Effects of UV radiation on natural and synthetic materials
Open accessThe DOI matches its Crossref record; 153 of the 153 references it cites were found in a registry or an index.
Abstract
The deleterious effects of solar ultraviolet (UV) radiation on construction materials, especially wood and plastics, and the consequent impacts on their useful lifetimes, are well documented in scientific literature. Any future increase in solar UV radiation and ambient temperature due to climate change will therefore shorten service lifetimes of materials, which will require higher levels of stabilisation or other interventions to maintain their lifetimes at the present levels. The implementation of the Montreal Protocol and its amendments on substances that deplete the ozone layer, controls the solar UV-B radiation received on Earth. This current quadrennial assessment provides a comprehensive update on the deleterious effects of solar UV radiation on the durability of natural and synthetic materials, as well as recent innovations in better stabilising of materials against solar UV radiation-induced damage. Pertinent emerging technologies for wood and plastics used in construction, composite materials used in construction, textile fibres, comfort fabric, and photovoltaic materials, are addressed in detail. Also addressed are the trends in technology designed to increase sustainability via replacing toxic, unsustainable, legacy additives with ‘greener’ benign substitutes that may indirectly affect the UV stability of the redesigned materials. An emerging class of efficient photostabilisers are the nanoscale particles that include oxide fillers and nanocarbons used in high-performance composites, which provide good UV stability to materials. They also allow the design of UV-shielding fabric materials with impressive UV protection factors. An emerging environmental issue related to the photodegradation of plastics is the generation of ubiquitous micro-scale particles from plastic litter exposed to solar UV radiation. Graphical abstract
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Degradation rates of plastics in the environment
Chamas, A., Moon, H., Zheng, J., Qiu, Y., Tabassum, T., Jang, J. H., Abu-Omar, M., Scott, S. L., & Suh, S. (2020) · ACS Sustainable Chemistry & Engineering · doi:10.1021/acssuschemeng.9b06635 · Cited by 3,463 · cited 2×
“Using a simple model, the study [19] demonstrates the geometry-dependence of the kinetics of photodegradation of HDPE (Fig.”
BackgroundMethodHierarchical-morphology metafabric for scalable passive daytime radiative cooling
Zeng, S., Pian, S., Su, M., Wang, Z., Wu, M., Liu, X., Chen, M., Xiang, Y., Wu, J., Zhang, M., et al. (2021) · Science · doi:10.1126/science.abi5484 · Cited by 1,135
Assessment of microplastics in freshwater systems: A review
Li, C., Busquets, R., & Campos, L. C. (2020) · Science of The Total Environment · doi:10.1016/j.scitotenv.2019.135578 · Cited by 954 · cited 1×
“1 3 terms of mass or area loss rates was carried out [19, 20].”
BackgroundApplication of graphene in energy storage device – A review
Olabi, A. G., Abdelkareem, M. A., Wilberforce, T., & Sayed, E. T. (2021) · Renewable and Sustainable Energy Reviews · doi:10.1016/j.rser.2020.110026 · Cited by 852
A strong, biodegradable and recyclable lignocellulosic bioplastic
Xia, Q., Chen, C., Yao, Y., Li, J., He, S., Zhou, Y., Li, T., Pan, X., Yao, Y., & Hu, L. (2021) · Nature Sustainability · doi:10.1038/s41893-021-00702-w · Cited by 759 · cited 1×
“UV radiation, and improved thermal stability [121].”
Advanced Textiles for Personal Thermal Management and Energy
Peng, Y., & Cui, Y. (2020) · Joule · doi:10.1016/j.joule.2020.02.011 · Cited by 747
Blum, A., Behl, M., Birnbaum, L. S., Diamond, M. L., Phillips, A., Singla, V., Sipes, N. S., Stapleton, H. M., & Venier, M. (2019) · Environmental Science & Technology Letters · doi:10.1021/acs.estlett.9b00582 · Cited by 651 · cited 1×
“Several ‘greener’ alternatives to PBDEs have emerged, including different (non-PBDE) brominated compounds, organophosphates [72, 73], dechlorane compounds, and aluminium hydroxides [74].”
BackgroundMin, K., Cuiffi, J. D., & Mathers, R. T. (2020) · Nature Communications · doi:10.1038/s41467-020-14538-z · Cited by 506 · cited 1×
“Another model on the rate of surface area loss on degradation in environmental degradation is based on polymer characteristics, such as the hydrophobicity, glass transition temperature, and the fractional crystallinity [21].”
BackgroundLignin: A Review on Structure, Properties, and Applications as a Light-Colored UV Absorber
Zhang, Y., & Naebe, M. (2021) · ACS Sustainable Chemistry & Engineering · doi:10.1021/acssuschemeng.0c06998 · Cited by 469 · cited 1×
“It can therefore serve as a promising ‘greener’ substitute for synthetic UV absorbers [112, 113].”
BackgroundDe Falco, F., Cocca, M., Avella, M., & Thompson, R. C. (2020) · Environmental Science & Technology · doi:10.1021/acs.est.9b06892 · Cited by 452
Lignin as a UV Light Blocker—A Review
Sadeghifar, H., & Ragauskas, A. (2020) · Polymers · doi:10.3390/polym12051134 · Cited by 451 · cited 1×
“It can therefore serve as a promising ‘greener’ substitute for synthetic UV absorbers [112, 113].”
BackgroundPlastic wastes to construction products: Status, limitations and future perspective
Awoyera, P. O., & Adesina, A. (2020) · Case Studies in Construction Materials · doi:10.1016/j.cscm.2020.e00330 · Cited by 431 · cited 1×
“The recycled plastic waste is formed into plastic blocks or bricks for building [38], especially in emerging economies [39].”
BackgroundSharkey, M., Harrad, S., Abou-Elwafa Abdallah, M., Drage, D. S., & Berresheim, H. (2020) · Environment International · doi:10.1016/j.envint.2020.106041 · Cited by 392 · cited 1×
“China, the largest producer and consumer of fire retardant chemicals, has regulated the levels of penta- and octa-PBDEs, but only in electronic goods that use them in circuit boards [71].”
BackgroundThe Chemistry and Promising Applications of Graphene and Porous Graphene Materials
Huang, H., Shi, H., Das, P., Qin, J., Li, Y., Wang, X., Su, F., Wen, P., Li, S., Lu, P., et al. (2020) · Advanced Functional Materials · doi:10.1002/adfm.201909035 · Cited by 388
The hidden threat of plastic leachates: A critical review on their impacts on aquatic organisms
Gunaalan, K., Fabbri, E., & Capolupo, M. (2020) · Water Research · doi:10.1016/j.watres.2020.116170 · Cited by 375
Bais, A. F., Lucas, R. M., Bornman, J. F., Williamson, C. E., Sulzberger, B., Austin, A. T., Wilson, S. R., Andrady, A. L., Bernhard, G., McKenzie, R. L., et al. (2018) · Photochemical & Photobiological Sciences · doi:10.1039/c7pp90043k · Cited by 350
Self-citationMicroplastic fibres from synthetic textiles: Environmental degradation and additive chemical content
Sait, S. T. L., Sørensen, L., Kubowicz, S., Vike-Jonas, K., Gonzalez, S. V., Asimakopoulos, A. G., & Booth, A. M. (2021) · Environmental Pollution · doi:10.1016/j.envpol.2020.115745 · Cited by 344
Graphene-based nano composites and their applications. A review
Lawal, A. T. (2019) · Biosensors and Bioelectronics · doi:10.1016/j.bios.2019.111384 · Cited by 344 · cited 1×
“Highvolume use of graphene in composites is currently limited by the high manufacturing costs and uncertainties related to their lifetime, operational stability, and reproducibility [143].”
BackgroundPolybrominated Diphenyl Ethers (PBDEs): New Pollutants-Old Diseases
Siddiqi, M. A., Laessig, R. H., & Reed, K. D. (2003) · Clinical Medicine & Research · doi:10.3121/cmr.1.4.281 · Cited by 339 · cited 1×
“In the USA, penta- and octa-PBDEs have been banned since 2004 [69], while the decabromo-PBDE, which was excluded, was regulated under the Toxic Substances Control Act in 2021 [70].”
BackgroundScalable aesthetic transparent wood for energy efficient buildings
Mi, R., Chen, C., Keplinger, T., Pei, Y., He, S., Liu, D., Li, J., Dai, J., Hitz, E., Yang, B., et al. (2020) · Nature Communications · doi:10.1038/s41467-020-17513-w · Cited by 336 · cited 2×
“In this technology, the lignin fraction of wood is replaced by either a synthetic [115] or a biopolymer [116, 117], to obtain a composite of cellulosic materials and polymer (Fig.”
BackgroundGlobal Historical Stocks and Emissions of PBDEs
Abbasi, G., Li, L., & Breivik, K. (2019) · Environmental Science & Technology · doi:10.1021/acs.est.8b07032 · Cited by 335 · cited 1×
“As with plasticisers, the phase-out of PBDEs does not significantly reduce the levels of these compounds in the environment in the medium term, because of persisting residue from their early use since 2004 [64].”
BackgroundAinali, N. M., Bikiaris, D. N., & Lambropoulou, D. A. (2021) · Journal of Analytical and Applied Pyrolysis · doi:10.1016/j.jaap.2021.105207 · Cited by 326 · cited 1×
“Photodegradation negatively affects appearance, compromises mechanical integrity, and encourages subsequent biodegradation, which all limit their service life [11].”
BackgroundGraphene coupled TiO2 photocatalysts for environmental applications: A review
Padmanabhan, N. T., Thomas, N., Louis, J., Mathew, D. T., Ganguly, P., John, H., & Pillai, S. C. (2021) · Chemosphere · doi:10.1016/j.chemosphere.2020.129506 · Cited by 311
A Review of the Degradation of Photovoltaic Modules for Life Expectancy
Kim, J., Rabelo, M. D. A., Padi, S. P., Yousuf, H., Cho, E., & Yi, J. (2021) · Energies · doi:10.3390/en14144278 · Cited by 307 · cited 1×
“It is critical to select encapsulants that are durable under continuous outdoor exposure; discolouration of encapsulants accounts for about 10% of the module failure [153].”
BackgroundAdditives for Plastics Handbook
(2001) · Elsevier eBooks · doi:10.1016/b978-1-85617-370-4.x5000-3 · Cited by 306
Distribution of phthalate esters in air, water, sediments, and fish in the Asan Lake of Korea
Lee, Y.-M., Lee, J.-E., Choe, W., Kim, T., Lee, J.-Y., Kho, Y., Choi, K., & Zoh, K.-D. (2019) · Environment International · doi:10.1016/j.envint.2019.02.059 · Cited by 294 · cited 1×
“Phthalates, identified as a common pollutant in the environment [49, 50] are also endocrine disruptor (ED) chemicals, that may cause inter-generational adverse impacts on reproductive and neurological health, especially in children [51].”
BackgroundSørensen, L., Groven, A. S., Hovsbakken, I. A., Del Puerto, O., Krause, D. F., Sarno, A., & Booth, A. M. (2021) · Science of The Total Environment · doi:10.1016/j.scitotenv.2020.143170 · Cited by 278
Ardusso, M., Forero-López, A. D., Buzzi, N. S., Spetter, C. V., & Fernández-Severini, M. D. (2021) · Science of The Total Environment · doi:10.1016/j.scitotenv.2020.144365 · Cited by 254
Systematic Study of Microplastic Fiber Release from 12 Different Polyester Textiles during Washing
Cai, Y., Yang, T., Mitrano, D. M., Heuberger, M., Hufenus, R., & Nowack, B. (2020) · Environmental Science & Technology · doi:10.1021/acs.est.9b07395 · Cited by 231
Neale, R. E., Barnes, P. W., Robson, T. M., Neale, P. J., Williamson, C. E., Zepp, R. G., Wilson, S. R., Madronich, S., Andrady, A. L., Heikkilä, A. M., et al. (2021) · Photochemical & Photobiological Sciences · doi:10.1007/s43630-020-00001-x · Cited by 225 · cited 1×
“While the initial research on TPO is promising, developmental work to validate its efficacy and economic feasibility is necessary especially in field studies of operational PV modules [162].”
BackgroundSelf-citationLaundering and textile parameters influence fibers release in household washings
Cesa, F. S., Turra, A., Checon, H. H., Leonardi, B., & Baruque-Ramos, J. (2020) · Environmental Pollution · doi:10.1016/j.envpol.2019.113553 · Cited by 205
Hou, R., Lin, L., Li, H., Liu, S., Xu, X., Xu, Y., Jin, X., Yuan, Y., & Wang, Z. (2021) · Water Research · doi:10.1016/j.watres.2021.117168 · Cited by 199 · cited 1×
“The concentration of PBDE replacements in the aquatic environment is higher than that of legacy PBDE’s and these are often bio-accumulative [66].”
BackgroundRecent advances in TiO2-functionalized textile surfaces
Rashid, M. M., Simončič, B., & Tomšič, B. (2021) · Surfaces and Interfaces · doi:10.1016/j.surfin.2020.100890 · Cited by 194
Santhakumari, M., & Sagar, N. (2019) · Renewable and Sustainable Energy Reviews · doi:10.1016/j.rser.2019.04.024 · Cited by 184 · cited 1×
“These undergo oxidation under solar UV irradiation causing brittleness [184, 185].”
BackgroundYue, X., Zhang, T., Yang, D., Qiu, F., Wei, G., & Zhou, H. (2019) · Nano Energy · doi:10.1016/j.nanoen.2019.06.004 · Cited by 175
High Performance, Fully Bio‐Based, and Optically Transparent Wood Biocomposites
Montanari, C., Ogawa, Y., Olsén, P., & Berglund, L. A. (2021) · Advanced Science · doi:10.1002/advs.202100559 · Cited by 166 · cited 1×
“With good thermal stability up to 315 °C, TWCs can be designed to filter out UV-B radiation and have potential applications in smart building technology [119, 120].”
BackgroundProperties and degradation behaviour of polyolefin encapsulants for photovoltaic modules
Oreški, G., Omazic, A., Eder, G. C., Voronko, Y., Neumaier, L., Mühleisen, W., Hirschl, C., Újvári, G., Ebner, R., & Edler, M. (2020) · Progress in Photovoltaics Research and Applications · doi:10.1002/pip.3323 · Cited by 156 · cited 1×
“TPO has been investigated as an alternative to EVA [160, 161] and has superior thermal stability, adhesive strength and resistance to discolouration.”
BackgroundFundamentals, materials and strategies for personal thermal management by next-generation textiles
Farooq, A. S., & Zhang, P. (2020) · Composites Part A Applied Science and Manufacturing · doi:10.1016/j.compositesa.2020.106249 · Cited by 145
Plastic additives: challenges in ecotox hazard assessment
Barrick, A., Champeau, O., Chatel, A., Manier, N., Northcott, G., & Tremblay, L. A. (2021) · PeerJ · doi:10.7717/peerj.11300 · Cited by 144 · cited 1×
“In selecting additives, including UV stabilisers [44] for plastics or coatings, increasing attention is being paid to minimising their potential ecotoxicity as these additives often leach out to contaminate the environment [45].”
BackgroundFlexible transparent wood prepared from poplar veneer and polyvinyl alcohol
Rao, A. N. S., Nagarajappa, G. B., Nair, S. V., Anish, M. C., & Pandey, K. K. (2019) · Composites Science and Technology · doi:10.1016/j.compscitech.2019.107719 · Cited by 142 · cited 1×
“In this technology, the lignin fraction of wood is replaced by either a synthetic [115] or a biopolymer [116, 117], to obtain a composite of cellulosic materials and polymer (Fig.”
BackgroundSelf-citationPolymer degradation: a short review
Vohlídal, J. (2021) · Chemistry Teacher International · doi:10.1515/cti-2020-0015 · Cited by 140
Stratospheric ozone, UV radiation, and climate interactions
Bernhard, G. H., Bais, A. F., Aucamp, P. J., Klekociuk, A. R., Liley, J. B., & McKenzie, R. L. (2023) · Photochemical & Photobiological Sciences · doi:10.1007/s43630-023-00371-y · Cited by 138
Xu, Q., Zheng, W., Duan, P., Chen, J., Zhang, Y., Fu, F., Diao, H., & Liu, X. (2018) · Carbohydrate Polymers · doi:10.1016/j.carbpol.2018.09.089 · Cited by 135 · cited 1×
“[188, 189], wound healing [190], and solar energy harvesting [191].”
BackgroundInteractive effects of solar UV radiation and climate change on material damage
Andrady, A. L., Pandey, K. K., & Heikkilä, A. M. (2019) · Photochemical & Photobiological Sciences · doi:10.1039/c8pp90065e · Cited by 132
Self-citationKärkkäinen, N., & Sillanpää, M. (2020) · Environmental Science and Pollution Research · doi:10.1007/s11356-020-11988-2 · Cited by 123
Preparation of Lignin Nanoparticles from Wood Waste for Wood Surface Treatment
Zikeli, F., Vinciguerra, V., D’Annibale, A., Capitani, D., Romagnoli, M., & Mugnozza, G. S. (2019) · Nanomaterials · doi:10.3390/nano9020281 · Cited by 113 · cited 1×
“Laboratory exposures of coatings with lignin NPs derived from waste wood on beech wood panels, show good control of UV-induced discolouration [114].”
BackgroundVedrtnam, A., Kumar, S., & Chaturvedi, S. (2019) · Composites Part B Engineering · doi:10.1016/j.compositesb.2019.107282 · Cited by 112 · cited 1×
“These stabilisers also work well in WPCs that also undergo UV-induced discolouration and loss of mechanical integrity [111].”
BackgroundEl-Hiti, G. A.-R., Ahmed, D. S., Yousif, E. A., Al-Khazrajy, O. S. A., Abdallh, M., & Alanazi, S. A. (2021) · Polymers · doi:10.3390/polym14010020 · Cited by 112 · cited 1×
“Potent radical traps, such as tertiary amines of tertiary phenols, are often used to inhibit the free-radical photodegradation reactions [15, 16].”
BackgroundGuan, Q., Han, Z., Yang, H., Ling, Z., & Yu, S. (2020) · National Science Review · doi:10.1093/nsr/nwaa230 · Cited by 111 · cited 1×
“Carbon emissions in the sector are mostly due to the use of Portland cement and neither engineered wood products [35] nor plastic materials typically have comparably high carbon emissions.”
BackgroundTurner, A., & Filella, M. (2021) · Environmental Science Processes & Impacts · doi:10.1039/d1em00213a · Cited by 111
Internally plasticized PVC by four different green plasticizer compounds
Najafi, V., & Abdollahi, H. (2020) · European Polymer Journal · doi:10.1016/j.eurpolymj.2020.109620 · Cited by 111
Engel, S. M., Patisaul, H. B., Brody, C., Hauser, R. B., Zota, A. R., Bennet, D. H., Swanson, M., & Whyatt, R. M. (2021) · American Journal of Public Health · doi:10.2105/ajph.2020.306014 · Cited by 110 · cited 1×
“Phthalates, identified as a common pollutant in the environment [49, 50] are also endocrine disruptor (ED) chemicals, that may cause inter-generational adverse impacts on reproductive and neurological health, especially in children [51].”
BackgroundKhan, M. M. H., Deviatkin, I., Havukainen, J., & Horttanainen, M. (2021) · The International Journal of Life Cycle Assessment · doi:10.1007/s11367-021-01953-7 · Cited by 106 · cited 1×
“A Finnish study [7] agreed with the finding, but found wood-plastic composites (WPC) to have even a lower carbon footprint relative to wood.”
BackgroundLife Cycle Assessment of Forest-Based Products: A Review
Sahoo, K., Bergman, R., Alanya-Rosenbaum, S., Gu, H., & Liang, S. (2019) · Sustainability · doi:10.3390/su11174722 · Cited by 102 · cited 1×
“Wood is a traditional, low-cost, and sustainable building material that has a relatively small carbon footprint relative to concretes, metals, or plastics [6].”
BackgroundČuk, N., Šala, M., & Gorjanc, M. (2021) · Cellulose · doi:10.1007/s10570-021-03715-y · Cited by 101 · cited 1×
“For instance, textile fibres surface-coated with silver NPs for antibacterial performance also provide a high degree of UV-screening because of the opacity of the particles [192].”
BackgroundMicroplastic particle versus fiber generation during photo-transformation in simulated seawater
Naik, R. A., Rowles, L. S., Hossain, A. I., Yen, M., Aldossary, R. M., Apul, O. G., Conkle, J., & Saleh, N. B. (2020) · Science of The Total Environment · doi:10.1016/j.scitotenv.2020.139690 · Cited by 99
Critical review of environmental impacts of microfibers in different environmental matrices
Kwak, J. I., Liu, H., Wang, D., Lee, Y. H., Lee, J., & An, Y. (2021) · Comparative Biochemistry and Physiology Part C Toxicology & Pharmacology · doi:10.1016/j.cbpc.2021.109196 · Cited by 91
Zhang, Q., Song, J., Li, X., Peng, Q., Yuan, H., Li, N., Duan, L., & Ma, J. (2019) · Marine Pollution Bulletin · doi:10.1016/j.marpolbul.2019.01.015 · Cited by 87 · cited 1×
“Phthalates, identified as a common pollutant in the environment [49, 50] are also endocrine disruptor (ED) chemicals, that may cause inter-generational adverse impacts on reproductive and neurological health, especially in children [51].”
BackgroundJirouš-Rajković, V., & Miklečić, J. (2019) · Advances in Materials Science and Engineering · doi:10.1155/2019/8621486 · Cited by 86 · cited 1×
“However, these improvements are obtained at the expense of its UV resistance with the treated wood discolouring readily on exposure to solar UV radiation [97, 98].”
BackgroundPhotostable transparent wood composite functionalized with an UV-absorber
Bisht, P., Pandey, K. K., & Barshilia, H. C. (2021) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2021.109600 · Cited by 85 · cited 2×
“However, even with the chromophore-carrying lignin removed, TWCs still undergo some photo-discolouration and degradation on extended exposure to solar UV radiation [122, 123] that might be due to photodegradation of residual lignin or the polymeric component (epoxy in this case).”
BackgroundSelf-citationEl‐Naggar, M. E., Khattab, T. A., Abdelrahman, M. S., Aldalbahi, A. K., & Hatshan, M. R. (2020) · Cellulose · doi:10.1007/s10570-020-03537-4 · Cited by 85
Effects of synthetic and natural microfibers on Daphnia magna—Are they dependent on microfiber type?
Kim, D., Kim, H., & An, Y.-J. (2021) · Aquatic Toxicology · doi:10.1016/j.aquatox.2021.105968 · Cited by 83
Mejjad, N., Cherif, E. K., Rodero, A., Krawczyk, D. A., Kharraz, J. E., Moumen, A., Laqbaqbi, M., & Fekri, A. (2021) · International Journal of Environmental Research and Public Health · doi:10.3390/ijerph18084382 · Cited by 81
Specific-accumulation and trophic transfer of UV filters and stabilizers in marine food web
Wang, W., Lee, I.-S., & Oh, J. (2022) · The Science of The Total Environment · doi:10.1016/j.scitotenv.2022.154079 · Cited by 79 · cited 1×
“[46] reported the presence of UV absorbers at ~ 100 ng/g level in marine organisms including fish.”
BackgroundAdothu, B., Bhatt, P., Chattopadhyay, S., Zele, S. R., Oderkerk, J., Sagar, H. P., Costa, F. R., & Mallick, S. (2019) · Solar Energy · doi:10.1016/j.solener.2019.11.018 · Cited by 77 · cited 2×
“For instance, the discolouration of TPO on exposure to UV radiation of 365 nm from an LED light source at 900 W m−2 at 90 °C and 10–13% RH was found to be nine times slower relative to EVA, and the polymer may also be easier to process [160].”
BackgroundShammi, M., Behal, A., & Tareq, S. M. (2021) · Environmental Science & Technology · doi:10.1021/acs.est.0c05117 · Cited by 77
All-biobased transparent-wood: A new approach and its environmental-friendly packaging application
Hải, L. V., Muthoka, R. M., Panicker, P. S., Agumba, D. O., Pham, D. H., & Kim, J. (2021) · Carbohydrate Polymers · doi:10.1016/j.carbpol.2021.118012 · Cited by 71 · cited 2×
“In this technology, the lignin fraction of wood is replaced by either a synthetic [115] or a biopolymer [116, 117], to obtain a composite of cellulosic materials and polymer (Fig.”
BackgroundNatural weathering of sixteen wood species: Changes on surface properties
ARPACI, S. S., Tomak, E. D., Ermeydan, M. A., & YILDIRIM, İ. (2020) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2020.109415 · Cited by 70
Lyu, Y., Fairbrother, A., Gong, M., Kim, J. H., Gu, X., Kempe, M., Julien, S., Wan, K., Napoli, S., Hauser, A., et al. (2020) · Solar Energy · doi:10.1016/j.solener.2020.02.020 · Cited by 68
Self-citationPeng, Y., Wang, Y., Zhang, R., Wang, W., & Cao, J. (2021) · Industrial Crops and Products · doi:10.1016/j.indcrop.2021.113606 · Cited by 67
Bajard, L., Melymuk, L. E., & Bláha, L. (2019) · Environmental Sciences Europe · doi:10.1186/s12302-019-0195-z · Cited by 65 · cited 1×
“The potential toxicity of the substitute fire retardants is being investigated [75].”
BackgroundUV protection properties of workwear fabrics coated with TiO2 nanoparticles
Rabiei, H., Farhang Dehghan, S., Montazer, M., Khaloo, S. S., & Koozekonan, A. G. (2022) · Frontiers in Public Health · doi:10.3389/fpubh.2022.929095 · Cited by 64
Shen, H., Zhang, S., Cao, J., Jiang, J., & Wang, W. (2018) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2018.03.036 · Cited by 59 · cited 2×
“Impregnating Scots pine wood with a titania sol in paraffin (at 212 °C) improved its UV resistance [98], with the colour change and lignin degradation reduced by more than 50% with the treatment compared to the control, after 1176 h of accelerated weathering.”
BackgroundCao, Y., Xu, P., Lv, P., Lemstra, P. J., Cai, X., Yang, W., Dong, W., Chen, M., Liu, T. X., Du, M., et al. (2020) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.0c14423 · Cited by 59 · cited 1×
“TiO2 NPs have been coated with SiO2 and then poly(D-lactide) (PDLA) grafted onto the coated surface to obtain a double-shell (TiO2@SiO2-gPDLA) hybrid nanoparticle [135].”
MethodDegradation of wood by UV light: A study by EGA-MS and Py-GC/MS with on line irradiation system
Mattonai, M., Watanabe, A., Shiono, A., & Ribechini, E. (2019) · Journal of Analytical and Applied Pyrolysis · doi:10.1016/j.jaap.2019.02.009 · Cited by 57
Aldalbahi, A. K., El‐Naggar, M. E., Khattab, T. A., & Hossain, M. (2021) · Luminescence · doi:10.1002/bio.4126 · Cited by 57 · cited 1×
“A luminescent TWC was reported from Basswood with poly(methyl methacrylate) (PMMA) [118].”
MethodLuan, M., Liang, H., Yang, F., Yuan, W., Chen, A., Liu, X., Ji, H., Wen, S., & Miao, M. (2019) · International Journal of Hygiene and Environmental Health · doi:10.1016/j.ijheh.2019.01.008 · Cited by 55 · cited 1×
“Exposure to PBDE adversely affects reproductive and neurological health [67, 68].”
BackgroundHassan, A. A., Abbas, A., Rasheed, T., Bilal, M., Iqbal, H. M. N., & Wang, S. (2019) · The Science of The Total Environment · doi:10.1016/j.scitotenv.2019.05.140 · Cited by 54
Gašparík, M., Gaff, M., Kačík, F., & Síkora, A. (2019) · BioResources · doi:10.15376/biores.14.2.2667-2683 · Cited by 54 · cited 1×
“Thermal treatment yields appealingly darker [93, 94] treated wood that is less hygroscopic and has improved dimensional stability [95].”
BackgroundZhang, L., Kong, H., Qiao, M., Ding, X., & Yu, M. (2020) · Applied Surface Science · doi:10.1016/j.apsusc.2020.146430 · Cited by 52 · cited 1×
“Subsequent exposure to UV radiation for up to 216 h, under a 40 W UV lamp (wavelength range 280–315 nm, complying with the Chinese Standard GB/T 14522-93) at 60 °C, the treated aramid fibres retained 93% of their average tensile strength, while that of control fibres was only ca 25% [132].”
MethodUV and thermal stability of soft PVC plasticized with cardanol derivatives
Greco, A., Ferrari, F., & Maffezzoli, A. (2017) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2017.07.009 · Cited by 52 · cited 1×
“1 3 were reported for cardanol, a ‘green’ plasticiser for PVC derived from waste cashew nut shells, which also displayed UV-stabiliser properties that are superior to the dioctyl phthalate (DOT) it replaced [60].”
BackgroundGraphene Oxide: Some New Insights into an Old Material
Raidongia, K., Tan, A. T. L., & Huang, J. (2014) · Elsevier eBooks · doi:10.1016/b978-0-08-098232-8.00014-0 · Cited by 51
Höglund, M., Garemark, J., Nero, M., Willhammar, T., Popov, S., & Berglund, L. A. (2021) · Chemistry of Materials · doi:10.1021/acs.chemmater.1c00806 · Cited by 50 · cited 1×
“With good thermal stability up to 315 °C, TWCs can be designed to filter out UV-B radiation and have potential applications in smart building technology [119, 120].”
BackgroundComparison on the Aging of Woods Exposed to Natural Sunlight and Artificial Xenon Light
Liu, R., Zhu, H., Li, K., & Yang, Z. H. (2019) · Polymers · doi:10.3390/polym11040709 · Cited by 50 · cited 2×
“It is the absorption of solar UV radiation (290–400 nm) by lignin in wood that initiates the degradation and discolouration often accompanied by surface cracking [77, 78, 88].”
BackgroundChen, J., Liu, Z., Wang, K., Huang, J., Li, K., Nie, X., & Jiang, J. (2018) · Journal of Applied Polymer Science · doi:10.1002/app.47142 · Cited by 49 · cited 1×
“The validation of sustainable alternatives for phthalates in PVC is well underway [52] and several classes of candidates have been identified: (a) branched and hyperbranched plastics [53–55]; (b) vegetable-oil-based plasticisers [56, 57]; and (c) other promising compounds such as esters derived from biomass [58, 59].”
BackgroundZhang, J., & Teng, C. (2020) · Materials & Design · doi:10.1016/j.matdes.2020.108774 · Cited by 49
Sustainable Solutions with Geosynthetics and Alternative Construction Materials—A Review
Palmeira, E. M., Araújo, G. L. S., & dos Santos, E. C. G. (2021) · Sustainability · doi:10.3390/su132212756 · Cited by 48 · cited 1×
“Being mostly thermoplastic, plastic waste can be readily melted into low-cost geocomposites for drainage systems and infill material for geosynthetic-encased granular columns [40].”
BackgroundEffectiveness of waste plastic bottles as construction material in Rohingya displacement camps
Haque, M. S., & Islam, S. A. (2021) · Cleaner Engineering and Technology · doi:10.1016/j.clet.2021.100110 · Cited by 48 · cited 1×
“The recycled plastic waste is formed into plastic blocks or bricks for building [38], especially in emerging economies [39].”
BackgroundUV resistant wood coating based on zinc oxide and cerium oxide dispersed linseed oil nano-emulsion
Bansal, R., Nair, S. V., & Pandey, K. K. (2022) · Materials Today Communications · doi:10.1016/j.mtcomm.2022.103177 · Cited by 48 · cited 1×
“Photodamage to wood surfaces is quantified as: (a) changes in surface colour, an important criterion of consumer acceptability of wood [77, 81–83]; and (b) chemical analysis using Fourier transform infrared spectroscopy to assess the extent of oxidative changes [82, 84, 85].”
MethodSelf-citationZhu, T., Sheng, J., Chen, J., Ren, K., Wu, Z., Wu, H., Li, J., & Lin, J. (2020) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2020.124770 · Cited by 47 · cited 2×
“) [31, 107] Dalbergia cohinchinensis [31] as well as the bark of Trembling Aspen (Populus tremuloides), lodgepole pine (Pinus contorta), and western red cedar (Thuja plicata) [108] have all been demonstrated to have UV-stabilising activity either in wood or wood composites.”
BackgroundSharma, B. K., Desai, U. V., Singh, A. K., & Singh, A. (2019) · Journal of Applied Polymer Science · doi:10.1002/app.48268 · Cited by 46 · cited 1×
“Based on an accelerated weathering study of several candidate EVA copolymers, one with 18–33% by weight of vinyl acetate was found to be the most UV stable, making it potentially well suited for PV use [158].”
BackgroundPeng, Y., Wang, Y., Chen, P., Wang, W., & Cao, J. (2020) · Progress in Organic Coatings · doi:10.1016/j.porgcoat.2020.105665 · Cited by 46 · cited 2×
“) [31, 107] Dalbergia cohinchinensis [31] as well as the bark of Trembling Aspen (Populus tremuloides), lodgepole pine (Pinus contorta), and western red cedar (Thuja plicata) [108] have all been demonstrated to have UV-stabilising activity either in wood or wood composites.”
BackgroundUV-resistant GFRP composite using carbon nanotubes
Chennareddy, R., Tuwair, H., Kandil, U. F., ElGawady, M. A., & Taha, M. R. (2019) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2019.05.167 · Cited by 44 · cited 1×
“0 wt% of multi-walled carbon nanotubes in fibre-filled epoxy matrices [139].”
BackgroundEmbodied Energy and Embodied GWP of Windows: A Critical Review
Asdrubali, F., Roncone, M., & Grazieschi, G. (2021) · Energies · doi:10.3390/en14133788 · Cited by 44 · cited 1×
“between metal, poly(vinyl chloride) (PVC), and wood used in constructing window frames found the latter to have the least environmental costs as measured by embodied nonrenewable energy and carbon emissions [9].”
BackgroundWeathering resistance of thermally modified wood finished with coatings of diverse formulations
Herrera, R., Sandak, J., Robles, E., Krystofiak, T., & Labidi, J. (2018) · Progress in Organic Coatings · doi:10.1016/j.porgcoat.2018.02.015 · Cited by 43 · cited 1×
“Ashwood heat-treated at 192–212 °C and clear-coated with polyurethane coating also yielded good resistance to discolouration in laboratory exposure of up to 2000 h under UV-340 fluorescent lamps [99].”
Kučerová, V., Lagaňa, R., & Hýrošová, T. (2019) · Journal of Wood Science · doi:10.1186/s10086-019-1800-x · Cited by 43 · cited 1×
“Thermal treatment yields appealingly darker [93, 94] treated wood that is less hygroscopic and has improved dimensional stability [95].”
BackgroundMiller, D. C., Bokria, J. G., Burns, D. M., Fowler, S. P., Gu, X., Hacke, P. L., Honeker, C. C., Kempe, M., Köhl, M., Phillips, N. H., et al. (2019) · Progress in Photovoltaics Research and Applications · doi:10.1002/pip.3103 · Cited by 43 · cited 1×
“The variability in degradation behaviour of the five EVAs suggests that their copolymer composition, residual monomer, and additives are important determinants of their UV degradation behaviour [163].”
BackgroundChen, J., Nie, X., & Jiang, J. (2020) · ACS Omega · doi:10.1021/acsomega.0c00119 · Cited by 41
Survey of Material Degradation in Globally Fielded PV Modules
Tracy, J. M., Gambogi, W. J., Felder, T. C., Garreau-Iles, L., Hu, H., Trout, T. J., Khatri, R., Xia, J., Heta, Y., & Choudhury, K. R. (2019) · Conference record of the IEEE Photovoltaic Specialists Conference · doi:10.1109/pvsc40753.2019.8981140 · Cited by 41 · cited 1×
“1 3 leakage, causing PV modules to be replaced or repaired to address the safety concern [154].”
BackgroundZhang, N., Xu, M., & Cai, L. (2019) · Scientific Reports · doi:10.1038/s41598-018-37363-3 · Cited by 40 · cited 1×
“Thermal treatment yields appealingly darker [93, 94] treated wood that is less hygroscopic and has improved dimensional stability [95].”
BackgroundA phosphorous/nitrogen-containing flame retardant with UV-curing for polyester/cotton fabrics
Yang, X., Liu, X., Yang, X., Zhang, Q., Zheng, Y., Ren, Y., & Cheng, B. (2022) · Cellulose · doi:10.1007/s10570-021-04346-z · Cited by 40 · cited 1×
“Several ‘greener’ alternatives to PBDEs have emerged, including different (non-PBDE) brominated compounds, organophosphates [72, 73], dechlorane compounds, and aluminium hydroxides [74].”
BackgroundNascimento, R. F., da Silva, A. O., Weber, R. P., & Monteiro, S. N. (2020) · Journal of Materials Research and Technology · doi:10.1016/j.jmrt.2020.07.046 · Cited by 39
Abedin, M. J., Khandaker, M. U., Uddin, M. R., Karim, M. R., Ahamad, M. S. U., Islam, M. A., Arif, A. M., Sulieman, A., & Idris, A. M. (2022) · Environmental Science and Pollution Research · doi:10.1007/s11356-021-17859-8 · Cited by 39
Effects of UV Stabilizers on Polypropylene Outdoors
Brostow, W., Lu, X., Gençel, O., & Osmanson, A. T. (2020) · Materials · doi:10.3390/ma13071626 · Cited by 38 · cited 2×
“Potent radical traps, such as tertiary amines of tertiary phenols, are often used to inhibit the free-radical photodegradation reactions [15, 16].”
BackgroundLi, Y., Yu, E., Yang, X., & Wei, Z. (2019) · Journal of Vinyl and Additive Technology · doi:10.1002/vnl.21713 · Cited by 37
Effect of UV Radiation on Optical Properties and Hardness of Transparent Wood
Wachter, I., Štefko, T., Rantuch, P., Martinka, J., & Pastierová, A. (2021) · Polymers · doi:10.3390/polym13132067 · Cited by 36 · cited 1×
“However, even with the chromophore-carrying lignin removed, TWCs still undergo some photo-discolouration and degradation on extended exposure to solar UV radiation [122, 123] that might be due to photodegradation of residual lignin or the polymeric component (epoxy in this case).”
BackgroundFang, D., Huang, Y., Dirican, M., Tian, Y., Xie, J., Jia, D., Yan, C., Liu, Y., Li, C., Liu, H., et al. (2021) · Carbohydrate Polymers · doi:10.1016/j.carbpol.2021.118175 · Cited by 36
Chemical and appearance changes of wood due to artificial weathering – Dose–response model
Petrillo, M., Sandak, J., Grossi, P., & Sandak, A. (2019) · Journal of Near Infrared Spectroscopy · doi:10.1177/0967033518825364 · Cited by 35 · cited 2×
“It is the absorption of solar UV radiation (290–400 nm) by lignin in wood that initiates the degradation and discolouration often accompanied by surface cracking [77, 78, 88].”
BackgroundHan, C., Sahle‐Demessie, E., Varughese, E. A., & Shi, H. (2019) · Environmental Science Nano · doi:10.1039/c9en00153k · Cited by 35
Grigsby, W. J., & Steward, D. (2017) · Journal of Polymers and the Environment · doi:10.1007/s10924-017-0999-0 · Cited by 34
Nasir, V., Fathi, H., Fallah, A., Kazemirad, S., Sassani, F., & Antov, P. (2021) · Materials · doi:10.3390/ma14216314 · Cited by 34
Koriem, A., Ollick, A. M., & Elhadary, M. (2021) · Alexandria Engineering Journal · doi:10.1016/j.aej.2021.03.024 · Cited by 34 · cited 1×
“For instance, weathering of high-density polyethylene (HDPE) stabilised with UV absorbers, under accelerated weathering using a Xenon lamp (generally following ASTM G155), showed that the non-stabilised HDPE was embrittled, with its tensile strength extensibility reducing to 21%, in 300 h of exposure, while the UV-sta…”
MethodEnd-capped biobased saturated polyesters as effective plasticizers for PVC
Pereira, V. A., Fonseca, A. C., Costa, C. S. M. F., Ramalho, A. L., Coelho, J. F. J., & Serra, A. C. (2020) · Polymer Testing · doi:10.1016/j.polymertesting.2020.106406 · Cited by 33
Owen‐Bellini, M., Moffitt, S. L., Sinha, A., Maes, A. M., Meert, J. J., Karin, T., Takacs, C., Jenket, D. R., Hartley, J. Y., Miller, D. C., et al. (2021) · Scientific Reports · doi:10.1038/s41598-021-81381-7 · Cited by 33 · cited 1×
“Currently ~ 12 GW of installed modules with polyamide backsheets have failed due to cracking, which has a large impact on the installed PV power plants [180].”
BackgroundSun, H., Kong, H., Ding, H., Xu, Q., Zeng, J., Jiang, F., Yu, M., & Zhang, Y. (2020) · Polymers · doi:10.3390/polym12010147 · Cited by 31 · cited 2×
“However, a significant drawback of the material is their inherent poor UV stability, mostly because of their aromatic structural features, limiting their use in outdoor applications [129].”
BackgroundSyafiuddin, A., Fulazzaky, M. A., Salmiati, S., Roestamy, M., Fulazzaky, M., Sumeru, K., & Yusop, Z. (2020) · SN Applied Sciences · doi:10.1007/s42452-020-2534-5 · Cited by 31 · cited 1×
“[188, 189], wound healing [190], and solar energy harvesting [191].”
BackgroundProsheva, M., Aboudzadeh, M. A., Leal, G. P., Gilev, J. B., & Tomovská, R. (2019) · Particle & Particle Systems Characterization · doi:10.1002/ppsc.201800555 · Cited by 30 · cited 2×
“This was adequate to completely suppress photodegradation in accelerated ageing of 400 h under a UV lamp (nominal wavelength 366 nm, P-Lab, 550 mW cm−2, distance 15 cm) at 55 °C [142].”
MethodÖzgenç, Ö., Durmaz, S., Şahin, S., & Boyacı, İ. H. (2020) · Journal of Coatings Technology and Research · doi:10.1007/s11998-019-00293-4 · Cited by 29 · cited 1×
“Also, extracts from the bark of alder and maritime pine species at a concentration of 5% in alkyd-based coatings provided excellent UV protection of Scot pine surfaces [110].”
BackgroundProgress in the chemistry of functional aramids properties
Mishra, N., Madhad, H. V., & Vasava, D. V. (2021) · Journal of Heterocyclic Chemistry · doi:10.1002/jhet.4336 · Cited by 29
Javed, A., Azeem, M., Wiener, J., Thukkaram, M., Šašková, J., & Mansoor, T. (2021) · Fibers and Polymers · doi:10.1007/s12221-021-0051-9 · Cited by 28
Tipton, D. A., & Lewis, J. W. (2008) · Journal of Prosthetic Dentistry · doi:10.1016/s0022-3913(08)60182-1 · Cited by 28 · cited 1×
“In selecting additives, including UV stabilisers [44] for plastics or coatings, increasing attention is being paid to minimising their potential ecotoxicity as these additives often leach out to contaminate the environment [45].”
BackgroundHan, H., Yan, H., Wang, X., Zhang, K., Huang, J., Sun, Y., Liu, J., Verlinden, P. J., Altermatt, P. P., Liang, Z., et al. (2019) · Solar Energy · doi:10.1016/j.solener.2019.10.014 · Cited by 27 · cited 1×
“This is due to oxygen bleaching of photodegradation produced chromophores [156].”
BackgroundNguyen, T., Kim, Y. J., Park, S., Lee, K., Park, J., Cho, J. K., & Shin, S. (2019) · ACS Omega · doi:10.1021/acsomega.9b02448 · Cited by 26 · cited 1×
“The validation of sustainable alternatives for phthalates in PVC is well underway [52] and several classes of candidates have been identified: (a) branched and hyperbranched plastics [53–55]; (b) vegetable-oil-based plasticisers [56, 57]; and (c) other promising compounds such as esters derived from biomass [58, 59].”
BackgroundSmith, S. A., Perry, L. N., Watson, S. S., Moffitt, S. L., Shen, S., Mitterhofer, S., Sung, L., Jacobs, D., & Gu, X. (2021) · Progress in Photovoltaics Research and Applications · doi:10.1002/pip.3494 · Cited by 26 · cited 2×
“Three types of transparent backsheets (outer/core/inner) have been tested including a PVF/ PET/FEVE1 coating backsheet, PVDF/PET/FEVE2, and a FEVE3/PET/EVA [183].”
MethodEffect of water leaching on photodegraded spruce wood monitored by IR spectroscopy
Bejó, L., Tolvaj, L., Kánnár, A., & Preklet, E. (2019) · Journal of Photochemistry and Photobiology A Chemistry · doi:10.1016/j.jphotochem.2019.111948 · Cited by 25 · cited 1×
“In accelerated weathering of wood [86], a higher intensity of UV radiation and increased temperatures are typically employed, as with plastics; in some instances, a water spray is also used to simulate the effect of rain [87].”
BackgroundDegradation Processes and Mechanisms of Backsheets
Fairbrother, A., Phillips, N. H., & Gu, X. (2019) · Elsevier eBooks · doi:10.1016/b978-0-12-811545-9.00007-0 · Cited by 25
Julien, S., Kempe, M., Eafanti, J. J., Morse, J., Wang, Y., Fairbrother, A., Napoli, S., Hauser, A. W., Ji, L., O’Brien, G. S., et al. (2020) · Solar Energy Materials and Solar Cells · doi:10.1016/j.solmat.2020.110524 · Cited by 23
Self-citationAssessing the reliability and degradation of 10–35 years field-aged PV modules
Noman, M., Tu, S., Ahmad, S., Zafar, F. U., Khan, H. A., Rehman, S. U., Waqas, M. M., Khan, A. D., & Rehman, O. U. (2022) · PLoS ONE · doi:10.1371/journal.pone.0261066 · Cited by 23 · cited 1×
“Solar UV radiation-induced degradation of these plastic components is a major factor in PV module failure [151] and many material failures in PV modules observed in the field involve encapsulant degradation, backsheet failure, or de-bonding of elements due to adhesive failure [151–154].”
BackgroundMultiple photostabilization actions of heartwood extract from Acacia confusa
Chang, T.-C., & Chang, S. (2017) · Wood Science and Technology · doi:10.1007/s00226-017-0930-9 · Cited by 22 · cited 1×
“Flavonoids extracted from Acacia confusa heartwood significantly reduced the UV-induced degradation of lignin in wood [101].”
BackgroundThe Montreal Protocol and the fate of environmental plastic debris
Jansen, M. A. K., Barnes, P. W., Bornman, J. F., Rose, K. C., Madronich, S., White, C. C., Zepp, R. G., & Andrady, A. L. (2023) · Photochemical & Photobiological Sciences · doi:10.1007/s43630-023-00372-x · Cited by 20
Self-citationGrigsby, W. J. (2017) · Progress in Organic Coatings · doi:10.1016/j.porgcoat.2017.03.007 · Cited by 20
Carbon footprint of an EUR-sized wooden and a plastic pallet
Deviatkin, I., & Horttanainen, M. (2020) · E3S Web of Conferences · doi:10.1051/e3sconf/202015803001 · Cited by 20 · cited 1×
“34 kg of carbon dioxide equivalent (CO2-e) four times lower than that of a plastic unit [8].”
BackgroundMutic, A. D., Barr, D. B., Hertzberg, V., Dunlop, A., Brennan, P., & McCauley, L. (2021) · International Journal of Environmental Research and Public Health · doi:10.3390/ijerph18073614 · Cited by 19 · cited 1×
“Exposure to PBDE adversely affects reproductive and neurological health [67, 68].”
BackgroundChang, T.-C., & Chang, S. (2019) · Wood Science and Technology · doi:10.1007/s00226-019-01084-1 · Cited by 17 · cited 1×
“, have marked radicalscavenging and singlet-oxygen quenching properties [102].”
BackgroundFungal and bacterial colonies growing on weathered wood surfaces
Buchner, J., Irle, M., Belloncle, C., Michaud, F., & Macchioni, N. (2018) · Wood Material Science and Engineering · doi:10.1080/17480272.2018.1443975 · Cited by 17
Prediction of wood surface discoloration for applications in the field of architecture
Forsthuber, B., & Grüll, G. (2018) · Wood Science and Technology · doi:10.1007/s00226-018-1015-0 · Cited by 17 · cited 1×
“It is the absorption of solar UV radiation (290–400 nm) by lignin in wood that initiates the degradation and discolouration often accompanied by surface cracking [77, 78, 88].”
BackgroundApplication of Functional Hybrids Incorporating Carbon Nanotubes or Graphene
Shearer, C. J., Cherevan, A. S., & Eder, D. (2014) · Elsevier eBooks · doi:10.1016/b978-0-08-098232-8.00016-4 · Cited by 16
Enhancement of Photostabilization of Poly(vinyl chloride) Doped with Sulfadiazine Tin Complexes
Ahmed, D. S., El-Hiti, G. A.-R., Ibraheem, H. A. E.-L., Alotaibi, M. H., Abdallh, M., Ahmed, A. A., Ismael, M., & Yousif, E. A. (2019) · Journal of Vinyl and Additive Technology · doi:10.1002/vnl.21752 · Cited by 16 · cited 1×
“5 wt% in rigid PVC, reduced the dehydrochlorination rate constants to less than half that for control PVC samples in accelerated weathering studies [22].”
BackgroundPan, F., Chen, L., He, L., Jiang, Y., Qi, J., Xiao, H., Chen, Y., Huang, X., Hu, H., Tu, L., et al. (2020) · Molecules · doi:10.3390/molecules25051145 · Cited by 15 · cited 1×
“For instance, a 1 wt% solution of the extractive of Phoebe zhennan wood by polar solvent ethyl acetate completely absorbs solar UV-A and UV-B wavelengths in laboratory studies [109].”
BackgroundDegradation Science and Pathways in PV Systems
Gök, A., Gordon, D. A., Wang, M., French, R. H., & Bruckman, L. S. (2019) · Elsevier eBooks · doi:10.1016/b978-0-12-811545-9.00003-3 · Cited by 14
Self-citationTin-Naphthalene Sulfonic Acid Complexes as Photostabilizers for Poly(vinyl chloride)
Jasem, H., Hadi, A. G., El-Hiti, G. A.-R., Baashen, M., Hashim, H., Ahmed, A. A., Ahmed, D. S., & Yousif, E. A. (2021) · Molecules · doi:10.3390/molecules26123629 · Cited by 12
Sánchez, M. B., Fito, C., & Cajaraville, M. P. (2021) · Elsevier eBooks · doi:10.1016/b978-0-12-820505-1.00004-3 · Cited by 11
Mechanical performance of wood under artificial and natural weathering treatments
de Almeida, T. H., de Almeida, D. H., Chahud, E., Branco, L. A. M. N., Pinheiro, R. V., Christoforo, A. L., & Lahr, F. A. R. (2019) · BioResources · doi:10.15376/biores.14.3.6267-6277 · Cited by 11 · cited 1×
“The correlation depends on the test parameters employed [92].”
Correa‐Puerta, J., Ferrada, P., Häberle, P., Diaz-Almeida, D., Sanz, A., Zubillaga, O., Marzo, A., Portillo, C., & del Campo, V. (2021) · Solar Energy · doi:10.1016/j.solener.2021.10.003 · Cited by 11 · cited 1×
“TPO and EVA underwent similar chemical changes determined by Raman spectroscopy, but EVA showed a slightly lower reduction in light transmittance [164].”
BackgroundChang, T.-C., Yeh, T., & Chang, S. (2019) · Journal of Wood Chemistry and Technology · doi:10.1080/02773813.2019.1578376 · Cited by 10
Safdar, F., Javid, A., & Ashraf, M. (2021) · Materials · doi:10.3390/ma15010038 · Cited by 10
Gedanken, A., Perkas, N., Perelshtein, I., & Lipovsky, A. (2017) · Current Medicinal Chemistry · doi:10.2174/0929867325666171229141635 · Cited by 9 · cited 1×
“[188, 189], wound healing [190], and solar energy harvesting [191].”
BackgroundNzangya, J. M., Ndunda, E. N., Bosire, G. O., Martincigh, B. S., & Nyamori, V. O. (2021) · IntechOpen eBooks · doi:10.5772/intechopen.93858 · Cited by 9
Lv, Y., Fan, D., & Kong, M. (2021) · Solar Energy Materials and Solar Cells · doi:10.1016/j.solmat.2021.111230 · Cited by 9 · cited 1×
“The mounting configuration and module design could be improved to reduce the effect of the UV albedo on PV module backsheets [173, 175, 177].”
BackgroundAhmed, N. A.-M. H., Kishk, D. M., & Nada, A. A. (2021) · Fibers and Polymers · doi:10.1007/s12221-021-0755-x · Cited by 9
Invasion of the biosphere by synthetic polymers: What our current knowledge may mean for our future
Moore, C. J. (2019) · Acta Oceanologica Sinica · doi:10.1007/s13131-019-1424-4 · Cited by 7
Dasaradhan, B., Das, B. R., Goswami, T. H., & Prasad, N. E. (2021) · Journal of the Textile Institute · doi:10.1080/00405000.2021.1952806 · Cited by 6
Kanbayashi, T., Matsunaga, M., & Kobayashi, M. (2021) · Wood Science and Technology · doi:10.1007/s00226-021-01301-w · Cited by 6 · cited 1×
“Extractives of the wood of other species, such as that of Japanese cedar (Cryptomeria japonica) [106], Merbau (Intsia sp.”
Background
Cited by
Energy transfer photocatalysis: exciting modes of reactivity
Dutta, S., Erchinger, J. E., Strieth-Kalthoff, F., Kleinmans, R., & Glorius, F. (2024) · Chemical Society Reviews · doi:10.1039/d3cs00190c · Cited by 516
The effects of exposure to solar radiation on human health
Neale, R. E., Lucas, R. M., Byrne, S. N., Hollestein, L., Rhodes, L. E., Yazar, S., Young, A. R., Berwick, M., Ireland, R. A., & Olsen, C. M. (2023) · Photochemical & Photobiological Sciences · doi:10.1007/s43630-023-00375-8 · Cited by 162
“1 3 on terrestrial [3] and aquatic [4] ecosystems, and materials [5].”
BackgroundStratospheric ozone, UV radiation, and climate interactions
Bernhard, G. H., Bais, A. F., Aucamp, P. J., Klekociuk, A. R., Liley, J. B., & McKenzie, R. L. (2023) · Photochemical & Photobiological Sciences · doi:10.1007/s43630-023-00371-y · Cited by 138
“This assessment sets the stage for subsequent assessments in this series that address the consequences of the interconnected effects of stratospheric ozone depletion, UV radiation, and climate change on human health [1] (including the COVID19 pandemic [2]), terrestrial [3] and aquatic [4] ecosystems, the carbon cycle…”
BackgroundNeale, P. J., Williamson, C. E., Banaszak, A. T., Häder, D.-P., Hylander, S., Ossola, R., Rose, K. C., Wängberg, S.-Å., & Zepp, R. (2023) · Photochemical & Photobiological Sciences · doi:10.1007/s43630-023-00370-z · Cited by 79
“[189], this issue), and it is presently unknown how much of these UV filters could be released into the natural environment.”
BackgroundMadronich, S., Bernhard, G. H., Neale, P. J., Heikkilä, A., Andersen, M. P. S., Andrady, A. L., Aucamp, P. J., Bais, A. F., Banaszak, A. T., Barnes, P. J., et al. (2024) · Photochemical & Photobiological Sciences · doi:10.1007/s43630-024-00577-8 · Cited by 15
“Comprehensive Quadrennial Assessments reflect this evolving knowledge and constitute the scientific basis for any Amendments and adjustments to the Montreal Protocol; i.e., the recent assessments of ozone science [1] and effects on related environmental effects [2] (see also [3–11]).”
Self-citation
Metadata
- Authors
- Andrady, A. L., Heikkilä, A. M., Pandey, K. K., Bruckman, L. S., White, C. C., Zhu, M., & Zhu, L.
- Venue
- Photochemical & Photobiological Sciences
- Published
- 2023-04-11
- Volume
- 22
- Issue
- 5
- Pages
- 1177-1202
- ISSN
- 1474-905X (ISSN-L)
- 1474-9092
- OpenAlex
- W4364353319
- Cited by
- 181
- References
- 153
- FWCI
- 13.48
- Type
- journal article
- Language
- en
- Open access
- hybrid
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.