An overview on rheology, mechanical properties and durability of high-volume slag used as a cement replacement in paste, mortar and concrete
The DOI matches its Crossref record; 92 of the 92 references it cites were found in a registry or an index.
Abstract
Abstract Disposal of slag resulting from pig iron process is one of the main eco-friendly confrontations. This confrontation is still increasing with the increase slag content and diminishing the landfill space latitude. Accordingly, studies have been achieved to reuse granulated ground blast-furnace slag (denoted as slag) by way of high-volume (HVS) as a cement replacement in building materials. This article offerings a review summary of the earlier investigations which concentrated on using HVS (≥45%) as a part of cement in conventional paste, mortar and concrete mixtures. Fresh properties, mechanical properties, durability and other properties of paste, mortar and concrete mixtures containing HVS as a cement replacement have been reviewed. Furthermore, curing conditions as well as different additives used to improve some properties of HVS system such as nano particles, cementitious materials, and other materials have been summarized.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
3 retracted
Nazari, A., & Riahi, S. (2010) · Energy and Buildings · doi:10.1016/j.enbuild.2010.12.006 · Cited by 119
RetractedNazari, A., & Riahi, S. (2010) · Energy and Buildings · doi:10.1016/j.enbuild.2010.12.025 · Cited by 114
RetractedNazari, A., & Riahi, S. (2011) · Science China Technological Sciences · doi:10.1007/s11431-011-4440-y · Cited by 39
RetractedTHE INTERGOVERNMENTAL PANEL ON CLIMATE CHANGE
Shine, K. (1990) · Weather · doi:10.1002/j.1477-8696.1990.tb05660.x · Cited by 5,462
Sustainable development and climate change initiatives
Damtoft, J. S., Lukasik, J., Herfort, D., Sorrentino, D., & Gartner, E. M. (2008) · Cement and Concrete Research · doi:10.1016/j.cemconres.2007.09.008 · Cited by 1,094
High performance cementing materials from industrial slags — a review
Shi, C., & Qian, J. (2000) · Resources, Conservation and Recycling · doi:10.1016/s0921-3449(99)00060-9 · Cited by 648
Alkali-activated cements Opportunities and challenges
Roy, D. M. (1999) · Cement and Concrete Research · doi:10.1016/s0008-8846(98)00093-3 · Cited by 608
Properties of sustainable concrete containing fly ash, slag and recycled concrete aggregate
Berndt, M. L. (2009) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2009.02.011 · Cited by 575
Carbonation of CH and C–S–H in composite cement pastes containing high amounts of BFS
Borges, P. H. R., Costa, J. O., Milestone, N. B., Lynsdale, C. J., & Streatfield, R. E. (2010) · Cement and Concrete Research · doi:10.1016/j.cemconres.2009.10.020 · Cited by 555
Zhang, M.-H., & Islam, J. (2012) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2011.11.013 · Cited by 494
Ramezanianpour, A. A., & Malhotra, V. M. (1995) · Cement and Concrete Composites · doi:10.1016/0958-9465(95)00005-w · Cited by 494
Demirboğa, R., Türkmen, İ., & Karakoç, M. B. (2004) · Cement and Concrete Research · doi:10.1016/j.cemconres.2004.04.017 · Cited by 393
Rashad, A. M. (2013) · Materials & Design (1980-2015) · doi:10.1016/j.matdes.2013.07.074 · Cited by 389
Self-citationRashad, A. M. (2013) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2013.04.011 · Cited by 387
Self-citationStudy of chloride binding and diffusion in GGBS concrete
Luo, R., Cai, Y., Wang, C., & Huang, X. (2003) · Cement and Concrete Research · doi:10.1016/s0008-8846(02)00712-3 · Cited by 373
Reactivity of blast-furnace slag in Portland cement blends hydrated under different conditions
Escalante-Garcia, J. I., Gómez, L., Johal, K. K., Mendoza, G., Mancha, H., & Méndez, J. (2001) · Cement and Concrete Research · doi:10.1016/s0008-8846(01)00587-7 · Cited by 362
Yazıcı, H., Yardımcı, M. Y., Yiğiter, H., Aydın, S., & Türkel, S. (2010) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2010.07.005 · Cited by 342
Hydration and properties of sodium sulfate activated slag
Rashad, A. M., Bai, Y., Basheer, P. A. M., Milestone, N. B., & Collier, N. C. (2013) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2012.12.010 · Cited by 335
Self-citationThe microstructure and mechanical properties of blended cements hydrated at various temperatures
Escalante-Garcı́a, J. I., & Sharp, J. H. (2001) · Cement and Concrete Research · doi:10.1016/s0008-8846(01)00471-9 · Cited by 324
Effect of admixtures on the setting times of high-strength concrete
Brooks, J. J., Johari, M. A. M., & Mazloom, M. (2000) · Cement and Concrete Composites · doi:10.1016/s0958-9465(00)00025-1 · Cited by 322
Yazıcı, H. (2007) · Building and Environment · doi:10.1016/j.buildenv.2006.03.013 · Cited by 312
Rashad, A. M. (2014) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2014.08.092 · Cited by 311
Self-citationElahi, A., Basheer, P. A. M., Nanukuttan, S. V., & Khan, Q. U. Z. (2010) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2009.08.045 · Cited by 302
Çakır, Ö. (2014) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2014.06.032 · Cited by 291
Durability of Portland blast-furnace slag cement concrete
Osborne, G. J. (1999) · Cement and Concrete Composites · doi:10.1016/s0958-9465(98)00032-8 · Cited by 291
A brief on high-volume Class F fly ash as cement replacement – A guide for Civil Engineer
Rashad, A. M. (2015) · International Journal of Sustainable Built Environment · doi:10.1016/j.ijsbe.2015.10.002 · Cited by 291
Self-citationUse of iron and steel industry by-product (GGBS) in cement paste and mortar
Siddique, R., & Bennacer, R. (2012) · Resources Conservation and Recycling · doi:10.1016/j.resconrec.2012.09.002 · Cited by 278
Use of waste glass as sand in mortar: Part II – Alkali–silica reaction and mitigation methods
Du, H., & Tan, K. H. (2012) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2012.08.029 · Cited by 276
Rashad, A. M., Bai, Y., Basheer, M., Collier, N. C., & Milestone, N. B. (2011) · Cement and Concrete Research · doi:10.1016/j.cemconres.2011.10.007 · Cited by 262
Self-citationChloride binding in GGBS concrete
Dhir, R. K., El-Mohr, M. A. K., & Dyer, T. D. (1996) · Cement and Concrete Research · doi:10.1016/s0008-8846(96)00180-9 · Cited by 262
Shi, H.-S., Xu, B.-W., & Zhou, X.-C. (2009) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2008.08.021 · Cited by 247
Feiz, R., Ammenberg, J., Baas, L., Eklund, M., Helgstrand, A., & Marshall, R. (2015) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2014.01.083 · Cited by 245
Gruyaert, E., Van den Heede, P., & De Belie, N. (2013) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2012.08.024 · Cited by 244
Carbonation of Concrete Containing Mineral Admixtures
Sulapha, P., Wong, S. F., Wee, T. H., & Swaddiwudhipong, S. (2003) · Journal of Materials in Civil Engineering · doi:10.1061/(asce)0899-1561(2003)15:2(134 · Cited by 244
Activation of blast furnace slag by a new method
Bellmann, F., & Stark, J. (2009) · Cement and Concrete Research · doi:10.1016/j.cemconres.2009.05.012 · Cited by 225
Rashad, A. M. (2014) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2014.09.080 · Cited by 216
Self-citationAn experimental study on corrosion resistance of concrete with ground granulate blast-furnace slag
Yeau, K. Y., & Kim, E. K. (2005) · Cement and Concrete Research · doi:10.1016/j.cemconres.2004.11.010 · Cited by 212
Utilizing Waste Recycled Glass as Sand/Cement Replacement in Concrete
Taha, B., & Nounu, G. (2009) · Journal of Materials in Civil Engineering · doi:10.1061/(asce)0899-1561(2009)21:12(709 · Cited by 209
Durability Properties and Microstructure of Ground Granulated Blast Furnace Slag Cement Concrete
Divsholi, B. S., Lim, T. Y. D., & Teng, S. (2014) · International Journal of Concrete Structures and Materials · doi:10.1007/s40069-013-0063-y · Cited by 200
Durability of concrete incorporating GGBS activated by water-glass
Al-Otaibi, S. (2008) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2007.07.023 · Cited by 199
Kayali, O., Khan, M. S. H., & Sharfuddin Ahmed, M. (2012) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2012.04.009 · Cited by 189
Güneyisi, E., & Gesoğlu, M. (2008) · Materials and Structures · doi:10.1617/s11527-007-9260-y · Cited by 180
Phase transformations and mechanical strength of OPC/Slag pastes submitted to high temperatures
Mendes, A., Sanjayan, J., & Collins, F. (2007) · Materials and Structures · doi:10.1617/s11527-007-9247-8 · Cited by 171
Li, Q., Li, Z., & Yuan, G. (2012) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2012.04.103 · Cited by 165
Effect of particle size on alkali–silica reaction in recycled glass mortars
Du, H., & Tan, K. H. (2014) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2014.05.092 · Cited by 163
Mounanga, P., Khokhar, M., El-Hachem, R., & Loukili, A. (2010) · Materials and Structures · doi:10.1617/s11527-010-9637-1 · Cited by 162
Development of a high-temperature-resistant mortar by using slag and pumice
Aydın, S. (2008) · Fire Safety Journal · doi:10.1016/j.firesaf.2008.02.001 · Cited by 161
Gruyaert, E., den Heede, P. V., Maes, M., & Belie, N. D. (2011) · Cement and Concrete Research · doi:10.1016/j.cemconres.2011.09.009 · Cited by 161
Durability properties of concrete containing 50% and 65% slag
Bouikni, A., Swamy, R. N., & Bali, A. (2009) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2009.02.040 · Cited by 158
Carbonation Curing of Slag-Cement Concrete for Binding CO2 and Improving Performance
Monkman, S., & Shao, Y. (2009) · Journal of Materials in Civil Engineering · doi:10.1061/(asce)mt.1943-5533.0000018 · Cited by 151
The effects of elevated temperature on cement paste containing GGBFS
Wang, H. Y. (2008) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2007.12.003 · Cited by 141
Investigation on early hydration of ternary Portland cement-blast-furnace slag–metakaolin blends
Boháč, M., Palou, M. T., Novotný, R., Másilko, J., Všianský, D., & Staněk, T. (2014) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2014.04.018 · Cited by 136
Bagheri, A., Zanganeh, H., & Moalemi, M. M. (2012) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2012.01.007 · Cited by 136
Tasong, W. A., Wild, S., & Tilley, R. J. D. (1999) · Cement and Concrete Research · doi:10.1016/s0008-8846(99)00007-1 · Cited by 135
Binici, H., Temiz, H., & Köse, M. M. (2006) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2005.11.005 · Cited by 133
The influence of different cements on chloride-induced corrosion of reinforcing steel
Page, C. L., Short, N. R., & Holden, W. R. (1986) · Cement and Concrete Research · doi:10.1016/0008-8846(86)90071-2 · Cited by 131
Oil palm shell lightweight concrete containing high volume ground granulated blast furnace slag
Shafigh, P., Jumaat, M. Z., Mahmud, H. B., & Alengaram, U. J. (2012) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2012.10.007 · Cited by 128
Transport properties of high volume fly ash or slag concrete exposed to high temperature
Karahan, O. (2017) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2017.07.051 · Cited by 122
Nazari, A., & Riahi, S. (2011) · Materials Science and Engineering: A · doi:10.1016/j.msea.2010.11.070 · Cited by 120
Influence of different additives on the properties of sodium sulfate activated slag
Rashad, A. M. (2015) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2015.01.022 · Cited by 115
Self-citationAkçaözoğlu, S., & Atiş, C. D. (2011) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2011.04.042 · Cited by 111
Effect of ground granulate blast-furnace slag on corrosion performance of steel embedded in concrete
Topçu, İ. B., & Boğa, A. R. (2010) · Materials & Design (1980-2015) · doi:10.1016/j.matdes.2010.01.057 · Cited by 106
Bouteiller, V., Crémona, C., Baroghel-Bouny, V., & Maloula, A. (2012) · Cement and Concrete Research · doi:10.1016/j.cemconres.2012.07.004 · Cited by 105
Jeong, Y., Park, H., Jun, Y., Jeong, J.-H., & Oh, J. E. (2015) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2015.07.158 · Cited by 104
Mo, K. H., Alengaram, U. J., Jumaat, M. Z., & Yap, S. P. (2014) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2014.12.021 · Cited by 104
Carbonation and pH in Mortars Manufactured with Supplementary Cementitious Materials
McPolin, D. O., Basheer, M., & Long, A. E. (2009) · Journal of Materials in Civil Engineering · doi:10.1061/(asce)0899-1561(2009)21:5(217 · Cited by 94
Escalante-Garcia, J. I., Espinoza-Pérez, L. J., Gorokhovsky, A. V., & Gómez-Zamorano, L. Y. (2009) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2009.02.002 · Cited by 92
McPolin, D. O., Basheer, M., Long, A. E., Grattan, K. T. V., & Sun, T. S. (2007) · Journal of Materials in Civil Engineering · doi:10.1061/(asce)0899-1561(2007)19:11(936 · Cited by 91
Mechano-chemical modification of cement with high volumes of blast furnace slag
Соболев, К. (2005) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2005.03.010 · Cited by 91
Thermo-mechanical properties of concrete containing high-volume mineral admixtures
Demirboğa, R., Türkmen, İ., & Karakoç, M. B. (2005) · Building and Environment · doi:10.1016/j.buildenv.2005.08.027 · Cited by 87
Rashad, A. M., & Khalil, M. H. (2012) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2012.10.014 · Cited by 87
Self-citationThe mineralogy and microstructure of three composite cements with high replacement levels
Hill, J., & Sharp, J. H. (2002) · Cement and Concrete Composites · doi:10.1016/s0958-9465(01)00041-5 · Cited by 83
Thermal conductivity of ternary mixtures for concrete pavements
Shin, A. H.-C., & Kodide, U. (2011) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2011.11.009 · Cited by 79
Some Engineering Properties of Slag Concrete as Influenced by Mix Proportioning and Curing
Swamy, R. N., & Bouikni, A. (1990) · ACI Materials Journal · doi:10.14359/2148 · Cited by 75
Introducing an effective curing method for mortar containing high volume cementitious materials
Aprianti, E., Shafigh, P., Zawawi, R., & Hassan, Z. F. A. (2016) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2015.12.100 · Cited by 63
McNally, C., & Sheils, E. (2011) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2011.11.029 · Cited by 62
Feasible use of large volumes of GGBS in 100% recycled glass architectural mortar
Ling, T., & Poon, C. S. (2014) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2014.05.012 · Cited by 62
Zhang, X., Zhou, X., Zhou, H., Gao, K. N., & Wang, Z. (2013) · Applied Clay Science · doi:10.1016/j.clay.2013.02.020 · Cited by 60
A preliminary study of autoclaved alkali-activated slag blended with quartz powder
Rashad, A. M., Zeedan, S. R., & Hassan, H. A. (2012) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2011.12.104 · Cited by 58
Self-citationAn investigation on very high volume slag pastes subjected to elevated temperatures
Rashad, A. M. (2014) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2014.10.019 · Cited by 56
Self-citationMechanical activation of cement–slag mortars
Sajedi, F. (2011) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2011.05.001 · Cited by 50
Al‐Amoudi, O. S. B., Rasheeduzzafar, A.-A., Maslehuddin, M., et al. (1994) · Cement Concrete and Aggregates · doi:10.1520/cca10555j · Cited by 49
Guo, X., & Shi, H. (2012) · Journal of Materials in Civil Engineering · doi:10.1061/(asce)mt.1943-5533.0000760 · Cited by 47
Jamshidi, A., Kurumisawa, K., Toyoharu, N. A. W. A., & Hamzah, M. O. (2014) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2014.11.046 · Cited by 46
Nazari, A., & Riahi, S. (2011) · Materials Research · doi:10.1590/s1516-14392011005000052 · Cited by 43
Mechanism of early age shrinkage of concretes
Aly, T., & Sanjayan, J. (2008) · Materials and Structures · doi:10.1617/s11527-008-9394-6 · Cited by 42
Shaikh, F. U. A. (2011) · Journal of Materials in Civil Engineering · doi:10.1061/(asce)mt.1943-5533.0000300 · Cited by 36
Bouzoubaa, N., & Fournier, B. (2005) · Canadian Journal of Civil Engineering · doi:10.1139/l04-109 · Cited by 33
Effect of Temperatures up to 90°C on the Early Hydration of Portland–Blastfurnace Slag Cements
Utton, C. A., Hayes, M., Hill, J., Milestone, N. B., & Sharp, J. H. (2008) · Journal of the American Ceramic Society · doi:10.1111/j.1551-2916.2007.02124.x · Cited by 28
Ahmed, M. S., Kayali, O., & Anderson, W. R. (2009) · Journal of Materials in Civil Engineering · doi:10.1061/(asce)0899-1561(2009)21:9(446 · Cited by 27
Carbonation and Permeability of Blastfurnace Slag Cement Concretes From Field Structures
Osborne, G. J. (1989) · CANMET/ACI International Conference on Fly Ash, Silica Fume, Slag, and Natural Pozzolans in Concrete · doi:10.14359/2599 · Cited by 20
Rashad, A. M., Nouhy, H. A. E., & Zeedan, S. R. (2017) · Arabian Journal for Science and Engineering · doi:10.1007/s13369-017-2985-1 · Cited by 11
Self-citation
Cited by
Behera, S. K., Mishra, D. P., Singh, P., Mishra, K., Mandal, S. K., Ghosh, C. N., Kumar, R., & Mandal, P. K. (2021) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2021.125120 · Cited by 307
A study of chloride binding capacity of concrete containing supplementary cementitious materials
Abd El-Fattah, H., Abd El-Zaher, Y., & Kohail, M. (2024) · Scientific Reports · doi:10.1038/s41598-024-62778-6 · Cited by 25
Metadata
- Authors
- Rashad, A. M.
- Venue
- Construction and Building Materials
- Publisher
- Elsevier BV
- Published
- 2018-10
- Volume
- 187
- Pages
- 89-117
- ISSN
- 0950-0618 (ISSN-L)
- OpenAlex
- W2887839477
- Cited by
- 174
- References
- 92
- FWCI
- 12.80
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.