Magnesium degradation under physiological conditions – Best practice
Open accessAbstract
This review focusses on the application of physiological conditions for the mechanistic understanding of magnesium degradation. Despite the undisputed relevance of simplified laboratory setups for alloy screening purposes, realistic and predictive in vitro setups are needed. Due to the complexity of these systems, the review gives an overview about technical measures, defines some caveats and can be used as a guideline for the establishment of harmonized laboratory approaches.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Electrochemical Methods: Fundamentals and Applications
de Rooij, D. M. R. (2003) · Anti-Corrosion Methods and Materials · doi:10.1108/acmm.2003.12850eae.001 · Cited by 13,009
How useful is SBF in predicting in vivo bone bioactivity?
Kokubo, T., & Takadama, H. (2006) · Biomaterials · doi:10.1016/j.biomaterials.2006.01.017 · Cited by 9,576
Hydrogen Ion Buffers for Biological Research*
Good, N. E., Winget, G. D., Winter, W., Connolly, T. N., Izawa, S., & Singh, R. M. M. (1966) · Biochemistry · doi:10.1021/bi00866a011 · Cited by 2,762
Fundamentals and advances in magnesium alloy corrosion
Esmaily, M., Svensson, J. E., Fajardo, S., Birbilis, N., Frankel, G. S., Virtanen, S., Arrabal, R., Thomas, S., & Johansson, L. G. (2017) · Progress in Materials Science · doi:10.1016/j.pmatsci.2017.04.011 · Cited by 2,073
Degradable biomaterials based on magnesium corrosion
Witte, F., Hort, N., Vogt, C., Cohen, S., Kainer, K. U., Willumeit, R., & Feyerabend, F. (2008) · Current Opinion in Solid State and Materials Science · doi:10.1016/j.cossms.2009.04.001 · Cited by 1,820
Self-citationMicrobiological precipitation of CaCO3
Stocks-Fischer, S., Galinat, J. K., & Bang, S. S. (1999) · Soil Biology and Biochemistry · doi:10.1016/s0038-0717(99)00082-6 · Cited by 1,607
Preparation and assessment of revised simulated body fluids
Oyane, A., Kim, H., Furuya, T., Kokubo, T., Miyazaki, T., & Nakamura, T. (2003) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.10482 · Cited by 1,117
Can bioactivity be tested in vitro with SBF solution?
Bohner, M., & Lemaitre, J. (2009) · Biomaterials · doi:10.1016/j.biomaterials.2009.01.008 · Cited by 923
Kirkland, N. T., Birbilis, N., & Staiger, M. P. (2012) · Acta Biomaterialia · doi:10.1016/j.actbio.2011.11.014 · Cited by 856
Toward a Human Blood Serum Proteome
Adkins, J. N., Varnum, S. M., Auberry, K. J., Moore, R. J., Angell, N. H., Smith, R. D., Springer, D. L., & Pounds, J. G. (2002) · Molecular & Cellular Proteomics · doi:10.1074/mcp.m200066-mcp200 · Cited by 793
Mg and Mg alloys: How comparable are in vitro and in vivo corrosion rates? A review
Sanchez, A. H. M., Luthringer, B. J. C., Feyerabend, F., & Willumeit, R. (2015) · Acta Biomaterialia · doi:10.1016/j.actbio.2014.11.048 · Cited by 503
Self-citationWang, J., Witte, F., Xi, T., Zheng, Y., Yang, K., Yang, Y., Zhao, D., Meng, J., Li, Y., Li, W., et al. (2015) · Acta Biomaterialia · doi:10.1016/j.actbio.2015.04.011 · Cited by 493
A survey of bio-corrosion rates of magnesium alloys
Kirkland, N. T., Lespagnol, J., Birbilis, N., & Staiger, M. P. (2010) · Corrosion Science · doi:10.1016/j.corsci.2009.09.033 · Cited by 482
CO2 mineral sequestration: physically activated dissolution of serpentine and pH swing process
Park, A.-H. A., & Fan, L.-S. (2004) · Chemical Engineering Science · doi:10.1016/j.ces.2004.09.008 · Cited by 475
Biodegradable Mg and Mg alloys: Corrosion and biocompatibility
Virtanen, S. (2011) · Materials Science and Engineering: B · doi:10.1016/j.mseb.2011.05.028 · Cited by 423
Xin, Y., Huo, K., Tao, H., Tang, G., & Chu, P. K. (2008) · Acta Biomaterialia · doi:10.1016/j.actbio.2008.05.014 · Cited by 408
Effect of inorganic salts, amino acids and proteins on the degradation of pure magnesium in vitro
Yamamoto, A., & Hiromoto, S. (2009) · Materials Science and Engineering: C · doi:10.1016/j.msec.2008.12.015 · Cited by 368
Hänzi, A. C., Gerber, I., Schinhammer, M., Löffler, J. F., & Uggowitzer, P. J. (2010) · Acta Biomaterialia · doi:10.1016/j.actbio.2009.10.008 · Cited by 365
Magnesium biomaterials for orthopedic application: A review from a biological perspective
Walker, J., Shadanbaz, S., Woodfield, T. B. F., Staiger, M. P., & Dias, G. J. (2014) · Journal of Biomedical Materials Research Part B: Applied Biomaterials · doi:10.1002/jbm.b.33113 · Cited by 352
Fast escape of hydrogen from gas cavities around corroding magnesium implants
Kuhlmann, J., Bartsch, I., Willbold, E., Schuchardt, S., Holz, O., Hort, N., Höche, D., Heineman, W. R., & Witte, F. (2013) · Acta Biomaterialia · doi:10.1016/j.actbio.2012.10.008 · Cited by 310
Temperature- and pH-Dependent Morphology and FT−IR Analysis of Magnesium Carbonate Hydrates
Zhang, Z., Zheng, Y., Ni, Y., Liu, Z., Chen, J., & Liang, X. (2006) · The Journal of Physical Chemistry B · doi:10.1021/jp061261j · Cited by 285
Ritchie, R. F., Palomaki, G. E., Neveux, L. M., Navolotskaia, O., Ledue, T. B., & Craig, W. Y. (1999) · Journal of Clinical Laboratory Analysis · doi:10.1002/(sici)1098-2825(1999)13:6<273::aid-jcla4>3.0.co;2-x · Cited by 270
Biocorrosion behavior of magnesium alloy in different simulated fluids for biomedical application
Yang, L., & Zhang, E. (2009) · Materials Science and Engineering: C · doi:10.1016/j.msec.2009.01.014 · Cited by 250
In vitro degradation behavior and cytocompatibility of Mg–Zn–Zr alloys
Huan, Z. G., Leeflang, M. A., Zhou, J., Fratila-Apachitei, L. E., & Duszczyk, J. (2010) · Journal of Materials Science: Materials in Medicine · doi:10.1007/s10856-010-4111-8 · Cited by 234
Corrosion of high purity Mg, Mg2Zn0.2Mn, ZE41 and AZ91 in Hank’s solution at 37 °C
Zainal Abidin, N. I., Atrens, A. D., Martin, D., & Atrens, A. (2011) · Corrosion Science · doi:10.1016/j.corsci.2011.06.030 · Cited by 227
Magnesium alloys: Predicting in vivo corrosion with in vitro immersion testing
Walker, J., Shadanbaz, S., Kirkland, N. T., Stace, E., Woodfield, T., Staiger, M. P., & Dias, G. J. (2012) · Journal of Biomedical Materials Research Part B: Applied Biomaterials · doi:10.1002/jbm.b.32680 · Cited by 223
The in vivo and in vitro corrosion of high-purity magnesium and magnesium alloys WZ21 and AZ91
Zainal Abidin, N. I., Rolfe, B., Owen, H., Malisano, J., Martin, D., Hofstetter, J., Uggowitzer, P. J., & Atrens, A. (2013) · Corrosion Science · doi:10.1016/j.corsci.2013.06.019 · Cited by 218
Kirkland, N. T., Birbilis, N., Walker, J., Woodfield, T., Dias, G. J., & Staiger, M. P. (2010) · Journal of Biomedical Materials Research Part B: Applied Biomaterials · doi:10.1002/jbm.b.31687 · Cited by 216
Shi, P., Ng, W. F., Wong, M. H., & Cheng, F. T. (2009) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2008.01.102 · Cited by 215
Xu, L., Zhang, E., Yin, D., Zeng, S., & Yang, K. (2008) · Journal of Materials Science: Materials in Medicine · doi:10.1007/s10856-007-3219-y · Cited by 209
Hiromoto, S., Inoue, M., Taguchi, T., Yamane, M., & Ohtsu, N. (2015) · Acta Biomaterialia · doi:10.1016/j.actbio.2014.09.026 · Cited by 201
Corrosion of magnesium in humid air
Lindström, R., Johansson, L.-G., Thompson, G. E., Skeldon, P., & Svensson, J.-E. (2004) · Corrosion Science · doi:10.1016/j.corsci.2003.09.010 · Cited by 181
Chen, X. B., Nisbet, D. R., Li, R. W., Smith, P. N., Abbott, T. B., Easton, M. A., Zhang, D.-H., & Birbilis, N. (2014) · Acta Biomaterialia · doi:10.1016/j.actbio.2013.11.016 · Cited by 163
In vitro degradation and cytotoxicity of Mg/Ca composites produced by powder metallurgy
Zheng, Y. F., Gu, X. N., Xi, Y. L., & Chai, D. L. (2010) · Acta Biomaterialia · doi:10.1016/j.actbio.2009.10.009 · Cited by 158
Flow-induced corrosion behavior of absorbable magnesium-based stents
Wang, J., Giridharan, V., Shanov, V. N., Xu, Z., Collins, B., White, L., Jang, Y., Sankar, J., Huang, N., & Yun, Y. (2014) · Acta Biomaterialia · doi:10.1016/j.actbio.2014.08.034 · Cited by 157
Johnston, S., Shi, Z., & Atrens, A. (2015) · Corrosion Science · doi:10.1016/j.corsci.2015.09.018 · Cited by 156
Borges, A. S., Divers, T. J., Stokol, T., & Mohammed, O. H. (2007) · Journal of Veterinary Internal Medicine · doi:10.1111/j.1939-1676.2007.tb02995.x · Cited by 146
Magnesium-based implants: a mini-review
Luthringer-Feyerabend, B., Feyerabend, F., & Willumeit‐Römer, R. (2014) · Magnesium Research · doi:10.1684/mrh.2015.0375 · Cited by 143
Self-citationIn vitro degradation of pure Mg in response to glucose
Zeng, R., Li, X., Li, S., Zhang, F., & Han, E. (2015) · Scientific Reports · doi:10.1038/srep13026 · Cited by 140
Influence of Test Solutions on In Vitro Studies of Biomedical Magnesium Alloys
Xin, Y., Hu, T., & Chu, P. K.-H. (2010) · Journal of The Electrochemical Society · doi:10.1149/1.3421651 · Cited by 131
Gu, X., Zheng, Y., & Chen, L. (2009) · Biomedical Materials · doi:10.1088/1748-6041/4/6/065011 · Cited by 119
Jang, Y., Collins, B., Sankar, J., & Yun, Y. (2013) · Acta Biomaterialia · doi:10.1016/j.actbio.2013.03.026 · Cited by 116
Lu, P., Cao, L., Liu, Y., Xu, X., & Wu, X. (2010) · Journal of Biomedical Materials Research Part B Applied Biomaterials · doi:10.1002/jbm.b.31744 · Cited by 110
In vivo evaluation of a magnesium-based degradable intramedullary nailing system in a sheep model
Rössig, C., Angrisani, N., Helmecke, P., Besdo, S., Seitz, J., Welke, B., Fedchenko, N., Kock, H., & Reifenrath, J. (2015) · Acta Biomaterialia · doi:10.1016/j.actbio.2015.07.025 · Cited by 107
Tie, D., Feyerabend, F., Hort, N., Willumeit‐Römer, R., & Höche, D. (2010) · Advanced Engineering Materials · doi:10.1002/adem.201080070 · Cited by 103
Self-citationInfluence of the Interfacial pH on Electrochemical CaCO[sub 3] Precipitation
Tlili, M., Benamor, M., Gabrielli, C., Perrot, H., & Tribollet, B. (2003) · Journal of The Electrochemical Society · doi:10.1149/1.1613294 · Cited by 99
In vitro degradation behavior of M1A magnesium alloy in protein-containing simulated body fluid
Wang, Y., Lim, C. S., Lim, C. V. S., Yong, M. S., Teo, E. K., & Moh, L. N. (2010) · Materials Science and Engineering C · doi:10.1016/j.msec.2010.11.017 · Cited by 94
Jo, J.-H., Kang, B.-G., Shin, K. S., Kim, H., Hahn, B., Park, D.-S., & Koh, Y. (2011) · Journal of Materials Science Materials in Medicine · doi:10.1007/s10856-011-4431-3 · Cited by 93
Yang, C., Yuan, G., Zhang, J., Tang, Z., Zhang, X., & Dai, K. (2010) · Biomedical Materials · doi:10.1088/1748-6041/5/4/045005 · Cited by 92
Total Iron Binding Capacity and Transferrin Concentration in the Assessment of Iron Status
Kasvosve, I., & Delanghe, J. (2002) · Clinical Chemistry and Laboratory Medicine (CCLM) · doi:10.1515/cclm.2002.176 · Cited by 89
Iron-Binding Antioxidant Potential of Plasma Albumin
Loban, A., Kime, R., & Powers, H. J. (1997) · Clinical Science · doi:10.1042/cs0930445 · Cited by 83
A physical corrosion model for bioabsorbable metal stents
Grogan, J. A., Leen, S. B., & McHugh, P. E. (2014) · Acta Biomaterialia · doi:10.1016/j.actbio.2013.12.059 · Cited by 80
Hou, L., Zhen, L., Zhao, H., Pan, Y., Павлинич, С. П., Liu, X., Li, X., Zheng, Y., & Li, L. (2016) · Journal of Material Science and Technology · doi:10.1016/j.jmst.2016.07.004 · Cited by 80
Buffer-regulated biocorrosion of pure magnesium
Kirkland, N. T., Waterman, J., Birbilis, N., Dias, G. J., Woodfield, T. B. F., Hartshorn, R. M., & Staiger, M. P. (2011) · Journal of Materials Science Materials in Medicine · doi:10.1007/s10856-011-4517-y · Cited by 79
Electrochemical behavior of Mg and some Mg alloys in aqueous solutions of different pH
Badawy, W. A., Hilal, N. H., El-Rabiee, M. M., & Nady, H. (2009) · Electrochimica Acta · doi:10.1016/j.electacta.2009.10.083 · Cited by 79
Johnson, I., Perchy, D., & Liu, H. H. (2011) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.33290 · Cited by 79
Influence of proteins and cells on in vitro corrosion of Mg–Nd–Zn–Zr alloy
Zhang, J., Kong, N., Shi, Y., Niu, J., Mao, L., Li, H., Xiong, M., & Yuan, G. (2014) · Corrosion Science · doi:10.1016/j.corsci.2014.04.020 · Cited by 77
Effects of corrosion environment and proteins on magnesium corrosion
Yang, L. J., Hort, N., Willumeit‐Römer, R., & Feyerabend, F. (2012) · Corrosion Engineering Science and Technology The International Journal of Corrosion Processes and Corrosion Control · doi:10.1179/1743278212y.0000000024 · Cited by 72
Self-citationProtective layer formation on magnesium in cell culture medium
Wagener, V., & Virtanen, S. (2016) · Materials Science and Engineering C · doi:10.1016/j.msec.2016.03.003 · Cited by 71
Magnesium degradation as determined by artificial neural networks
Willumeit‐Römer, R., Feyerabend, F., & Huber, N. W. (2013) · Acta Biomaterialia · doi:10.1016/j.actbio.2013.02.042 · Cited by 69
Self-citationDezfuli, S. N., Huan, Z., Mol, J. M. C., Leeflang, M. A., Chang, J., & Zhou, J. (2014) · Progress in Natural Science Materials International · doi:10.1016/j.pnsc.2014.08.009 · Cited by 67
In vivo monitoring the biodegradation of magnesium alloys with an electrochemical H2 sensor
Zhao, D., Wang, T., Kuhlmann, J., Dong, Z., Chen, S., Joshi, M., Salunke, P., Shanov, V. N., Hong, D., Kumta, P. N., et al. (2016) · Acta Biomaterialia · doi:10.1016/j.actbio.2016.03.039 · Cited by 67
Cui, L., Hu, Y., Zeng, R., et al. (2017) · Journal of Material Science and Technology · doi:10.1016/j.jmst.2017.01.005 · Cited by 67
In vivo and in vitro degradation comparison of pure Mg, Mg-10Gd and Mg-2Ag: a short term study
Marco, I., Myrissa, A., Martinelli, E., Feyerabend, F., Willumeit‐Römer, R., Weinberg, A.-M., & der Biest, O. V. (2017) · European Cells and Materials · doi:10.22203/ecm.v033a07 · Cited by 67
Self-citationEffect of bicarbonate on biodegradation behaviour of pure magnesium in a simulated body fluid
Li, Z., Song, G., & Song, S. (2013) · Electrochimica Acta · doi:10.1016/j.electacta.2013.10.131 · Cited by 64
Dynamic degradation of porous magnesium under a simulated environment of human cancellous bone
Saad, A. P. M., Jasmawati, N., Harun, M. N., Kadir, M. R. A., Nur, H., Hermawan, H., & Syahrom, A. (2016) · Corrosion Science · doi:10.1016/j.corsci.2016.08.017 · Cited by 64
Agha, N. A., Willumeit‐Römer, R., Laipple, D., Luthringer-Feyerabend, B., & Feyerabend, F. (2016) · PLoS ONE · doi:10.1371/journal.pone.0157874 · Cited by 63
Self-citationWang, J., Liu, L., Wu, Y., Maitz, M. F., Wang, Z., Koo, Y., Zhao, A., Sankar, J., Kong, D., Huang, N., et al. (2016) · Acta Biomaterialia · doi:10.1016/j.actbio.2016.12.039 · Cited by 61
In Vitro Degradation of Pure Magnesium―The Effects of Glucose and/or Amino Acid
Wang, Y., Cui, L., Zeng, R., Li, S., Zou, Y.-H., & Han, E. (2017) · Materials · doi:10.3390/ma10070725 · Cited by 58
On the Determination of Magnesium Degradation Rates under Physiological Conditions
Nidadavolu, E., Feyerabend, F., Ebel, T., Willumeit‐Römer, R., & Dahms, M. (2016) · Materials · doi:10.3390/ma9080627 · Cited by 57
Self-citationThe in vitro and in vivo evaluation of the biocompatibility of Mg alloys
Walker, J., Shadanbaz, S., Woodfield, T. B. F., Staiger, M. P., & Dias, G. J. (2013) · Biomedical Materials · doi:10.1088/1748-6041/9/1/015006 · Cited by 46
Schinhammer, M., Hofstetter, J., Wegmann, C., Moszner, F., Löffler, J. F., & Uggowitzer, P. J. (2013) · Advanced Engineering Materials · doi:10.1002/adem.201200218 · Cited by 45
Kannan, M. B., Khakbaz, H., & Yamamoto, A. (2017) · Materials Chemistry and Physics · doi:10.1016/j.matchemphys.2017.05.024 · Cited by 25
In vitro analysis of magnesium corrosion in orthopaedic biomaterials
Feyerabend, F. (2014) · Elsevier eBooks · doi:10.1533/9780857098104.2.225 · Cited by 11
Self-citation
Cited by
Biodegradable magnesium-based implants in orthopedics-a general review and perspectives
Wang, J., Xu, J., Hopkins, C., Chow, D. H., & Qin, L. (2020) · Advanced Science · doi:10.1002/advs.201902443 · Cited by 574
Mei, D., Lamaka, S. V., Lu, X., & Zheludkevich, M. L. (2020) · Corrosion Science · doi:10.1016/j.corsci.2020.108722 · Cited by 284
Ben Amara, H., Martinez, D. C., Shah, F. A., Loo, A. J., Emanuelsson, L., Norlindh, B., Willumeit-Römer, R., Plocinski, T., Swieszkowski, W., Palmquist, A., et al. (2023) · Bioactive Materials · doi:10.1016/j.bioactmat.2023.02.014 · Cited by 42
“To maintain semistatic immersion conditions [37], the medium was exchanged every 2–3 days.”
MethodSelf-citationKwesiga, M. P., Gillette, A. A., Razaviamri, F., Plank, M. E., Canull, A. L., Alesch, Z., He, W., Lee, B. P., & Guillory, R. J. (2023) · Bioactive Materials · doi:10.1016/j.bioactmat.2022.10.017 · Cited by 25
Metadata
- Authors
- Gonzalez, J., Hou, R. Q., Nidadavolu, E. P. S., Willumeit-Römer, R., & Feyerabend, F.
- Venue
- Bioactive Materials
- Publisher
- Elsevier BV
- Published
- 2018-06
- Volume
- 3
- Issue
- 2
- Pages
- 174-185
- ISSN
- 2097-1192 (ISSN-L)
- 2452-199X
- OpenAlex
- W2789333639
- Cited by
- 262
- References
- 74
- FWCI
- 7.40
- Type
- journal article
- Language
- en
- Open access
- gold
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.