High CO2 Storage Capacity in Alkali‐Promoted Hydrotalcite‐Based Material: In Situ Detection of Reversible Formation of Magnesium Carbonate
The DOI matches its Crossref record; 43 of the 43 references it cites were found in a registry or an index.
Abstract
Alkali‐promoted hydrotalcite‐based materials showed very high CO 2 storage capacity, exceeding 15 mmol g−1 when the carbonation reaction was carried out at relatively high temperature (300–500 °C) and high partial pressure of steam and CO 2. In situ XRD experiments have allowed correlation of high CO 2 capacity to the transformation of magnesium oxide centres into magnesium carbonate in alkali‐promoted hydrotalcite‐based material. Moreover, it has been clearly shown that crystalline magnesium carbonate may be reversibly formed at temperatures above 300 °C in the presence of sufficient partial pressure of steam in the gas phase, conditions that are prevalent in pre‐combustion CO 2 capture. The role of steam appears to be of utmost importance for the formation of the bulk carbonate phase and for its reversibility. It is proposed that a high partial pressure of steam keeps the magnesium oxide periclase phase sufficiently hydroxylated to allow magnesium carbonate formation if a relatively high partial pressure CO 2 is present in the gas phase.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“Due to its crystal structure, the interlayer space, presenting a large specific surface area comparable to that of C-S-H gel phase [61], was the natural site to fix free CO 2 molecules [47,48].”
From The role of hydrotalcite-like phase and monosulfate in slag cement paste during atmospheric and accelerated carbonation (2022) · cites this paper as [47]
In the citing paper
“On the one hand, it had been verified that part of water molecules that were originally absorbed in the interlayer space was replaced by CO 2 during carbonation, which changed the interlayer distance of hydrotalcite-like phase (d-spacing value d ( 003) ) [47][48][49], which might also modify its decomposition peak shown in the DTG curve.”
From The role of hydrotalcite-like phase and monosulfate in slag cement paste during atmospheric and accelerated carbonation (2022) · cites this paper as [47]
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Hydrotalcite-type anionic clays: Preparation, properties and applications.
Cavani, F., Trifirò, F., & Vaccari, A. (1991) · Catalysis Today · doi:10.1016/0920-5861(91)80068-k · Cited by 5,980
Layered double hydroxides : present and future
Rives, V. (2001) · CERN Document Server (European Organization for Nuclear Research) · Cited by 1,502
Theoretical Study of the Dehydration Process of Boehmite to γ-Alumina
Krokidis, X., Raybaud, P., Gobichon, A.-E., Rebours, B., Euzen, P., & Toulhoat, H. (2001) · The Journal of Physical Chemistry B · doi:10.1021/jp0038310 · Cited by 577
Debecker, D. P., Gaigneaux, E. M., & Busca, G. (2009) · Chemistry – A European Journal · doi:10.1002/chem.200900060 · Cited by 517
Sorption‐enhanced reaction process for hydrogen production
Hufton, J. R., Mayorga, S., & Sircar, S. (1999) · AIChE Journal · doi:10.1002/aic.690450205 · Cited by 483
Millange, F., Walton, R. I., & O'Hare, D. M. (2000) · Journal of Materials Chemistry · doi:10.1039/b002827o · Cited by 423
Characterisation of layered double hydroxides and their decomposition products
Rives, V. (2002) · Materials Chemistry and Physics · doi:10.1016/s0254-0584(02)00024-x · Cited by 405
Yang, W., Kim, Y., Liu, P. K. T., Sahimi, M., & Tsotsis, T. T. (2002) · Chemical Engineering Science · doi:10.1016/s0009-2509(02)00185-9 · Cited by 401
Equilibria and kinetics of CO2 adsorption on hydrotalcite adsorbent
Ding, Y., & Alpay, E. (2000) · Chemical Engineering Science · doi:10.1016/s0009-2509(99)00596-5 · Cited by 362
Rey, F., Fornés, V., & Rojo, J. M. (1992) · J. Chem. Soc., Faraday Trans. · doi:10.1039/ft9928802233 · Cited by 304
Bellotto, M. P., Rebours, B., Clause, O., Lynch, J. R., Bazin, D. C., & Elkaïm, E. (1996) · The Journal of Physical Chemistry · doi:10.1021/jp960040i · Cited by 285
Rocha, J., del Arco, M., Rives, V., & Ulibarri, M. A. (1999) · Journal of Materials Chemistry · doi:10.1039/a903231b · Cited by 230
Hydrotalcite-like compounds as adsorbents for carbon dioxide
Yong, Z., & Rodrigues, A. E. (2002) · Energy Conversion and Management · doi:10.1016/s0196-8904(01)00125-x · Cited by 222
Roelofs, J. C. A. A., van Bokhoven, J. A., van Dillen, A. J., Geus, J. W., & de Jong, K. P. (2002) · Chemistry - A European Journal · doi:10.1002/1521-3765(20021216)8:24<5571::aid-chem5571>3.0.co;2-r · Cited by 210
Hydrotalcite as CO2 Sorbent for Sorption-Enhanced Steam Reforming of Methane
Reijers, H. T. J., Valster-Schiermeier, S. E. A., Cobden, P. D., & van den Brink, R. W. (2006) · Industrial & Engineering Chemistry Research · doi:10.1021/ie050563p · Cited by 204
Self-citationStructural Effects on the High Temperature Adsorption of CO2 on a Synthetic Hydrotalcite
Hutson, N. D., Speakman, S. A., & Payzant, E. A. (2004) · Chemistry of Materials · doi:10.1021/cm040060u · Cited by 204
Kanezaki, E. (1998) · Solid State Ionics · doi:10.1016/s0167-2738(97)00494-3 · Cited by 181
Hibino, T., & Tsunashima, A. (1998) · Chemistry of Materials · doi:10.1021/cm980478q · Cited by 179
Pérez‐Ramírez, J., Abelló, S., & van der Pers, N. M. (2007) · Chemistry - A European Journal · doi:10.1002/chem.200600767 · Cited by 170
Walspurger, S., Boels, L., Cobden, P. D., Elzinga, G. D., Haije, W. G., & van den Brink, R. W. (2008) · ChemSusChem · doi:10.1002/cssc.200800085 · Cited by 161
Self-citationvan Selow, E. R., Cobden, P. D., Verbraeken, P. A., Hufton, J. R., & van den Brink, R. W. (2009) · Industrial & Engineering Chemistry Research · doi:10.1021/ie801713a · Cited by 155
Self-citationStabilized magnesia: A novel catalyst (support) material
Schaper, H., Berg-Slot, J. J., & Stork, W. H. J. (1989) · Applied Catalysis · doi:10.1016/s0166-9834(00)82356-8 · Cited by 152
Decoration of Nickel and Magnesium Oxide Crystallites with Spinel-Type Phases
Rebours, B., de Lacaillerie, J.-B. D., & Clause, O. (1994) · Journal of the American Chemical Society · doi:10.1021/ja00084a011 · Cited by 141
Béarat, H., McKelvy, M. J., Chizmeshya, A. V. G., Sharma, R., & Carpenter, R. W. (2002) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2002.tb00166.x · Cited by 133
Decomposition Processes and Characterization of the Surface Basicity of Cl-and CO32-Hydrotalcites
Tichit, D., Bennani, M. N., Figueras, F., & Ruiz, J. R. (1998) · Langmuir · doi:10.1021/la970543v · Cited by 121
Reynolds, S. P., Ebner, A. D., & Ritter, J. A. (2006) · Industrial & Engineering Chemistry Research · doi:10.1021/ie051232f · Cited by 113
Kinetics of Thermal Dehydroxylation and Carbonation of Magnesium Hydroxide
Butt, D. P., Lackner, K. S., Wendt, C. H., Conzone, S. D., Kung, H., Lu, Y., & Bremser, J. K. (1996) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1996.tb08010.x · Cited by 109
Ebner, A. D., Reynolds, S. P., & Ritter, J. A. (2006) · Industrial & Engineering Chemistry Research · doi:10.1021/ie060389k · Cited by 101
Novel Regenerable Magnesium Hydroxide Sorbents for CO2 Capture at Warm Gas Temperatures
Siriwardane, R. V., & Stevens, R. W. (2008) · Industrial & Engineering Chemistry Research · doi:10.1021/ie8011598 · Cited by 98
Ebner, A. D., Reynolds, S. P., & Ritter, J. A. (2007) · Industrial & Engineering Chemistry Research · doi:10.1021/ie061042k · Cited by 82
Effects of Steam Addition on the Properties of High Temperature Ceramic CO2 Acceptors
Ochoa‐Fernández, E., Zhao, T., Rønning, M., & Chen, D. (2009) · Journal of Environmental Engineering · doi:10.1061/(asce)ee.1943-7870.0000006 · Cited by 82
van Bokhoven, J. A., Roelofs, J. C. A. A., de Jong, K. P., & Koningsberger, D. C. (2001) · Chemistry - A European Journal · doi:10.1002/1521-3765(20010316)7:6<1258::aid-chem1258>3.0.co;2-i · Cited by 82
Gazzano, M., Kagunya, W., Matteuzzi, D., & Vaccari, A. (1997) · The Journal of Physical Chemistry B · doi:10.1021/jp963761q · Cited by 80
Lee, K. B., Beaver, M. G., Caram, H. S., & Sircar, S. (2007) · Industrial & Engineering Chemistry Research · doi:10.1021/ie0701064 · Cited by 78
Rives, V. (1999) · Inorganic Chemistry · doi:10.1021/ic980739y · Cited by 71
Corma, A., Miguel, P. J., & ́s, A. V. O. (1994) · Applied Catalysis A General · doi:10.1016/0926-860x(94)80156-8 · Cited by 67
Thermal stability of aluminium hydroxycarbonates with monovalent cations
Hernandez, M. J., Ulibarri, M. A., Cornejo, J., Peña, M. J., & Serna, C. J. (1985) · Thermochimica Acta · doi:10.1016/0040-6031(85)85269-2 · Cited by 59
Advanced De-SOx catalyst: Mixed solid solution spinels with cerium oxide
Yoo, J. S., Bhattacharyya, A. A., Radlowski, C. A., & Karch, J. A. (1992) · Applied Catalysis B: Environmental · doi:10.1016/0926-3373(92)80022-r · Cited by 54
In situ studies during thermal activation of dawsonite-type compounds to oxide catalysts
Yalfani, M. S., Santiago, M., & Pérez‐Ramírez, J. (2007) · Journal of Materials Chemistry · doi:10.1039/b615264c · Cited by 34
Walspurger, S., Cobden, P. D., Haije, W. G., Westerwaal, R. J., Elzinga, G. D., & Safonova, О. V. (2010) · European Journal of Inorganic Chemistry · doi:10.1002/ejic.201000263 · Cited by 30
Self-citationThermal behavior of Mg–Al–CO3 layered double hydroxide characterized by emanation thermal analysis
Stanimirovа, T., Hibino, T., & Balek, V. (2006) · Journal of Thermal Analysis and Calorimetry · doi:10.1007/s10973-005-7283-6 · Cited by 30
Application of synchrotron radiation to in situ characterization of catalysts
Shido, T., & Prins, R. (1998) · Current Opinion in Solid State and Materials Science · doi:10.1016/s1359-0286(98)80041-7 · Cited by 28
Synthesis and thermal behavior of the dawsonite-type solid solution K1−x(NH4)xAl(OH)2CO3
Zhang, X., Wen, Z., Gu, Z., Xu, X., & Lin, Z. (2005) · Thermochimica Acta · doi:10.1016/j.tca.2005.02.006 · Cited by 13
Cited by
Advances in CO2 capture technology: A patent review
Li, B., Duan, Y., Luebke, D., & Morreale, B. (2013) · Applied Energy · doi:10.1016/j.apenergy.2012.09.009 · Cited by 657
Bernal, S. A., San Nicolas, R., Myers, R. J., Mejía de Gutiérrez, R., Puertas, F., van Deventer, J. S. J., & Provis, J. L. (2014) · Cement and Concrete Research · doi:10.1016/j.cemconres.2013.12.003 · Cited by 493
Ali, M., Jha, N. K., Pal, N., Keshavarz, A., Hoteit, H., & Sarmadivaleh, M. (2022) · Earth-Science Reviews · doi:10.1016/j.earscirev.2021.103895 · Cited by 490
An in-situ IR study on the adsorption of CO2 and H2O on hydrotalcites
Coenen, K., Gallucci, F., Mezari, B., Hensen, E., & van Sint Annaland, M. (2018) · Journal of CO2 Utilization · doi:10.1016/j.jcou.2018.01.008 · Cited by 320
Progress in hydrotalcite like compounds and metal-based oxides for CO2 capture: a review
Bhatta, L. K. G., Subramanyam, S., Chengala, M. D., Olivera, S., & Venkatesh, K. (2015) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2014.12.059 · Cited by 235
Metadata
- Authors
- Walspurger, S., Cobden, P. D., Safonova, O. V., Wu, Y., & Anthony, E. J.
- Venue
- Chemistry – A European Journal
- Publisher
- Wiley
- Published
- 2010-09-17
- Volume
- 16
- Issue
- 42
- Pages
- 12694-12700
- ISSN
- 0947-6539 (ISSN-L)
- 1521-3765
- OpenAlex
- W1974761178
- Cited by
- 58
- References
- 43
- FWCI
- 7.30
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.