Abstract
The environmental degradation of high‐density polyethylene (HDPE) has been studied, in addition to that of HDPE blends, containing various concentrations of ethylene carbon monoxide copolymer. Extruded sheets of each material were exposed to natural Arizona sunlight for times up to 6 months. Exposed samples were then analyzed with respect to molecular weight, density, thermal behavior, mechanical properties, and infrared absorption. Additional samples were exposed to laboratory weathering conditions, evaluated in terms of property changes, melted, reformed, and then reevaluated without further weathering exposure. Results indicate that sunlight exposure causes decreased elongation to break, increased embrittlement, decreased molecular weight, and increased crystallinity. Environmental oxidative degradation is elucidated by the measurement of specific infrared bands, sensitive to the formation of carbonyl and vinyl end groups. As environmental degradation causes reductions of molecular weight, polymer chain mobility increases, leading to a higher degree of crystallinity. This increased crystallinity, along with the decreased molecular weight, accounts for the loss of ductility, indicated by a sharp decrease in ultimate elongation. The presence of carbon monoxide copolymer in the blended samples accelerates the process of environmental degradation, however, the degradation mechanisms appear to be similar to those observed for nonblended HDPE. © 1994 John Wiley & Sons, Inc.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“Structural modifications and brittleness, although a usual observation, do not always correspond to mechanical strength and molecular weight changes (Andrady, 1990;Jabarin and Lofgren, 1994;Tidjani, 2000;Carrasco et al., 2001).”
From Microplastics Generation: Onset of Fragmentation of Polyethylene Films in Marine Environment Mesocosms (2017) · cites this paper as Jabarin and Lofgren, 1994
In the citing paper
“Essentially, at this degree of weathering no measurement is possible due to sample breakage (Andrady et al., 1993;Jabarin and Lofgren, 1994;Tidjani, 2000).”
From Microplastics Generation: Onset of Fragmentation of Polyethylene Films in Marine Environment Mesocosms (2017) · cites this paper as Jabarin and Lofgren, 1994
In the citing paper
“Jabarin and Lofgren (1994), using FTIR to measure crystallinity were able to deduce that absorbance bands tended to be wider with higher peaks with exposure time, in a similar manner to Tidjani (2000).”
From Microplastics Generation: Onset of Fragmentation of Polyethylene Films in Marine Environment Mesocosms (2017) · cites this paper as Jabarin and Lofgren, 1994
In the citing paper
“Jabarin and Lofgren (1994) reported that the molecular weight of HDPE decreased from 147,000 in the original sample to 34,100 after 6 months of exposure to artificial UV light.”
From Microplastics Generation: Onset of Fragmentation of Polyethylene Films in Marine Environment Mesocosms (2017) · cites this paper as Jabarin and Lofgren, 1994
Citations
Cites
Experiments in Polymer Science
Collins, E. A., Bareš, J., & Billmeyer, F. W. (1973) · Medical Entomology and Zoology · Cited by 408
Photochemistry of Ketone Polymers. I. Studies of Ethylene-Carbon Monoxide Copolymers
Hartley, G. H., & Guillet, J. E. (1968) · Macromolecules · doi:10.1021/ma60002a012 · Cited by 227
International symposium on macromolecular chemistry
(1978) · Fibre Chemistry · doi:10.1007/bf00546430 · Cited by 189
The effect of processing conditions on the u.v. stability of polyolefins
Mellor, D. C., Moir, A. B., & SCOTT, G. (1973) · European Polymer Journal · doi:10.1016/0014-3057(73)90129-8 · Cited by 118
Blais, P., Carlsson, D. J., & Wiles, D. M. (1972) · Journal of Polymer Science Part A-1 Polymer Chemistry · doi:10.1002/pol.1972.150100412 · Cited by 114
Mechanism of the photo-initiation process in polyethylene
Amin, M. U., Scott, G., & Tillekeratne, L. M. (1975) · European Polymer Journal · doi:10.1016/0014-3057(75)90179-2 · Cited by 108
Okada, T., & Mandelkern, L. (1967) · Journal of Polymer Science Part A-2 Polymer Physics · doi:10.1002/pol.1967.160050201 · Cited by 104
Chakraborty, K. B., & SCOTT, G. (1977) · European Polymer Journal · doi:10.1016/0014-3057(77)90074-x · Cited by 87
Photodegradation and stabilization of commercial polyolefins
Allen, N. S., & McKellar, J. F. (1975) · Chemical Society Reviews · doi:10.1039/cs9750400533 · Cited by 66
Autoxidation of semicrystalline polyethylene
Winslow, F. H., Hellman, M. Y., Matreyek, W., & Stills, S. M. (1966) · Polymer Engineering & Science · doi:10.1002/pen.760060317 · Cited by 65
Research works printed but not linked: 3
- Heaps J. M., 1966, Weathering and Degradation of Plastics
- Omichi H., 1983, Degradation and Stabilization of Polyolefins
- Wunderlich B., 1973, Macromolecular Physics: Volume 1 Crystal Structure, Morphology, Defects
Cited by
Understanding plastic degradation and microplastic formation in the environment: A review
Zhang, K., Hamidian, A. H., Tubić, A., Zhang, Y., Fang, J. K. H., Wu, C., & Lam, P. K. S. (2021) · Environmental Pollution · doi:10.1016/j.envpol.2021.116554 · Cited by 1,539
Brandon, J., Goldstein, M., & Ohman, M. D. (2016) · Marine Pollution Bulletin · doi:10.1016/j.marpolbul.2016.06.048 · Cited by 626
“Although our crystallinity results were inconclusive, we observed an increase in brittleness, and brittleness has been associated with an increase in crystallinity (Jabarin and Lofgren, 1994).”
Stark, N. M., & Matuana, L. M. (2004) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2003.11.002 · Cited by 392
“Like carbonyl group formation, vinyl group formation is an indication of polymer chain scission [ 9 ] of either HDPE or WF, which can be a result of carbonyl degradation via Norrish II. Fig. 6 shows the increase in”
InfluentialKalogerakis, N., Karkanorachaki, K., Kalogerakis, G. C., Triantafyllidi, E. I., Gotsis, A. D., Partsinevelos, P., & Fava, F. (2017) · Frontiers in Marine Science · doi:10.3389/fmars.2017.00084 · Cited by 361
“Recently, studies have focused on the potential for effective biodegradation of PE (Restrepo-Flórez et al., 2014; Kumar Sen and Raut, 2015).”
BackgroundMethodWood plastic composites weathering: Visual appearance and chemical changes
Fabiyi, J. S., McDonald, A. G., Wolcott, M. P., & Griffiths, P. R. (2008) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2008.05.024 · Cited by 254
Changes during the weathering of polyolefins
Grause, G., Chien, M.-F., & Inoue, C. (2020) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2020.109364 · Cited by 229
Temperature and light intensity effects on photodegradation of high-density polyethylene
Fairbrother, A., Hsueh, H.-C., Kim, J. H., Jacobs, D., Perry, L., Goodwin, D., White, C., Watson, S., & Sung, L.-P. (2019) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2019.05.002 · Cited by 221
Effect of processing method on surface and weathering characteristics of wood–flour/HDPE composites
Stark, N. M., Matuana, L. M., & Clemons, C. M. (2004) · Journal of Applied Polymer Science · doi:10.1002/app.20529 · Cited by 203
The efficacy of photostabilizers on the color change of wood filled plastic composites
Muasher, M., & Sain, M. (2006) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2005.06.024 · Cited by 177
Stark, N. M., & Matuana, L. M. (2004) · Journal of Applied Polymer Science · doi:10.1002/app.20996 · Cited by 154
Vieira, Y., Lima, E. C., Foletto, E. L., & Dotto, G. L. (2021) · Science of The Total Environment · doi:10.1016/j.scitotenv.2020.141981 · Cited by 162
Ultraviolet weathering of photostabilized wood‐flour‐filled high‐density polyethylene composites
Stark, N. M., & Matuana, L. M. (2003) · Journal of Applied Polymer Science · doi:10.1002/app.12886 · Cited by 160
Investigating the role of metal oxidation state on the degradation behaviour of LDPE
Roy, P. K., Surekha, P., Raman, R., & Rajagopal, C. (2009) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2009.04.025 · Cited by 152
Hsu, Y., Weir, M. P., Truss, R. W., Garvey, C. J., Nicholson, T. M., & Halley, P. J. (2012) · Polymer · doi:10.1016/j.polymer.2012.03.044 · Cited by 137
Studies on the photo-oxidative degradation of LDPE films in the presence of oxidised polyethylene
Roy, P. K., Surekha, P., Rajagopal, C., Chatterjee, S. N., & Choudhary, V. (2007) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2007.01.010 · Cited by 130
“Such an increase in crystallinity of polyethylene films upon irradiation has been reported in literature [13,22].”
BackgroundInvestigating the Degradability of HDPE, LDPE, PE-BIO, and PE-OXO Films under UV-B Radiation
Martínez-Romo, A., González-Mota, R., Soto‐Bernal, J. J., & Rosales-Candelas, I. (2015) · Journal of Spectroscopy · doi:10.1155/2015/586514 · Cited by 129
“The carbonyl and vinyl groups are considered the main photooxidation products of the PE [8]; therefore, carbonyl index (ICO) and vinyl index (IV) are parameters used to evaluate the effect of UV-B radiation in PE films [33, 36].”
MethodBajracharya, R. M., Manalo, A. C., Karunasena, W., & Lau, K.-T. (2014) · Materials & Design (1980-2015) · doi:10.1016/j.matdes.2014.04.081 · Cited by 129
Mechanical, thermal and microstructure evaluation of HDPE after weathering in Rio de Janeiro City
Mendes, L. C., Rufino, E. S., de Paula, F. O. C., & Torres, A. C., Jr. (2003) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(02)00337-3 · Cited by 127
Song, Y. K., Hong, S. H., Eo, S., & Shim, W. J. (2022) · Environmental Pollution · doi:10.1016/j.envpol.2022.119847 · Cited by 121
Natural weathering properties of acetylated bamboo plastic composites
Hung, K., Chen, Y.-L., & Wu, J. (2012) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2012.06.016 · Cited by 103
“The resulting shorter molecules are believed to produce sufficient chain mobility to cause secondary crystallization [36].”
BackgroundDegradation and Fragmentation of Microplastics
Andrady, A. L., & Koongolla, J. B. (2022) · Wiley eBooks · doi:10.1002/9781119768432.ch8 · Cited by 95
Alimi, O. S., Claveau-Mallet, D., Lapointe, M., Biu, T., Liu, L., Hernandez, L. M., Bayen, S., & Tufenkji, N. (2023) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2023.131855 · Cited by 90
Hamzah, M., Khenfouch, M., Rjeb, A., Sayouri, S., Houssaini, D. S., Darhouri, M., & Srinivasu, V. (2018) · Journal of Physics Conference Series · doi:10.1088/1742-6596/984/1/012010 · Cited by 84
Wood Modification Effects on Weathering of HDPE-Based Wood Plastic Composites
Fabiyi, J. S., McDonald, A. G., & McIlroy, D. N. (2009) · Journal of Polymers and the Environment · doi:10.1007/s10924-009-0118-y · Cited by 81
Zafar, R., Park, S. Y., & Kim, C. G. (2020) · Environmental Engineering Research · doi:10.4491/eer.2020.412 · Cited by 80
“indicator of changes taken place from oxidatively deformed polymers [39] which can in turn 11 provide the evident clue for their possible oxidative modifications occurred referring to the 12 Norrish type I and II reactions.”
BackgroundFei, P., Xiong, H., Cai, J., Liu, C., Zia-ud-Din, & Yu, Y. (2016) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2016.03.166 · Cited by 74
Hsueh, H.-C., Kim, J. H., Orski, S. V., Fairbrother, A., Jacobs, D., Perry, L. N., Hunston, D. L., White, C. C., & Sung, L. (2020) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2020.109098 · Cited by 73
“Reports on the degradation of HDPE in a hot natural environment showed a decrease of tensile elongation-at-failure and molar mass accompanying with an increase of crystallinity [4], and embrittlement associated with increasing carbonyl formation [5].”
BackgroundMethodMicrobial Degradation of HDPE Secondary Microplastics: Preliminary Results
Tsiota, P., Karkanorachaki, K., Syranidou, E., Franchini, M., & Kalogerakis, N. E. (2017) · Springer water · doi:10.1007/978-3-319-71279-6_24 · Cited by 73
Engineered Wood Products for Construction
Gong, M. (2021) · IntechOpen eBooks · doi:10.5772/intechopen.92960 · Cited by 65
NIMS polymer database PoLyInfo (I): an overarching view of half a million data points
Ishii, M., Ito, T., Sado, H., & Kuwajima, I. (2024) · Science and Technology of Advanced Materials Methods · doi:10.1080/27660400.2024.2354649 · Cited by 61
“For example, for high-density polyethylene (PID: P010001, Sample ID: 0014069-001-001-001 ~ 004), the effects on crystallinity, density, and thermal and mechanical properties for various sunlight exposure periods [20] are summarized in a table to show the weather resistance.”
Ghanadi, M., & Padhye, L. P. (2024) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2024.133509 · Cited by 59
Natural weathering of rape straw flour (RSF)/HDPE and nano-SiO2/RSF/HDPE composites
Zou, P., Xiong, H., & Tang, S. (2008) · Carbohydrate Polymers · doi:10.1016/j.carbpol.2007.12.002 · Cited by 56
Rasouli, D., Dintcheva, N. T., Faezipour, M., Mantia, F. P. L., Farahani, M. R., & Tajvidi, M. (2016) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2016.08.004 · Cited by 56
Badji, C., Beigbeder, J., Garay, H., Bergeret, A., Bénézet, J., & Desauziers, V. (2018) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2018.01.002 · Cited by 55
Wang, Z., He, H., Zhai, Y., Chen, Y., Xu, Z., & Wang, W. (2024) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2024.142783 · Cited by 54
Yang, T.-C., Noguchi, T., Isshiki, M., & Wu, J. (2014) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2014.03.023 · Cited by 52
“Similar results have been observed for other polyolefins during accelerated weathering [33].”
ResultPetchwattana, N., Sanetuntikul, J., Sriromreun, P., & Narupai, B. (2017) · Journal of Bionic Engineering · doi:10.1016/s1672-6529(16)60443-2 · Cited by 51
Zjačić, J. P., Katančić, Z., Kovačić, M., Kušić, H., Hrnjak‐Murgić, Z., Dionysiou, D. D., Karamanis, P., & Božić, A. L. (2024) · The Science of The Total Environment · doi:10.1016/j.scitotenv.2024.173344 · Cited by 48
Nguyen, V., Hao, J., & Wang, W. (2018) · Polymers · doi:10.3390/polym10080831 · Cited by 46
“In the Norrish II reaction, vinyl groups and terminal carbonyl groups are produced and a chain scission occurs [7,48,49].”
BackgroundTuttle, E. E., Wiman, C., Muñoz, S. E., Law, K. L., & Stubbins, A. (2024) · Environmental Science & Technology · doi:10.1021/acs.est.3c07161 · Cited by 46
Degradation of polypropylene in naturally and artificially weathered plastic matrix composites
Fabiyi, J. S., & McDonald, A. G. (2014) · Maderas Ciencia y tecnología · doi:10.4067/s0718-221x2014005000021 · Cited by 44
Effects of polymeric matrix on accelerated UV weathering properties of wood-plastic composites
Lee, C.-H., Hung, K., Chen, Y.-L., Wu, T.-L., Chien, Y.-C., & Wu, J. (2012) · Holzforschung · doi:10.1515/hf-2011-0198 · Cited by 43
“The resulting shorter molecules may have suffi cient chain mobility to facilitate secondary crystallization, which leads to crack initiation (Figure 2) (Jabarin and Lofgren 1994 ).”
BackgroundMechanical Properties and Weathering Behavior of Polypropylene‐Hemp Shives Composites
Popa, M. I., Pernevan, M. S., Sîrghie, C., Spiridon, I., Chambre, D. R., Copolovici, D. M., & Popa, N. (2013) · Journal of Chemistry · doi:10.1155/2013/343068 · Cited by 41
“The formation of C=O groups in various oxidized products can be explained by the mechanism represented by theNorrish type I and II reactions [33].”
BackgroundDas, S. C., Srivastava, C., & Grammatikos, S. (2025) · Journal of Natural Fibers · doi:10.1080/15440478.2025.2540480 · Cited by 41
“These carbonyl groups may further degrade the polymer materials (Jabarin and Lofgren 1994; Shahzad and Isaac 2015; N. M. Stark and Matuana 2004).”
Assessment of Changes Due to Accelerated Weathering of Low-Density Polyethylene/Feather Composites
Spiridon, I., Păduraru, O. M., Rudowski, M., Kozłowski, M., & Darie-Niță, R. N. (2012) · Industrial & Engineering Chemistry Research · doi:10.1021/ie300738d · Cited by 39
Liu, C., Mei, C., Xu, B., Chen, W., Yong, C., Wang, K., & Wu, Q. (2018) · Royal Society Open Science · doi:10.1098/rsos.180074 · Cited by 38
Sorasan, C., Ortega‐Ojeda, F. E., Rodríguez, A., & Rosal, R. (2022) · Microplastics · doi:10.3390/microplastics1010013 · Cited by 35
“The photodegradation of polyolefins has been shown to start by the photolytic cleavage of chemical bonds in the polymer backbone to form radical pairs (Norrish Type I reaction) or pairs of saturated and unsaturated chain ends (Norrish Type II reaction) [15,16].”
BackgroundThe effect of thermoplastic starch on the properties of HDPE/TPS blends during UV-accelerated aging
Méndez-Hernández, M. L., Tena-Salcido, C.-S., Sandoval‐Arellano, Z., González‐Cantú, M. C., Mondragón, M., & Rodríguez‐González, F. (2011) · Polymer Bulletin · doi:10.1007/s00289-011-0501-4 · Cited by 34
Wood Plastic Composites: Their Properties and Applications
Xu, K., Du, G., & Wang, S. (2022) · IntechOpen eBooks · doi:10.5772/intechopen.98918 · Cited by 32
Oxidation of gamma-irradiated ultrahigh molecular weight polyethylene
COOTE, C. F., Hamilton, J., McGimpsey, W. G., & Thompson, R. W. (2000) · Journal of Applied Polymer Science · doi:10.1002/1097-4628(20000912)77:11<2525::aid-app22>3.0.co;2-i · Cited by 32
Weathering of wood-polypropylene composites containing pigments
Butylina, S., Hyvärinen, M., & Kärki, T. (2012) · European Journal of Wood and Wood Products · doi:10.1007/s00107-012-0606-y · Cited by 26
“Figure 2 shows the lightness of the WPCs as a function of the exposure time.”
BackgroundInfluentialInvestigating the effect of the aging process on LDPE composites with UV protective additives
Ovalı, S., & Sancak, E. (2020) · Journal of Thermoplastic Composite Materials · doi:10.1177/0892705720941908 · Cited by 25
“Two photodegradation mechanisms, called Norrish I and Norrish II, increased the crystallinity by decreasing the density in amorphous regions in the polymer with the formation of chain breakage and cross-linking and so higher crystallinity values were measured.(74) As a result of the 240-h accelerated aging process, th…”
BackgroundWang, Z., Zhai, Y., Liu, G., Liu, X. H., Liu, X., Zhou, Y., Huang, C., Wang, W., & Xu, M. (2023) · The Science of The Total Environment · doi:10.1016/j.scitotenv.2023.165399 · Cited by 25
Wu, T.-L., Chien, Y.-C., Chen, T.-Y., & Wu, J. (2012) · Holzforschung · doi:10.1515/hf-2012-0087 · Cited by 25
“Jabarin and Lofgren (1994) and Beg and Pickering (2008) observed similar trends for surface cracks on weathered WPCs and neat plastics, which were ascribed to elevated polymer crystallinity.”
BackgroundUV Aging Behavior of Functionalized Mullite Nanofiber-Reinforced Polypropylene
Varghese, A. M., Vengatesan, M. R., Luckachan, G. E., & Mittal, V. (2020) · ACS Omega · doi:10.1021/acsomega.0c02437 · Cited by 24
Kazemi‐Najafi, S., & Englund, K. R. (2013) · Journal of Applied Polymer Science · doi:10.1002/app.39021 · Cited by 24
Rajakumar, K., Sarasvathy, V., Thamaraichelvan, A., Chitra, R., & Vijayakumar, C. T. (2010) · Journal of Applied Polymer Science · doi:10.1002/app.32582 · Cited by 23
Atiqullah, M., Winston, M. S., Bercaw, J. E., Hussain, I., Fazal, A. D., Al-Harthi, M. A., Emwas, A. H., Khan, M. J., & Hossaen, A. (2012) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2012.03.042 · Cited by 22
Rolón-Garrido, V. H., Kruse, M., & Wagner, M. H. (2014) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2014.10.022 · Cited by 22
Carbon Nanotube Reinforced High Density Polyethylene Materials for Offshore Sheathing Applications
Okolo, C., Rafique, R., Iqbal, S. S., Saharudin, M. S., & Inam, F. (2020) · Molecules · doi:10.3390/molecules25132960 · Cited by 20
Zhang, W., Jing, X., Bai, Y., Shan, X., Qi, X., Yan, M., & Cui, Z. (2022) · Materials · doi:10.3390/ma15165599 · Cited by 19
Schirp, A., Deetz, R., Kopitzky, R., & Schirp, C. (2024) · Polymer Composites · doi:10.1002/pc.28840 · Cited by 19
Performance of UV weathered HDPE composites containing hull fiber from DDGS and corn grain
Pandey, P., Bajwa, S. G., Bajwa, D. S., & Englund, K. R. (2017) · Industrial Crops and Products · doi:10.1016/j.indcrop.2017.06.050 · Cited by 19
Antiweathering effects of vitamin E on wood flour/polypropylene composites
Peng, Y., Liu, R., Cao, J., & Luo, S. (2014) · Polymer Composites · doi:10.1002/pc.22870 · Cited by 18
Gray, A., Gore, B., Gaesser, M., Sequeira, L. R., Thibodeau, T., Montgomery, A., Purvis, S., Ouimet, K., Dura, T., & Mayer, K. (2025) · Environmental Toxicology and Chemistry · doi:10.1093/etojnl/vgaf116 · Cited by 17
Vujanović, A., Puhar, J., Čolnik, M., Plohl, O., Vidovič, T., Valh, J. V., Škerget, M., & Čuček, L. (2022) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2022.133301 · Cited by 17
Arredondo-Navarro, A., Gallardo-Owens, D., Scott, J., Farias, S., Wang, X., Cochran, W., Hayek, E. E., Minghetti, M., Cerrato, J. M., & González-Estrella, J. (2026) · Microplastics and Nanoplastics · doi:10.1186/s43591-026-00178-5 · Cited by 17
“In contrast, studies focused solely on UV degrada-tion—such as those by Jabarin and Lofgren [74] and Bonyadinejad et al. [75]—found that carbonyl and vinyl bands of HDPE and LDPE increased, in agreement with our findings of MPs subjected to mechanical abrasion alone.”
Yost, S. F., Smith, J. C., Pester, C. W., & Vogt, B. D. (2025) · RSC Applied Polymers · doi:10.1039/d5lp00045a · Cited by 16
Photodegradation and photostabilization of weathered wood flour filled polyethylene composites
Stark, N. M. (2003) · Digital Commons - Michigan Tech (Michigan Technological University) · doi:10.37099/mtu.dc.etds/133 · Cited by 16
Evaluation of UV‐induced embrittlement of PE‐HD by Charpy impact test
Erdmann, M., Niebergall, U., Wachtendorf, V., & Böhning, M. (2020) · Journal of Applied Polymer Science · doi:10.1002/app.49069 · Cited by 15
Pan, K., Chen, C. C., Lin, L., Xu, H., Chen, F., Li, Y., Zhu, X., Ma, J., & Lan, W. (2022) · Bulletin of Environmental Contamination and Toxicology · doi:10.1007/s00128-022-03570-y · Cited by 14
“1 3 weight in the polymers (Jabarin and Lofgren 1994).”
Peng, Y., Guo, X., Cao, J., & Wang, W. C. (2015) · Polymer Composites · doi:10.1002/pc.23683 · Cited by 14
Photooxidative degradation of graphene‐reinforced high‐density polyethylene nanocomposites
Shehzad, F., Ahmad, M. I., & Al-Harthi, M. A. (2018) · Journal of Applied Polymer Science · doi:10.1002/app.47030 · Cited by 14
Hussain, I., Atiqullah, M., Fazal, A., Alam, K., & Hossaen, A. (2010) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2010.09.004 · Cited by 14
Klein, J. M., Ramos, G. R., Grisa, A. M. C., Brandalise, R. N., & Zeni, M. (2013) · Progress in Rubber Plastics and Recycling Technology · doi:10.1177/147776061302900103 · Cited by 14
Wang, L., Qi, Z., Yang, C., Ding, X., Deng, Q., Yang, B., & Hu, N. (2025) · npj Materials Degradation · doi:10.1038/s41529-025-00606-6 · Cited by 13
“Studies have shown that HDPE fi lms exhibit signi fi cant degradation within less than a year of outdoor exposure 8,9 , with temperature variations having a more pronounced impact than solar radiation 10 .”
Huang, Z., Li, Y., & Ren, X. (2014) · Journal of Applied Polymer Science · doi:10.1002/app.40904 · Cited by 13
Long-term outdoor weathering evaluation of wood plastic composites
Wei, L., Cappellazzi, J., Manning, M. J., McDonald, A. G., Foster, S. K., & Morrell, J. J. (2021) · European Journal of Wood and Wood Products · doi:10.1007/s00107-021-01762-7 · Cited by 13
Long-term performance of natural-fiber composites
Mishra, S. K., & Sain, M. M. (2008) · Elsevier eBooks · doi:10.1533/9781845694593.3.460 · Cited by 13
Guan, S., Zhang, X., Ma, Y., & Niu, Z. (2023) · Environmental Science Processes & Impacts · doi:10.1039/d2em00432a · Cited by 12
Zhang, S., Lin, T., Zhang, C., Yang, W., Zhou, X., Cable, R. N., Choi, J., Michaelson, E., Thakre, P., Serrat, C., et al. (2024) · ChemistrySelect · doi:10.1002/slct.202404334 · Cited by 12
Wypych, G. (2013) · Elsevier eBooks · doi:10.1016/b978-1-895198-62-1.50017-2 · Cited by 14
Xue, P., Jia, M., Wang, K., Ding, Y. H., & Wang, L. (2012) · Journal of Wuhan University of Technology-Mater Sci Ed · doi:10.1007/s11595-012-0516-1 · Cited by 11
“The photodegradation mechanisms of wood and plastic separately are well documented in literatures([8-10]).”
BackgroundSato, T., Takahashi, M., Saito, T., Toyonaga, M., Tanuma, I., Yamada, R., & Hosoda, S. (2023) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2023.110589 · Cited by 10
Belmokhtar, Z., Sanchez‐Diaz, S., Cousin, P., Elkoun, S., & Robert, M. (2024) · Waste · doi:10.3390/waste2030019 · Cited by 9
“This result is in contrast with some studies suggesting that chain scission increases the mobility of polymer chains, facilitating their crystallization and consequently leading to a higher degree of crystallinity [50,51].”
ResultEnhanced stabilisation performance of HDPE via siloxane bonded ZnO with phenolic antioxidants
Ai, J., Zheng, Y., & Zhang, J. (2025) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2025.111276 · Cited by 9
Grossutti, M., D’Amico, J., Quintal, J., MacFarlane, H., Wareham, W. C., Quirk, A., & Dutcher, J. (2023) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.3c02564 · Cited by 9
Grossutti, M., Hiles, M., D’Amico, J., Wareham, W. C., Morling, B., Graham, S., & Dutcher, J. (2022) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2022.109963 · Cited by 9
Critical stress of high‐density polyethylene during stress and photo‐oxidative aging
Li, Y., Liu, W., & Ren, X. (2015) · Polymer Engineering and Science · doi:10.1002/pen.24114 · Cited by 9
The molecular level degradation state of drift plastics in the Sea of Japan coastline
Saito, J., Katte, Y., & Nagato, E. G. (2023) · Marine Pollution Bulletin · doi:10.1016/j.marpolbul.2023.115707 · Cited by 8
Doshi, B. N., Fu, J., Oral, E., & Muratoglu, O. K. (2015) · Journal of Applied Polymer Science · doi:10.1002/app.42735 · Cited by 8
Photochemical Behavior of Synthetic Polymeric Multicomponent Materials Composites and Nanocomposites
Zănoagă, M., & Tanasă, F. (2016) · Advanced structured materials · doi:10.1007/978-3-319-25196-7_5 · Cited by 8
Fabrication life prediction model for HDPE/Cr2O3 composites toward roof passive cooling
Jiang, T., Zhang, J., Wei, H., & Keda, Z. (2022) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2023.130495 · Cited by 8
On the use of low-density polyethylene as disposable drip tape for field irrigation
Zhu, D., Wu, S., & Guo, B. (2018) · Plastics Rubber and Composites Macromolecular Engineering · doi:10.1080/14658011.2018.1443874 · Cited by 8
“in ductility (embrittlement) of PE and a consequent loss in the elongation [5,6,15].”
BackgroundEffect of Changing Environments on Microstructure of HDPE Polymer
Bal, S., Mahesh, D., Sen, T. K., & Ray, J. K. (2007) · Journal of Minerals and Materials Characterization and Engineering · doi:10.4236/jmmce.2007.61001 · Cited by 8
Surface characterization of weathered wood-plastic composites produced from modified wood flour
Fabiyi, J. S., McDonald, A. G., & Stark, N. M. (2007) · Cited by 7
Bodur, M. S., Bakkal, M., & Sönmez, H. E. (2017) · Polymer Engineering and Science · doi:10.1002/pen.24670 · Cited by 7
Photo-oxidation and weathering of LDPE studied by surface and bulk analysis
Ramanujam, M. (2013) · DepositOnce · doi:10.14279/depositonce-3500 · Cited by 7
Resistência ao intemperismo natural e ataque fúngico de compósitos polímero-madeira
Catto, A. L. (2015) · Americanae (AECID Library) · Cited by 9
Metadata
- Authors
- Jabarin, S. A., & Lofgren, E. A.
- Affiliations
- University of Toledo (US)
- Corresponding author
- Jabarin, Saleh A.
- ORCID
- Jabarin, Saleh A.
- Venue
- Journal of Applied Polymer Science
- Publisher
- Wiley
- Published
- 1994-07-25
- Volume
- 53
- Issue
- 4
- Pages
- 411-423
- ISSN
- 0021-8995 (ISSN-L)
- 1097-4628
- OpenAlex
- W2071338174
- Semantic Scholar
- c87f49685727efc7ab08e8d264f22431c2f4f77d
- Cited by
- 128
- References
- 19
- Citations by year
- 2026: 4 · 2025: 10 · 2024: 15 · 2023: 8 · 2022: 11 · 2021: 5 · 2020: 8 · 2019: 2 · 2018: 8 · 2017: 6 · 2016: 6 · 2015: 5 · 2014: 7 · 2013: 6 · 2012: 8
- FWCI
- 0.00
- Type
- journal article
- Language
- en
- Open access
- closed
- Locations
- Journal of Applied Polymer Science (publishedVersion)
- Topics
- Physical Sciences › Materials Science › Polymers and Plastics › Polymer crystallization and properties
- Physical Sciences › Materials Science › Polymers and Plastics › Polymer Science and PVC
- Physical Sciences › Materials Science › Polymers and Plastics › Polymer Synthesis and Characterization
- Keywords
- high-density polyethylene, photooxidation, environmental degradation, polymer blends, sun exposure, weathering, molecular weight reduction, crystallinity, embrittlement, ductility loss, vinyl end groups, chain mobility
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.