A Microstructural and Kinetic Investigation of the KCl-Induced Corrosion of an FeCrAl Alloy at 600 °C
Open accessThe DOI matches its Crossref record; 46 of the 46 references it cites were found in a registry or an index.
Abstract
The corrosion behaviour of a FeCrAl alloy was investigated at 600 °C in O2 + H2O with solid KCl applied. A kinetics and microstructural investigation showed that KCl accelerates corrosion and that potassium chromate formation depletes the protective scale in Cr, thus triggering the formation of a fast-growing iron-rich scale. Iron oxide was found to grow both inward and outward, on either side of the initial oxide. A chromia layer is formed with time underneath the iron oxide. It was found that although the alloy does not form a continuous pure alumina scale at the investigated temperature, aluminium is, however, always enriched at the oxide/alloy interface.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Figures














Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
(2026) · Materials science forum · doi:10.4028/www.scientific.net/msf · Cited by 2,250
Combustion properties of biomass
Jenkins, B. M., Baxter, L. L., Miles, T. R., & Miles, T. R. (1998) · Fuel Processing Technology · doi:10.1016/s0378-3820(97)00059-3 · Cited by 1,938
(2006) · Electrochemistry and Corrosion Science · doi:10.1007/1-4020-7860-9_10 · Cited by 1,814
FactSage thermochemical software and databases — recent developments
Bale, C. W., Bélisle, E., Chartrand, P., Decterov, S. A., Eriksson, G., Hack, K., Jung, I.-H., Kang, Y.-B., Melançon, J., Pelton, A. D., et al. (2009) · Calphad · doi:10.1016/j.calphad.2008.09.009 · Cited by 1,666
BIRKS, N., MEIER, G. H., & PETTIT, F. S. (1989) · Superalloys Supercomposites Superceramics · doi:10.1016/b978-0-12-690845-9.50020-8 · Cited by 1,513
The implications of chlorine-associated corrosion on the operation of biomass-fired boilers
Nielsen, H. P., Frandsen, F. J., Dam-Johansen, K., & Baxter, L. L. (2000) · Progress in Energy and Combustion Science · doi:10.1016/s0360-1285(00)00003-4 · Cited by 785
The behavior of inorganic material in biomass-fired power boilers: field and laboratory experiences
Baxter, L. L., Miles, T. R., Miles, T. R., Jenkins, B. M., Milne, T., Dayton, D., Bryers, R. W., & Oden, L. L. (1998) · Fuel Processing Technology · doi:10.1016/s0378-3820(97)00060-x · Cited by 669
Grabke, H. J., Reese, E., & Spiegel, M. (1995) · Corrosion Science · doi:10.1016/0010-938x(95)00011-8 · Cited by 537
High-Temperature Corrosion and Materials Applications
Lai, G. Y. (2007) · ASM International eBooks · doi:10.31399/asm.tb.htcma.9781627083041 · Cited by 407
Asteman, H., Svensson, J.-E., Norell, M., & Johansson, L.-G. (2000) · Oxidation of Metals · doi:10.1023/a:1004642310974 · Cited by 325
Self-citationHigh temperature corrosion of coatings and boiler steels below chlorine-containing salt deposits
Uusitalo, M. A., Vuoristo, P. M. J., & Mäntylä, T. A. (2004) · Corrosion Science · doi:10.1016/j.corsci.2003.09.026 · Cited by 260
Deposition and high temperature corrosion in a 10 MW straw fired boiler
Michelsen, H. P., Frandsen, F., Dam-Johansen, K., & Larsen, O. H. (1998) · Fuel Processing Technology · doi:10.1016/s0378-3820(97)00062-3 · Cited by 258
Corrosion behaviour of various model alloys with NaCl–KCl coating
Li, Y. S., Spiegel, M., & Shimada, S. (2005) · Materials Chemistry and Physics · doi:10.1016/j.matchemphys.2005.03.015 · Cited by 181
Kassman, H., Liske, J., Steenari, B., & Åmand, L.-E. (2011) · Fuel Processing Technology · doi:10.1016/j.fuproc.2011.06.025 · Cited by 169
Properties of Danish biofuels and the requirements for power production
Sander, B. (1997) · Biomass and Bioenergy · doi:10.1016/s0961-9534(96)00072-4 · Cited by 167
Biomass-fired power generation
Bain, R. L., Overend, R. P., & Craig, K. R. (1998) · Fuel Processing Technology · doi:10.1016/s0378-3820(97)00058-1 · Cited by 158
Are NaCl and KCl equally corrosive on superheater materials of steam boilers?
Enestam, S. H., Bankiewicz, D., Tuiremo, J., Mäkelä, K., & Hupa, M. M. (2012) · Fuel · doi:10.1016/j.fuel.2012.07.020 · Cited by 152
Halvarsson, M., Tang, J. E., Asteman, H., Svensson, J.-E., & Johansson, L.-G. (2006) · Corrosion Science · doi:10.1016/j.corsci.2005.08.012 · Cited by 146
Self-citationCorrosion of superheater materials in a waste-to-energy plant
Viklund, P., Hjörnhede, A., Henderson, P., Stålenheim, A., & Pettersson, R. F. A. (2011) · Fuel Processing Technology · doi:10.1016/j.fuproc.2011.06.017 · Cited by 140
Zahs, A., Spiegel, M., & Grabke, H. (1999) · Materials and Corrosion · doi:10.1002/(sici)1521-4176(199910)50:10<561::aid-maco561>3.0.co;2-l · Cited by 131
Temperature dependence of oxide scale formation on high-Cr ferritic steels in Ar–H2–H2O
Young, D. J., Zurek, J., Singheiser, L., & Quadakkers, W. J. (2011) · Corrosion Science · doi:10.1016/j.corsci.2011.02.031 · Cited by 124
Alkali Induced High Temperature Corrosion of Stainless Steel: The Influence of NaCl, KCl and CaCl2
Karlsson, S., Pettersson, J., Johansson, L. G., & Svensson, J. E. (2012) · Oxidation of Metals · doi:10.1007/s11085-012-9293-7 · Cited by 118
Self-citationPettersson, J., Folkeson, N., Johansson, L.-G., & Svensson, J.-E. (2011) · Oxidation of Metals · doi:10.1007/s11085-011-9240-z · Cited by 117
Self-citationGötlind, H., Liu, F., Svensson, J.-E., Halvarsson, M., & Johansson, L.-G. (2007) · Oxidation of Metals · doi:10.1007/s11085-007-9055-0 · Cited by 116
Self-citationPettersson, C., Pettersson, J., Asteman, H., Svensson, J.-E., & Johansson, L.-G. (2006) · Corrosion Science · doi:10.1016/j.corsci.2005.05.018 · Cited by 112
Self-citationOxidation of FeCrAl alloys at 500–900°C in dry O2
Josefsson, H., Liu, F., Svensson, J. ‐., Halvarsson, M., & Johansson, L. ‐. (2005) · Materials and Corrosion · doi:10.1002/maco.200503882 · Cited by 110
Self-citationConcentration profiles in the underlying alloy during the oxidation of iron-chromium alloys
Whittle, D. P., Wood, G. C., Evans, D. J., & Scully, D. B. (1967) · Acta Metallurgica · doi:10.1016/0001-6160(67)90066-1 · Cited by 96
High temperature interaction of Al/Si-modified Fe–Cr alloys with KCl
Li, Y. S., Niu, Y., & Spiegel, M. (2006) · Corrosion Science · doi:10.1016/j.corsci.2006.10.019 · Cited by 92
Engkvist, J., Canovic, S., Hellström, K., Järdnäs, A., Svensson, J. E., Johansson, L. G., Olsson, M., & Halvarsson, M. (2009) · Oxidation of Metals · doi:10.1007/s11085-009-9177-7 · Cited by 91
Self-citationJonsson, T., Folkeson, N., Svensson, J., Johansson, L.-G., & Halvarsson, M. (2011) · Corrosion Science · doi:10.1016/j.corsci.2011.03.007 · Cited by 88
Self-citationHigh temperature corrosion of superheater steels by KCl and K2CO3 under dry and wet conditions
Lehmusto, J., Yrjas, P., Skrifvars, B.-J., & Hupa, M. M. (2012) · Fuel Processing Technology · doi:10.1016/j.fuproc.2012.05.020 · Cited by 79
Jonsson, T., Froitzheim, J., Pettersson, J., Svensson, J.-E., Johansson, L.-G., & Halvarsson, M. (2009) · Oxidation of Metals · doi:10.1007/s11085-009-9156-z · Cited by 76
Self-citationSimultaneous Internal Oxidation and Nitridation of Ni–Cr–Al Alloys
Han, S., & Young, D. J. (2001) · Oxidation of Metals · doi:10.1023/a:1010304026026 · Cited by 68
In-situ corrosion investigation at Masnedø CHP plant - a straw-fired power plant
Montgomery, M., & Karlsson, A. (1999) · Materials and Corrosion · doi:10.1002/(sici)1521-4176(199910)50:10<579::aid-maco579>3.0.co;2-m · Cited by 67
Initial Stages of the HCl-Induced High-Temperature Corrosion of Alloy 310
Folkeson, N., Johansson, L.-G., & Svensson, J.-E. (2007) · Journal of The Electrochemical Society · doi:10.1149/1.2754174 · Cited by 66
Self-citationIsraelsson, N., Engkvist, J., Hellström, K., Halvarsson, M., Svensson, J.-E., & Johansson, L.-G. (2015) · Oxidation of Metals · doi:10.1007/s11085-014-9507-2 · Cited by 53
Self-citationMicrostructural Investigation of Protective and Non-Protective Oxides on 11% Chromium Steel
Liu, F., Tang, J. E., Jonsson, T., Canovic, S., Segerdahl, K., Svensson, J., & Halvarsson, M. (2006) · Oxidation of Metals · doi:10.1007/s11085-006-9035-9 · Cited by 52
Self-citationKCl-Induced Corrosion of the FeCrAl Alloy Kanthal ® AF at 600 °C and the Effect of H2O
Israelsson, N., Hellström, K., Svensson, J.-E., & Johansson, L.-G. (2015) · Oxidation of Metals · doi:10.1007/s11085-014-9506-3 · Cited by 46
Self-citationHigh Temperature Interaction of Pure Cr with KCl
Li, Y. S., Sánchez-Pastén, M., & Spiegel, M. (2004) · Materials science forum · doi:10.4028/www.scientific.net/msf.461-464.1047 · Cited by 45
Pettersson, C., Johansson, L.-G., & Svensson, J.-E. (2008) · Oxidation of Metals · doi:10.1007/s11085-008-9118-x · Cited by 40
Self-citationViklund, P., & Pettersson, R. F. A. (2010) · Oxidation of Metals · doi:10.1007/s11085-010-9227-1 · Cited by 36
Nicholls, J. R., Bennett, M. J., & Newton, R. (2003) · Materials at High Temperatures · doi:10.1179/mht.2003.050 · Cited by 27
Phase Relations of Some Potassium Compounds to very high Pressures
Pistorius, C. W. F. T. (1962) · Zeitschrift für Physikalische Chemie · doi:10.1524/zpch.1962.35.1_3.109 · Cited by 17
Deposition and Corrosion in Straw- and Coal-Straw Co-Fired Utility Boilers
Frandsen, F., Nielsen, H. P., Jensen, P. A., Hansen, L. A., Livbjerg, H., Dam‐Johansen, K., Hansen, P. F. B., Andersen, K. H., Sørensen, H. S., Larsen, O. H., et al. (2005) · Kluwer Academic Publishers eBooks · doi:10.1007/0-306-46920-0_20 · Cited by 15
Internal Oxidation–Nitridation of Ferritic Fe(Al) Alloys in Air
Pint, B. A., Dwyer, M., & Deacon, R. M. (2008) · Oxidation of Metals · doi:10.1007/s11085-008-9094-1 · Cited by 13
Crevice corrosion of Cr2O3and Al2O3forming alloys in mixed nitrogen-oxygen environments
Bennett, M. J., Nicholls, J. R., Borchardt, G., & Strehl, G. (2002) · Materials at High Temperatures · doi:10.1179/mht.2002.017 · Cited by 7
Research works printed but not linked: 1
- 41. C. Pettersson, J. Pettersson, H. Asteman, J.-E. Svensson and L.-G. Johansson, Corrosion Science 48, 1368 (2005). · DOI · Paper page
Cited by
Sadeghi, E., Markocsan, N., & Joshi, S. V. (2019) · Journal of Thermal Spray Technology · doi:10.1007/s11666-019-00938-1 · Cited by 164
Zhang, S., Li, H., Jiang, Z., Zhang, B., Li, Z., Wu, J., Feng, H., Zhu, H., & Duan, F. (2019) · Corrosion Science · doi:10.1016/j.corsci.2019.108295 · Cited by 97
Sadeghi, E., Reddy, L., Hussain, T., Markocsan, N., & Joshi, S. V. (2017) · Corrosion Science · doi:10.1016/j.corsci.2017.12.033 · Cited by 95
“[35], [38] that instead of Cl2 (proposed in the chlorine-active corrosion mechanism), Cl could penetrate the oxide scale through the grain boundaries, leading to failure (with time) of the protective oxide layer.”
BackgroundBai, M., Reddy, L., & Hussain, T. (2018) · Corrosion Science · doi:10.1016/j.corsci.2018.02.047 · Cited by 81
Influence of KCl and HCl on high temperature corrosion of HVAF-sprayed NiCrAlY and NiCrMo coatings
Sadeghi, E., Reddy, L., Hussain, T., Huhtakangas, M., Markocsan, N., & Joshi, S. V. (2018) · Materials & Design · doi:10.1016/j.matdes.2018.03.048 · Cited by 74
Metadata
- Authors
- Israelsson, N., Unocic, K. A., Hellström, K., Jonsson, T., Norell, M., Svensson, J.-E., & Johansson, L.-G.
- Affiliations
- Chalmers University of Technology (SE)
- Oak Ridge National Laboratory (US)
- Corresponding author
- Israelsson, N.
- Venue
- Oxidation of Metals
- Published
- 2015-03-18
- Volume
- 84
- Issue
- 1-2
- Pages
- 105-127
- ISSN
- 0030-770X (ISSN-L)
- 1573-4889
- OpenAlex
- W1991279420
- Cited by
- 54
- References
- 45
- Citations by year
- 2026: 4 · 2025: 1 · 2024: 9 · 2023: 8 · 2022: 5 · 2021: 6 · 2020: 3 · 2019: 7 · 2018: 5 · 2017: 3 · 2016: 1 · 2015: 2
- FWCI
- 5.31
- Type
- journal article
- Language
- en
- Open access
- hybrid
- doi.org
- Locations
- Oxidation of Metals (publishedVersion, cc-by)
- OSTI OAI (U.S. Department of Energy Office of Scientific and Technical Information) (submittedVersion, other-oa)
- Chalmers Research (Chalmers University of Technology) (submittedVersion)
- Funders
- U.S. Department of Energy
- Basic Energy Sciences
- Topics
- Physical Sciences › Materials Science › Surfaces, Coatings and Films › High-Temperature Coating Behaviors
- Physical Sciences › Materials Science › Metals and Alloys › Hydrogen embrittlement and corrosion behaviors in metals
- Physical Sciences › Engineering › Mechanical Engineering › Intermetallics and Advanced Alloy Properties
- Keywords
- FeCrAl alloys, high-temperature corrosion, corrosion kinetics, microstructure, potassium chromate, iron oxide scale, alumina scale, oxide scale growth
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.