Alkali Induced High Temperature Corrosion of Stainless Steel: The Influence of NaCl, KCl and CaCl2

Open access

Abstract

The influence of KCl, NaCl and CaCl 2 on the oxidation of 304-type (Fe18Cr10Ni) stainless steel at 600 °C in 5 %O 2 + 40 %H 2 O was investigated. Prior to exposure, a small amount of the preferred salt (cation equivalent: 1.35 μmol/cm 2 ) was deposited on the samples. Exposure time was 1–168 h. The oxidized samples were analyzed by SEM/EDX, XRD, FIB and IC. The presence of KCl and NaCl strongly accelerates high temperature corrosion of 304L. Corrosion attack is initiated by the formation of alkali chromate through the reaction of alkali with the protective oxide. Chromate formation is a sink for chromium in the oxide and leads to a loss of its protective properties. Subsequently a rapidly growing scale forms, consisting of an outer hematite layer with chromate particles on top and an inner spinel oxide layer. In contrast to NaCl and KCl, CaCl 2 is not very corrosive. At temperature, CaCl 2 is rapidly converted to CaO. Small amounts of CaCrO 4 form where CaO is in direct contact with the scale. CaO also reacts with the scale to form Ca 2 Fe 2 O 5 .

Overview

CoChat Summary

TL;DR

KCl and NaCl strongly accelerate high-temperature corrosion of 304L stainless steel at 600 °C in 5% O₂ + 40% H₂O by forming alkali chromates that deplete chromium from the protective oxide, while CaCl₂ is only slightly corrosive because it rapidly converts to CaO. The resulting thick scale consists of outer hematite and inner spinel oxide, with chromate particles on top.

Key findings

  • NaCl and KCl both caused strong mass gain and breakdown of the protective oxide; NaCl initially caused higher mass gain than KCl, but the two mass-gain curves were similar during later stages. CaCl₂ did not significantly increase mass gain compared with salt-free reference exposures.
  • Chromate formation was detected early: after 1 h, about 80% of applied alkali and about 60% of added chlorine were detected for NaCl/KCl. After 24 h, 44% of Na⁺ remained for NaCl versus 19% of K⁺ for KCl; chromate formation was 30% of theoretical yield for NaCl and 20% for KCl. After 168 h, chromate was 33% for NaCl and 11% for KCl.
  • For CaCl₂, after 1 h 52% of applied Ca²⁺ and 12% of chloride remained; chromate formation was 2% of theoretical yield, rising only to 4% at 24 h and 5% at 168 h. CaCl₂ converted to CaO, with small amounts of CaCrO₄ and Ca₂Fe₂O₅.
  • Corrosion products on NaCl/KCl-treated samples included outer hematite (Fe₂O₃), inner spinel-type oxide (Fe, Cr, Ni)₃O₄, and alkali chromate (Na₂CrO₄ or K₂CrO₄). NaCl-treated samples also formed a product containing Na, Fe and O, possibly Na₂Fe₂O₄.

Methods

  • Austenitic stainless steel 304L (Fe18Cr10Ni) samples, 5.56 cm², were polished and sprayed with NaCl, KCl or CaCl₂ to a cation equivalent of 1.35 µmol/cm².
  • Isothermal exposures were performed in a silica tube furnace at 600 °C (±1 °C) in 5% O₂ + 40% H₂O with N₂ carrier gas, flow rate 2.5 cm/s, for 1, 24, 72 or 168 h.
  • Samples were analyzed by gravimetry, SEM/EDX, grazing-incidence XRD, FIB cross sections, and ion chromatography for water-soluble cations and anions.

Limitations

  • The paper states that ion chromatography analyses had a relative standard deviation of about ±5%; unaccounted Ca²⁺ was attributed mainly to Ca₂Fe₂O₅ and substantial scale spallation, and unaccounted chloride mainly to thermal decomposition/evaporation.
  • The paper states that the slightly lower mass gain of CaCl₂-exposed samples compared with salt-free exposures was not considered significant because of substantial scale spallation at former CaCl₂ agglomerations.
  • Evident from the text: no explicit limitations section is provided; the study covers only one alloy (304L), one temperature (600 °C), one gas composition, and exposures up to 168 h. Some proposed phases, such as Na₂Fe₂O₄ and calcium hydroxy-/oxy-chlorides, are described as possible or poorly crystalline rather than directly confirmed by XRD.

Model-written summary. Check it against the paper before relying on it.

Integrity signals

Registry

Crossref · 10.1007/s11085-012-9293-7

Cites

23 of 23 references verified0 citation errors · 0 not checkable

Statistics

Nothing to recompute.

Verification

Claims the paper makes

3 Valid · 5 Not valid · 16 Not checked · 122 Own results and interpretations

95 more claims

Create a free account to see all 146 claims and every source verdict.

See all claims — free account
  • Probably not a substantial claim. 12
  • Borderline: one of the tests for a substantial claim is unclear. 2
  • It may state two separate claims as one. 32
  • The quote only partly states this claim. 1

Create a free account to see these claims.

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

Each contradiction between two passages listed here was confirmed by an independent check.

1 of 1

Citations

Cites

Show all 23 references

Cited by

See all 118

Metadata

Authors
Karlsson, S., Pettersson, J., Johansson, L. G., & Svensson, J. E.
Affiliations
Chalmers University of Technology (SE)
Corresponding author
Karlsson, S.
Venue
Oxidation of Metals
Published
2012-04-27
Volume
78
Issue
1-2
Pages
83-102
ISSN
  • 0030-770X (ISSN-L)
  • 1573-4889
OpenAlex
W2019797599
Cited by
118
References
23
Citations by year
2026: 10 · 2025: 9 · 2024: 12 · 2023: 7 · 2022: 12 · 2021: 8 · 2020: 5 · 2019: 11 · 2018: 4 · 2017: 7 · 2016: 14 · 2015: 7 · 2014: 7 · 2013: 4 · 2012: 1
FWCI
10.22
Type
journal article
Language
en
Open access
Licence
cc-by
Locations
  • Oxidation of Metals (publishedVersion, cc-by)
  • Chalmers Publication Library (Chalmers University of Technology) (submittedVersion)
  • Chalmers Research (Chalmers University of Technology) (submittedVersion)
Funders
Chalmers Tekniska Högskola
Topics
  • Physical Sciences › Materials Science › Surfaces, Coatings and Films › High-Temperature Coating Behaviors
  • Physical Sciences › Materials Science › Metals and Alloys › Hydrogen embrittlement and corrosion behaviors in metals
  • Physical Sciences › Materials Science › Materials Chemistry › Corrosion Behavior and Inhibition
Keywords
high-temperature corrosion, 304L stainless steel, sodium chloride, KCl, calcium chloride, chromium depletion, spinel oxides, calcium chromate, calcium oxide, Ca2Fe2O5, water vapor oxidation

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

A language model drew the claims from the paper on 2026-09-30, under version 3 of the claim definition (model deepseek-v4.1-flash, prompt extract-v3).

A second model labelled each claim on 2026-09-30 (model jev-1.13-20260917, definition revision gold-guideline-v0.2).

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

How to cite

Cite CoChat for the checks on this page, and the paper for its own findings.

This page
CoChat. (2026). Citation check: Alkali Induced High Temperature Corrosion of Stainless Steel: The Influence of NaCl, KCl and CaCl2. https://app.cochat.ai/papers/10.1007/s11085-012-9293-7
The paper
Karlsson, S., Pettersson, J., Johansson, L. G., & Svensson, J. E. (2012). Alkali Induced High Temperature Corrosion of Stainless Steel: The Influence of NaCl, KCl and CaCl2. Oxidation of Metals. https://doi.org/10.1007/s11085-012-9293-7

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.