (2023) · Nanomaterials · doi:10.3390/nano13243131 · Cited by 6
“Decomposition reactions arise from the carbonyl group through Norrish type I and II reactions [38].”
BackgroundZhang, X., Li, X., Lyu, J., Zhu, X., Xu, L. S., Gao, L., Yang, M. H., & Chang, X. (2024) · Polymer Composites · doi:10.1002/pc.28170 · Cited by 6
Nayrac, N., Bellenger, J., & Segura, P. A. (2022) · Analytical Methods · doi:10.1039/d2ay01201d · Cited by 6
TESTING METHODS OF WEATHERED SPECIMEN
Wypych, G. (2013) · Elsevier eBooks · doi:10.1016/b978-1-895198-62-1.50016-0 · Cited by 6
Properties of paper mill sludge–wood fiber–HDPE composites after exposure to xenon-arc weathering
Yang, X., Zhang, X., Wang, W., Huang, H., & Sui, S. (2015) · Journal of Forestry Research · doi:10.1007/s11676-015-0051-y · Cited by 5
“Carbonyl groups are postulated to be the main light-absorbing species responsible for photochemical-induced degradation reactions of UV-exposed polymers (Jabarin and Lofgren 1994).”
BackgroundHung, K., Chang, W.-C., Xu, J.-W., Wu, T.-L., & Wu, J. (2021) · Polymers · doi:10.3390/polym13162681 · Cited by 6
“On the other hand, Jabarin and Lofgren [61] and Zo et al. [62] reported that photooxidation causes chain scission in the amorphous phase of polyolefins during the initial weathering period, and the resulting shorter molecules are believed to possess sufficient chain mobility to cause secondary crystallization.”
BackgroundInfluentialUV Radiation Effect in New Materials Developed for the Construction of Beehives
Rubiano-Navarrete, A. F., Fabián, C. L., Torres-Pérez, Y., & Gómez-Pachón, E. Y. (2023) · Polymers · doi:10.3390/polym15214249 · Cited by 5
Ezugwu, E. P., Lopez, E., Ortín, A., Bhattacharya, M., & Mantell, S. C. (2024) · Polymer · doi:10.1016/j.polymer.2024.127752 · Cited by 5
Wypych, G. (2018) · Elsevier eBooks · doi:10.1016/b978-1-927885-31-4.50016-9 · Cited by 5
DESENVOLVIMENTO DE POLIPROPILENO AMBIENTALMENTE DEGRADÁVEL
Montagna, L. S. (2014) · LA Referencia (Red Federada de Repositorios Institucionales de Publicaciones Científicas) · doi:10.13140/rg.2.1.1856.4085 · Cited by 5
Collett, G., Akhavan, J., & Critchley, R. (2024) · Discover Materials · doi:10.1007/s43939-024-00090-w · Cited by 4
Infrared Spectroscopic Study of the Thermo-Oxidative Aging of Polyethylene Containing Pro-Oxidant
Kérouani, S., Sadoun, T., & Azzouz, N. (2013) · Advanced materials research · doi:10.4028/www.scientific.net/amr.685.316 · Cited by 4
Photochemical Process of Wood-Thermoplastic Composites
Peng, Y., & Cao, J. (2016) · Advanced structured materials · doi:10.1007/978-3-319-25196-7_10 · Cited by 4
Influence of UV irradiation on the degradation of composites based on polyethylene
Podzorova, M. V., Varyan, I. A., Kiselev, N., Tertyshnaya, Y. V., & Храмкова, А. В. (2023) · E3S Web of Conferences · doi:10.1051/e3sconf/202341302018 · Cited by 4
Ribeiro, M. V. (2004) · Digital Library of Theses and Dissertations (Universidade de São Paulo) · doi:10.11606/d.3.2004.tde-17092004-145545 · Cited by 4
Avaliação da degradação abiótica de filmes de PEAD/PEBD processados com aditivos pró-degradantes
Brandão, J. A. O. (2021) · LA Referencia (Red Federada de Repositorios Institucionales de Publicaciones Científicas) · Cited by 4
Testing Methods of Weathered Specimen
Wypych, G. (2018) · Elsevier eBooks · doi:10.1016/b978-1-927885-31-4.50015-7 · Cited by 3
Chen, B. (2025) · Enlighten: Theses (The University of Glasgow) · doi:10.5525/gla.thesis.85634 · Cited by 3
Abutalib, M. M., & Guirguis, O. W. (2014) · British Journal of Applied Science & Technology · doi:10.9734/bjast/2014/12723 · Cited by 2
Brandalise, R. N., Martins, J. D. N., Zeni, M., & Forte, M. M. C. (2008) · Revista Iberoamericana de Polímeros · Cited by 2
Galgani, F., Pham, C. K., & Reisser, J. (2017) · Frontiers research topics · doi:10.3389/978-2-88945-330-6 · Cited by 2
Brandalise, R. N. (2008) · Americanae (AECID Library) · Cited by 2
Assessment of Polyethylene Geomembrane Properties after Accelerated Thermal Ageing
Hamma, A., Bezza, A., & Bouhelal, S. (2022) · Annales de Chimie Science des Matériaux · doi:10.18280/acsm.460404 · Cited by 1
“From the normalised spectra, vinyl, carbonyl and hydroxyl indexes were calculated as the ratio between the peak areas, of 1330-880 cm -1 , 1850-1650 cm -1 and 3575-3125 cm -1 and the peak area of the symmetric C-H stretching band of methylene groups [32-37].”
UV Aging of Poly (Butylene) Succinate/Date Palm Fibers Composites
Chaari, R., Khlif, M., Bradaï, C., Lacoste, C., & Dony, P. (2024) · Lecture notes in mechanical engineering · doi:10.1007/978-3-031-65007-9_11 · Cited by 1
Romero, F., Kelly-Walley, J., McCourt, M. P., Suárez, L., & Ortega, Z. (2025) · Materials · doi:10.3390/ma18204723 · Cited by 1
“It was expected to obtain a reduction in the elongation at break for samples, due to the embrittlement of the matrix induced by the UV-radiation, as found in previous works [71,72].”
Chen, B., Xie, D., Xue, J., Zhao, J., Cheng, S., Cai, D., Cao, H., You, S., & Watson, I. (2026) · Industrial Crops and Products · doi:10.1016/j.indcrop.2026.123071 · Cited by 1
“It has been reported the degradation of HDPE was caused by chain scission via Norrish Type I and II reactions and resulted in shorter polymer chains (Jabarin and Lofgren, 1994).”
InfluentialKharraf, A. E., Rabiller‐Baudry, M., Real, A., Sandt, C., Guin, J., Vantelon, D., Wiesner, M. R., Dutruch, L., & Davranche, M. (2026) · Water Research · doi:10.1016/j.watres.2026.126333 · Cited by 1
Podzorova, M. V., Var’an, I. A., Tertyshnaya, Y. V., Kolesnikova, N. N., Popov, A. A., & Abushakhmanova, Z. R. (2024) · Polymer Science Series D · doi:10.1134/s1995421223700260 · Cited by 1
Effects of UV Light on the Structure and Properties of Glyoxal Polymers
Yang, Y., Wei, Y., Zhou, H., Wu, T., Fang, B., & Zhao, Y. (2025) · Journal of Applied Polymer Science · doi:10.1002/app.56919 · Cited by 1
Selüloz esaslı lif takviyeli kompozit otomotiv parçası tasarımı ve geliştirilmesi
Ovalı, S. (2020) · Dspace Repository (Marmara Üniversitesi) · Cited by 1
Zhang, J. (2005) · TSpace (University of Toronto) · Cited by 1
Grob, M. C., Huber, G., Herbst, H., Gal, A. L., Müller, D., Priest, H., Tartarini, C., Thürmer, A., Schulz, L., Wegmann, A., et al. (2016) · Carl Hanser Verlag GmbH & Co. KG eBooks · doi:10.1007/978-3-446-43291-8_2
Tuttle, E. E. (2023) · Digital Repository Service (Northeastern University) · doi:10.17760/d20560793
Effect of low/high hybrid of coffee husk powder on weathering resistance of WPCs compositesPreprint
Wang, M., Di, Y., Zhong, C., Wang, R., & Wu, Z. (2024) · Research Square · doi:10.21203/rs.3.rs-3918112/v1
Wypych, G. (2025) · Elsevier eBooks · doi:10.1016/b978-1-77467-058-3.50018-0
TESTING METHODS OF WEATHERED SPECIMEN
Wypych, G. (2025) · Elsevier eBooks · doi:10.1016/b978-1-77467-058-3.50017-9
Thermal aging effects on LDPE greenhouse films: anisotropy and degradation
Babaghayou, M. I., Mourad, A. I., Belaid, S., Yadav, A. A., & Hunge, Y. M. (2025) · International Journal of Environmental Science and Technology · doi:10.1007/s13762-025-06601-3
“These factors limit molecular mobility in the amorphous phase during thermal aging, resulting in increased heterogeneity of the local structure and enhanced chemical dispersion (Jabarin and Lofgren 1994; Assink et al. 2001; Celina et al. 1998).”
(n.d.) · Research Publication Repository of King Fahd University of Petroleum and Minerals (King Fahd University of Petroleum and Minerals)
聂旭阳, Zhong, W., Tang, Y., Liu, X., & Chen, S. (2025) · Proceedings of the World Congress on Mechanical, Chemical, and Material Engineering · doi:10.11159/icmie25.132
Razgradnja mikroplastike v okolju
Budhiraja, V. (2024) · RUNG
Bodur, M. S. (2016) · Istanbul Technical University Academic Open Archive (Istanbul Technical University)
Contrôle avancé de production de polyéthylène par spectroscopie Raman
Jumeau, R. (2013) · theses.fr (ABES) · doi:10.70675/28ff3f4fz9c44z4d96zb14ez8201d401d246
Preparation and Characterization of HDPE/Graphene Nano-Composites by In-situ Polymerization
Farrukh, S. (2014) · Research Publication Repository of King Fahd University of Petroleum and Minerals (King Fahd University of Petroleum and Minerals)
Effects of Wind Conditions and Surface Roughness on Ice Accretion on Bridge Stay Cables
Li, W., Lin, C., Xiao, H., Yang, K., Pei, Y., & Chen, Z. (2026) · Journal of Cold Regions Engineering · doi:10.1061/jcrgei.creng-1196
Metadata
- Authors
- Jabarin, S. A., & Lofgren, E. A.
- Affiliations
- University of Toledo (US)
- Corresponding author
- Jabarin, Saleh A.
- ORCID
- Jabarin, Saleh A.
- Venue
- Journal of Applied Polymer Science
- Publisher
- Wiley
- Published
- 1994-07-25
- Volume
- 53
- Issue
- 4
- Pages
- 411-423
- ISSN
- 0021-8995 (ISSN-L)
- 1097-4628
- OpenAlex
- W2071338174
- Semantic Scholar
- c87f49685727efc7ab08e8d264f22431c2f4f77d
- Cited by
- 128
- References
- 19
- Citations by year
- 2026: 4 · 2025: 10 · 2024: 15 · 2023: 8 · 2022: 11 · 2021: 5 · 2020: 8 · 2019: 2 · 2018: 8 · 2017: 6 · 2016: 6 · 2015: 5 · 2014: 7 · 2013: 6 · 2012: 8
- FWCI
- 0.00
- Type
- journal article
- Language
- en
- Open access
- closed
- Locations
- Journal of Applied Polymer Science (publishedVersion)
- Topics
- Physical Sciences › Materials Science › Polymers and Plastics › Polymer crystallization and properties
- Physical Sciences › Materials Science › Polymers and Plastics › Polymer Science and PVC
- Physical Sciences › Materials Science › Polymers and Plastics › Polymer Synthesis and Characterization
- Keywords
- high-density polyethylene, photooxidation, environmental degradation, polymer blends, sun exposure, weathering, molecular weight reduction, crystallinity, embrittlement, ductility loss, vinyl end groups, chain mobility
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.